Dow Dowlex 2078g Linear Low Density Polyethylene

Dow DOWLEX™ 2078G Linear Low Density Polyethylene

    • Product Name: Dow DOWLEX™ 2078G Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 335795
    Product Name Dow DOWLEX™ 2078G Linear Low Density Polyethylene
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Octene-1
    Density 0.920 g/cm3
    Melt Index 190 C 2 16 Kg 0.75 g/10 min
    Melting Temperature 124 °C
    Vicat Softening Temperature 98 °C
    Tensile Strength At Yield 9.7 MPa
    Tensile Strength At Break 22.0 MPa
    Elongation At Break 800%
    Flexural Modulus 240 MPa
    Shore D Hardness 49
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 400 g
    Elmendorf Tear Strength Td 500 g
    Brittleness Temperature < -70 °C

    As an accredited Dow DOWLEX™ 2078G Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene-lined bags, 55 bags per pallet, totaling 1,375 kg per pallet.
    Container Loading (20′ FCL) 20′ FCL loading for Dow DOWLEX™ 2078G Linear Low Density Polyethylene: palletized 25 kg bags, safely stowed for ocean transport.
    Shipping DOWLEX™ 2078G LLDPE is shipped as non-hazardous solid resin pellets in 25 kg bags, bulk bags, octabins, or bulk trucks/railcars. Store in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. No special transport classification required; follow local regulations and good industrial handling practices.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep bags or containers closed to prevent moisture and contamination. Use original packaging, avoid excessive stacking, and rotate stock. Maintain moderate temperatures. Follow the manufacturer’s SDS and local regulations. Handle pallets carefully to avoid puncturing containers. Do not store near food, feed, or drinking water.
    Shelf Life Typical shelf life is 24 months when stored dry, sealed in original packaging, away from heat and direct sunlight.
    Application of Dow DOWLEX™ 2078G Linear Low Density Polyethylene

    Cast Stretch Film Line Speeds Above 800 m/min Impose Melt Fracture Boundaries

    DOWLEX™ 2078G linear low density polyethylene is processed on five-layer cast stretch film lines as the core-layer resin at loadings of 65–80 wt%, with the balance typically split between metallocene-catalyzed LLDPE and a minor LDPE component of 5–10 wt% to maintain edge stability at the die exit. The resin’s nominal density of 0.920 g/cm³ is determined by ASTM D792 and its melt index of 1.0 g/10 min by ASTM D1238 at 190 °C/2.16 kg. On a five-layer cast line equipped with 30:1 L/D barrier screws of 65 mm and 90 mm diameter, a feedblock coextrusion unit, a 0.50–0.75 mm die gap, an air gap of 100–150 mm, and a chill roll held at 15–25 °C, the primary failure thresholds are edge-tear initiation at the peel point and draw resonance. Extruder temperature profiles follow a 180–240 °C barrel gradient, with adapter and die held at 245 °C and screw speed on the 90 mm core extruder set to 60–90 min⁻¹, yielding a specific energy input of 0.18–0.22 kWh/kg. Production-scale observations show that when line speed exceeds 800 m/min, melt fracture appears at the die exit if the die gap is below 0.45 mm and the melt temperature is below 240 °C; the defect is suppressed by raising the die gap by 0.05 mm or by increasing the final extruder barrel temperature by 5–8 °C. When the DOWLEX™ 2078G core fraction falls below 65 wt%, cling-layer tack becomes dependent on the skin-layer polyisobutylene concentration rather than core-layer deformation. Compliance verification for industrial pallet wrap is conducted under REACH Regulation (EC) No 1907/2006 Annex XVII; if direct food contact is required, FDA 21 CFR 177.1520(c) 3.2a and Commission Regulation (EU) No 10/2011 apply. Terminal products include machine-grade pallet wrap from 17 µm to 35 µm, pre-stretch hand film from 8 µm to 15 µm, and reinforced core wrap used for corner-board retention.

    Five-layer cast stretch film formulation gradient with DOWLEX™ 2078G
    Layer positionDOWLEX™ 2078G (wt%)mLLDPE (wt%)LDPE (wt%)Additive loading
    Outer release layer09010antiblock 3000–5000 ppm
    Core 110000not added
    Core 270300not added
    Core 3652510processing aid 200–400 ppm
    Cling layer603010polyisobutylene 10000–20000 ppm; processing aid 200–400 ppm

    For quick-frozen food packaging, blown film formulations combine 70–85 wt% DOWLEX™ 2078G with 15–30 wt% LDPE in monolayer high-stalk extrusion, while three-layer A/B/A structures typically place 85–100 wt% DOWLEX™ 2078G in the core and load slip and antiblock masterbatch into the skins. The applicable food-contact framework is FDA 21 CFR 177.1520(c) 3.2a and Commission Regulation (EU) No 10/2011, with overall migration tested according to EN 1186-1 and EN 1186-14 at 40 °C/10 days in 10% ethanol, 3% acetic acid, and isooctane as fatty food simulant. Downstream processing is performed on a three-layer blown film line with a 250–350 mm die diameter, 1.8–2.4 mm die gap, blow-up ratio 2.5:1–3.0:1, internal bubble cooling, and frost line height 600–900 mm above the die face. The screw configuration includes a Maddock mixing section and a screen pack of 120/100/80 mesh to capture agglomerated antiblock. Melt temperature is controlled at 185–210 °C because degraded slip/antiblock masterbatch forms deposits on the lower lip and increases film haze beyond the ASTM D1003 acceptance limit for optical-grade frozen food packaging. Terminal finished product types include pillow pouches for frozen vegetables, side-gusseted bags for seafood, and lidding sealant webs with thicknesses from 25 µm to 50 µm. Low-temperature dart drop is characterized by ASTM D1709 at −35 °C; when the LDPE fraction falls below 10 wt%, bubble oscillation occurs on conventional single-lip air rings unless the air volume is increased to at least 1.2 m³/s per meter of die circumference.

    What Limits Bubble Stability when DOWLEX™ 2078G Exceeds 85 wt% in High-Stalk Blown Film?

    When the DOWLEX™ 2078G fraction exceeds 85 wt% in high-stalk blown film, the process boundary is determined by the stalk’s resistance to diameter fluctuation under varying air pressure rather than by melt temperature alone. Production-scale trials on a 350 mm die with internal bubble cooling and a lower-nip height of 4.5–6.0 m show that stalk diameter variation of ±3–5 mm appears when frost line height exceeds 9 die diameters; the variation is reduced by increasing the die gap from 1.8 mm to 2.2 mm or by reducing melt temperature from 200 °C to 185 °C. The formulation addition ratio for heavy-duty industrial sacks and liners is 85–100 wt% DOWLEX™ 2078G with 0–15 wt% LDPE; when 100 wt% DOWLEX™ 2078G is run on a standard grooved-feed extruder, a fluoroelastomer processing aid at 300–500 ppm is required to control die-lip deposit. Qualification is based on ASTM D882 tensile properties, ASTM D1922 tear resistance, and ASTM D1709 dart impact at 23 °C; sacks intended for dangerous goods are evaluated under the UN Model Regulations Chapter 6.5, but published data for this specific configuration is limited. Terminal products include heavy-duty shipping sacks with thicknesses from 80 µm to 200 µm, bulk container liners, and dunnage air cushions. The operational boundary is that below 5 wt% LDPE, bubble instability and die-lip buildup become observable on equipment without adjustable air-ring decks; above 15 wt% LDPE, the secant modulus drops to a level that reduces stack-load stability in filled sacks.

    Extrusion Coating Sealant Webs and Neck-In Control

    In extrusion coating and liquid packaging lamination, DOWLEX™ 2078G is combined with 15–30 wt% LDPE to limit neck-in and draw resonance at the die exit; the specific addition ratio for the sealant web is 70–85 wt% DOWLEX™ 2078G, with a maleic anhydride grafted tie layer at 5–10 wt% when adhesion to aluminum foil or paperboard is required. Compliance follows FDA 21 CFR 176.170(c) for paper and paperboard components and Commission Regulation (EU) No 10/2011 for the food-contact sealant layer, with extraction testing conducted according to EN 1186-1 and EN 1186-14. The downstream process uses a tandem extrusion coating line with slot-die widths from 1200 mm to 1800 mm, an air gap of 150–250 mm, a chill roll at 10–18 °C, and line speed from 200 m/min to 400 m/min. Melt temperature is held at 290–315 °C; above 315 °C, gel particles formed by oxidation are detected as surface pinholes in the coating. The sealant web is applied at 15–30 g/m² depending on the packaging substrate. Terminal products include aseptic beverage carton inner sealant layers, sachet laminates for dry powders, and paper-based soap wrap. A processing limit is that below 15 wt% LDPE, neck-in increases beyond 15 mm per edge on a 1500 mm die and causes uneven coating thickness at the deckle boundary.

    Compliance verification matrix by downstream application
    Application segmentStandard or regulationTest method or clauseVerification criterion
    Food-contact filmsFDA 21 CFR 177.1520(c) 3.2a; EU 10/2011EN 1186-1; EN 1186-14overall migration < 10 mg/dm²
    Industrial stretch filmREACH Annex XVII; ASTM D4649-20ASTM D5459-18stretch force retention; no SVHC above 0.1 wt%
    Agricultural covering filmEN 13206:2017ISO 527-3; EN 13206 Annex Btensile elongation and light transmission as specified by crop use
    Extrusion coating on paperboardFDA 21 CFR 176.170(c); EU 10/2011EN 1186-1; EN 1186-14extraction with food simulants; overall migration < 10 mg/dm²
    Heavy-duty sacksUN Model Regulations Chapter 6.5drop and stacking testsno rupture or siftage; published data limited

    Agricultural greenhouse covering and silage wrap formulations use 85–95 wt% DOWLEX™ 2078G, with a hindered amine light stabilizer concentrate at 1.0–2.5 wt% and a polyolefin elastomer at 5–10 wt% for puncture resistance. The applicable product standards are EN 13206:2017 for agricultural covering films and EN 14932:2018 for stretch films for wrapping bales. Downstream processing is performed on a three-layer blown film line with die diameters from 500 mm to 800 mm, a die gap of 1.6–2.2 mm, a blow-up ratio of 2.0:1–2.5:1, and melt temperature of 180–210 °C. Greenhouse films are produced at 150–200 µm, silage wrap at 25–50 µm, and silage sheets at 100–150 µm. The terminal product types include multi-season greenhouse tunnels, bale wrap for silage preservation, and mulch films. An operational limitation is that increasing the UV stabilizer masterbatch above 2.5 wt% leads to die-lip plate-out on long runs exceeding 48 h and reduces the light transmission required by the greenhouse crop; when such plate-out appears, the line is purged with a low-MI LDPE grade before shutdown.

    For vertical form-fill-seal packaging of dry powders, DOWLEX™ 2078G is used as the sealant web at 75–90 wt%, with erucamide slip at 400–600 ppm, silica antiblock at 1000–2000 ppm, and fluoroelastomer processing aid at 200–400 ppm. Food-contact qualification is carried out under FDA 21 CFR 177.1520(c) 3.2a and Commission Regulation (EU) No 10/2011, with GMP documented according to Regulation (EC) No 2023/2006. The sealant web is extruded at 30–60 µm and laminated to biaxially oriented PET or BOPP in a solvent-free or solvent-based adhesive laminator; the finished laminate is converted on vertical form-fill-seal machines with seal bar temperature 110–150 °C, dwell time 0.2–0.5 s, and jaw pressure 0.4–0.8 MPa. Terminal products include pillow pouches for dry mixes, salt and sugar sachets, powdered beverage sticks, and pet food pouches. Hot tack is measured by ASTM F1921 and seal strength by ASTM F88/F88M; below 0.15 s dwell time, the sealant layer does not develop adequate hot tack to hold product filling pressure, and above 600 ppm erucamide, heat-seal strength decreases due to surface bloom.

    Free Quote

    Competitive Dow DOWLEX™ 2078G Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction
    Dow DOWLEX™ 2078G Linear Low Density Polyethylene is a high-flow ethylene-based polymer with a nominal melt index of 7.0 g/10 min (ASTM D1238, 190 °C/2.16 kg) and a representative density of 0.920 g/cm³ (ASTM D792). The product is classified as a linear low-density polyethylene and is positioned for injection-molded and rotational-molded articles in which moderate stiffness, high flow, and low-temperature ductility are required. The molecular architecture is predominantly linear with controlled short-chain branching; this structure raises tensile yield and environmental stress crack resistance relative to high-pressure low-density polyethylene while reducing melt strength. The values discussed are typical published resin data, not batch-release limits; converters should confirm the current grade specification and regulatory certificate before qualifying tooling.
    Representative published typical property profile for DOWLEX 2078G; values are not batch-release specifications.
    PropertyTypical valueMethod
    Density0.920 g/cm³ASTM D792 / ISO 1183-1:2019
    Melt index7.0 g/10 minASTM D1238 / ISO 1133-1:2022
    Tensile strength at yield11 MPaASTM D638 / ISO 527-2
    Tensile strength at break15 MPaASTM D638 / ISO 527-2
    Elongation at break>800%ASTM D638 / ISO 527-2
    Flexural modulus310 MPaASTM D790 / ISO 178
    Vicat softening point96 °CASTM D1525
    Environmental stress crack resistance>1000 hASTM D1693
    Processing of 2078G in injection molding uses a general-purpose polyethylene screw with L/D 20:1–24:1 and compression ratio 2.5:1–3.5:1. Barrel profiles from 180 °C in the feed zone to 220–240 °C in the metering zone are commonly applied, with nozzle temperature held near 230 °C and mold temperature between 20 °C and 40 °C. The resin is not hygroscopic; drying is normally unnecessary unless surface condensation has formed during cold-weather storage, in which case 70–80 °C for 1–2 h may be used. Grade-specific processing maps for this exact product are limited; initial set points based on melt-index-equivalent LLDPE grades are validated with short-shot studies, cavity-pressure measurement, and purge tests after interruptions. For rotational molding, the relevant process boundary is not barrel temperature but peak internal air temperature. Typical LLDPE rotational molding cycles reach an internal air temperature of 190–210 °C to densify the sintered powder layer; holding the mold at peak temperature for 2–5 min permits bubble dissolution and weld-line consolidation. Peak internal air temperature tolerance is approximately ±5 °C; lower values leave unmelted porosity, while higher values can accelerate oxidative degradation and gas bubble formation. Cooling is then staged through forced air and water mist to control warpage. DOWLEX 2078G in powder form may be used for medium-to-large hollow parts, but published data for this specific grade’s rotomolding cycle are limited. A mold-in-process thermocouple or equivalent profiling system is required to establish the grade-specific end point because oven variability and part wall thickness shift the optimum by several minutes.

    How Does 2078G Differ from Low-Melt-Index DOWLEX Film Grades?

    Compared with DOWLEX blown-film grades in the 0.5–2.0 g/10 min melt-index interval, the 7.0 g/10 min value of 2078G shifts the rheological response toward reduced viscosity under shear. This reduces injection pressure and improves filling of thin-walled cavities, but it also lowers melt strength and drawdown tension. In blown-film conversion, that lower melt strength produces less bubble stability, greater neck-in, and a narrower operating window; therefore 2078G is not positioned for monolayer blown film. In injection molding and rotational molding, however, the same flow characteristic reduces cycle time and permits reproduction of fine mold details. The molecular weight decrease associated with higher melt index can reduce tensile strength and environmental stress crack resistance relative to lower-melt-index DOWLEX grades, although the difference is application-dependent and must be confirmed by comparative testing under ASTM D638, ASTM D1693, and ASTM D3763. Production-scale injection molding of high-flow LLDPE sometimes exhibits batch-to-batch variation in mold shrinkage due to melt index fluctuation within the producer tolerance. A shift of melt index from 6.0 g/10 min to 8.0 g/10 min can alter packing behavior in thin-wall tools and should be monitored by in-line melt flow rate according to ISO 1133-1:2022. In practice, tooling validation includes at least three lots to capture this variation; dimensional stability is then correlated with injection speed, hold pressure, and gate seal time. This avoids misinterpretation of lot-to-lot differences as mold maintenance issues. Regrind addition in non-critical injection-molded and rotational-molded articles is common. A post-industrial regrind content up to 20 wt% may be evaluated for molded non-food or industrial articles if the granulate is dry and free of foreign polymer fractions. Higher regrind loadings can reduce low-temperature impact and increase melt-flow instability, particularly at thin walls. Because no published data specific to 2078G regrind blends are available, the processor should establish a shrinkage compensation curve and verify tensile and environmental stress crack resistance retention against virgin resin using ASTM D638, ASTM D1693, and ASTM D3763. For food-contact articles, any regrind use must comply with the applicable polymer migration framework and supply-chain documentation.

    Processing Thresholds and Shrinkage Compensation in Thin-Wall Tools

    Thin-wall injection moldings in linear low-density polyethylene typically show mold shrinkage from 1.5% to 2.0% when measured by ASTM D955; the exact value for 2078G is influenced by gate geometry, packing pressure, melt temperature, and mold cooling. In a 0.8 mm wall-thickness cavity with flow length above 150 mm, injection velocity must be high enough to prevent premature freeze-off at the advancing melt front. Cavity pressure near the gate of 30–60 MPa during packing is typical for polyethylene in this density class, but gate dimensions and hot-runner pressure losses require local optimization. At melt temperatures above 240 °C or residence times beyond 5 min, oxidative chain scission can shift color and reduce mechanical properties; interrupted production should be purged with a high-flow polyethylene compound. Oscillatory shear data for LLDPE of this melt index indicate zero-shear viscosity on the order of 10³–10⁴ Pa·s at 190 °C; the shear thinning onset shifts with molecular weight distribution and comonomer incorporation. For injection molding simulation, a Cross-WLF viscosity model fitted from capillary rheometry at shear rates from 10¹ s⁻¹ to 10⁴ s⁻¹ is normally sufficient. Grade-specific data for DOWLEX 2078G should be obtained from the producer or by oscillatory rheometry according to ISO 6721-10. Use of a generic LLDPE viscosity dataset may overpredict pressure drop by 10–20% in thin-wall feed systems, so simulation should be calibrated against actual machine data.

    When DOWLEX 2078G Replaces High-Pressure LDPE in Impact-Dominated Parts

    Substitution of high-pressure LDPE with DOWLEX 2078G is most justifiable when low-temperature ductility and environmental stress crack resistance are limiting factors. In instrumented puncture testing according to ASTM D3763, linear low-density polyethylene of equivalent density often exhibits higher total energy to break than high-pressure LDPE, although published data for this exact grade are limited. The trade-off is increased melt elasticity loss and reduced clarity; where optical transparency or high melt strength is the primary control, high-pressure LDPE or a specialty copolymer remains preferable. The substitution also changes shrink and ejection characteristics; tooling may require greater draft angles and mold release because the lower modulus and higher elongation can increase ejection drag in deep-draw cavities. Regulatory conformance for food-contact uses of DOWLEX 2078G should be verified against 21 CFR 177.1520(c) in the United States and Regulation (EU) 10/2011 in the European Union. Under EU compliance testing, overall migration must remain below 10 mg/dm² under the intended time and temperature conditions, and specific migration limits for authorized additives apply. Because processing can deepen oxidation or introduce external contaminants, the final article manufacturer carries the obligation to validate the entire manufacturing chain. REACH and RoHS status are provided through supplier regulatory data sheets rather than the grade datasheet.

    Environmental Stress Crack Resistance and Short-Chain Branch Distribution in 2078G

    The stress-crack resistance of linear low-density polyethylene is strongly dependent on comonomer type, branch distribution, and tie-chain density. In general, low-pressure LLDPE with a density near 0.920 g/cm³ can exceed 1000 h in ASTM D1693 environmental stress crack resistance testing, while a high-pressure LDPE of similar melt index may fail much earlier under the same surfactant load. For DOWLEX 2078G, the producer typical value is useful for screening but is not a batch-release criterion. End users should conduct environmental stress crack resistance testing on actual molded parts because processing-induced orientation and wall thickness change the failure mechanism from surface craze to plane-stress shear and alter the time-to-failure distribution. Compared with high-density polyethylene at 0.955–0.965 g/cm³, DOWLEX 2078G has lower flexural modulus, lower heat deflection temperature, and higher low-temperature impact resistance. This makes the product suited for cold-chain boxes, caps with deep thread profiles, and large-area thin-wall articles where flexural stiffness is secondary. Hot-fill and autoclave applications above 100 °C are outside the realistic use boundary because the low crystallinity of this density cannot resist creep under load at those temperatures; published data for DOWLEX 2078G in continuous load above 60 °C are limited, so creep testing under ISO 899-1 is required for structural applications. Pellets or powder form depend on conversion route. For injection molding, the material is supplied as free-flowing pellets; for rotational molding, the producer supplies a ground powder with controlled particle-size distribution. Moisture absorption is negligible, but storage in a clean, closed hopper at 20–30 °C reduces contamination. Static discharge around polyethylene pellets can occur in pneumatic conveying; grounding and controlled transfer velocities below 20 m/s reduce fines and pellet-surface damage.
    Top