| HS Code | 441501 |
| Productname | Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Grade | Heavy Duty Film Grade |
| Comonomer | Octene-1 |
| Density | 0.920 g/cm³ |
| Meltindex 190c 2 16kg | 0.75 g/10 min |
| Meltingpoint Dsc | 122 °C |
| Vicatsofteningpoint | 100 °C |
| Tensilestrengthatyield Md | 10 MPa |
| Tensilestrengthatyield Td | 10 MPa |
| Tensilestrengthatbreak Md | 36 MPa |
| Tensilestrengthatbreak Td | 32 MPa |
| Elongationatbreak Md | 700 % |
| Elongationatbreak Td | 800 % |
| Secantmodulus 1pct Md | 190 MPa |
| Secantmodulus 1pct Td | 220 MPa |
| Elmendorftear Md | 300 g |
| Elmendorftear Td | 500 g |
| Dartdropimpact | 200 g |
| Haze | 11 % |
| Gloss 45deg | 55 |
As an accredited Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Typically supplied in 25 kg polyethylene bags, 1,000 kg bulk bags, or bulk trucks/railcars for industrial handling. |
| Container Loading (20′ FCL) | Dry 20′ FCL; 25 kg bags on pallets, shrink-wrapped and secured; evenly distributed; typical payload 18–20 MT; clean, ambient conditions. |
| Shipping | Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade is non-hazardous and not DOT/IMDG/IATA regulated. It is supplied as polyethylene pellets in 25-kg PE bags, 40 bags (1,000 kg) per stretch-wrapped pallet; bulk trucks or railcars may be available. Store dry, avoid heat, and use standard industrial handling. No special placards required. |
| Storage | Store DOWLEX™ 2245D in original, unopened bags or closed containers in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep pallets off floor, avoid moisture and contamination, and use first-in, first-out stock rotation. Maintain normal warehouse temperatures and inspect packaging for damage before use. Store away from acids, bases, and incompatible materials. |
| Shelf Life | Shelf life: 24 months when stored in original packaging in a cool, dry, well-ventilated area away from direct sunlight. |
Published data for this specific blend configuration is limited; the following design targets are derived from blown-film trials on octene LLDPE grades with similar density and melt index.
| Blend ratio (DOWLEX™ 2245D / LDPE) | Dart impact F50 (ASTM D1709 Method A) | Elmendorf tear MD/TD (ASTM D1922) | Tensile at break MD/TD (ASTM D882) |
|---|---|---|---|
| 100/0 | 220–280 g | 70/90 N/mm | 38/32 MPa |
| 90/10 | 260–310 g | 75/95 N/mm | 36/31 MPa |
| 80/20 | 280–350 g | 80/100 N/mm | 34/30 MPa |
Because round bale wrapping subjects silage film to repeated stretch, puncture, and ultraviolet exposure, three-layer lines position DOWLEX™ 2245D in the outer white UV-resistant layer rather than in the tacky cling layer. At total film thickness of 25–45 µm, raising the frost line above 600 mm from the die face increases transverse-direction gauge scatter to ±10% and reduces dart impact F50 by 15–25% when tested per ASTM D1709 Method A; setting the frost line below 300 mm restores impact but can induce blocking on the collapsing frame when ambient air temperature exceeds 35 °C. A common three-layer mass distribution allocates 20–40 wt% of total film mass to DOWLEX™ 2245D in the white outer layer, 40–60 wt% to metallocene LLDPE in the puncture-resistant core, and 15–25 wt% to a cling layer containing 2–4 wt% polyisobutylene tackifier; the outer layer adds 8–12 wt% titanium dioxide masterbatch for solar reflectance. Published data for this exact resin distribution in round bale wrap is limited, so converters adjust the layer split based on line gauge-control capability and bale density. Qualification references EN 14932:2006 for thermoplastic silage films, ASTM D5748 for protrusion puncture resistance, ASTM D1922 for tear propagation, and ISO 527-3 for tensile strain at break; outdoor durability is evaluated through ASTM D4329 or ISO 4892-2 accelerated weathering. Processing on three-layer coextrusion lines with 70 mm outer-layer extruders, a 90 mm core extruder, and a 450 mm die uses die gap 1.2–1.8 mm, blow-up ratio 2.8–3.5:1, melt temperature 199–232 °C, and internal bubble cooling with chilled air at 10–15 °C; line speeds of 120–180 m/min are attainable only when the frost line is locked at 300–450 mm and air-ring blower settings prevent bubble flutter at the collapsing frame. Terminal products include 750 mm × 1500 m round bale wrap at 25 µm, 250–500 µm pit silage covers, and heavy-gauge tube-stretch film for low-oxygen forage preservation.
In pallet unitization, the elastic recovery of a 60–120 µm stretch hood after 100% elongation is the primary variable separating stable loads from shifted freight. DOWLEX™ 2245D is placed in the core layer of three-layer blown stretch hood structures to resist puncture from nail ends, steel strapping, and irregular brick packages. The outer layers are compounded with 1–2.5 wt% polyisobutylene or sorbitan monooleate-based cling agent and 1,000–3,000 ppm antistatic to reduce dust adhesion; the core layer remains cling-free to prevent blocking after post-extrusion annealing. Blend ratios typically fall at 70–85 wt% DOWLEX™ 2245D with 15–30 wt% metallocene LLDPE or LDPE in the core to raise transverse-direction Elmendorf tear to 45–90 N/mm per ASTM D1922; exceeding 30 wt% LDPE lowers elastic recovery below the 85% threshold and permits load loosening on irregular pallets. Mechanical qualification follows ASTM D882 for tensile at break, ASTM D5458 for cling force, ASTM D5459 for elastic recovery after 100% elongation, and ASTM D5748 for protrusion puncture; finished hoods must comply with heavy-metal limits under EU Packaging Directive 94/62/EC. Extrusion uses three-layer blown film with die gap 1.6–2.0 mm, blow-up ratio 3.0–3.5:1, and melt temperature 199–232 °C, followed by slitting to 1,000–2,200 mm layflat width. Stretch hood applicators pre-stretch the film 50–70% at 180–300 N tension, then impulse-weld the top seal at 110–130 °C. End products cover concrete block packs, insulation batts, beverage cans on automated palletizers, and chemical pails where load retention must withstand 0.3–0.5 g lateral acceleration during truck transport.
Where temporary construction containment must remain sealed during 12 months of outdoor exposure, 150–250 µm films based on DOWLEX™ 2245D are processed on monolayer blown-film lines with 250–400 mm dies, die gap 2.5 mm, blow-up ratio 2.0–2.5:1, and output rates of 250–400 kg/h. The grade’s low gel level permits continuous running without screen-pack pressure rise above 45 bar across 72 h campaigns. Outdoor-formulation ratios are 95–98 wt% DOWLEX™ 2245D, 2–3 wt% hindered amine light stabilizer masterbatch, and 1.5–2.5 wt% TiO₂; where flame resistance is specified, 8–15 wt% brominated flame-retardant masterbatch with antimony trioxide is added, and the separated film is tested separately because the base resin alone has no inherent fire-retardant classification and melt dripping remains a defined operational limitation. Compliance testing follows ASTM D4397 for polyethylene sheeting, ASTM E96/E96M water vapor transmission at 23 °C and 50% RH, and ASTM D2103 for dimensional and tensile properties; lead-paint containment enclosures in regulated renovation markets additionally require documentation under EPA 40 CFR Part 745 work-practice provisions. Terminal products include crawl-space vapor barriers, temporary demolition dust curtains, formwork liners, asbestos abatement enclosures, and lead-paint containment sheeting joined by heat-welded seams.
Frozen food laminate sealant webs produced with a 50–70 µm DOWLEX™ 2245D layer are qualified less by total thickness than by seal initiation temperature and low-temperature package burst resistance. The sealant layer is blended from 60–80 wt% DOWLEX™ 2245D, 15–30 wt% LDPE for low-temperature seal initiation, and 5–10 wt% white masterbatch, with slip/antiblock masterbatch at 500–1,000 ppm to prevent blocking on high-speed vertical form-fill-seal lines. Food-contact compliance is verified under FDA 21 CFR 177.1520(c), EU 10/2011 overall migration limit of 10 mg/dm², and China GB 4806.7 for food-contact polyethylene; seal strength is measured under ASTM F88/F88M, package burst under ASTM F2054, and coefficient of friction under ISO 8295. Blown film coextrusion uses die gap 1.4–1.8 mm, blow-up ratio 2.5–3.0:1, and melt temperature 199–232 °C; solventless lamination to PET or OPP applies adhesive at 1.5–2.5 g/m². Seal bars operate at 115–145 °C, dwell 0.5–1.0 s, and pressure 2–4 bar; reducing DOWLEX™ 2245D content below 60 wt% lowers hot-tack strength and is not recommended for packages requiring resistance to 0.7 bar pressure-differential burst. Terminal packages include IQF vegetable pouches, seafood pouches, ice-cream overwrap, frozen ready-meal lidding web, and frozen bakery bags.
| Market | Standard / Regulation | Test protocol | Threshold / Limit |
|---|---|---|---|
| United States | FDA 21 CFR 177.1520(c) | Extraction testing per food type | Olefin polymer specification |
| European Union | EU 10/2011 | Overall migration OM2 | 10 mg/dm² |
| China | GB 4806.7 | Food-contact polyethylene limits | Specific migration limits |
| Seal integrity | ASTM F88/F88M | Heat-seal strength | ≥ 2.5 N/15 mm frozen-state target |
| Burst resistance | ASTM F2054 | Package burst test | ≥ 20 kPa target |
High-speed fill-spout operations on 25 kg heavy-duty sacks generate crease flexing and product impact that expose weak spots at gusset folds. DOWLEX™ 2245D is converted into 150–250 µm gusseted tubing at blow-up ratio 2.5–3.0:1, die gap 2.0–2.5 mm, and melt temperature 199–232 °C; internal bubble cooling reduces blocking before the collapsing frame. Film blends commonly contain 70–85 wt% DOWLEX™ 2245D, 15–30 wt% recycled LLDPE, and 2–3 wt% carbon black masterbatch; the recycled fraction must be screened to 100 µm before re-extrusion to avoid gel-related pinholing. Qualification tests include dart impact F50 of 250–400 g on 200 µm film per ASTM D1709 Method A, Elmendorf tear of 50–90 N/mm MD per ASTM D1922, tensile at yield per ISO 527-3, and filled-sack drop testing per ASTM D5276; dangerous goods versions are tested under the applicable UN packaging group requirements, and food-contact surfaces for resin shipments are evaluated under FDA 21 CFR 177.1520(c). Terminal products include 25 kg fertilizer sacks, 25 kg polymer resin bags, mineral wool sacks, and agricultural seed bags with side gussets and heat-sealed bottom flaps.
Competitive Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade is an ethylene–octene-1 copolymer supplied in pellet form for blown-film extrusion of heavy-duty packaging and industrial sheeting. The manufacturer technical data sheet identifies a nominal density of 0.920 g/cm³ when measured under ASTM D1505 or ISO 1183-1 and a melt index of 0.50 g/10 min under ASTM D1238 or ISO 1133-1 at 190 °C and 2.16 kg. These indices place the resin in the low-melt-flow segment of linear low density polyethylene film grades, with sufficient molecular weight to generate high melt strength in blown-film processes.
The base resin is typically supplied without deliberately added slip or antiblock concentrate. Film processors add masterbatches to modify blocking force, coefficient of friction, and surface haze according to the converting line speed and winding tension. The solution polymerization route used for DOWLEX™ resins yields a narrow short-chain branching distribution compared with many gas-phase LLDPE products, and octene-1 incorporation suppresses high-density crystalline domains. These structural features are indirectly reflected in the tensile and dart impact values measured on blown film, but the supplier does not publish molecular weight distribution as a release parameter.
The melt flow ratio I21/I2 is more relevant for process control than a single melt index value. It provides a relative indication of shear thinning, which governs die pressure, bubble stability, and the response to high-shear extrusion conditions. In practice, the low melt index of 0.50 g/10 min differentiates this grade from general-purpose LLDPE film resins that commonly carry melt indexes from 0.8 g/10 min to 1.5 g/10 min; the lower flow rate increases melt pressure and reduces specific output at fixed screw speed but improves bubble stability in high-stalk configurations.
The dominant differentiators are the 0.50 g/10 min melt index and the 0.920 g/cm³ density. General-purpose LLDPE film grades with higher melt indexes reduce melt pressure and permit higher specific output on shallow-groove extruders, but their bubble stability in high-stalk lines is often lower. The lower melt index of 2245D increases pressure loss across the die and screen pack, often requiring a 60/80/100 mesh screen pack and a melt temperature of 210 °C to 240 °C to balance motor load and film surface quality.
The density is deliberately held in the lower portion of the 0.915 g/cm³ to 0.925 g/cm³ LLDPE film range to maintain secant modulus while preserving dart impact. Compared with a high-pressure low density polyethylene film resin at equivalent density, the linear polyethylene architecture produces higher tensile strength and better puncture propagation resistance but lower optical clarity and lower melt extensibility. These differences are measurable through ASTM D882, ASTM D1709, and ASTM D1922.
Table 1 lists the resin parameters most often used for incoming quality control. The values are typical data, not release limits; certificates of analysis state batch-specific values and the applicable test methods.
| Property | Typical value | Test method |
|---|---|---|
| Melt index, 190 °C / 2.16 kg | 0.50 g/10 min | ASTM D1238, ISO 1133-1 |
| Density | 0.920 g/cm³ | ASTM D1505, ISO 1183-1 |
| Base comonomer | octene-1 | Supplier technical data |
| Slip and antiblock as supplied | None | Supplier technical data |
| Food-contact base resin status | 21 CFR 177.1520(c) 3.2a | FDA |
When the resin is substituted for a butene-based LLDPE in a heavy-duty sack structure, the transition generally improves dart impact at the same thickness but may reduce line speed if the extruder drive is not sized for the higher torque. The direct comparison should be made using ASTM D1709 and ASTM D1922 values at the same gauge and production parameters. Published data for this specific configuration is limited, and converter trials must confirm the required film properties on the specific line before production release.
On high-stalk blown-film lines with 24:1 to 30:1 L/D single-screw extruders, the recommended die gap for heavy-duty film is 1.8 mm to 2.5 mm. The blow-up ratio is typically held at 2.0:1 to 3.0:1, while the frost line height is maintained at 4 to 8 die diameters to stabilize the stalk and reduce film blocking. A barrier screw with a Maddock mixing section provides sufficient dispersive mixing when regrind and masterbatch are introduced; extruder barrel temperatures from hopper to die are usually segmented between 180 °C and 220 °C, with the final die temperature verified by a needle thermocouple.
Pre-drying is normally unnecessary if pellet storage remains below 60 % relative humidity and sealed bags are opened at ambient conditions. When outdoor or humid warehouse storage causes moisture condensation on pellets, hopper drying at 60 °C to 70 °C for 2 h to 4 h with a desiccant unit at a dew point of -40 °C or lower prevents surface pitting and melt-pressure fluctuation. Process temperatures above 250 °C are not recommended because oxidative degradation in the film edge trim increases gel counts and may generate odor. Conversely, melt temperatures below 190 °C may promote melt fracture and reduce frost line stability on air-cooled bubbles.
On a 90 mm grooved-feed extruder with a 24:1 L/D screw, the resin typically demands higher torque than a 1.0 g/10 min LLDPE at the same screw speed. Backpressure of 35 MPa to 45 MPa can be observed before the screen changer; this is a practical reason to install a melt-pressure transducer and use pressure-limiting control. Screen packs with a final filter mesh of 100 mesh remove contaminants but increase melt temperature, so the setpoint profile may need to be reduced by 5 °C to 10 °C near the die compared to a 60 mesh final filtration.
Edge trim regrind from DOWLEX™ 2245D can be reintroduced up to 15 wt% to 30 wt% in heavy-duty film lines, but the exact fraction is constrained by the number of regrind heat histories and the antioxidant package. At regrind levels above 30 wt%, gel counts measured by optical defect inspection may exceed typical liner acceptance limits. Melt temperatures above 250 °C accelerate consumption of phenolic antioxidants and create carbonyl species detectable by Fourier-transform infrared spectroscopy; therefore the temperature profile is deliberately kept below that threshold.
In coextrusion, DOWLEX™ 2245D is placed in the outer or skin layer where puncture and tear resistance are required, while recycled polyethylene or lower-cost cores are used to control cost and stiffness. The melt index mismatch between the skin resin and a core resin with 1.0 g/10 min to 2.0 g/10 min melt index can create interfacial instability if the die temperature is below 210 °C. Processors typically raise the die temperature to 220 °C to 230 °C and use matched melt pipes for the skin and core streams to minimize viscosity-layer differences. Layer distribution control is verified by cross-sectional microscopy or by film delamination tests under ASTM D882 tensile conditions.
The product is not intended for cast film or extrusion coating as the primary conversion route. Blown film is the standard processing window; cast film lines may experience higher backpressure and lower specific output due to the low melt index, and the die-lip temperatures required for cast film may exceed the thermal oxidation threshold before the melt leaves the lip. This limitation is relevant when converters attempt to use the same resin as a drop-in replacement for higher-melt-index cast film grades.
Table 2 summarizes the primary processing differences between 2245D and adjacent polyethylene film resins used in heavy-duty applications.
| Resin class | Melt index | Density | Primary conversion route | Technical implication |
|---|---|---|---|---|
| DOWLEX™ 2245D | 0.50 g/10 min | 0.920 g/cm³ | High-stalk blown film | Higher melt strength; lower output at fixed screw speed |
| General-purpose LLDPE film resin | 1.0 g/10 min | 0.920 g/cm³ | Blown and cast film | Higher output; lower dart impact at equal gauge under ASTM D1709 |
| High-pressure LDPE film resin | 2.0 g/10 min | 0.923 g/cm³ | Blown film and extrusion coating | Higher optical clarity; lower tensile strength at break under ASTM D882 |
Heavy-duty sack, industrial liner, and agricultural film converters typically process the resin in thicknesses from 75 µm to 250 µm. After conditioning for at least 40 h at 23 ± 2 °C and 50 ± 5 % relative humidity according to ASTM D618, film tensile properties are evaluated under ASTM D882, Elmendorf tear under ASTM D1922, and dart impact under ASTM D1709 method A. For applications requiring puncture propagation resistance, ASTM D2582 is used. The low melt index and the linear backbone of the LLDPE structure increase draw-down tension in the machine direction; converters must therefore measure machine-direction and transverse-direction Elmendorf tear balance on production film rather than extrapolate from pellet data.
The resin is used with carbon black or UV stabilizer concentrates when long-term outdoor exposure is required. For agricultural films, the required stabilizer concentration is determined by the total effective concentration of hindered amine light stabilizer and the geographic exposure zone, with typical carbon black loading at 2.0 wt% to 2.5 wt% for multi-season applications. Pellets should be stored below 40 °C, away from direct sunlight and oxidizing environments. The base resin is not stabilized against prolonged outdoor UV exposure without additional concentrate.
For food-contact applications, the base resin is generally classified under 21 CFR 177.1520(c) 3.2a for olefin polymers when used in finished articles that meet the extraction limits of that section. In the European Union, the converter must confirm migration limits under Regulation (EU) No 10/2011 and its amendments; the polymer itself is not the only compliance variable because slip, antiblock, processing aid, and pigment masterbatches contribute to specific migration. The supplier product stewardship documentation should be consulted before assigning the material to food, medical, or pharmaceutical packaging.
Published data for this specific configuration is limited, and converter trials must confirm the required film properties on the specific line before production release.