Dow Dowlex 2244a Linear Low Density Polyethylene Cast Film Grade

Dow DOWLEX™ 2244A Linear Low Density Polyethylene, Cast Film Grade

    • Product Name: Dow DOWLEX™ 2244A Linear Low Density Polyethylene, Cast Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 634826
    Density 0.920 g/cm³
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Melt Flow Ratio I10 I2 8.0
    Vicat Softening Point 100 °C
    Dsc Melting Point 122 °C
    Dsc Crystallization Temperature 104 °C
    Tensile Strength At Yield Md 10 MPa
    Tensile Strength At Break Md 35 MPa
    Tensile Strength At Break Td 30 MPa
    Elongation At Break Md 500%
    Elongation At Break Td 700%
    1 Secant Modulus Md 190 MPa
    1 Secant Modulus Td 200 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Resistance Md 200 g
    Elmendorf Tear Resistance Td 400 g
    Haze 3%
    Gloss At 45 80
    Coefficient Of Friction 0.2

    As an accredited Dow DOWLEX™ 2244A Linear Low Density Polyethylene, Cast Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene-lined bags, also available in 1,000 kg bulk bags.
    Container Loading (20′ FCL) Container Loading (20′ FCL): DOWLEX™ 2244A LLDPE cast film grade, 25 kg bags, 20 pallets, 20,000 kg net, shrink-wrapped, secured.
    Shipping Dow DOWLEX™ 2244A Linear Low Density Polyethylene, Cast Film Grade, is not regulated for transport. It is supplied in 25 kg polyethylene bags, palletized, or in bulk trucks/railcars. Store in a cool, dry, ventilated area, away from heat, moisture, and direct sunlight. Keep containers closed.
    Storage Store DOWLEX 2244A in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers closed, palletized, and off the floor. Avoid excessive stacking, moisture, and contamination. Protect from UV and physical damage. Maintain FIFO inventory. Follow SDS and local regulations. Use appropriate PPE when handling. Do not store near food, feed, or incompatible materials.
    Shelf Life Shelf life is typically 24 months from manufacture when stored in original sealed packaging, dry, away from direct sunlight and heat.
    Application of Dow DOWLEX™ 2244A Linear Low Density Polyethylene, Cast Film Grade

    DOWLEX 2244A is a linear low density polyethylene produced with octene comonomer and configured for cast film conversion. Its published density is 0.917 g/cm³ when determined by ASTM D792, and its published melt index is 4.0 g/10 min when determined by ASTM D1238 at 190°C and 2.16 kg. Cast film lines quench the web on polished chill rolls rather than air-cooled blown film towers; the rapid quench behavior and melt characteristics of DOWLEX 2244A therefore differ from those of blow-film resins in the same density range. The application scenarios below are limited to established cast film conversion sectors: pallet unitization, fresh produce overwrap, lamination sealant webs, surface protection backings, silage stretch wrap, and heavy-duty liners. Each scenario specifies the relevant compliance framework, addition ratio range in the cast layer or total formulation, downstream conversion process, and terminal article types.

    Why Does Pallet Stretch Film Retain Machine Speed Without Sacrificing Cling?

    Pallet-unitization cast film is converted on three-layer coextrusion lines with die widths commonly between 2,200 mm and 2,800 mm. In the core layer, DOWLEX 2244A is added at 30 wt% to 55 wt%; the remaining core fraction is a metallocene-catalyzed ethylene-hexene LLDPE or a fractional-melt LDPE selected to raise extensional viscosity. Outer layers carry polyolefin plastomers or cling additives, because DOWLEX 2244A in an uncored monolayer does not provide sufficient tack for direct pallet transfer. Chill roll temperatures between 20°C and 30°C are maintained to stabilize film gauge before the edge trim and winding section. On production-scale lines with 90 mm/120 mm/90 mm screw diameters and 30:1 L/D coextruders, output rates up to 600 kg/h are typical; surface melt fracture is controlled by increasing die lip gap to 0.7–1.0 mm when core-layer viscosity diverges from the outer layers. Mechanical evaluation follows ASTM D5458 for peel cling, ASTM D5748 for protrusion puncture resistance, and ASTM D882 for tensile properties in the machine and transverse directions. The terminal product forms include 50 mm-core hand wrap, 76 mm-core machine wrap, and pre-stretched carriage film spooled for automated wrapping stations.

    Winding tension above 400 N/m on the primary winder has generated edge gauge bands and telescoping roll defects in cast stretch lines running below 15 µm; the defect frequency increases when the DOWLEX 2244A content exceeds 55 wt% in the core. At pre-stretch ratios above 250%, edge tear initiation is influenced by trim blade sharpness and by the orientation state of the cast web. Films containing DOWLEX 2244A are not recommended for high-cling monolayer structures above 70 wt% because cling force drops below the levels required on rough-textured pallet surfaces. REACH registration and national packaging regulations apply to the formulated film, but mechanical performance is not defined by a single mandatory standard. The operational boundary is set by the viscosity divergence between the DOWLEX 2244A-containing core and the high-cling skin layers; reclaim streams containing maleic anhydride-modified tie resins should be checked before reintroduction into the core layer.

    At 12–25 µm, fresh produce overwrap films are cast and converted into perforated or macro-perforated webs after winding. In monolayer structures, DOWLEX 2244A is added at 60–90 wt%, with the balance comprising a low-melt-index LDPE for melt stability and a silica antiblock masterbatch at 500–1,500 ppm active content. The polyethylene substrate used in raw fruit and vegetable contact is governed by FDA 21 CFR 177.1520(c) and by EU Regulation 10/2011, where overall migration must not exceed 10 mg/dm² under the food simulant assigned by the intended use. Cast lines producing produce wrap run polished chill rolls at 18–24°C; at these temperatures the web retains sufficient clarity and blocks only when roll tension exceeds the winder compression threshold. Terminal articles include perforated overwrap for lettuce, celery sleeves, mushroom punnet overwrap, and film for ambient bakery display. The material is not recommended for continuous package temperature above 80°C or for hot-fill produce applications because distortion may occur.

    At film thickness below 12 µm, gauge variation on cast lines with vacuum boxes may exceed ±8%, causing inconsistent perforation geometry and premature tear. Condensation on chilled rolls at relative humidity above 60% can produce surface moisture streaks unless the air conditioning and edge-trim extraction are balanced; the resin does not require pre-drying under ambient conditions below that threshold. Reclaim quality is critical for clarity: incorporation of contaminated edge trim above 20 wt% may elevate haze and reduce transverse elongation at break below 300% as measured by ASTM D882, which is a boundary condition for automatic overwrap of wet produce.

    Hot-Tack and Seal Through Contamination Are Controlled by Layer Composition

    In lamination sealant webs, DOWLEX 2244A is introduced at 20–50 wt% into the sealant layer of multi-layer structures where low seal-initiation temperatures are required for high-speed vertical form-fill-seal lines. The remainder of the sealant layer is typically a low-density polyethylene or a metallocene plastomer selected to reduce the seal initiation temperature below 105°C. When the cast web is used as a monolayer sealant film for dry food pouches, addition ratios of DOWLEX 2244A between 80 wt% and 100 wt% are common, with slip and antiblock concentrates making up the balance. The cast web is corona treated to surface energies of 38–42 mN/m before adhesive lamination to oriented polyester, biaxially oriented polypropylene, or foil. For polyethylene-containing food contact structures, compliance is assessed under FDA 21 CFR 177.1520(c) and EU Regulation 10/2011, with overall migration limits specified by the final laminate composition. Seal strength is measured by ASTM F88, and hot-tack behavior is measured by ASTM F1921 on samples cut from production reels. Terminal articles include gusseted dry food pouches, frozen food lamination, and non-food industrial pouch structures where seal-through-packaging contamination is a known production constraint.

    On rotary jaw sealers with 0.5–0.8 s dwell times, hot-tack failure occurs when sealant viscosity remains too high to wet the opposing film surface under jaw pressure. In structures containing DOWLEX 2244A above 50 wt%, seal temperatures should be maintained between 115°C and 135°C; below 110°C, hot tack decreases sharply, and above 140°C, edge thinning and web distortion become progressive. Contamination by polypropylene or wax arising from post-industrial reclaim reduces seal strength; a limit of 5 wt% polypropylene contamination in the sealant layer is generally imposed to maintain consistent ASTM F88 values. The cast film is not intended for retort or boil-in-bag packaging because the polyethylene sealant layer lacks the thermal resistance of cast polypropylene or high-temperature laminating grades.

    For temporary protection of stainless steel sheet and anodized aluminum profiles, cast backing webs are produced at thicknesses between 30 µm and 80 µm. DOWLEX 2244A is used at 60–100 wt% in the backing layer; where a coextruded tie layer is required for aqueous acrylic or rubber adhesive anchorage, a maleic anhydride-modified polyethylene or ethylene-vinyl acetate layer may constitute 10–25% of the total film thickness. Backside corona treatment is applied at 2.0–3.5 kW across a 1,500 mm web width to raise surface energy above 40 mN/m before coating. Peel adhesion is measured with ASTM D3330 using a 180° peel angle after 24 h dwell on the intended metal or glass substrate. The converted rolls serve as protective films for embossed stainless steel, brushed aluminum architectural panels, powder-coated building profiles, and flat glass sheet during transport and installation. Because this is a non-food industrial segment, the applicable chemical regulation is REACH; no food-contact compliance statement is required or implied for the polyethylene backing.

    When cast on commercial lines, unwind tension oscillations above 150 N/m have caused edge chatter during inline adhesive coating; the defect is reduced by maintaining closed-loop tension control on the secondary unwind and by controlling cast roll temperature between 20°C and 28°C. Outdoor exposure of the protected article beyond 6 months is an operational boundary: prolonged UV exposure may increase removal torque and leave adhesive residue on sensitive powder-coated or anodized surfaces. DOWLEX 2244A backings without UV stabilization are not recommended for exterior exposure periods beyond this threshold. Reclaim of edge trim from adhesive-coated webs should be avoided unless the adhesive is fully removed before re-extrusion; nitrogen purge and vacuum venting on the extruder are insufficient to eliminate adhesive-derived volatiles at high reclaim levels.

    When Silage Wrap Moves from Blown to Cast Film Structures

    Agricultural silage stretch film can be produced on cast lines when the converter accepts the orientation and puncture-resistance trade-offs of cast film. In a typical cast silage structure, DOWLEX 2244A is added at 20–40 wt%, with the balance comprising a lower-density LLDPE or LDPE and a UV stabilizer masterbatch at 1.0–3.0 wt% active concentration. The film is pigmented in white, black, or green depending on the baler wrap requirement. The cast web passes through a pre-stretch unit before winding; production lines commonly use a vacuum trimming system and edge trim refeed at controlled rates to maintain gauge stability. Applicable mechanical evaluations include ISO 527-3 for tensile properties and ASTM D1709 for dart impact. Agricultural silage film falls under EN 13207 for silage thermoplastic films; the standard addresses mechanical durability and oxygen permeability characteristics required for anaerobic fermentation. Terminal products include round bale wrap, square bale wrap, and pit silo cover film. The grade is not intended for multi-season storage beyond 12 months without additional UV stabilization or coextruded barrier design.

    Dart impact measured by ASTM D1709 on cast silage film is typically lower than that of blown film of equivalent thickness; field failures on stone-contaminated bales are therefore more common at 20 µm gauge. Converters compensate by raising film thickness to 25–35 µm or by increasing the DOWLEX 2244A fraction with a tougher metallocene LLDPE in the core. The melt index of DOWLEX 2244A supports melt stability on cast film lines but restricts maximum line speed when the die gap is below 0.6 mm; die lip build-up increases when the formulation contains high levels of low-molecular-weight cling additives. Pre-drying is not required, but moisture condensation on chilled rolls must be controlled when the cast line operates in unconditioned warehouses at relative humidity above 70%.

    Compliance and test method matrix for cast DOWLEX 2244A application sectors
    SectorChemical / food-contact complianceMechanical test standardPerformance boundary
    Pallet stretch filmREACH, national packaging regulationsASTM D5458, ASTM D5748, ASTM D882Core-layer addition above 55 wt% increases telescoping risk
    Fresh produce overwrapFDA 21 CFR 177.1520(c), EU 10/2011ASTM D882Continuous package temperature below 80°C
    Lamination sealant webFDA 21 CFR 177.1520(c), EU 10/2011ASTM F88, ASTM F1921Seal temperature 115–135°C for DOWLEX 2244A above 50 wt%
    Surface protection backingREACHASTM D3330, ASTM D882Outdoor exposure below 6 months without UV stabilization
    Silage stretch wrapEN 13207ISO 527-3, ASTM D1709Cast film below 20 µm shows field puncture risk on stone-contaminated bales
    Heavy-duty liners49 CFR Part 178 package certification; ISO 175 chemical resistanceASTM D1709, ASTM D1922Maximum continuous service temperature 60–70°C

    Heavy-Duty Cast Liners for Chemically Resistant Bulk Packaging

    Heavy-duty cast liners for bulk chemical packaging are converted from monolayer or two-layer webs, with DOWLEX 2244A added at 80–100 wt% in the film core and an optional LDPE-rich outer layer to control heat seal response on bag-making equipment. The cast film is drawn to a thickness of 80–150 µm before inline slitting and gusseting. Downstream conversion includes tubular welding or side-seal bag forming, gusseted drum liners, and VFFS heavy-duty bags. Impact resistance is evaluated according to ASTM D1709, and tear resistance according to ASTM D1922; these values support replacement of thicker LDPE liners with thinner LLDPE structures in non-regulated bulk packaging. Where the liner is used inside UN-certified combination packaging, certification applies to the complete package under 49 CFR Part 178, not to the liner alone. The chemical resistance of polyethylene is validated through ISO 175 or ASTM D543 immersion testing for the specific chemical class; DOWLEX 2244A is not recommended for strong oxidizing acids, low-molecular-weight aromatic solvents, or chlorinated hydrocarbons in long-term service. Terminal product types include drum liners, box liners, gaylord liners, and FIBC liners. The maximum continuous service temperature for these liners is 60°C to 70°C; above that range, deformation and weld failure are likely.

    On production-scale cast lines, the draw resonance threshold limits the melt draw ratio when the monolayer fraction of DOWLEX 2244A exceeds 90 wt%. Increasing the chill roll temperature to 25–30°C and maintaining die gap above 0.8 mm reduces draw resonance at line speeds between 80 m/min and 150 m/min. Reclaim generated from gusseted liner conversion containing polyethylene dust and slitting trim can be re-fed at 20–40 wt% without loss of dart impact if the reclaim stream is free of paper labels and adhesive tapes. The material is not suitable for direct food contact unless the specific liner structure is separately tested under FDA 21 CFR 177.1520(c) and EU 10/2011; the standard industrial liner configuration is not automatically food-contact compliant.

    Free Quote

    Competitive Dow DOWLEX™ 2244A Linear Low Density Polyethylene, Cast Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DOWLEX™ 2244A Linear Low Density Polyethylene, Cast Film Grade, is an ethylene-1-octene copolymer supplied in pellet form for flat die cast film extrusion. The producer’s published typical density is 0.917 g/cm³ measured by ASTM D792, and the melt mass-flow rate is 4.0 g/10 min at 190 °C/2.16 kg per ASTM D1238. For regional documentation, the same property may be reported under ISO 1133-1:2022 using an equivalent condition. The 1-octene comonomer introduces C6 short-chain branches; this branch length differentiates the resin from ethylene-butene LLDPE grades and from high-pressure low density polyethylene. The product is intended for cast films in the 20–100 µm thickness range, but the final property envelope depends on die gap, draw ratio, and chill roll temperature.

    Published typical resin property and test methods
    PropertyMethodPublished typical value
    DensityASTM D7920.917 g/cm³
    Melt mass-flow rateASTM D12384.0 g/10 min

    Converters select the product for industrial overwrap, lamination substrates, hygiene films, and agricultural films where high output and balanced toughness are required. Qualification should evaluate dart drop by ASTM D1709, Elmendorf tear by ASTM D1922, haze by ASTM D1003, gloss by ASTM D2457, and coefficient of friction by ISO 8295. These methods are not interchangeable with blown-film tests at the same gauge because cast film orientation is primarily in the machine direction and produces different tear anisotropy. Published data for every film thickness and line configuration is limited; converter-generated film data remains the basis for product acceptance.

    What Distinguishes an Octene-Based Cast Film LLDPE from Butene or Hexene Grades?

    Relative to ethylene-butene linear low density polyethylene of equivalent nominal density, DOWLEX™ 2244A is expected to show a different short-chain branching distribution. The C6 branch derived from 1-octene is more effective than a C2 branch derived from 1-butene at disrupting crystal regularity and increasing tie-chain probability. This does not produce a uniform improvement in all film properties. The most reliable comparison is made on the same cast line at equal film gauge, orientation, and chill roll temperature using ASTM D1709 for dart impact and ASTM D1922 for tear resistance. Tear anisotropy in cast films can be pronounced; machine-direction tear and transverse-direction tear should be reported separately.

    Relative to high-pressure LDPE, the absence of long-chain branching reduces extensional melt strength. In cast film, this can increase neck-in and can lower the critical draw ratio for draw resonance. Some converters compensate by blending a small amount of LDPE or by adjusting the die-to-roll distance and air knife. However, LLDPE films of this density class generally provide higher dart impact and better puncture resistance than LDPE at equal thickness when tested under ASTM D1709 and ISO 7765-1. Relative to hexene-based LLDPE, the difference is smaller and often controlled by catalyst technology, molecular weight distribution, and stabilizer package rather than comonomer alone. Comparative data for this specific grade against all hexene grades is limited.

    Thermal analysis can provide a product-specific fingerprint. For an LLDPE of density 0.917 g/cm³, differential scanning calorimetry at 10 K/min per ASTM D3418 typically gives a peak melting temperature near 121 °C and a crystallization onset below 110 °C. The exact values vary with comonomer distribution and thermal history; the certificate of analysis should be consulted. Oxidative induction time measured by ASTM D3895 at 200 °C is a relative indicator of stabilizer content, but it does not replace long-term aging studies.

    Extruder, Die, and Chill Roll Configuration for 4.0 g/10 min LLDPE

    A single-screw extruder with L/D of 24:1 to 30:1 and a barrier screw is normally adequate for this melt index. Plant experience on cast film lines with 90 mm extruders indicates that the 4.0 g/10 min melt mass-flow rate permits high throughput without a grooved feed section; screw speed must be matched to chill roll speed to avoid melt curtain flapping. Melt temperature is maintained at 260–290 °C, with die zones at 260–280 °C. Sustained operation above 300 °C is not recommended because thermo-oxidative degradation accelerates rapidly. Residence time above 300 °C should be kept below 2 min. Degradation can be detected as a loss of melt flow stability, an increase in gel count, or a reduction in film dart impact measured by ASTM D1709. Melt temperature variation should be held within ±3 °C to avoid thickness variation and optical bands.

    Melt pressure is not a product-specific constant; it depends on die width, lip gap, throughput, and temperature. A capillary rheometer operated under ISO 11443 provides the shear viscosity data needed for die and feedblock pressure-drop calculations. The single-point melt index of 4.0 g/10 min should not be used alone to predict die pressure because it does not capture the shear-thinning slope at cast film shear rates.

    Chill roll temperatures in the range 15–30 °C are common for this density class. Lower chill roll temperatures increase quench rate and may reduce haze measured by ASTM D1003, but can increase film curl, static charge, and blocking. Higher temperatures can promote web adhesion to the roll if slip additives are not optimized. Blocking load should be measured by ASTM D3354; dynamic coefficient of friction should be measured by ISO 8295 after the required aging time, because migrating slip agents are time-dependent.

    Die lip gap is commonly set at 0.5–1.0 mm for thin films, but the optimum depends on target thickness and draw ratio. Neck-in and edge bead are sensitive to draw ratio, melt temperature, and die-to-roll distance. An air knife can stabilize the melt curtain and reduce edge bead. Published quantitative neck-in data for DOWLEX™ 2244A is limited; line trials should map final film width and edge bead height as a function of die gap and output. Draw resonance may appear when the draw ratio exceeds the stable envelope; the critical draw ratio for this resin should be determined on the production line because it is influenced by die-to-roll distance and air knife pressure.

    For food-contact applications, DOWLEX™ 2244A is manufactured to satisfy the compositional requirements of 21 CFR 177.1520 for olefin polymers. In the European Union, the finished article must comply with Regulation (EU) No 10/2011 on plastic materials and articles intended to come into contact with food; overall migration testing in food simulants is required at the article level. Under REACH Regulation (EC) No 1907/2006, the supplier’s registration dossier addresses the polymer substance; users must verify article-level obligations for substances of very high concern. The safety data sheet is the controlling document for occupational handling and emergency response.

    Regulatory references and application boundaries
    RequirementReferenceBoundary
    U.S. food-contact polymer compliance21 CFR 177.1520Resin as supplied; finished article testing may still be required.
    EU plastic food-contact materialsRegulation (EU) No 10/2011Finished article migration testing required.
    REACHRegulation (EC) No 1907/2006Registration and article-level communication obligations.

    The resin does not require predrying under normal sealed-container storage. If high-humidity storage has occurred, feed throat temperature in the range 40–60 °C can reduce surface moisture and improve feed stability. DOWLEX™ 2244A is nonpolar and is not an adhesion resin; polyester, polyamide, and EVOH layers will not bond directly with acceptable peel strength. Corona treatment of the film surface can modify surface wetting tension for printing and lamination, but it does not replace a tie layer at a barrier interface. Surface wetting tension after treatment is commonly measured by ASTM D2578; target values for printing are generally in the 38–42 mN/m range.

    When Coextrusion with EVOH or Polyamide Is Required

    Multilayer cast structures can combine DOWLEX™ 2244A skins with an EVOH or polyamide barrier layer. The LLDPE skin is nonpolar, so a maleic anhydride-grafted polyolefin tie layer must be placed at the barrier interface. Peel strength is measured by ASTM D1876; heat seal strength is measured by ASTM F88 when the interface includes a sealant. EVOH should be processed below 250 °C to limit acetic acid formation, while the LLDPE skin can be processed at 260–290 °C. This temperature difference requires a feedblock and die that can maintain thermal separation between layers. Viscosity mismatch at the interface must be minimized; capillary rheometry per ISO 11443 should be used to compare layer viscosities at the same apparent shear rate.

    In coextruded films, interfacial instability can appear as waviness or delamination if the viscosity ratio is outside the stable range. The exact stable viscosity ratio depends on layer thickness ratio and die geometry. Published data for the specific DOWLEX™ 2244A/EVOH/tie-layer combination is limited; qualification must be performed on the target converting line. For liquid packaging, adhesion after contact with the intended food simulant should be evaluated under Regulation (EU) No 10/2011 or the relevant national standard.

    Film structures intended for outdoor service require ultraviolet stabilizers unless the converter adds them via masterbatch. DOWLEX™ 2244A is not inherently weather resistant. Long-term outdoor performance cannot be inferred from short-term mechanical testing; it requires accelerated weathering according to ASTM G154 or ISO 4892-2 and correlation with end-use exposure data.

    Top