| HS Code | 721975 |
| Productname | Dow DOWLEX™ 2077G Linear Low Density Polyethylene |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.920 g/cm³ |
| Meltindex | 0.85 g/10 min (190°C/2.16 kg) |
| Meltingpoint | 124 °C |
| Vicatsofteningpoint | 101 °C |
| Tensilestrengthatyield | 10.3 MPa |
| Tensilestrengthatbreak | 31 MPa |
| Elongationatbreak | 700 % |
| Flexuralmodulus | 240 MPa |
| Dartdropimpact | 200 g |
| Elmendorftearmd | 250 g |
| Elmendorfteartd | 400 g |
| Haze | 12 % |
| Gloss | 50 % |
As an accredited Dow DOWLEX™ 2077G Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow DOWLEX™ 2077G Linear Low Density Polyethylene is supplied in 25 kg moisture-resistant polyethylene bags, palletized for safe storage and transport. |
| Container Loading (20′ FCL) | 20′ FCL: Dow DOWLEX™ 2077G Linear Low Density Polyethylene in 25 kg bags, 20 MT net, securely stowed for export. |
| Shipping | DOWLEX 2077G LLDPE is typically shipped as solid pellets in 25-kg PE bags, octabins, or bulk trucks/railcars. Keep dry; avoid direct sunlight, heat, and contamination. Not classified as dangerous goods for transport; comply with local shipping and handling regulations. Maintain sealed packaging and label identification during transit. Store pallets securely. |
| Storage | Store DOWLEX™ 2077G in original, sealed packaging in a cool, dry, well-ventilated area. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources and strong oxidizing agents. Maintain ambient temperatures, avoid excessive stacking, and follow first-in, first-out rotation. Keep containers closed when not in use and inspect regularly for damage. |
| Shelf Life | Shelf life: 24 months when stored in original unopened packaging, in a cool, dry, well-ventilated area away from sunlight and heat. |
Because the solution-polymerised octene comonomer distribution in DOWLEX 2077G produces a nominal density of 0.917 g/cm³ (ASTM D792) and a melt mass-flow rate of 2.3 g/10 min (ASTM D1238 at 190°C/2.16 kg), the resin is directed into high-speed cast pallet-wrapping lines where the melt must be distributed through a flat die at 240–260°C without forming cross-machine thickness bands. In this segment the core layer is typically run at 100 wt% DOWLEX 2077G while a cling-rich skin layer, metered from a satellite extruder at 8–15% of total throughput, is modified with 1.5–3.0 wt% polyisobutylene or a propylene-based cling masterbatch. The cling level is not fixed by resin grade but adjusted on the line because the unwinding force measured after 24 h ageing by ASTM D5458 must remain below the carriage load-cell trip threshold of the automatic wrapper; too little cling causes film flagging on the pallet, while excessive tackifier increases roll blocking and reduces pre-stretch consistency. The cast-film line specification in this application is a 30:1 L/D barrier screw with a Maddock mixing section, a 100/80/100 mesh screen pack, flat die gap 0.5–0.8 mm, chrome-plated primary chill roll at 18–26°C, and secondary cooling roll at 12–18°C. The quench temperature influences coefficient of friction, tested under ASTM D1894, and haze, tested under ASTM D1003; a higher chill-roll surface temperature increases both values and can destabilize the edge contact in pre-stretch. The film is drawn to 12–23 µm gauge and tested for tensile break under ASTM D882 and puncture propagation under ASTM D5748, with machine-direction and transverse-direction ratios used as quality gates. Terminal articles are machine-grade stretch films in 500 mm roll width for automatic turntable wrappers, and 750 mm roll width for ring wrappers operating at 200–280% pre-stretch on pallet loads with high film demand. The processing boundary is residence-time controlled: at melt temperatures above 260°C for more than 20 minutes, oxidised gel specks appear in the cast web and the film's puncture resistance on sharp pallet edges drops below the line-specific minimum. Lines that stop for more than 30 minutes at temperature should be purged with a lower-MFI polyethylene before restart, and reprocessing of edge trim must be limited to 15–20 wt% unless the trim is continuously re-fed into the same core stream.
In three-layer blown lamination webs for printed overwrap used in frozen and ambient food packaging, the core layer percentage is constrained by bubble stability rather than by optical performance. DOWLEX 2077G is blended at 70–85 wt% with high-pressure LDPE of 0.923 g/cm³ density in the core, while the outside layers are LDPE-rich or contain a PPA processing aid at 400–800 ppm. The LLDPE-rich core raises dart impact measured by ASTM D1709, but the bubble becomes more sensitive to internal pressure fluctuations when the frost line drifts more than ±50 mm from its set point, and melt pressure typically rises as the LLDPE fraction exceeds 80 wt%. Food-contact compliance is established by FDA 21 CFR 177.1520(c) 3.1(a) for the olefin polymer base resin and by Regulation (EU) No 10/2011 as amended, with overall migration tested according to EN 1186 against the 10 mg/dm² limit; any slip, antiblock or PPA masterbatch must itself be a food-contact grade with a documented migration status. The mix is processed on a grooved-feed blown-film line with a die gap 1.2–2.0 mm, blow-up ratio 2.2–2.8, neck height 4–6 die diameters, frost line 550–700 mm, and melt temperature 190–210°C at the adaptor. Output is normally reduced by 10–15% relative to an LDPE control when the DOWLEX 2077G fraction exceeds 80 wt% because die-lip deposit accumulation requires a die-lip clean every 48–72 h. The finished film is slit and converted into form-fill-seal pouches for frozen bakery and vegetable portions, with seal strength tested under ASTM F88/F88M using a seal-bar temperature of 130–155°C and dwell time 0.2–0.4 s. Published hot-tack response data for this exact grade in a 70/30 DOWLEX 2077G/LDPE blend are limited; a start-up hot-tack curve on a J&B-type instrument or equivalent should therefore be generated before line speed is advanced beyond 30 m/min. The blend should not be processed with reclaimed material of unknown post-consumer content because residual contaminants from the prior life cycle can shorten bubble-triggered tear resistance and introduce off-odor in sealed food packs.
| Application segment | Normative reference | Measured property | Typical process or compliance criterion |
|---|---|---|---|
| Cast pallet stretch film | ASTM D5458 | Peel cling after 24 h | Set by wrapper line-specific unwind trip threshold |
| Food contact film | FDA 21 CFR 177.1520(c) 3.1(a) | Olefin polymer compliance | Base resin conforms; masterbatch migration documented |
| EU food contact | EU 10/2011 as amended | Overall migration | 10 mg/dm² |
| Mechanical film performance | ASTM D882 | Tensile break, MD/TD | Report as MD/TD ratio |
| Melt flow characterisation | ISO 1133-1 | MFR 190°C/2.16 kg | 2.3 g/10 min nominal |
A round-bale silage wrap produced from DOWLEX 2077G must balance the puncture energy requirement of ISO 7765-1 Method A against the oxygen transmission rate measured under ASTM D3985 at 23°C and 0% RH. The film is usually blown in a three-layer line rather than cast because the bubble-induced orientation produces an elongation gradient that withstands bale expansion. The formulation comprises 70–85 wt% DOWLEX 2077G in the core, with outer layers containing 0.4–1.0 wt% HALS-based UV stabiliser masterbatch and, when a multi-season UV requirement exceeds 12 months of field exposure, 0.2–0.5 wt% carbon black or TiO₂. The blown-film line is operated with a die gap 1.8–2.4 mm, blow-up ratio 2.5–3.0, frost line 650–900 mm, and film thickness 25 µm as the centreline, with the film slit to 750 mm rolls. Puncture impact is tested under ISO 7765-1 after 1,000 h of accelerated weathering under ISO 4892-2; a drop below the line-specific as-extruded baseline after UV exposure indicates insufficient HALS dispersion or an incompatible additive package. The cling performance of the underside is adjusted with a low-temperature tackifier that must remain functional down to -5°C because silage film is applied in late-autumn conditions. The terminal article is a pre-stretched silage bale wrap for forage preservation, where the oxygen transmission rate through the film controls the aerobic spoilage boundary at the bale surface. Processors should avoid blending with reclaimed LLDPE from post-consumer greenhouse film or film carrying residual crop-protection chemicals and elemental sulfur from fumigation because these contaminants can accelerate thermo-oxidative degradation of the stabiliser package and lower the film's outdoor puncture retention. Published data for the precise DOWLEX 2077G silage formulation with region-specific UV loadings are limited; outdoor exposure trials should therefore be conducted before committing to a multi-year warranty.
On cast extrusion coating lines running at 120–250 m/min, DOWLEX 2077G is used as the sealant web when a low-temperature sealing layer is required on the reverse side of metallised polyester or aluminium foil. The resin is applied at 18–30 g/m² coat weight through a slot die onto a corona-treated substrate, and is normally blended with 15–25 wt% high-pressure LDPE to reduce neck-in and draw resonance. Melt temperature at the die is held at 285–310°C; below 280°C adhesion to the substrate is usually insufficient because the melt has not undergone the required oxidation on the air gap, while above 320°C the resin produces measurable fuming and gel formation. The air gap is set at 80–150 mm, the substrate is corona-treated to 42–48 mN/m immediately before the nip, and the chill-roll is maintained at 10–18°C to prevent blocking during roll winding. The laminate is intended for shelf-stable snack packs and confectionery wrappers, so the food-contact status of the sealant layer is governed by FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011; the aluminium foil or metallised polyester layer must also meet applicable metal and print-ink migration limits. Interlayer adhesion is measured by ASTM F88 peel separation after 48 h conditioning at 40°C, and the sealant should be checked for pinholing after folding. A processing restriction applies: DOWLEX 2077G is not a retort-grade sealant, and direct contact with high-acid liquid foods above 65°C may exceed its soak-age performance envelope. Published adhesion data for this specific grade in aluminium metallisation laminates are limited; line-side peel testing at start-up is therefore required before reducing coat weight below 20 g/m². Gel-count controls are typically based on a 20 µm cast film sample inspected under a 10× transmitted-light viewer, and any spot greater than 0.6 mm is cause for screen-pack and die-lip cleaning.
For heavy-duty open-mouth sacks converted on multi-layer blown-film lines, DOWLEX 2077G is specified in the core and seal layers because the resin's narrow molecular weight distribution lowers the seal initiation temperature relative to high-pressure LDPE while retaining a dart impact resistance measured by ASTM D1709. The formulation is 60–80 wt% DOWLEX 2077G, 20–40 wt% high-pressure LDPE, and 2–4 wt% antiblock masterbatch in the outside layers. The film is produced with a blow-up ratio 1.8–2.2, die gap 1.4–2.0 mm, melt temperature 190–210°C, and final gauge 80–120 µm. Outside layers are corona-treated to 38–42 mN/m for flexographic or digital ink adhesion. The terminal products are 25 kg and 50 kg fertiliser and polymer-pellet sacks, plus open-mouth liners for FIBCs; closure integrity is assessed by the filled-bag drop test of ASTM D5276 or ISO 7965-2, and the sack converter performs a design-type test at the finished article level when the contents are classified as dangerous goods under the UN Model Regulations Chapter 6.5. DOWLEX 2077G alone does not confer UN certification; the sack construction, closure hardware, and filling/discharge test results define the certification status. The film is not suitable for direct contact with strong oxidising agents, aromatic hydrocarbons, or ketones above 40°C because the resultant permeation and environmental stress-cracking behaviour are outside the typical LLDPE chemical-resistance envelope. To maintain tear resistance, the film should be conditioned for 48 h at 23°C and 50% RH before Elmendorf tear testing under ASTM D1922, and any post-industrial recyclate should not exceed 15 wt% unless its gel content and density have been verified by the film converter.
Competitive Dow DOWLEX™ 2077G Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DOWLEX™ 2077G Linear Low Density Polyethylene is a solution-polymerized ethylene-octene copolymer supplied for blown film extrusion, heavy-duty sack structures, and industrial packaging. The grade is specified by a nominal density of 0.920 g/cm3 under ASTM D792 or ISO 1183-1 and a nominal melt index of 0.80 g/10 min at 190 °C with a 2.16 kg load under ASTM D1238 or ISO 1133-1:2022. The density classification places the product in the linear low-density polyethylene range below 0.930 g/cm3, while the linear backbone and octene comonomer differentiate it from high-pressure LDPE and butene-based LLDPE. The designation 2077G identifies a film extrusion grade within the DOWLEX family; product selection should be confirmed against the current supplier technical data sheet and certificate of analysis.
| Property | Test method | Nominal value |
|---|---|---|
| Melt index | ASTM D1238 / ISO 1133-1:2022 | 0.80 g/10 min |
| Density | ASTM D792 / ISO 1183-1 | 0.920 g/cm3 |
| Comonomer | Supplier documentation | 1-octene |
At the product-family level, 2077G is differentiated from butene-based LLDPE by the α-olefin comonomer and from high-pressure LDPE by chain architecture. Butene-based resins of the same nominal density and melt index can show lower machine-direction Elmendorf tear and lower dart impact in many blown film structures; high-pressure LDPE gives higher melt strength and lower shear sensitivity, but typically lower tensile strength at break under ASTM D882. The practical consequences appear on the extrusion line: a conversion from butene-based LLDPE to 2077G may require die gap widening, and a conversion from LDPE to 2077G may require bubble support changes. Published comparative data for this specific grade against every competing resin is limited, so the following processing statements should be confirmed with films produced on the target line.
In blown film extrusion on single-screw machines with screw diameters from 40 mm to 75 mm and length-to-diameter ratios of 24:1 to 30:1, 2077G is processed at melt temperatures from 190 °C to 230 °C. Barrier screws with Maddock-type mixing sections or trough mixers are used to homogenize the melt and avoid unmelted resin at the die lip. For 2077G, die gaps from 1.6 mm to 2.8 mm are more common than the narrow gaps used for LDPE because the shear-thinning behavior of LLDPE is less pronounced and narrow gaps increase die-exit wall shear stress. Blow-up ratios from 2.0:1 to 3.0:1 and frost line heights of 6 to 10 die diameters are used to control orientation and bubble stability. The processing window for 2077G is narrower than that of a typical butene-based LLDPE at the same nominal melt index when the line is not equipped with internal bubble cooling. Operators converting from butene-based grades often must increase die lip temperature or reduce screw speed to prevent sharkskin melt fracture; the exact adjustment is determined by die-exit wall shear stress rather than by melt temperature alone.
Mechanical qualification of films containing 2077G is performed on 25 µm to 100 µm monolayer or coextruded samples. Tensile yield strength, tensile strength at break, and elongation at break are measured under ASTM D882 or ISO 527-3; the test report separates machine-direction and transverse-direction properties because take-off speed and blow-up ratio produce anisotropic mechanical response. Elmendorf tear propagation is measured under ASTM D1922; in blown film, octene-based LLDPE of the 2077G type typically shows higher machine-direction tear resistance than butene-based LLDPE at the same density and melt index because the longer branch forms a more uniform tie-chain population across lamellar boundaries. Dart impact resistance is measured under ASTM D1709 Method A or B, with the specimen width, gauge, and extrusion history controlled. Film stiffness is quantified as secant modulus under ASTM D882. These comparative values are not transferable across film thicknesses; a result from a 25 µm film is not linearly scalable to a 75 µm film because failure mechanisms shift from bending to puncture-dominated deformation as thickness increases.
Capillary rheometry under ASTM D3835 or ISO 11443 quantifies the shear viscosity function of 2077G at 190 °C. The resin exhibits lower shear sensitivity than high-pressure LDPE: as apparent shear rate increases from 100 s-1 to 1000 s-1, the viscosity of LLDPE decreases less steeply than that of LDPE. On film lines, this means that screw-speed increases produce a larger rise in die pressure than would be observed with LDPE at the same output. Sharkskin is governed by the wall shear stress at the die lip, not by output in kg/h alone. Published processing studies for linear polyethylenes identify a critical wall shear stress for sharkskin onset in the range of 0.1 MPa to 0.4 MPa. When the die-exit stress in 2077G exceeds this threshold, the film surface develops a repeating herringbone roughness that reduces sealing consistency and print uniformity. Corrective actions include increasing die lip temperature, opening the die gap, reducing screw speed, or adding 5 wt% to 15 wt% high-pressure LDPE as a melt-strength modifier. The LDPE addition reduces wall shear stress but alters Elmendorf tear and dart impact values; each blend ratio must be re-qualified under ASTM D1922 and ASTM D1709 because the structure-property relationship is not linear.
Bubble stability in 2077G is controlled by the geometry of the air ring and internal bubble cooling. On high-blow-up-ratio lines, a dual-lip air ring with internal bubble cooling provides more heat removal than a single-lip air ring; the higher heat removal allows a shorter frost line and reduces bubble wander. The frost line distance for 2077G is set from 6 to 10 die diameters. If the frost line is too low, quench-related surface defects and elevated haze can occur. Because LLDPE has a narrower molecular weight distribution than LDPE, the bubble is less self-supporting, and air ring pressure must be reduced to avoid flapping. Melt pressure at the adapter and die should be monitored during start-up; an adapter melt pressure above 30 MPa typically indicates a screen pack or screw issue requiring inspection. Screen packs of 40/60/80 mesh are common on film lines, and a pressure drop increase of 5 MPa to 10 MPa above the clean-pack baseline is used as a change-out criterion.
Thermal analysis under ASTM D3418 or ISO 11357-3 yields the melting peak and crystallization exotherm. For a 0.920 g/cm3 ethylene-octene copolymer, the melting peak is lower than that of a 0.940 g/cm3 MDPE because higher comonomer content reduces lamellar thickness. The measured crystallization temperature influences heat removal in the blown film line; fast crystallization from a low frost line yields a different crystalline orientation than slower crystallization above the frost line. This thermal behavior affects heat-seal and hot-tack performance in downstream packaging operations. Seam strength and failure mode are tested under ASTM F88 as a function of jaw temperature, dwell time, and pressure. No single seal initiation temperature applies across all film structures because comonomer type, surface treatment, gauge, and lamination structure all shift the seal response.
Replacing high-pressure LDPE with 2077G on an existing heavy-duty sack line is not a direct material substitution. High-pressure LDPE contains long-chain branches that support bubble stability at high blow-up ratios and high frost lines; 2077G has a narrower molecular weight distribution and lower melt strength. On a line designed for 100% LDPE, the first observable change after conversion may be bubble flutter or sag above the frost line, particularly at blow-up ratios greater than 2.8:1. Processors commonly widen the die gap from 0.8 mm–1.2 mm to 1.6 mm–2.8 mm, raise melt temperature by 5 °C to 15 °C, or lower the frost line height to restore bubble support. In heavy-duty sack film, blends of 70 wt% to 90 wt% 2077G with high-pressure LDPE are often used; the LDPE fraction improves bubble stability while retaining much of the LLDPE dart impact and tear resistance. The effect of LDPE content on dart impact is not linear because intermediate LDPE levels can alter crystalline morphology and produce a local minimum in impact resistance. A matrix of dart impact tests under ASTM D1709 and tear tests under ASTM D1922 is therefore required for each film gauge and blend ratio before commercialization.
Film structures based on 2077G are used in heavy-duty sacks, industrial liners, agricultural covers, and carrier bags. These applications are specified by dart impact under ASTM D1709 and tear resistance under ASTM D1922 rather than optical clarity alone. Surface treatment for lamination or printing is typically set to a wetting tension of 38 mN/m to 42 mN/m; the corona treatment level decays with time and must be measured immediately before lamination. In coextrusion, 2077G may be used in core or skin layers depending on sealant and stiffness requirements. A skin layer may contain slip and antiblock additives, while a core layer may include controlled regrind. Layer ratio control within ±1 wt% is needed to maintain gauge uniformity; interfacial instability can appear as wave-like gauge bands if the skin and core melt viscosities are mismatched. Matching viscosity at the processing shear rate is therefore more important than matching melt index alone.
Incoming quality control for 2077G includes pellet density under ASTM D792 and melt index under ASTM D1238. The supplier certificate of analysis is compared against the received lot number before silo discharge. Because repeated heat history shifts yellowness index and can increase gel formation, regrind content is controlled and test films are checked under ASTM D1709. Polyethylene absorbs negligible moisture, so predrying of 2077G is not normally required. However, cold pellets moved from outdoor storage into a warm production hall can carry surface condensation, which may introduce pinholes or surface splay in the extruded film. If surface moisture is observed, drying at 70 °C to 80 °C for 1 h to 2 h in a desiccant hopper dryer is sufficient; longer drying does not improve processing because the moisture is on the pellet surface, not inside the polymer. For food-contact applications, the supplier can provide documentation referencing FDA 21 CFR 177.1520 and, where applicable, (EU) No 10/2011 as amended. These clearances are conditions-of-use specific; food type, temperature, film thickness, and lamination structure must be checked against the supplier letter. During silo and hopper transitions from a previous resin, the equipment should be purged with a lower-viscosity PE or a commercial purge compound because LLDPE at 0.80 g/10 min can retain previous material in dead spots for longer than higher-melt-index grades. The safety data sheet should be reviewed before bulk conveying, because polyethylene dust can form combustible dust-air mixtures in pneumatic transport systems.