Dow Dowlex 2077 Linear Low Density Polyethylene Food Grade

Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade

    • Product Name: Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 559903
    Product Name Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade
    Generic Name Linear Low Density Polyethylene (LLDPE)
    Polymer Type Ethylene/butene-1 copolymer
    Density 0.920 g/cm³
    Melt Index 2.3 g/10 min
    Melting Point 121 °C
    Vicat Softening Point 94 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 24.1 MPa
    Ultimate Elongation 800%
    Flexural Modulus 241 MPa
    Hardness Shore D 50
    Brittleness Temperature < -70 °C
    Food Contact Compliance FDA 21 CFR 177.1520(c) 3.1a; EU 10/2011
    Form Pellets
    Color Natural

    As an accredited Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing DOWLEX™ 2077 Food Grade comes in 25 kg polyethylene-lined bags and 1,000 kg bulk bags for industrial food-contact handling.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized 25 kg bags of Dow DOWLEX™ 2077 food-grade LLDPE, stretch-wrapped and secured for export.
    Shipping Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade is shipped as a non-hazardous solid resin in 25 kg bags, 1,000 kg octabins, or bulk trucks/railcars. Keep packaging sealed, dry, clean, and away from direct sunlight/heat to prevent contamination and maintain food-contact compliance. Follow local transport regulations.
    Storage Store DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade, in a clean, cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong odors. Keep original packaging sealed, palletized, and off the floor. Prevent moisture, dust, and contamination. Avoid excessive stacking, prolonged UV exposure, and incompatible materials. Follow the manufacturer’s SDS and local regulations; rotate stock.
    Shelf Life DOW DOWLEX 2077 has a five-year shelf life when stored unopened in original packaging in a cool, dry, well-ventilated area.
    Application of Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade

    On a cast film line running flow-wrap for washed, ready-to-eat leafy greens, DOWLEX 2077 is processed neat at 100 wt% through a barrier screw extruder with L/D 30:1 and a melt temperature held between 245 °C and 255 °C. The resin, an octene-1 based linear low density polyethylene with nominal density 0.920 g/cm³ and melt index 2.3 g/10 min per ASTM D1238, is used in this segment because its narrow comonomer distribution permits chill roll contact at 20 °C to 30 °C without excessive plate-out. Food-contact compliance for the finished film is established under U.S. 21 CFR 177.1520(c) and European Regulation (EU) No 10/2011 as amended; the converter must nonetheless verify overall migration below 10 mg/dm² and organoleptic neutrality in the actual pack. At 50 µm gauge, haze measured per ASTM D1003 is typically below 5%, and dart impact per ASTM D1709 falls between 250 g and 350 g. The downstream process runs at haul-off speeds above 120 m/min; film chatter at these speeds is controlled by the resin’s relatively high melt index and by maintaining a chill roll air gap below 100 mm. Terminal articles produced from this film include pillow packs for fresh-cut lettuce and spinach, lidding film for CPET trays of cut fruit, and flow-wrap for celery sticks and shredded cabbage.

    JurisdictionDesignationCondition / limit to be verified on finished article
    United States21 CFR 177.1520(c)Olefin polymer food-contact status; extractive limits per 21 CFR 176.170(c) Table 2 for the intended condition of use
    European UnionRegulation (EU) No 10/2011 as amendedOverall migration limit 10 mg/dm²; specific migration of authorised monomers and additives to be validated in finished laminate or container
    North AmericaNSF/ANSI 51 where applicableFood equipment material evaluation for finished articles used in commercial food handling

    What governs heat-seal integrity in vertical form-fill-seal frozen vegetable packaging?

    In vertical form-fill-seal (VFFS) operations, heat-seal integrity is governed by seal bar temperature, dwell time, and the presence of surface frost, not solely by resin melt index. A typical formulation for IQF vegetable pouches blends 70 wt% DOWLEX 2077 with 30 wt% LDPE of melt index 0.75 g/10 min; the LDPE component stabilises the blown-film bubble at blow-up ratio 2.5:1 and reduces melt fracture at die gaps below 2.0 mm. The monolayer blown film is extruded on a die with diameter 250 mm at melt temperature 205 °C to 215 °C, with frost line height maintained at 6 to 8 die diameters. Compliance rests on 21 CFR 177.1520(c) for U.S. food contact and Regulation (EU) No 10/2011 for the European market, with the additional requirement that cold-temperature impact of the pouch survives distribution at -25 °C; dart impact per ASTM D1709 at 50 µm is typically not less than 200 g. Heat seal initiation on film of this structure occurs near 105 °C, with hot tack force measured by ASTM F1921 exceeding 4 N/25 mm at 150 °C seal bar temperature, and ultimate seal strength per ASTM F88 reaching 12 N/25 mm after cooling. On the VFFS packaging line, dwell times of 0.3 s to 0.5 s are typical; failure modes observed on production-scale machines include seal tear at the top corners of pillow packs and channel leakers caused by product fines trapped under the seal area. End products include pouches for frozen peas, corn kernels, diced carrots, and mixed vegetable blends.

    Coating weight alone does not determine adhesion to liquid packaging board

    At coating weights below 18 g/m², adhesion failures on gable-top cartons are more often caused by insufficient oxidation time in the air gap than by polymer quantity. DOWLEX 2077 is processed in extrusion coating as the food-contact heat-seal layer, generally at 100 wt% unless a lower coefficient of friction is required; for that case a masterbatch containing slip additive is introduced at 2 wt% to 3 wt%. The line configuration is a tandem coextrusion coating station with air gap 200 mm to 250 mm, melt temperature 285 °C to 305 °C, and a melt temperature window held within ±5 °C to prevent edge neck-in exceeding 50 mm. Board surface temperature is maintained above 30 °C and moisture content below 6%. The critical process conflict is the narrow oxidation window: if air gap oxidation is too low, the polymer-to-board adhesion is insufficient; if the air gap or melt temperature is too high, low-molecular-weight oxidation products form on the coating surface and can migrate into liquid foods. Compliance for the finished carton includes U.S. 21 CFR 176.170(c) extractive limitations in Table 2 and 21 CFR 177.1520(c) for the olefin polymer, as well as Regulation (EU) No 10/2011 overall migration limits; specific migration for the octene-1 comonomer is validated in the finished laminate. Peel adhesion is measured in-line by ASTM D903, with production specifications commonly requiring not less than 2.5 N/15 mm; values below that threshold are associated with delamination at the paperboard-polymer interface during jaw folding. Coating weight is typically 20 g/m² to 25 g/m² for milk and juice cartons. Published data for DOWLEX 2077 in this specific extrusion coating configuration are limited; converter validation is therefore based on in-line peel adhesion rather than published design allowables. Terminal packages include gable-top paperboard cartons for pasteurised milk, liquid egg, and juice concentrates.

    When DOWLEX 2077 enters rotational molding for food-contact bulk bins

    Pulverization of DOWLEX 2077 to 35 mesh (500 µm) is required before charging to a biaxial rotational molder. In this process the resin is used at 100 wt% of the polymer charge, with additives limited to 0.2 wt% antioxidant and, for outdoor bins, 0.15 wt% hindered amine light stabiliser; both additives must appear on the positive list of Regulation (EU) No 10/2011 or be covered by 21 CFR 177.1520(c). Oven temperature is set at 280 °C; internal air temperature measured inside the mold must reach 190 °C for 15 min to 20 min to achieve full consolidation of the pulverized bed. After heating, forced-air cooling is applied until the part surface reaches 60 °C before demolding. Wall thickness is typically 3 mm to 6 mm depending on bin capacity; corner sections below 3 mm exhibit higher pinholing risk due to powder bridging at the mold surface. Exceeding 200 °C internal air temperature in thin wall sections leads to oxidative yellowing and loss of ASTM D3895 oxidative induction time below 20 min. Compliance for food-contact dry bulk storage is demonstrated under 21 CFR 177.1520(c) and Regulation (EU) No 10/2011; for equipment housings in USDA-inspected facilities, the finished bin may also be evaluated under NSF/ANSI 51. Mechanical acceptance includes tensile yield per ASTM D638 not less than 10 MPa and oxidative induction time per ASTM D3895 above 40 min at 200 °C. Terminal products include bins and totes for sugar, flour, rice, and dry ingredient handling in bakeries and food-processing plants.

    For cold-runner injection molding of thin-wall dairy tubs, DOWLEX 2077 is typically let down at 30 wt% into a high-flow LLDPE with melt index 20 g/10 min to balance impact toughness and fill pressure. The blend is processed at melt temperature 220 °C to 240 °C, mold temperature 10 °C to 15 °C, injection speed 120 mm/s to 180 mm/s, and clamp force from 2,500 kN to 3,500 kN on stack molds. Increasing the DOWLEX 2077 fraction above 40 wt% reduces spiral flow length below 300 mm at 220 °C, raising short-shot frequency in side gated tubs with nominal wall thickness 0.8 mm to 1.2 mm. Food-contact compliance for the molded parts is established under 21 CFR 177.1520(c) and Regulation (EU) No 10/2011; specific migration of processing aids and the octene-1 comonomer must be verified on the finished container at stored contact temperatures up to 40 °C. Tensile properties are tested per ASTM D638; the blend typically exhibits yield strength of 10 MPa to 12 MPa and elongation at break above 300%. In production, batch-to-batch variance in the high-flow LLDPE carrier can shift melt pressure at the injection nozzle by ±8%, requiring closed-loop transfer position adjustment. Terminal articles include thin-wall tubs for yoghurt, sour cream, and cottage cheese, as well as snap-on lids for chilled dairy and deli containers.

    Parison sag, die swell, and wall distribution in extrusion blow molding of food-safe squeeze bottles

    A 25 wt% let-down of DOWLEX 2077 into a fractional-melt HDPE homopolymer modifies the parison sag behaviour in shuttle blow molding. The blend is processed at melt temperature 190 °C to 205 °C, die gap 0.8 mm, and blow air pressure 0.6 MPa; parison programming is engaged to correct wall thinning at the bottle pinch-off. Food-contact compliance is governed by 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, with no specific migration limit exceeded at filling temperatures below 60 °C. The resulting bottle sidewall thickness is 0.45 mm to 0.70 mm, and the blend’s environmental stress crack resistance measured per ASTM D1693 condition B typically exceeds 100 h in 10% Igepal. Drop impact at -20 °C per ASTM D2463 is specified at not less than 2.0 m for filled bottles, a requirement that filters out brittle failures caused by excessive HDPE content or insufficient let-down dispersion. On shuttle blow molders, the main production bottleneck is parison curvature due to differential swell when the die-head temperature drifts more than ±3 °C; this produces sidewall thickness variance above 0.15 mm and intermittent leakers at the neck shoulder. Terminal products include squeeze bottles for ketchup, mayonnaise, mustard, and honey.

    Free Quote

    Competitive Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade is a pelletized ethylene/α-olefin copolymer produced by a solution polymerization route and intended for thin-gauge food packaging layers. The material is classified as an LLDPE because the polymer backbone is linear with short-chain branches introduced by comonomer incorporation rather than the long-chain branching characteristic of high-pressure LDPE. The nominal density is 0.920 g/cm³ when tested under ASTM D792-20, and the nominal melt mass-flow rate is 2.3 g/10 min at 190 °C/2.16 kg under ASTM D1238-20. The equivalent melt-flow-rate determination under ISO 1133-1:2022 may be reported when the converter’s laboratory is aligned to ISO methods. The food-grade designation reflects a formulation managed for food-contact suitability, principally 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, but it does not remove the packer’s obligation to validate the finished article.

    Applications are concentrated in monolayer and coextruded cast film for dry foods, fresh produce overwrap, lamination films, and form-fill-seal structures. Because the grade is supplied as virgin pellets with low intrinsic moisture, predrying is generally unnecessary. If open silo storage allows surface condensation at relative humidity above 60 %, or if in-house regrind is introduced, dehumidified-air drying at 60 °C for 2 h is applied before extrusion. The material’s medium melt index places it in the class used for high-output cast film, but the exact line conditions must be set from the lot certificate of analysis and the extruder’s screw design.

    What Limits Melt Fracture and Chill-Roll Condensation in Cast Film?

    Linear polyethylenes of this density class are sensitive to sharkskin or melt fracture when the wall shear stress in the die land exceeds a critical value. For DOWLEX™ 2077, the published datasheet does not state a universal critical shear rate because the onset depends on die gap, die-land finish, and melt temperature. A stepped-throughput trial should therefore be run on the target cast film die; the appearance of roughness is recorded against a physical standard because no single optical index captures the transition. On lines with single-screw extruders of L/D 30:1 and a general-purpose polyolefin screw, the die and adapter setpoints are normally kept 5–10 °C below the final barrel zone to increase melt extensional viscosity at the lip. Typical die exit melt temperatures fall between 210 °C and 240 °C. Operation above 250 °C is not recommended because oxidative chain scission may generate gel particles and reduce the film’s impact resistance, even with stabilised food-grade formulations.

    In production-scale cast film, a common suppression measure is reduction of the die gap from 0.8 mm to 0.5 mm, with a die-land length ratio maintained between 10:1 and 15:1. The thinner land gap raises wall shear stress but shortens residence time at high shear, and the effect on melt fracture is not monotonic; the operator must map the response by varying screw speed in 10 rpm increments while holding melt temperature constant. If edge weave appears, reducing the die lip adjustment in the outermost zones by 0.02 mm and raising chill roll tension by 5–10 % have been used to stabilise the web, but these changes alter machine-direction orientation and require subsequent tensile verification under ASTM D882.

    Chill-roll temperature control uses chilled water at 20–30 °C to quench the web. Condensation on the first chill roll is a process-defect source in humid production halls; the chilled water inlet temperature must be held above the measured dew point. A dew-point transmitter in the cooling circuit is the standard control loop because visible moisture on the roll forms only after the surface has already dropped below the condensation threshold. If the film is not quenched uniformly, trans-crystallinity differences across the web produce gauge-dependent haze that is measurable by ASTM D1003 but may not be visible at line speed.

    Mechanical Property Verification Through ASTM and ISO Test Designations

    Material specifications for DOWLEX™ 2077 are controlled by lot release testing rather than by generic tabulated values. The two properties most commonly recorded on the certificate of analysis are density and melt mass-flow rate; mechanical, thermal, and optical data are typical values that depend on sample preparation and should be compared only when the same test speed, specimen thickness, and conditioning protocol are used. For thin film, tensile properties are determined under ASTM D882, not ASTM D638-14, because ASTM D638 is intended for rigid or thicker extruded shapes and yields different grip and extension conditions. Tear, dart impact, and haze are measured under ASTM D1922, ASTM D1709, and ASTM D1003, respectively. A packaging engineer comparing DOWLEX™ 2077 with another food-grade LLDPE must therefore specify the test standard and the film gauge; a tensile comparison at 25 µm and 500 mm/min is not transferable to a 100 µm lamination web without revalidation.

    PropertyTest methodTypical nominal value
    Melt mass-flow rateASTM D1238-20, 190 °C/2.16 kg2.3 g/10 min
    DensityASTM D792-200.920 g/cm³
    Physical formManufacturer visual standardPellets
    Food-contact status21 CFR 177.1520(c); Regulation (EU) No 10/2011Supplier compliance statement required

    Food-contact compliance for a pellet is not equivalent to food-contact compliance for a finished package. The resin supplier may state that DOWLEX™ 2077 is manufactured to the olefin polymer criteria of 21 CFR 177.1520(c), which applies to polyethylene and its copolymers and imposes extractive restrictions on the base polymer. For the European Union, Commission Regulation (EU) No 10/2011 is the governing plastics framework, and the overall migration limit from the finished article is 10 mg/dm² of food-contact surface when tested under the food simulant and time/temperature conditions assigned to the intended use. Specific migration limits for the comonomer and for stabiliser additives must be checked against the regulation’s positive list; the comonomer-specific value depends on whether the short-chain branch source is 1-octene and on the current lot formulation. REACH registration under EC No 1907/2006 is a separate obligation for substances supplied in the European Economic Area.

    A converter cannot infer compliance solely from the word “food grade” because processing can lower molecular weight, generate oxidation products, or leave processing aids at the surface. The correct verification path is a three-part record: the supplier’s food-contact compliance statement for the specific grade, the lot certificate of analysis, and migration testing on the finished article under the intended contact conditions. For many long-term storage applications at refrigerated or ambient temperature, the relevant EU simulant condition may be 10 days at 40 °C, but the time/temperature assignment must be selected from Annex V of Regulation (EU) No 10/2011 based on the actual food type and package service temperature. If the structure is gamma-irradiated or autoclaved, post-treatment migration testing is necessary because irradiation can alter the stabiliser package.

    RequirementReferenceLimit or condition
    U.S. olefin polymer food-contact use21 CFR 177.1520(c)Base polymer extractives and end-use conditions
    EU plastics overall migrationRegulation (EU) No 10/201110 mg/dm²
    EU chemical registrationEC No 1907/2006Monomer/additive registration; SDS availability

    If the Material Is Run in a Coextruded Food Contact Layer with Reclaimed Content

    Coextruded packaging may place DOWLEX™ 2077 as the food-contact sealant layer while a reclaimed stream is confined to a middle or back layer. When this structure is used for food, the buried layer must not compromise the food-contact surface; if the reclaimed stream is not food-contact approved, a functional barrier between the reclaimed layer and the food must be demonstrated by migration testing. In the European Union, the use of recycled plastics in food packaging is controlled by Regulation (EU) 2022/1616; non-food-contact reclaimed material behind a functional barrier may be acceptable only when the finished article meets the same migration limits as virgin material. The U.S. FDA position depends on the source of the recycled polymer and may require a no-objection letter unless the recycle is generated in-house from the same compliant package.

    Processors that reintroduce in-house edge trim into a DOWLEX™ 2077 cast film line should measure the melt mass-flow rate of the flake before blending. Heat-aged trim may exhibit a higher melt index than virgin pellets, and at 10–20 wt% reclaim addition the blend melt index may shift sufficiently to alter gauge distribution at the die. The standard control is to blend a fixed proportion by weight, dry the flake, and run a narrow melt-temperature profile. A drop in die pressure of 5–10 % at constant screw speed may accompany the shift; the downstream takeoff must then be adjusted to maintain target gauge, and film tensile properties are confirmed by ASTM D882. If the reclaimed layer creates optical defects in a clear structure, haze is quantified by ASTM D1003 before the line is released.

    Seal Initiation Temperature Must Be Measured on the Finished Structure

    Seal initiation and hot-tack are not intrinsic resin properties that can be transferred from a datasheet to a packaging machine. The sealant layer thickness, film gauge, sealing pressure, dwell time, and jaw temperature all interact. For structures sealed on vertical or horizontal form-fill-seal equipment, hot-tack strength is measured under ASTM F1921, and seal strength after cooling is measured under ASTM F88/F88M. A seal initiation temperature obtained from a 25 µm monolayer cast film cannot be applied to a 50 µm coextruded film with an EVOH barrier without revalidation. The medium melt index of DOWLEX™ 2077 contributes to rapid interdiffusion at the seal interface, but the converter should determine the lowest reliable seal temperature by a gradient seal test on the actual production web.

    On high-speed packaging machines, hot-tack is the limiting factor because the product drops into the pouch before the seal has cooled. A comparative evaluation against an mLLDPE of similar density may show a higher or lower hot-tack depending on the machine’s dwell time and jaw pressure; published data for this specific comparison is limited. Therefore, a sealability study should include at least three dwell times and three jaw temperatures, with hot-tack and final seal strength reported as functions of sealing pressure. Without such data, downgauging a sealant layer below the existing qualified thickness is not technically justified, even if the density and melt index are equivalent.

    Compared with high-pressure LDPE of equal density, DOWLEX™ 2077 has a predominantly linear main chain and short-chain branches caused by the α-olefin comonomer. High-pressure LDPE contains long-chain branches that increase melt elasticity and improve blown film bubble stability but reduce tensile strength and puncture resistance. As a result, a switch from LDPE to DOWLEX™ 2077 in a cast film or lamination layer can allow thickness reduction in some structures while retaining yield strength as measured by ASTM D882; however, the exact downgauge margin is package-dependent and cannot be assumed from density alone. In blown film, the same architectural difference lowers bubble stability, so an LLDPE run may require a smaller blow-up ratio or a dedicated air ring. The melt index comparison under ASTM D1238-20 is not a reliable predictor of extruder head pressure when LDPE and LLDPE are compared because the shear-rate dependence of viscosity differs.

    Compared with metallocene-catalysed LLDPE of similar density, the conventional Ziegler-Natta architecture of DOWLEX™ 2077 typically produces a broader molecular weight distribution. This often lowers melt pressure at a given throughput and can make the material more tolerant of extruders with older screw designs. The trade-off may appear in optical and impact properties; an mLLDPE of equivalent density can show higher dart impact under ASTM D1709 and lower haze under ASTM D1003 in blown film, while the cast film optics may be closer because chill-roll quenching dominates surface roughness. Any substitution decision should be based on parallel measurements on the same line: ASTM D882 for tensile yield and elongation, ASTM D1922 for tear, ASTM D1709 for dart impact, ASTM D1003 for haze, and ASTM D2457 for gloss. If the target is a food-contact package, the migration documentation for the replacement structure must also be updated.

    Within the DOWLEX™ LLDPE family, grades are differentiated by density, melt index, and comonomer type. A higher-density grade generally increases stiffness and oil resistance but reduces low-temperature toughness, while a lower melt index grade raises melt strength and is preferred for heavy-duty sacks. DOWLEX™ 2077 with a nominal density of 0.920 g/cm³ and a melt index of 2.3 g/10 min is positioned for medium-viscosity cast film and lamination where both flow and film toughness are required. Selection between DOWLEX™ 2077 and a lower-MI grade should be made by comparing the specific film’s properties rather than by nominal property tables because differences in fabrication can exceed the differences among resin grades.