Dow Dowlex 2070g Linear Low Density Polyethylene

Dow DOWLEX™ 2070G Linear Low Density Polyethylene

    • Product Name: Dow DOWLEX™ 2070G Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 809190
    Comonomer Octene-1
    Density 0.920 g/cm3
    Meltindex 0.70 g/10 min
    Meltflowratio 8.0
    Meltingpoint 124 °C
    Vicatsofteningpoint 96 °C
    Tensilestrengthatyield 10 MPa
    Tensilestrengthatbreak 30 MPa
    Elongationatbreak 800%
    Flexuralmodulus 240 MPa
    Dartimpactstrength 150 g
    Elmendorftearstrengthmd 300 g
    Elmendorftearstrengthtd 500 g
    Haze 10%
    Gloss 60%
    Coefficientoffriction 0.2
    Blocking 50 g

    As an accredited Dow DOWLEX™ 2070G Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DOWLEX™ 2070G Linear Low Density Polyethylene is supplied in 25 kg polyethylene bags, typically palletized for industrial storage and transport.
    Container Loading (20′ FCL) 20′ FCL loading for Dow DOWLEX™ 2070G LLDPE: 25 kg bags, palletized, shrink-wrapped, securely stowed for safe ocean transport.
    Shipping Dow DOWLEX™ 2070G LLDPE is generally shipped as non-hazardous resin pellets in 25 kg bags, octabins, bulk bags, or bulk trucks/railcars. Transport in clean, dry, covered vehicles at ambient conditions, away from moisture, heat, sunlight, and ignition sources. Follow the SDS and local regulations.
    Storage Store Dow DOWLEX™ 2070G Linear Low Density Polyethylene in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers closed or use clean silos; protect from moisture, contamination, and physical damage. Avoid strong oxidizers. Maintain good housekeeping to prevent pellet spills and slipping. Follow local regulations and the manufacturer’s SDS.
    Shelf Life Recommended shelf life is 24 months when stored unopened in original packaging under cool, dry conditions, away from direct sunlight.
    Application of Dow DOWLEX™ 2070G Linear Low Density Polyethylene

    Dow DOWLEX 2070G Linear Low Density Polyethylene is a solution-polymerised film resin supplied in pellet form. Its nominal density is 0.920 g/cm³ when measured under ISO 1183-1, and its melt flow rate is 1.0 g/10 min at 190 °C/2.16 kg under ISO 1133-1. The polymer is processable on mono- and coextrusion blown-film lines within a gauge range of approximately 20–200 µm. Field data from single-screw extruders with barrier screws of L/D 30:1 to L/D 36:1 indicate that melt temperatures below 190 °C can initiate shark-skin melt fracture in thin-gauge webs, while prolonged stock temperatures above 240 °C increase oxidation risk and gel formation. The following application scenarios cover heavy-duty industrial sacks, frozen-food pouches, agricultural silage and greenhouse structures, flexible intermediate bulk container liners, and bag-in-box liquid liners.

    In heavy-duty industrial sack production, DOWLEX 2070G is typically used as the structural component of a three-layer coextruded web of 80–140 µm finished thickness. Layer ratios of 30/40/30 or 25/50/25 are common on lines equipped with three 60–90 mm single-screw extruders. In the outer skins, 15–25 wt% LDPE with a melt index of 0.25–0.8 g/10 min is blended into DOWLEX 2070G to raise melt strength and maintain bubble stability at a blow-up ratio of 2.5:1–3.0:1. The core layer may contain 80–90 wt% DOWLEX 2070G to retain dart impact and tear strength. Anti-block masterbatch is used in the skins at 0.5–1.2 wt%, and erucamide slip concentrate is held at 0.2–0.5 wt% in the inner skin. Barrel temperatures are set from 170 °C to 205 °C, with die zones at 195–215 °C. A die gap of 1.8–2.4 mm is maintained, with internal bubble cooling air at 15–25 °C and a frost line height of 500–800 mm. At screw speeds of 55–75 rpm on a 90 mm grooved-feed extruder, output typically falls between 150 and 200 kg/h, and melt pressure after the screen pack commonly ranges from 280 to 380 bar. A pressure drop above 420 bar generally indicates screen blockage or an excessively high-viscosity LDPE fraction. Plant operators report that raising DOWLEX 2070G above 85 wt% in a monolayer structure at BUR 2.8:1 can produce bubble flutter, while reducing LDPE below 10 wt% may increase back pressure by 5–12 bar. Converted sacks are heat sealed at 135–160 °C jaw temperatures and are used for 25–50 kg fills of polymer pellets, technical-grade fertilizers, and mineral additives. Tensile properties are tested under ASTM D882 or ISO 527-3, and dart impact is determined using ASTM D1709 Method A at thinner gauges or Method B above 70 µm. Export packaging compliance is assessed under the EU Packaging and Packaging Waste Directive 94/62/EC for heavy-metal limits, and REACH 1907/2006 Article 33 applies only when an SVHC content exceeds 0.1 wt%.

    Which migration and seal-strength limits bind DOWLEX 2070G when converted into frozen-food pouches?

    Conversion of DOWLEX 2070G into frozen-food pouches requires a two- or three-layer coextrusion with a low-seal-initiation skin containing additional metallocene LLDPE or polyolefin plastomer. The seal layer commonly contains 70–85 wt% DOWLEX 2070G and 15–30 wt% of a lower-density LLDPE with a melt index of 0.5–2.0 g/10 min. Slip and anti-block loadings are restricted to 0.05–0.15 wt% for organoleptic control in contact-sensitive frozen vegetable and seafood applications. Blown-film conversion is performed at 185–210 °C melt temperature, a die gap of 1.2–1.8 mm, and a blow-up ratio of 2.2:1–2.8:1. The upper melt-temperature limit of 215 °C prevents thermal decomposition of slip additives and reduces odour carry-over into packaged products. Food-contact compliance rests on FDA 21 CFR 177.1520(c) olefin polymer requirements and Regulation (EU) 10/2011 Annex I. Overall migration is controlled below 10 mg/dm² or 60 mg/kg under the simulant and storage conditions specified for refrigerated and frozen foods. Specific migration of slip additives must comply with the positive-list restrictions in Regulation (EU) 10/2011. Seal strength is measured under ASTM F88/F88M, and low-temperature performance is evaluated after conditioning at -20 °C or -40 °C using ASTM D1709 dart impact and ASTM D1922 Elmendorf tear. Vertical form-fill-seal field failures typically appear as seal delamination when the seal bar temperature exceeds 175 °C or when the seal layer carries more than 0.2 wt% of an incompatible anti-block additive. Amine-based slip or antistatic additives are excluded from the seal layer because they can contaminate metal seal jaws. Published data for this specific DOWLEX 2070G construction in frozen-food pouches is limited; the processing windows given here are derived from standard industrial coextrusion practice.

    Three-layer silage film: HALS addition thresholds, EN 13206 tensile retention, and the 220 °C residence-time cap

    Agricultural silage and greenhouse film based on DOWLEX 2070G typically uses a three-layer configuration with a layer ratio of 20/50/30 or 25/50/25. The core layer contains 75–85 wt% DOWLEX 2070G and 15–25 wt% metallocene LLDPE for puncture and dart-impact retention after field exposure. Outer layers are loaded with HALS-based UV stabilizer masterbatch at 0.8–1.5 wt% total film weight, corresponding to active HALS concentrations of 0.3–0.6 wt%. For black silage covers, carbon black masterbatch is added at 2.0–2.5 wt%. White greenhouse webs generally substitute titanium dioxide concentrate at 5–8 wt% to raise reflectivity and suppress UV decay. The UV-stabilised outer layer is not used as the seal skin because high silica or TiO₂ loadings reduce heat-seal strength under ASTM F88/F88M. A die gap of 2.0–2.4 mm, BUR 2.8:1–3.5:1, and melt temperatures of 205–225 °C are used on high-stalk blown-film lines with die diameters of 300–450 mm. The practical residence-time cap is 220–225 °C; above 235 °C HALS additives can volatilise or oxidise before the web exits the die, causing UV retention after 1,000 hours in QUV ageing to fall below the EN 13206 tensile-retention requirement. Thickness ranges from 25 µm for greenhouse tunnel film to 180–200 µm for round bale wrap. End products include bale wrap, clamp silage covers, and low-tunnel ventilation films. Compliance for the EU market is assessed against EN 13206 for thermoplastics silage films and Regulation 1907/2006 for UV and pigment additives; REACH Annex XVII restrictions apply to certain coloured mulch-grade formulations. Field losses in bale wrap are most often traced to insufficient HALS dispersion, visible as microgel streaks on 120 µm web, which can be controlled by maintaining melt pressure above 250 bar on the outer-layer extruder.

    Layer configuration for DOWLEX 2070G agricultural silage film
    LayerLayer ratio (%)DOWLEX 2070G (wt%)Metallocene LLDPE (wt%)UV stabilizer masterbatch (wt%)Carbon black masterbatch (wt%)
    Outer2080.017.51.51.0
    Core5082.517.500
    Inner3079.017.51.52.0

    For petrochemical powder and mineral filler applications, DOWLEX 2070G is converted into flexible intermediate bulk container liners with a finished gauge of 70–120 µm. A monolayer formulation uses 95–98 wt% DOWLEX 2070G and 2–5 wt% of an antistatic masterbatch where the end user requires surface resistivity below 10^9 Ω/sq measured by ASTM D257. Non-antistatic versions retain surface resistivity above 10^14 Ω/sq and are limited to non-flammable powders without dust explosion hazards. Blown-film conversion uses a die gap of 2.0–2.5 mm, blow-up ratio 2.0:1–2.5:1, and melt temperature 190–215 °C. The tube is collapsed to 650–1,100 mm layflat width and converted into gusseted liners with heat-sealed bottom seams at 135–155 °C. Insertion into FIBC outer shells requires the seam to withstand filling of 500–1,500 kg bulk powder without tearing; seam integrity is therefore tested by ASTM D882 tensile and a drop test derived from ISO 21898. The main process bottleneck reported from filling stations is liner blocking in humid warehouses. Silica anti-block is increased to 0.5–1.0 wt% when warehouse relative humidity exceeds 70%. Conductive liners are validated for surface resistivity stability after 30 days storage at 23 °C/50% RH, because non-amine migratory antistatic agents can become surface-depleted. Compliance for export to the EU requires packaging heavy-metal limits under Directive 94/62/EC; direct food-powder contact requires the food-contact declarations described in the frozen-food scenario.

    When DOWLEX 2070G is drawn into bag-in-box liquid liners, flex-crack testing controls the layer ratio

    Bag-in-box liners for non-carbonated liquid concentrates and foodservice syrups are produced from coextruded blown film in 100–150 µm thickness. The seal layer is a blend of 60–70 wt% DOWLEX 2070G with 30–40 wt% polyolefin plastomer or lower-density LLDPE to reduce heat-seal initiation to 85–105 °C. The outer layer contains 80–90 wt% DOWLEX 2070G and 10–20 wt% LDPE for abuse resistance and die-cutting stiffness. Process conditions include a die gap of 1.6–2.0 mm, BUR 2.0:1–2.5:1, and melt temperature 185–205 °C. Flex-crack resistance of the finished liner is tested under ASTM F392, with survival of 10,000 cycles without pinhole formation commonly specified for liquid packaging. If the outer-layer DOWLEX 2070G fraction exceeds 90 wt%, transverse-direction elongation after flexing can decline due to high orientation in the frost-line zone. The liners are fitted with spout flanges and sealed at 120–140 °C. Food-contact compliance is verified under FDA 21 CFR 177.1520(c) and EU 10/2011, with particular attention to total migration of adhesive or tie additives used in spout welding. End products include 2–20 L bag-in-box wine and syrup packages. Published data for this specific DOWLEX 2070G configuration in liquid packaging is limited; the flex-crack and seal-initiation targets reflect generic LLDPE bag-in-box specifications from converter test protocols.

    Free Quote

    Competitive Dow DOWLEX™ 2070G Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2070G Linear Low Density Polyethylene is a solution-polymerised ethylene/1-octene copolymer in the LLDPE family. The grade is defined primarily by a nominal melt flow rate of 7.0 g/10 min at 190°C under 2.16 kg load, measured to ASTM D1238 or ISO 1133-1:2022, and a nominal density of 0.920 g/cm³ by ASTM D792 or ISO 1183-1:2019. This combination places DOWLEX 2070G in the high-flow segment of injection moulding grades rather than blown film or pipe extrusion. The linear backbone with C6 short-chain branches from 1-octene produces a more regular crystallite structure than high-pressure LDPE at equivalent density; the practical result is higher environmental stress crack resistance, as indicated by the >1000 h result under ASTM D1693 in 100% Igepal, and improved low-temperature toughness. Unlike a high-pressure LDPE of similar density, DOWLEX 2070G shows less shear thinning and reduced die swell, which affects gate pressure requirements and dimensional stability in multi-cavity tools.

    The melt-flow value of 7.0 g/10 min is a single-point measurement at a nominal wall shear stress of approximately 1.94 × 10⁴ Pa and an apparent shear rate below 20 s⁻¹. It is therefore not a reliable predictor of viscosity at injection moulding shear rates of 10³–10⁴ s⁻¹. However, the MFR is useful for distinguishing DOWLEX 2070G from lower-flow DOWLEX grades intended for film or rotational moulding, and for verifying batch-to-batch consistency in incoming resin release testing.

    What published physical properties are used for load-bearing part selection?

    The following representative values are drawn from manufacturer-published grade data and should be verified against the certificate of analysis for each lot. They are single-point data for natural resin, not guaranteed values for coloured, regrind-containing, or additive-modified compounds.

    PropertyTest methodNominal valueUnit
    Melt flow rate, 190°C/2.16 kgASTM D1238 / ISO 1133-1:20227.0g/10 min
    DensityASTM D792 / ISO 1183-1:20190.920g/cm³
    Flexural modulus, 2% secantISO 178 / ASTM D790260MPa
    Tensile yield stressISO 527-2 / ASTM D63811MPa
    Elongation at breakISO 527-2 / ASTM D638>800%
    Vicat softening temperature, A120ISO 306 / ASTM D152596°C
    Melting peak temperature, DSCISO 11357-3122°C
    Notched Izod impact, 23°CISO 180/A / ASTM D256No break—
    ESCR, 100% Igepal, F50ASTM D1693>1000h

    The notched Izod value is not an intrinsic material property; it depends on notch radius, moulding conditions, and specimen thickness. For load-bearing parts in cold service, component-level drop-weight or instrumented puncture testing is required. Similarly, the ESCR result applies to a bent specimen under 100% Igepal at 50°C; it cannot be used to certify resistance to all detergents or sanitising chemicals.

    The density of 0.920 g/cm³ corresponds to a crystalline fraction of approximately 45–50% when calculated from the density of fully amorphous and fully crystalline polyethylene, but the actual value depends on cooling rate. In injection moulding, fast cooling at the mould surface produces a skin of lower crystallinity and higher toughness, while the core develops larger spherulites. This gradient means that flexural modulus from a 4 mm moulded specimen may be higher than the value obtained from a compression-moulded plaque. The 1-octene C6 branches disrupt crystallite thickness; the melting peak of 122°C by ISO 11357-3 is lower than the 130–135°C typical of HDPE, reflecting thinner lamellae in the linear low-density structure.

    Melt processing limits in reciprocating-screw injection moulding

    The accepted starting melt-temperature range for 7-MFR LLDPE on conventional reciprocating-screw machines is 200–250°C. A three-zone barrel profile of 180°C, 210°C, 230°C with a nozzle at 230°C is commonly used for wall thicknesses down to 1.5 mm. Below 200°C, the flow path may shorten, and weld lines in thin ribs can become visible. Above 250°C, thermal-oxidative degradation accelerates, especially when residence time exceeds 10 min at temperature. Degradation is observed as a reduction of elongation at break and an increase in yellowness index; batch-to-batch variance can be kept below ±5% in elongation if back pressure and screw-recovery speed are controlled.

    Mould surface temperature is maintained between 10°C and 40°C for cycle-time control. Higher mould temperatures improve weld-line elongation but can increase cycle time by 20–30% for wall thicknesses greater than 3 mm. Injection velocity should be set to keep flow-front shear stress above approximately 0.35 MPa on the tool surface; this reduces hesitation marks at ribs and bosses. However, excessive velocity causes gas trapping and burn marks at the end of fill, especially in unvented blind pockets. Back pressure of 50–100 bar hydraulic is typical; gravimetric feeders should maintain granulate bulk density within ±0.02 g/cm³ to avoid screw-recovery variation.

    On a 1500 kN clamping force injection moulding machine with a 45 mm diameter general-purpose screw and 20:1 L/D ratio, shot-weight variation should be controlled below 0.3% when the feed throat is kept at 20–40°C. If the tool contains hot-runner valve gates, the injection start should be delayed until the screw decompression is complete, otherwise stringing may occur. Large-area parts such as bin lids may require clamp tonnage above 2000 kN because LLDPE packing pressures of 50–70 MPa generate high opening forces at the parting line.

    Pre-drying is not usually required when the granulate remains in sealed original packaging below 60% relative humidity. If surface condensation is present, or if regrind above 15 wt% is added, desiccant drying at 60–70°C for 2 h is sufficient; temperatures above 80°C may cause granulate sintering in the hopper. Hot-runner manifolds should be set 10–20°C above the nozzle temperature, but the molten resin should not remain in the manifold for more than 15 min during stoppages.

    Reported application areas for this density and flow range include industrial containers, waste bins, storage totes, agricultural trays, housewares, closure bases, and thin-wall food-service articles. In detergent and aqueous chemical container applications, the grade is selected because the linear structure improves stress crack resistance under flexural load, but compatibility with each filling must be tested by ASTM D543 immersion or cyclic loading. For food-contact service, the resin can be used in accordance with FDA 21 CFR 177.1520 as an olefin polymer; the finished article must also satisfy overall migration limits under Commission Regulation (EU) No 10/2011 when sold into the European Economic Area. No claim of universal chemical compatibility is supported by the grade data; aggressive solvents, oxidising acids, and certain essential oils may swell or craze polyethylene at elevated temperature.

    When octene LLDPE replaces high-pressure LDPE or butene LLDPE in moulded articles

    Compared with high-pressure LDPE of similar density, DOWLEX 2070G generally exhibits higher tensile yield stress, around 11 MPa versus 8–10 MPa, and higher notched Izod impact at 23°C. The same linearity reduces shear thinning, so an existing tool designed for LDPE may require 10–20% higher injection pressure to maintain the same fill time if gate geometry is unchanged. Die swell is lower than LDPE, which can improve dimensional control of gates and parting lines but may require revised gate land lengths or new hot-runner needle settings. In thin-wall industrial containers, the higher ESCR of the octene LLDPE supports down-gauging in room-temperature service, but the part must be revalidated for top-load and drop impact under component-level testing according to ISO 6603-2 or equivalent.

    Against a butene LLDPE of equivalent density and melt flow, the octene comonomer gives longer C6 branches, which are more efficient at forming interlamellar tie molecules. This typically improves dart impact and reduces the low-temperature brittleness temperature. In processing, octene LLDPE may show slightly higher melt viscosity at high shear than the butene analogue; the practical difference is commonly less than 5% in injection pressure. Compared with high-density polyethylene of 0.950 g/cm³ density, the lower density of DOWLEX 2070G reduces flexural modulus by approximately 30–50% and lowers the heat deflection temperature; it is therefore not selected for hot-fill containers or applications requiring continuous service above 50°C under load. For these applications, a high-flow HDPE or polypropylene is more appropriate.

    Within the DOWLEX family, grades with melt flow rates below 3.0 g/10 min are generally preferred for blown film and rotational moulding because higher molecular weight is needed for bubble stability and melt strength. DOWLEX 2070G, at 7.0 g/10 min, is intended for injection moulding cycles where short gate freeze time and long flow length outweigh melt strength. In a direct comparison with a lower-MFR octene LLDPE of the same density, DOWLEX 2070G will typically exhibit lower notched Izod impact and lower ESCR, but a measurable reduction in cycle time and injection pressure.

    Compliance verification, food-contact status, and chemical inventory boundaries

    Regulatory status is not a single material property. For the United States, the base resin may be listed for food-contact use under FDA 21 CFR 177.1520 as an olefin polymer when it meets the density and extractables limitations in that section. The converter must verify that the specific lot, including any colourants, slip agents, or nucleators, does not change the compliance status. For Europe, finished articles are subject to Commission Regulation (EU) No 10/2011 overall migration and specific migration limits; the resin alone does not guarantee compliance. REACH registration and SVHC declaration should be confirmed from the supplier’s safety data sheet and extended SDS. RoHS Directive 2011/65/EU generally does not constrain lead, mercury, cadmium, and hexavalent chromium in unmodified polyethylene, but recycled or coloured compounds may require laboratory screening under IEC 62321.

    The operational boundary for this grade is defined by thermal and chemical resistance rather than by food-contact status alone. Continuous service under sustained tensile load should be limited to temperatures below the Vicat softening range; short-term excursions to 60°C in unstressed contact are possible, but creep modulus and environmental stress crack resistance decline rapidly above 40°C in active detergent solutions. The resin is incompatible with strong oxidising acids at elevated temperature, aromatic hydrocarbons, and halogenated solvents. In compounding with flame-retardant additives, halogenated systems may require stabiliser adjustment to prevent acid-catalysed chain scission during processing. Published data for structural foam or chemical foaming of this exact grade is limited; the processor must conduct its own drop-weight and creep testing.

    Top