Dow Dowlex 2083g Linear Low Density Polyethylene

Dow DOWLEX™ 2083G Linear Low Density Polyethylene

    • Product Name: Dow DOWLEX™ 2083G Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 667065
    Density 0.920 g/cm³
    Melt Index 190 C 2 16 Kg 0.95 g/10 min
    Melting Point 124 °C
    Vicat Softening Point 98 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 26 MPa
    Elongation At Break 750%
    Flexural Modulus 240 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 270 g
    Elmendorf Tear Strength Td 420 g
    Haze 7%
    Gloss 45 75
    Coefficient Of Friction 0.12
    Low Temperature Brittleness < -70 °C
    Environmental Stress Crack Resistance > 1000 h

    As an accredited Dow DOWLEX™ 2083G Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DOWLEX™ 2083G Linear Low Density Polyethylene is typically supplied in 25 kg polyethylene-lined bags, palletized for industrial shipment.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Dow DOWLEX™ 2083G Linear Low Density Polyethylene, 25 kg bags, palletized, approximately 18–20 MT net.
    Shipping DOWLEX™ 2083G Linear Low Density Polyethylene ships as non-hazardous, non-regulated solid resin pellets. Typical packaging: 25 kg bags, 1000 kg bulk bags, or bulk trucks/railcars. Store and transport in dry, cool conditions away from direct sunlight. Handle using normal industrial hygiene practices; no special DOT/IMDG placards required.
    Storage Store Dow DOWLEX™ 2083G Linear Low Density Polyethylene in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or containers closed, clean, clearly labeled, and off the floor. Protect pellets from moisture, dust, and contamination. Avoid prolonged high temperatures and UV exposure. Maintain FIFO stock rotation and follow the SDS and local regulations.
    Shelf Life Dow DOWLEX™ 2083G has an indefinite shelf life when stored cool, dry, and away from moisture, heat, and direct sunlight.
    Application of Dow DOWLEX™ 2083G Linear Low Density Polyethylene
    Blown film conversion of DOWLEX™ 2083G for industrial heavy-duty sack liners is routinely configured on a 65 mm single-screw extruder with a 30:1 L/D barrier screw and a 300 mm low-pressure die. Barrel temperature is profiled from 180°C in the feed zone to 205°C at the adapter, with die zone setpoints held at 210°C. A die gap of 1.6–2.0 mm, blow-up ratio of 2.4:1–2.6:1, and frost line height of 260–340 mm produce a bubble geometry that stabilizes MD/TD tear balance under high-speed oscillation. Edge-trim regrind is metered at 15–25 wt% through a gravimetric blender; regrind moisture is maintained below 0.05 wt% to avoid melt channeling, surging, and bubble instability. Film produced at 70–110 μm is converted into valve sacks, form-fill-seal gusseted bags, and FIBC liner inserts.The mechanical acceptance window for 80 μm industrial sack film is monitored by an Elmendorf tear ratio MD/TD of at least 0.60 under ASTM D1922 and a dart drop of 4.5–6.0 g/μm under ASTM D1709 Method A. Elongation at break is measured under ISO 527-3 and is maintained above 600% in the machine direction; MD elongation below 500% generally indicates excessive regrind degradation or melt-pressure override in the metering section. Because sack fill speeds exceed 20 bags/min on bulk filling lines, the film surface requires a slip/antiblock system based on 0.8–1.2 wt% silica-loaded masterbatch and 0.4–0.8 wt% erucamide masterbatch. Seal strength is checked at 0.30 MPa jaw pressure and 0.45 s dwell with a target of ≥10 N/25 mm under ASTM F88.
    Process variableHeavy-duty sack film 70–110 μmFrozen food lamination 25–40 μmAgricultural cover 150–200 μm
    Die gap1.6–2.0 mm1.0–1.4 mm2.2–2.8 mm
    Die melt temperature205–215°C195–210°C210–225°C
    Blow-up ratio2.4:1–2.6:12.8:1–3.2:12.0:1–2.2:1
    Frost line height260–340 mm120–180 mm400–550 mm
    Output on 75 mm extruder120–170 kg/h90–130 kg/h180–240 kg/h

    Agricultural Silage Covers and Low-Temperature Tear Retention

    Film constructions destined for ensiled forage storage use a 150–200 μm monolayer fabricated on a 80 mm single-screw extruder with a 500 mm die and dual-lip air ring. The die gap is set to 2.2–2.8 mm, die melt temperature to 210–225°C, and blow-up ratio to 2.0:1–2.2:1. The reduced BUR shifts mechanical anisotropy toward machine-direction toughness, which is required for anchor-trench holding and repeated wind load. Frost line height is raised to 400–550 mm to increase crystalline orientation and improve room-temperature dart impact under ASTM D1709. A black/white or green/black structure is produced by adding 2.0–3.0 wt% carbon black masterbatch or a coextruded white reflective cap layer.Accelerated weathering screening follows ISO 4892-3 with irradiance set at 0.51 W/(m²·nm) at 340 nm, black-panel temperature 60°C, and exposure up to 1000 h. Retained elongation under ISO 527-3 is specified by the buyer because HALS dose, film gauge, and carbon black dispersion shift retention independently. Oxidation induction time is measured under ISO 11357-6 when HALS and sulfur-bearing acid scavengers are combined; the resulting time-to-oxidation is used as the batch-release gate. The terminal product is a 160 μm black/white silage cover in widths up to 12 m, with edge-fold heat sealing and eyelet reinforcement.For frozen-food vertical form-fill-seal operations running at 80–120 bags/min, the 25–40 μm sealant web is blown on a high-clarity line with chilled air at 5–10°C. A narrow die gap of 1.0–1.4 mm and elevated blow-up ratio of 2.8:1–3.2:1 are required to increase trans-direction tear and reduce directionality during bag opening. Melt temperature at the die is held at 195–210°C to limit thermal degradation and gel formation. Haze is controlled below 8% under ASTM D1003, while gloss at 60° geometry under ISO 2813 is maintained above 70 GU. Cold-crack resistance is screened on a 1 m flexed film sample at −20°C using ASTM D1790; visible transverse cracking at the flex point constitutes rejection.Seal strength is generated on a horizontal jaw sealer at 110–125°C jaw setpoint, 0.25 MPa pressure, and 0.40 s dwell, with a minimum seal strength of 8 N/25 mm under ASTM F88. The terminal product is a 30 μm reverse-printed frozen vegetable bag with a 350 g fill weight. Since the film enters direct food contact, the structure is evaluated under FDA 21 CFR 177.1520(c) as an olefin polymer and under EU Regulation 10/2011 with migration testing appropriate to aqueous and fatty frozen food simulants.

    What Limits Seal Integrity in High-Speed Liquid Pouch Laminates?

    In 250 mL liquid stand-up pouch laminates, DOWLEX™ 2083G is coextruded as a 12–20 μm sealant layer against a PET reverse-printed substrate through a two-component solventless adhesive. Seal initiation is measured according to ASTM F2029; the sealant layer typically enters a plateau at 110–125°C jaw setpoint, with seal strength exceeding 12 N/25 mm under ASTM F88. The limiting process conflict is pressure and dwell control on horizontal form-fill-seal machinery. Dwell below 0.35 s at 0.25 MPa produces channel leakers at the bottom gusset, while dwell above 0.60 s can induce edge thinning and web transfer failure. The stable processing corridor is 0.40–0.50 s dwell at 0.28–0.35 MPa jaw pressure and 120–130°C jaw temperature.Burst integrity of finished pouches is tested under ASTM F1140 with a pressurization rate of 10 kPa/s; failure threshold is set at ≥35 kPa for hot-filled liquid. Leak detection uses ASTM F2096 at 10 kPa internal pressure for 30 s. Because the sealant layer is in direct contact with liquid food, migration is evaluated under EU Regulation 10/2011 OM2 conditions for aqueous and oily foods and under FDA 21 CFR 177.1520(c). Published data for this exact PET/adhesive/LLDPE configuration is limited; the responsible converter validates total non-volatile migration against the current supplier certificate of analysis.
    FrameworkScopeTest or conditionDocumentation
    FDA 21 CFR 177.1520(c) 3.1aOlefin polymer food contactAqueous, acidic, alcoholic up to boilingSupplier CoA
    EU Regulation 10/2011Plastic articles intended for food contactOM2 migration, 10 days at 40°CEU DoC
    REACH 1907/2006 Annex XVIIRestriction of PAHs, phthalates in packagingEntry 50–52 verificationREACH SDS
    EN 15343Recycled plastic traceabilityBatch qualitative compositionRecycler certificate

    When Contaminated Recyclate Dilution Demands Rheological Adjustments

    When post-consumer recycled LDPE film contaminated with 0.5–2.0 wt% polypropylene and undispersed gel bodies is blended at 30–40 wt%, bubble stability on a high-output blown film line is recovered by introducing DOWLEX™ 2083G as a viscosity-normalizing resin. The grade’s nominal melt flow rate of 3.3 g/10 min under ISO 1133-1 at 190°C and 2.16 kg reduces upstream melt pressure compared with a 0.5–1.0 g/10 min fractional MI film resin, allowing extruder screw speed to be reduced by 10–15% at constant output. Melt filtration ahead of the die is upgraded to 100–150 μm screen packs; a three-stage continuous melt filter with 0.42 m² screen area is specified when gel bodies exceed 1 wt%. The die gap is increased from 1.6 mm to 2.0 mm, blow-up ratio is reduced from 2.5:1 to 2.2:1, and melt temperature is lowered by 5°C to limit free-radical crosslinking in degraded LDPE fractions.Film containing 30 wt% post-consumer recyclate is tested under ISO 527-3 for tensile elongation and ASTM D1922 for Elmendorf tear. A specification floor of 3.0 g/μm for dart drop under ASTM D1709 Method A is retained for refuse sack applications. Because recyclate composition is batch-dependent, incoming inspection uses ISO 15270 and EN 15343 traceability data; when the recyclate melt flow rate under ISO 1133-1 falls below 0.7 g/10 min, the blend ratio is adjusted or the extrusion temperature profile is stepped up by 5–8°C. Operators report transverse die flow marks when BUR drops below 2.0:1, indicating that the film cannot tolerate an over-reduction in transverse draw without visible gauge banding.Starting conversion trials for 45 μm collation bundling film require a blend of 50–70 wt% DOWLEX™ 2083G with LDPE. The blown film line is run at 190–210°C melt temperature, 1.2 mm die gap, and 3.0:1 blow-up ratio. Free shrink under ASTM D2732 at 120°C is moderate: 15–25% MD and 8–15% TD. Dart drop at 45 μm under ASTM D1709 Method A is targeted above 250 g. The terminal product is a 12-can collation shrink bundle with a shrink tunnel residence time of 4–6 s at 130–150°C.Construction-grade 150 μm films specified under EN 13984 as vapour control layers are blown on a 90 mm extruder with a 500 mm die and oscillating haul-off. Surface slip is controlled with 0.8–1.2 wt% slip/antiblock masterbatch; film width tolerance is held at ±2 mm on a 3 m web. Puncture resistance is determined under ASTM D5748; a threshold of 120 N/mm at 23°C is used for sub-slab applications. Water vapour transmission is tested according to ASTM F1249 at 38°C and 90% RH; typical values for 150 μm butene-LLDPE are 0.6–1.0 g/(m²·day). The terminal product is a flat-folded rollstock placed as a damp-proof course.
    Free Quote

    Competitive Dow DOWLEX™ 2083G Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2083G Linear Low Density Polyethylene is an ethylene/α-olefin copolymer produced by a solution polymerization route and supplied as pellets. The nominal melt mass-flow rate is 3.3 g/10 min when measured at 190 °C under 2.16 kg load in accordance with ISO 1133-1:2022; the nominal density is 0.919 g/cm³ when determined under ISO 1183-1:2019 or ASTM D792-20. The product contains a migratory slip additive and an antiblock additive, which differentiate it from additive-free polyolefins used in coextruded cling layers or extrusion coating. The resin is intended primarily for cast film extrusion, including monolayer and coextruded industrial stretch film, liners, overwrap, and protective sheeting. It is not intended for blown film equipment operating with a high blow-up ratio or for blow molding, rotational molding, or injection molding, where molecular architecture and melt strength requirements differ.

    Representative supplier-published property profile for DOWLEX™ 2083G; values are not specification limits and may vary by production lot and film line.
    PropertyTest methodRepresentative value
    Melt mass-flow rate at 190 °C/2.16 kgISO 1133-1:20223.3 g/10 min
    DensityISO 1183-1:20190.919 g/cm³
    Vicat softening temperatureISO 306/A12094 °C
    Melting temperatureISO 11357-3:2018121 °C
    Tensile stress at break, machine direction/transverse direction, 25 µm filmASTM D882-1838/30 MPa
    Elongation at break, machine direction/transverse direction, 25 µm filmASTM D882-18620/760%
    Dart impact, 25 µm filmISO 7765-1:2004130 g
    Haze, 25 µm filmISO 14782:20212.8%
    Gloss at 45°, 25 µm filmASTM D2457-1982
    Kinetic coefficient of friction after 24 h agingISO 8295:20040.12–0.18

    What Distinguishes DOWLEX™ 2083G from Low-Density Polyethylene and Metallocene LLDPE?

    The primary molecular difference is the absence of long-chain branching. High-pressure low-density polyethylene possesses long-chain branches that provide high melt strength and strain hardening, but reduce solid-state tensile and puncture performance at equivalent thickness. DOWLEX 2083G has a linear backbone with short-chain branches from the α-olefin comonomer. Under ASTM D1709-22 dart impact Method A, a 25 µm cast film of DOWLEX 2083G typically shows higher impact energy than a comparable low-density polyethylene film of the same gauge, while sacrificing some optical clarity and melt elongation. Compared with metallocene-catalyzed LLDPE, the broader molecular weight distribution of DOWLEX 2083G reduces melt-pressure variability in single-screw cast film lines and lowers the tendency for melt fracture, but may produce slightly higher haze and lower gloss. The distinction is measured by ASTM D1003-21 for haze and ASTM D2457-19 for gloss; metallocene-catalyzed grades often report haze below 2% at 25 µm, whereas DOWLEX 2083G typically falls between 2.5% and 4.0% depending on chill roll temperature and additive dispersion.

    Within the DOWLEX cast film family, the grade is positioned between lower-melt-flow and higher-melt-flow products by ISO 1133-1:2022 melt mass-flow rate. DOWLEX 2045G is typically used where higher melt strength reduces neck-in at wide die widths; DOWLEX 2049G is used where low melt pressure and high throughput are required. DOWLEX 2083G is selected when medium melt flow and sufficient drawdown are required; optical properties are moderate relative to metallocene grades. Published direct property comparisons for all film structures are limited, so converter trials are required.

    On a cast film line equipped with a 90 mm barrier screw, 30:1 L/D, and a die width of 1,800 mm, the resin is processable at throughputs of 150–250 kg/h when melt temperatures are held between 230 °C and 250 °C. The feed zone is typically set at 40–60 °C, the compression zone at 180–220 °C, and the metering zone at 220–240 °C. The die gap is normally set at 0.5–0.8 mm for film gauges of 15–25 µm; wider die gaps of 0.8–1.2 mm are used when reducing neck-in or when higher melt strength is required. Chill roll temperatures are controlled between 15 °C and 30 °C. Exceeding a melt temperature of 280 °C can cause gel formation and odor due to oxidative degradation; residence times above 10 min at high temperature should be avoided. If the screw is worn or the die lip is fouled, surface melt fracture may appear at high output; the broader molecular weight distribution of this grade usually permits higher shear rates before melt fracture than narrow-distribution metallocene grades.

    Cast Film Extrusion Parameters and Melt Stability Limits

    Precise control of the air gap and chill roll temperature is required because the optical and structural properties are quench-dependent. An air gap of 25–100 mm is typical. If the air gap is too short, surface haze may increase because the melt contacts the chill roll before surface relaxation. If the air gap is too long, the web may oscillate and draw resonance can occur. Draw resonance in cast film is associated with periodic thickness variation and occurs when the critical draw ratio is exceeded; for linear polymers with narrow molecular weight distributions, the critical draw ratio is lower than for branched low-density polyethylene. DOWLEX 2083G, because of its broader molecular weight distribution, generally tolerates a higher draw ratio than metallocene LLDPE before draw resonance occurs.

    On production-scale chill rolls, a temperature shift of 5 °C has been observed to change haze by 0.5–1.0 percentage point and to alter the level of post-crystallization in wound rolls. The target chill roll temperature should therefore be controlled within ±5 °C to maintain batch-to-batch optical consistency. At 25 µm thickness, film produced from DOWLEX 2083G typically shows machine-direction tensile stress at break of 38 MPa and transverse-direction tensile stress at break of 30 MPa under ASTM D882-18. Elongation at break exceeds 600% in both directions. Dart impact by ISO 7765-1:2004 Method A is typically in the range of 120–160 g. Elmendorf tear values are generally higher in the transverse direction than in the machine direction because of orientation effects in cast film. These values support industrial stretch film and heavy-gauge liners where puncture resistance and tear propagation resistance are required.

    In five-layer stretch film structures, the resin is often placed in the core or sub-skin layers. The outer cling layer is typically an ethylene-vinyl acetate copolymer or a metallocene-catalyzed plastomer. The melt temperature difference between adjacent layers should be held below 20 °C to avoid interfacial instability and curl. If a higher-melt-flow skin is combined with a lower-melt-flow core, flow acceleration at the feedblock can distort the layer thickness; flat die pressure should be monitored across the die width.

    After film is wound into mill rolls, the migratory slip additive in DOWLEX 2083G moves to the film surface over time. Immediately after casting, the kinetic coefficient of friction is often higher than after a maturation period of 24–48 h. Migration kinetics depend on temperature, thickness, and the presence of coextruded skins. At 40 °C, migration is accelerated relative to ambient storage; at 5 °C, migration is suppressed. This behavior means that coefficient of friction measurements should be conducted after controlled aging, not immediately on the winder. The appropriate test method is ASTM D1894-14 or ISO 8295:2004, with conditioned film samples and stainless steel sled surfaces. If rolls are slit and packed before migration is complete, blocking may occur in the core even though the antiblock additive is present because the slip system has not yet reached the film surface.

    When Regulatory Compliance Requires 21 CFR 177.1520 Documentation

    Under 21 CFR 177.1520, olefin polymers may be used in contact with food if they meet the specified extractive and density limitations, but the converter must confirm that the final film, including all coextruded layers, additives, and surface treatments, is compliant for the intended temperature and food type. For applications sold in the European Union, the relevant framework is Regulation (EU) No 10/2011 and its amendments; migration testing under EN 1186-1 or EN 13130-1 may be required depending on the food-contact surface and storage temperature. DOWLEX 2083G is not supplied as a medical-grade or pharmaceutical-grade resin; it is not intended for implantation or long-term tissue contact. The supplier should be consulted for REACH and RoHS declarations; polyethylene resins of this class generally do not contain heavy metals or phthalates.

    Pellets should be stored in a dry, indoor area at temperatures below 40 °C and away from direct sunlight to limit additive loss and atmospheric oxidation. If packages are opened and exposed to relative humidity above 60% for prolonged periods, surface moisture may require dehumidified-air drying at 60–70 °C for 2–4 h. The resin is incompatible with high levels of strong oxidizing agents and should not be exposed to prolonged melt temperatures above 280 °C. Published data for localized processing behavior on every possible cast film line is limited; therefore, trials on target equipment with lot-specific material are required to establish the optimum temperature profile, air gap, and winding tension.

    Top