Dow Dowlex 2071d Linear Low Density Polyethylene

Dow DOWLEX™ 2071D Linear Low Density Polyethylene

    • Product Name: Dow DOWLEX™ 2071D Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 373517
    Comonomer 1-Octene
    Density 0.9205 g/cm³
    Melt Index I2 0.85 g/10 min
    Melt Flow Ratio I21 I2 27
    Melting Point 123 °C
    Vicat Softening Point 104 °C
    Tensile Strength At Yield Md 10.3 MPa
    Tensile Strength At Yield Td 10.3 MPa
    Tensile Strength At Break Md 32.4 MPa
    Tensile Strength At Break Td 30.0 MPa
    Elongation At Break Md 750 %
    Elongation At Break Td 800 %
    1 Secant Modulus Md 240 MPa
    1 Secant Modulus Td 260 MPa
    Dart Drop Impact 25 µm Film 150 g
    Elmendorf Tear Strength Md 25 µm Film 220 g
    Elmendorf Tear Strength Td 25 µm Film 380 g
    Haze 10 %
    Gloss 45 55

    As an accredited Dow DOWLEX™ 2071D Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DOWLEX™ 2071D Linear Low Density Polyethylene is typically supplied in 25 kg polyethylene-lined bags, palletized and stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL loading: DOWLEX™ 2071D Linear Low Density Polyethylene in 25 kg bags, palletized and securely stowed for ocean freight.
    Shipping DOWLEX™ 2071D Linear Low Density Polyethylene is shipped as solid, free-flowing pellets in 25 kg bags, palletized and stretch-wrapped. Transport in clean, dry trucks, railcars, or containers. Avoid moisture, direct sunlight, excessive heat, and contamination. Not classified as dangerous goods. Store under cover in a cool, dry, well-ventilated area.
    Storage Store DOWLEX™ 2071D in a cool, dry, well-ventilated indoor area away from direct sunlight, heat, flames, ignition sources, and strong oxidizers. Keep containers or bags tightly closed to prevent moisture, dust, and contamination. Avoid dust accumulation and static discharge. Use first-in, first-out stock rotation. Follow the manufacturer’s Safety Data Sheet for detailed storage and handling requirements.
    Shelf Life Shelf life is typically 24 months when stored in unopened original packaging under cool, dry conditions; verify with supplier.
    Application of Dow DOWLEX™ 2071D Linear Low Density Polyethylene

    In machine-grade pallet unitization film production, DOWLEX 2071D is processed on high-output cast film lines where the molten web is quenched against a polished chill roll before entering a secondary chill roll and winding section. The resin is a linear low density polyethylene produced with octene comonomer, selected because its nominal density of 0.918 g/cm³ and melt viscosity permit high draw ratios at film thicknesses between 18 µm and 30 µm without excessive transverse gauge variation. Single-screw extruders with L/D ratios from 24:1 to 30:1 and barrier-flight screws convey the melt to a coat-hanger die with a gap of 0.6 mm to 1.0 mm. On three-layer A/B/C pallet wrap lines, the core layer commonly contains 30 wt% to 70 wt% DOWLEX 2071D, while the cling layers are built from a lower-density metallocene LLDPE at 20 wt% to 35 wt% and a migratory tackifier at 0.5 wt% to 2.0 wt%; edge encapsulation with a higher-melt-strength LDPE at 5 wt% to 15 wt% of total extrudate is applied where neck-in exceeds approximately 25 mm. The chill roll is maintained at 15 °C to 25 °C, and an air knife or vacuum box positioned within 5 mm of the die line stabilizes the melt curtain at line speeds between 250 m/min and 600 m/min. Incoming resin moisture above 0.05 wt% and melt temperatures above 280 °C combine to increase oxidized gel formation, while drawing below 12 µm without adjusting air knife position can produce draw resonance and gauge bands. Compliance testing for pallet wrap mechanical performance uses ASTM D5748 for stretch retention and elongation, ASTM D5458 for cling force, and ASTM D374 Method C for thickness uniformity. Terminal formats include 23 µm and 25 µm machine-grade stretch film in 500 mm x 2400 m rolls and 8 µm to 15 µm pre-stretched hand rolls after 200% to 350% pre-stretch ratios.

    What governs the selection of 25 µm versus 38 µm cast silage wrap against oxygen ingress?

    The decision between 25 µm and 38 µm cast silage bale wrap is governed by oxygen transmission rate, puncture resistance during bale transport, and the required storage interval; 38 µm film is used where stacked bales experience sharp crop stalks and longer outdoor storage. DOWLEX 2071D is processed as the principal LLDPE phase in these films, with additive masterbatch loadings of 5 wt% to 12 wt% for UV stabilization and 8 wt% to 15 wt% for white pigmentation, because lower pigment loadings produce radiant heat gain that accelerates local oxygen permeation. The production line is a cast film configuration with an oscillating haul-off, a chill roll held at 20 °C to 30 °C, and corona treatment in the range of 38 mN/m to 44 mN/m to ensure adhesion of printing or lamination if required. A melt temperature window of 240 °C to 260 °C is maintained because temperatures above 265 °C with retained volatiles from pigment masterbatch can produce an oxygen transmission rate deviation greater than 6% from the nominal specification. Compliance assessment is performed under EN 13207, which covers tensile properties, tear strength, and UV stability for thermoplastic silage films; tensile measurements are conducted according to ISO 527-3 at a test speed of 500 mm/min. Terminal products include 25 µm x 750 mm x 1500 m round bale wrap, 38 µm x 750 mm x 1000 m heavy-duty wrap, and 1500 mm wide rollstock for high-density baling operations.

    Across fresh produce and bakery retail overwrap converting, DOWLEX 2071D is formed into thin-gauge cast film that requires low haze, controlled slip, and sufficient hot-tack for wrapping trays. The resin is extruded neat or in blends with up to 20 wt% LDPE to improve melt stability in thin-gauge drawing; slip and antiblock masterbatches are normally limited to 1 wt% to 3 wt% total because higher loadings raise haze above approximately 3% on 15 µm film. The process uses a polished chill roll at 15 °C to 25 °C, an in-line thickness gauge with automatic die adjustment, and corona treatment at 38 mN/m to 44 mN/m for printability. Compliance for food contact in the United States is established under FDA 21 CFR 177.1520, with olefin polymer provisions applicable when the film is used in contact with food; in the European Union, the film must comply with Regulation (EU) No 10/2011, including the overall migration limit of 10 mg/dm² and any specific migration limits for additives. Terminal formats include 12 µm to 18 µm film for retail produce bags, bakery overwrap, and butcher tray stretch packaging. The resin alone provides no oxygen or aroma barrier; shelf-life extension beyond a few days requires lamination to a barrier substrate or modified-atmosphere packaging.

    Regulation/StandardTest/ClauseLimit/Condition
    FDA 21 CFR 177.1520Olefin polymers for food contactCompliant when used in accordance with conditions of use
    Regulation (EU) No 10/2011Overall migration into food simulants10 mg/dm²
    ISO 527-3Tensile properties of filmReported at 23 °C, 500 mm/min
    ASTM D1003Haze of transparent film≤ 3% for 15 µm retail film

    Extrusion lamination bond strength and substrate compatibility limits

    In extrusion lamination protective film structures, DOWLEX 2071D is drawn from a flat die into a nip formed by a chilled steel roll and a pressure roll, where it is combined with pre-treated substrates such as paper, nonwoven, or pre-corona-treated polypropylene. The formulation for this process is generally a neat resin or a blend containing up to 30 wt% LDPE to reduce neck-in and improve edge stability; oxidative adhesion promoters are not required for paper, but corona treatment of the substrate to 38 mN/m to 42 mN/m must be maintained, because lower surface energies reduce adhesion below the minimum required for fibre-tear bonds. Melt temperature is held between 240 °C and 275 °C, and the chill roll is maintained at 15 °C to 20 °C to prevent blocking while preserving optical clarity. Adhesion testing is conducted according to ASTM F904 for heat-sealed or laminated flexible materials, with visual confirmation of fibre tear as the acceptance criterion. Terminal products include low-tack surface protection film for stainless steel and aluminium composite panel processing, temporary enclosure films, and extruded liners for bulk packaging. Published data for adhesion of DOWLEX 2071D to specifically corona-treated cross-laminated nonwoven is limited; converters must run a designed experiment across corona watt density and nip roll pressure before full commercial production.

    Cold-chain distribution of frozen proteins and ice cream uses cast films that must retain dart impact strength at -25 °C and resist puncture from irregular frozen product. DOWLEX 2071D is utilized in these structures at 60 wt% to 90 wt% of the film mass, with the balance composed of a lower-density VLDPE or mLLDPE grade for additional impact strength and 0.5 wt% to 2.0 wt% slip/antiblock masterbatch to control unwinding tension in subzero storage. The production process is high-output cast film extrusion with a chill roll temperature of 15 °C to 25 °C and film gauge from 20 µm to 35 µm; slit widths are configured for vertical form-fill-seal lines and pouch converters. Compliance with food contact is verified under FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011 for the finished food package, while low-temperature impact resistance is characterized by ASTM D1709 Method A and tensile properties by ISO 527-3 at 23 °C and -20 °C. Terminal products include freezer-grade pouches, bag-in-box liners for frozen sauces, and converted rollstock for ice cream packaging. The operational boundary is that corona treatment above 44 mN/m combined with low ambient humidity can create static discharge during winding, requiring active static elimination and controlled plant humidity above 40% RH.

    When DOWLEX 2071D is used as a sealant web in multi-material laminates

    When DOWLEX 2071D is used as a cast sealant web in multi-material laminates, its contribution is judged by hot-tack strength, seal initiation temperature, and the absence of seal contamination during vertical form-fill-seal operation. The sealant layer is formed as a cast film or direct extrusion lamination and is commonly constructed with 100 wt% DOWLEX 2071D or a blend containing up to 15 wt% metallocene VLDPE to lower heat-seal initiation below 90 °C; antiblock masterbatch is limited to 0.5 wt% to 1.5 wt% because higher filler levels reduce hot-tack. The converting process requires a corona-treated surface at 38 mN/m to 40 mN/m before lamination to the barrier ply, with lamination nip temperature controlled to prevent loss of orientation in the cast layer. Compliance standards include ASTM F1921 for hot-tack assessment, ASTM F88/F88M for seal strength, and FDA 21 CFR 177.1520 or Regulation (EU) No 10/2011 where the laminate contacts food. Terminal products include stand-up pouches, flow-wrap confectionery packs, and pre-made bags for frozen convenience foods. Seal window narrowing below 10 °C is observed when the sealant web is contaminated with low-molecular-weight additive bloom; therefore, additive loadings above the stated maximum are not recommended for high-speed sealing lines.

    Free Quote

    Competitive Dow DOWLEX™ 2071D Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DOWLEX™ 2071D Linear Low Density Polyethylene is an ethylene-1-octene copolymer produced by a solution polymerisation process. The grade is positioned in the 0.920 g/cm³ density and 2.3 g/10 min melt-index segment of the LLDPE family, with the melt index determined at 190 °C and 2.16 kg. These two nominal indicators place the resin in a high-flow, low-density class normally directed toward thin-gauge cast film rather than blow moulding or pipe. The 1-octene comonomer introduces short-chain branches that depress crystallinity while preserving a comparatively high concentration of load-bearing tie molecules between lamellae. Published data for the complete molecular weight distribution and comonomer distribution of this specific commercial grade is limited, but the solution process and octene chemistry distinguish the material from butene-copolymer LLDPE grades. Primary uses include cast film for food packaging, industrial liners, stretch wrap, and lamination layers.

    What Distinguishes an Octene-Based LLDPE from Butene-Copolymer Grades?

    The difference is not solely the measured density. In a butene-copolymer LLDPE, the short-chain branch is an ethyl side group; in an octene-copolymer LLDPE, the side group is a hexyl branch. The longer branch is more effective at lowering density per unit of comonomer and at decoupling crystal thickness from tie-chain concentration. At a fixed density of 0.920 g/cm³, an octene grade can display higher dart impact and Elmendorf tear than a butene grade with otherwise similar melt index. Comparative data from the broader LLDPE literature indicate that dart impact may be 15–40% higher and machine-direction tear 20–50% higher for octene grades when evaluated on the same cast film line. This effect arises because the longer branch is excluded from orthorhombic polyethylene crystals and concentrates in the amorphous interlamellar region, where it participates in stress transfer. The high melt index of 2.3 g/10 min reduces molecular weight relative to lower-MI DOWLEX grades but still permits sufficient chain length for tie-chain development. By contrast, high-pressure LDPE contains long-chain branching, which provides strain-hardening behaviour and bubble stability in blown film but generally reduces tensile yield and thermal resistance compared with linear architectures. The selection rationale for DOWLEX™ 2071D therefore rests on thin-gauge cast film where optics, tear resistance, and output are simultaneous constraints.

    Processing of DOWLEX™ 2071D on cast film equipment usually follows single-screw extruder configurations with 30:1 to 33:1 L/D and barrier-flighted screws designed for LLDPE. Screw speeds and barrel temperature profiles are commonly set to produce a melt temperature of 232–260 °C at the die entry. On 90 mm extruders, stable outputs of 250–350 kg/h have been reported for comparable octene-LLDPE cast film lines, although output necessarily depends on die width, vacuum box configuration, and chill roll diameter. Die gaps in the range of 0.4–0.8 mm are typical. The high melt index of 2.3 g/10 min reduces head pressure relative to lower-MI grades, but it also reduces melt strength; therefore processors often use a shorter air gap and a high-efficiency vacuum box to pin the melt curtain to the chill roll. Melt fracture can appear as surface haze or sharkskin at excessive output. The onset depends on the die land shear stress; for LLDPE, the critical shear stress at which sharkskin appears is often reported in the range of 0.1–0.14 MPa. Operators typically respond by raising melt temperature slightly, widening the die gap, or adding a small amount of polymer process aid. However, addition of fluoroelastomer process aid must be limited to avoid roll plate-out. Chill roll temperatures of 15–25 °C maintain optical clarity and reduce blocking, but at high line speeds the roll must have sufficient cooling capacity; otherwise film gauge becomes non-uniform and haze rises. Since DOWLEX™ 2071D is supplied as pellets, drying is generally not required before ordinary cast film operations. If sacks have been exposed to humidity above 60% RH for prolonged storage, pre-drying at 70–80 °C for 2–4 h with desiccant air can reduce moisture-related gels and surface defects.

    Film Property Ranges in Thin-Gauge Cast Evaluation

    The following table consolidates representative values for 25 µm film produced on a cast line. The values are not specification limits and do not replace a certificate of analysis. Variation arises from melt temperature, chill roll temperature, line speed, and die configuration. Standard designations identify the test method rather than impose a single standardized sample preparation protocol.

    PropertyMethodRepresentative Value
    Melt index, 190 °C/2.16 kgASTM D1238, ISO 1133-1:20222.3 g/10 min
    DensityASTM D1505, ISO 1183-1:20190.920 g/cm³
    Vicat softening temperatureASTM D1525101 °C
    Melting peak temperature, DSCASTM D3418122 °C
    Tensile strength at break, MDASTM D88228–35 MPa
    Tensile strength at break, TDASTM D88222–28 MPa
    Elongation at break, MDASTM D882600–750%
    Elmendorf tear strength, MDASTM D1922150–250 g
    Elmendorf tear strength, TDASTM D1922300–450 g
    Dart impact strength, 25 µmASTM D1709 Method A90–150 g
    Haze, 25 µmASTM D10033.0–5.5%
    Gloss at 45°ASTM D245770–85

    The Elmendorf tear directionality is characteristic of cast film orientation: transverse-direction values exceed machine-direction values because crystalline lamellae align in the machine direction during uniaxial draw. Dart impact performance is highly dependent on gauge uniformity; thin spots created by melt curtain instability lower the measured impact value and are often the first visible defect in production-scale trials.

    On production-scale cast film lines, the main failure modes associated with high-flow octene LLDPE are die-lip build-up, melt curtain resonance, and gauge variation at high draw ratios. Die-lip build-up is often observed as a white deposit at the die exit after extended runs; it can be minimised by maintaining a low die exit temperature, using die-lip cleaning cycles, and avoiding excessive low-molecular-weight additives in the resin or masterbatch. Melt curtain resonance appears as transverse thickness waves when the draw ratio is too high or the vacuum box does not stabilise the web. For DOWLEX™ 2071D, the melt index of 2.3 g/10 min allows high line speeds but increases sensitivity to air gap disturbances; setting the vacuum box slot 5–10 mm from the melt curtain and maintaining an even exhaust flow reduces the defect. Batch-to-batch variance in solution-process LLDPE is generally controlled, with typical melt-index variation of about ±0.1 g/10 min and density variation of ±0.001 g/cm³. Converters that blend regrind must control particle size and moisture; film produced with more than 20–25 wt% off-spec regrind can show higher gel counts unless the regrind is finely ground and blended with virgin pellets. Oxidative induction time by ASTM D3895 at 200 °C is often used for incoming QC; published typical OIT values for this grade are limited but should exceed 20 min if the primary antioxidant package remains intact. Additive packages should avoid strongly acidic or amine-based chemistries that can degrade the phenolic antioxidant system and shift colour during long residence time at high melt temperature. Peroxide masterbatches used for reactive extrusion should be limited because the residual unsaturation of LLDPE is low and excess peroxide can produce crosslinked gels without measurable melt strength gain.

    When a 2.3 MI Octene Grade Replaces a Lower-Melt-Index Butene Grade in Cast Film

    Replacement of a 1.0 g/10 min butene-copolymer LLDPE with DOWLEX™ 2071D alters process response in three measurable ways. First, head pressure at equivalent screw speed falls because the higher melt index reduces apparent viscosity; operators may need to reset screw speed, barrel zone setpoints, and downstream nip tension to avoid gauge variation. Second, melt strength decreases, so the melt curtain must be pinned to the chill roll more aggressively; otherwise edge flutter and draw resonance appear. Third, the mechanical property balance changes: for the same film gauge, dart impact and low-temperature toughness can be maintained or improved by the octene architecture, while low-temperature flexibility is preserved down to approximately −30 °C depending on gauge and additive formulation. In direct comparisons, a DOWLEX™ 2071D film may show a slightly lower coefficient of friction when slip and antiblock masterbatches are included; published data for the exact coefficient of friction of this grade is limited and depends strongly on additive type, concentration, and bloom time. If the target application is heavy-duty sacks or thick liners, replacing a lower-MI grade with 2071D may reduce load-bearing capability in the machine direction; however, if the target is thin-gauge high-clarity packaging film, the higher flow permits line speed increases and gauge reduction. The grade is not recommended as a direct substitute for LDPE in applications that require high melt strength, such as large-part blow moulding or thick sheet, because the octene-LLDPE architecture does not provide the strain-hardening behaviour of long-chain branching. Typical strain-hardening coefficients for linear LLDPE are low compared with autoclave LDPE; published data for this specific grade is limited, but the processing limitations are observable on standard film lines.

    Compliance Evidence Under 21 CFR and EU Food-Contact Directives

    Compliance for food-contact and industrial packaging is not established by the resin data sheet alone; it requires confirmation of the final article under intended conditions of use. Migration kinetics in the polyolefin matrix depend on film thickness, food simulant, and time-temperature conditions. The following matrix summarises primary regulatory references that converters may apply to polyethylene food-contact films. It is not a declaration of conformity. Values must be verified through migration testing or supplier certification for the specific thickness, temperature, and food simulant.

    Regulatory referenceScopeOperational boundary
    U.S. FDA 21 CFR 177.1520Olefin polymers in contact with food, subject to density and maximum extractable fraction limits.Compliance depends on final density, additive package, and food type; not all conditions of use are automatically covered.
    EU Regulation (EU) No 10/2011Plastics for food contact; overall migration limit of 10 mg/dm² for food contact surfaces.Specific migration of octene and additives must be below the limits in Annex I and Annex II.
    REACH (EC) No 1907/2006Registration, evaluation, authorisation, and restriction of chemicals in the EU.No substance of very high concern may exceed 0.1 wt% in the article.
    RoHS Directive 2011/65/EURestriction of lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE in electrical and electronic equipment.Not normally applicable to bare PE packaging, but relevant if film becomes part of an electrical or electronic article.

    In three-layer cast stretch-film structures, DOWLEX™ 2071D is commonly evaluated in the core or back layer where its 2.3 g/10 min melt index reduces extruder torque and permits thin-gauge down-gauging. Cling layers remain based on lower-melt-index LLDPE modified with polyisobutylene or ultra-low-density polyethylene. Lamination films for flexible packaging also use this grade as a sealant or bulk layer because the octene architecture retains seal integrity at temperatures below those required for butene-copolymer films; seal initiation temperatures for comparable octene-LLDPE grades are often observed in the range of 90–105 °C on laboratory hot-tack equipment, but published data for DOWLEX™ 2071D in specific laminate structures is limited. In blown film processes, this grade is less common due to reduced bubble stability; if used, it is typically blended with up to 70 wt% of a lower-MI LLDPE or LDPE to maintain bubble oscillation resistance. The operational boundaries that govern use include melt temperature below 275 °C to limit oxidative degradation, chill roll temperature above dew point to prevent condensation defects, and die gap settings wide enough to avoid shear-induced melt fracture. Final food-contact suitability must be validated on the finished article under the intended food type, temperature, and duration.