Dow Dowlex 2056g Linear Low Density Polyethylene

Dow DOWLEX™ 2056G Linear Low Density Polyethylene

    • Product Name: Dow DOWLEX™ 2056G Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 725502
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Octene-1
    Density 0.920 g/cm³
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Melt Flow Ratio I10 I2 8.0
    Melting Point 123 °C
    Vicat Softening Point 105 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 800%
    Flexural Modulus 240 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Haze 10%
    Gloss 45 80
    Coefficient Of Friction 0.2

    As an accredited Dow DOWLEX™ 2056G Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DOWLEX 2056G LLDPE is supplied in 25 kg polyethylene-lined bags, palletized, or 1,000 kg bulk bags for transport.
    Container Loading (20′ FCL) 20′ FCL: 18 pallets of DOWLEX™ 2056G LLDPE, 55 x 25 kg bags per pallet, total net weight 24.75 MT.
    Shipping Dow DOWLEX™ 2056G Linear Low Density Polyethylene is a non-hazardous, non-regulated resin. It is shipped in 25 kg bags, palletized and stretch-wrapped, or in bulk. No UN number, hazard class, or packing group applies. Keep dry and avoid contamination, heat, and dust during transport.
    Storage Store DOWLEX™ 2056G in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep original containers or bags closed, clean, and palletized to prevent moisture, dust, and contamination. Avoid prolonged elevated temperatures and UV exposure. Maintain good housekeeping; prevent spills, which can create slipping hazards. Follow the supplier’s SDS and local regulations.
    Shelf Life Shelf life: 24 months from the date of manufacture when stored in original packaging at temperatures below 50°C (122°F).
    Application of Dow DOWLEX™ 2056G Linear Low Density Polyethylene

    On a cast film line producing pallet unitization wrap, DOWLEX 2056G is fed from a drying hopper only when ambient relative humidity exceeds 60%; at lower RH, the resin is processed directly from the silo. Melt flow rate measured at 190°C under 2.16 kg load is 1.0 g/10 min (ASTM D1238) and density is 0.920 g/cm³ (ASTM D792). The standard formulation for hand wrap uses 100 phr DOWLEX 2056G with 0.8–1.5 wt% of a cast-film sorbitan oleate tackifier masterbatch and 0.5–1.0 wt% of an LDPE-based anti-block concentrate containing 10% synthetic silica. The extruder on a 1,200 mm die has a 30:1 L/D barrier screw with a Maddock mixing section and a screen pack of 120/120/60 mesh. Barrel temperatures are set at 175°C, 215°C, 235°C, 245°C, and 250°C from feed to metering; die body and lip temperatures are held at 255°C. Melt temperature is 247°C at the adapter by an immersion thermocouple. Die gap is 0.45 mm for a final gauge of 0.017 mm. Chill roll temperature is maintained at 19°C, with an air knife pressure of 0.06 MPa and a pinned film wrap of 180°. At line speeds above 750 m/min, neck-in measured at the die exit exceeds 6% and edge trim rises above 12%, so line speed is derated to 680–720 m/min. The draw ratio at that speed is 3.8:1, below the documented draw-resonance onset for this melt at 4.2:1. The wound film is conditioned for 24 h at 23°C and 50% RH before puncture testing under ASTM D5748; values below 32 N in a 20 µm film indicate either insufficient tackifier dispersion or excessive thermal degradation from a worn screw. Peel cling under ASTM D5458 is controlled between 1.0 N/cm and 2.5 N/cm on the outside face; inside-face slip is maintained at a coefficient of friction below 0.4 under ISO 8295 to allow pallet-layer separation. Terminal products include pre-stretched hand pallet wrap with 200% mechanical pre-stretch and machine wrap for automatic rotating ring wrappers.

    What Limits Heat-Seal Initiation in Thin Lamination Sealant Webs?

    In solventless lamination for snack packaging, DOWLEX 2056G is converted into 25–35 µm cast films used as the sealant web against biaxially oriented polypropylene or polyethylene terephthalate. The resin is blended with 2–3 wt% of a low-density polyethylene masterbatch containing 5% erucamide and 3–5 wt% of an anti-block concentrate with 20% natural silica. A three-layer coextrusion line with a feedblock and 40/30/20 layer distribution positions DOWLEX 2056G in the sealant layer, while the core uses a high-pressure LDPE with density 0.923 g/cm³. The sealant layer is processed at melt temperature 242°C and the die gap is 0.50 mm; the chill roll is set at 18°C to reduce sealant-surface haze. Heat-seal initiation temperature measured at 0.5 N/25 mm peel force under ASTM F88 is reported between 105°C and 110°C on a 30 µm film; the exact value depends on erucamide bloom density and oxidation level on the seal surface. Hot tack strength under ASTM F1921 drops below 1.0 N/25 mm when sealing bar temperature exceeds 135°C, limiting the sealing window on high-speed vertical form-fill-seal machines that run at 120 cycles/min. If the sealant layer is diluted with more than 20% of a high-density polyethylene to reduce elongation, seal initiation shifts above 112°C and the film becomes unusable for cold-seal overprint applications. Food-contact compliance is established through FDA 21 CFR 177.1520(c) for the base polyolefin and through EU Regulation (EU) No 10/2011 migration testing with simulant D for fatty matrices; the final laminate must show overall migration below 10 mg/dm². Terminal products include stand-up pouches for dried fruit, flow-wrap film for muffins, and snack bar wrappers where the LLDPE sealant web is reverse-printed and solventlessly laminated.

    When Silage Wrap Must Maintain Tear Resistance Above 70 N/mm After 400 h UV Weathering

    Agricultural bale wrap is produced on a five-layer blown film line with die diameter 250 mm and blow-up ratio 2.5:1. The full-layer formulation uses 70–85 wt% DOWLEX 2056G, 10–20 wt% of a metallocene plastomer or EVA with vinyl acetate content 14%, 2–4 wt% of a green or white masterbatch containing 10% hindered amine light stabilizer, and 1.5–2.5 wt% of a polyisobutene tackifier masterbatch in the cling layers. The outer surfaces receive an additional 1,500 ppm HALS and a benzotriazole UV absorber based on total film weight, while the core layer is kept free of migratory tackifier to prevent interlayer bleed. The extruder zone temperatures are 170°C, 190°C, 210°C, 220°C, and 225°C; die temperature is 228°C; melt pressure before the screen pack must remain below 380 bar to avoid gel formation from masterbatch carrier degradation. Film gauge is set at 25 µm for round bale silage wrap and 30 µm for high-moisture rye silage, with total thickness tolerance ±4%. Cling force under ASTM D5458 is maintained at 1.2–2.0 N/cm on both surfaces to ensure field adhesion at 4°C. Tear resistance parallel to machine direction is measured under ASTM D1004; the film is accepted only if MD tear exceeds 70 N/mm after 400 h of accelerated weathering under ISO 4892-2 UV-A 340 nm at 60°C black panel temperature. If the EVA content exceeds 20%, oxygen transmission under ASTM D3985 at 23°C and 0% RH falls below 8,000 cm³/m²·d·atm but tear resistance and film toughness after winding are compromised. Terminal products include 750 mm wide bale wrap rolls for round balers and 500 mm wrap for square bale tubes.

    Application segmentPrimary test standardControlled parameterTypical line acceptance boundary
    Pallet stretch filmASTM D5748puncture resistance32 N at 20 µm
    Lamination sealant webASTM F88heat-seal initiation at 0.5 N/25 mm105–110°C
    Silage bale wrapASTM D1004machine-direction tear after 400 h UV≥70 N/mm
    Frozen food VFFS filmASTM D1709Adart impact at -18°C≥150 g at 60 µm

    In blown film conversion for heavy-duty shipping sack liners and FIBC internal liners, DOWLEX 2056G is dry-blended with 15–25 wt% high-pressure LDPE and 2–3 wt% of a processing aid masterbatch containing 2% fluoroelastomer. The line is a single-layer/single-station extruder with 65 mm screw diameter and 28:1 L/D; die diameter is 350 mm, die gap is 1.8 mm, and blow-up ratio is 2.8:1. The frost line is maintained at 550 mm above the die by external air ring pressure of 0.5 MPa, yielding a final film thickness of 65 µm for industrial sacks. Melt temperature is measured at 235°C; output is derated when melt pressure exceeds 420 bar at the screen changer, which occurs after 8–10 h of continuous operation with recycled edge trim above 20 wt%. The film is tested for Elmendorf tear under ASTM D1922; machine-direction tear below 350 gf at 65 µm indicates excessive gel content or polymer degradation. Puncture resistance under ASTM D5748 must exceed 180 N for bulk bag liners used in mineral powder transport; seal strength under ASTM F88 after side welding at 150°C and 0.3 MPa jaw pressure must exceed 25 N/25 mm. Final products include heavy-duty shipping sacks for polymer granules, FIBC liners for construction chemicals, and industrial liners for post-consumer resin collection.

    Deep-Freeze Puncture Resistance in Irregular-Shaped Frozen Vegetable Packaging Film

    For vertical form-fill-seal packaging of frozen broccoli and mixed vegetables, DOWLEX 2056G is converted into a 50–70 µm blown film with a three-layer structure. The structure is 35% DOWLEX 2056G in the outer layers and 30% in the core, together with 10% high-pressure LDPE and 5% slip/anti-block masterbatch. The film is processed on a high-speed blown film line at melt temperature 210°C, with die gap 1.2 mm, blow-up ratio 2.2:1, and frost line height 300 mm. Low-temperature impact resistance is tested under ASTM D1709A at -18°C after 7 days conditioning in a deep-freeze chamber; the acceptance level is ≥150 g for a 60 µm film. Sealing through frost and condensation is evaluated under ASTM F88 at -5°C jaw temperature; seal strength must remain above 18 N/25 mm despite ice crystal formation on the sealant surface. If the line speed exceeds 85 m/min, the film gauge variation measured by online capacitance gauge exceeds ±6%, causing puncture failures at sharp broccoli floret tips. The frozen food converter uses 5–8 N of back tension on the unwind brake to reduce film stretching during registration; the resin’s low elastic recovery at -25°C prevents misregistration. Terminal products include 500 g and 1 kg pillow packs for frozen vegetables, boil-in-bag pouches for rice, and institutional food service packs.

    Post-Consumer Recyclate in the Core Does Not Forgive Cling Layer Dilution

    Coextruded cast stretch film with post-consumer recyclate places DOWLEX 2056G in the two external cling layers, while the core contains 30–50 wt% of LLDPE-based PCR with melt flow rate 0.7–1.2 g/10 min. The layer distribution is 10/80/10 for A/B/A structures or 15/70/15 when higher cling is required. The core is fed through a separate extruder with a vented barrel and 40:1 L/D to devolatilize residual moisture; melt temperature in the core is kept below 240°C because PCR with oxidized polyolefin fractions degrades above 245°C. The external DOWLEX 2056G layers are processed at 250°C to promote tackifier dispersion. Final film gauge is 12–20 µm; the cast line runs at 600–700 m/min with die gap 0.50 mm and chill roll temperature 20°C. Gel contamination from PCR is controlled by a continuous screen changer with 80/80/40 mesh pack and by a melt gear pump upstream of the die. Film break rate is monitored over a 24 h run; a break rate above 1.0 breaks/100 km triggers a reduction in PCR content to 30 wt% or an increase in core extruder first-zone barrel temperature to 190°C. Cling force under ASTM D5458 must remain at 1.0–1.8 N/cm; puncture under ASTM D5748 must exceed 28 N at 15 µm. Terminal products include machine stretch film with 30% recycled content, hand wrap for e-commerce parcel bundling, and pallet wrap certified under the EuCertPlast audit scheme.

    Free Quote

    Competitive Dow DOWLEX™ 2056G Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2056G Linear Low Density Polyethylene is an ethylene/1-octene copolymer produced by a solution polymerization route and supplied as pelletized reactor-grade resin. The material is specified for heavy-duty sacks, freezer film, carrier bags, laminating film, and coextruded seal layers where a combination of density, melt index, and comonomer type is used to balance toughness and processability. Melt index is 1.0 g/10 min at 190 °C/2.16 kg using ASTM D1238 or ISO 1133-1:2022, and density is 0.920 g/cm³ using ASTM D792 or ISO 1183-1:2019. Differential scanning calorimetry to ISO 11357-3:2018 gives a melting peak near 122 °C. The resin contains 1-octene as the comonomer, resulting in C6 short-chain branches that differentiate it from 1-butene LLDPE and from long-chain-branched high-pressure LDPE.

    PropertyTest methodRepresentative value
    Melt index (190 °C/2.16 kg)ASTM D1238 / ISO 1133-1:20221.0 g/10 min
    DensityASTM D792 / ISO 1183-1:20190.920 g/cm³
    ComonomerSupplier specification1-octene
    Melting peak (DSC)ISO 11357-3:2018122 °C

    The values in Table 1 are representative data from the manufacturer, not specification limits. Lot-to-lot variation is controlled under the supplier’s ISO 9001 system, and converters should verify actual certificates of analysis before qualification.

    What distinguishes 1-octene solution LLDPE from conventional butene-based grades?

    The primary structural difference lies in comonomer branch length and intermolecular uniformity. 1-Octene introduces a C6 branch that disrupts crystallinity while maintaining chain extension between lamellae; 1-butene introduces a shorter C2 branch. At equivalent density and melt index, the octene-based resin can achieve a higher tie-chain concentration, which translates into different film mechanical response when tested by ASTM D1709A and ASTM D1922. The solution polymerization process used for DOWLEX 2056G also yields a narrower composition distribution than conventional Ziegler-Natta gas-phase butene copolymers. Composition distribution breadth can be characterized by temperature rising elution fractionation or crystallization analysis fractionation; published data for this specific configuration is limited, but the performance differences are consistent with reduced low-molecular-weight, high-comonomer fractions that contribute to blocking, extractables, and weak seal surfaces.

    Relative to butene-based LLDPE at the same thickness, the 1-octene system is typically specified for higher dart impact and transverse-direction Elmendorf tear values. The effect is most pronounced in films below 50 µm, where tie-chain population becomes the limiting factor. Relative to high-pressure LDPE, DOWLEX 2056G lacks long-chain branching, so melt extension viscosity and bubble stability are lower. The processing response therefore requires different air-ring and die-gap settings than an LDPE reference grade.

    At 0.920 g/cm³, the resin contains sufficient short-chain branch content to lower crystallinity and increase toughness. Octene branches are excluded from the orthorhombic crystal lattice; during crystallization, branch points concentrate in the amorphous phase and increase the probability of multiple lamellae bridged by the same chain. This mechanism is measured indirectly by dynamic mechanical analysis and by the temperature dependence of storage modulus. The result is a resin that is not a physical blend of LDPE and HDPE but a reactor-grade copolymer with controlled branch distribution.

    On production lines using grooved-feed extruders of L/D 24:1 to 30:1, melt temperatures from 190 °C to 240 °C are used for the resin. Barrier screws with mixing sections are preferred because the linear resin generates higher melt pressure at equivalent screw speed than long-chain-branched LDPE. Die gap is a threshold parameter: values below 1.5 mm increase die-land shear stress and can induce sharkskin melt fracture at moderate output; values above 2.5 mm may reduce orientation and degrade gauge uniformity in thin films. Blow-up ratios from 2.0:1 to 3.0:1 and frost-line heights of 3–5 die diameters are standard starting points for monolayer and coextruded film lines. At high output, internal bubble cooling or a dual-lip air ring is required to remove the heat load associated with the 0.920 g/cm³ density.

    Melt fracture and bubble flutter arise when die gap and stalk height are unbalanced

    In high-stalk blown-film lines, the lower melt extension viscosity of DOWLEX 2056G reduces the maximum stable stalk height before bubble flutter or draw resonance appears. Field data from 100–250 mm dies indicate that stable operation at 2.5:1 BUR is restored when the stalk is shortened and the air-ring venturi is repositioned toward the die face. If LDPE is blended to increase melt strength, addition rates of 20–40 wt% are typical; below 20 wt% the effect on bubble stability is often insufficient, while above 40 wt% the blend loses measurable dart impact under ASTM D1709A. The exact limit depends on die diameter, output, and air-ring design. In low-stalk configurations, less LDPE is required, and the resin can be processed without major bubble instability provided the die gap remains above 1.5 mm.

    Melt fracture is managed by increasing melt temperature above 210 °C, widening the die gap, or reducing output. Pigmented masterbatch additions can alter shear viscosity and may require output derating of 5–15% depending on carrier resin and letdown ratio. These adjustments are confirmed on the converting line by film inspection after the collapsing frame, not solely by laboratory rheology. At melt temperatures below 190 °C, die pressure rises and melt fracture can appear; above 240 °C, oxidative degradation becomes temperature- and residence-time dependent. Purge with LDPE at shutdown is used where residence time in the extruder and die exceeds 10 min.

    Film property balance and downgauging limits

    The downgauging limit of a film structure is evaluated by tensile, tear, and puncture testing at application thickness. Tensile properties are measured by ASTM D882; tear resistance by ASTM D1922; puncture energy by ASTM D5748. Tear values are anisotropic: at 2.5:1 BUR, machine-direction tear is typically lower than transverse-direction tear because of molecular orientation in the machine direction. Balanced tear values are adjusted through BUR, frost-line height, or extrusion rate. The C6 comonomer of 2056G improves transverse-direction tear resistance relative to butene-based LLDPE of equivalent melt index and density, but reported values vary with gauge, melt temperature, and cooling configuration. Published data for this specific configuration is limited; qualification trials should therefore include complete film characterization on the target production line rather than reliance on melt index alone.

    For incoming resin qualification, melt index and density are checked by ASTM D1238 and ASTM D792. Film tensile tests are carried out after conditioning at 23 °C ± 2 °C and 50% ± 10% relative humidity. Dart impact testing to ASTM D1709A uses a free-falling dart with a 38 mm diameter hemispherical head; results are reported as the mass at 50% failure. Elmendorf tear testing to ASTM D1922 measures the force required to propagate a 20 mm tear from an initial slit; reported values are strongly influenced by film orientation and gauge. Puncture testing to ASTM D5748 measures the ultimate puncture force and energy to rupture using a hydraulic probe at a defined rate. These tests should be performed on film samples from the same production campaign to reduce lot-to-lot convolution.

    When converters replace LDPE in high-stalk coextrusion

    In coextruded seal layers, DOWLEX 2056G is placed against lower melting point plastomers or EVA when low seal initiation is required. The seal initiation temperature of the 1-octene LLDPE is governed by density and comonomer distribution; converters should establish the actual seal initiation and hot-tack envelope on the packaging machine because line speed, film gauge, and sealing bar dwell time shift the window. The resin is also used in core layers of stretch-hood and heavy-duty sack films where its density provides stiffness and its comonomer type provides tear propagation resistance. When replacing LDPE in high-stalk coextrusion, total replacement is uncommon due to melt strength loss; a structured blend of 2056G with 20–40 wt% LDPE is used to retain bubble stability while preserving downward-gauge capability.

    Heavy-duty sack films are typically produced at 100–200 µm in three-layer or five-layer lines. 2056G is used in core layers because its 1-octene comonomer improves tear propagation resistance under filled-bag drop tests. The outer layers may use LDPE for heat seal and gloss. Drop test standards for filled sacks include ISO 7965-1 or ASTM D5276; performance depends on film structure and seal quality. Freezer film applications require low-temperature flexibility; polyethylene remains ductile below −30 °C, but the exact impact threshold should be confirmed by end-use conditioning because gauge and orientation shift the ductile-to-brittle transition.

    Regulatory compliance is verified to FDA 21 CFR 177.1520 for olefin polymers and EU 10/2011 for food-contact plastics, with overall migration evaluated at 10 mg/dm² under specified test conditions. The resin is also subject to REACH registration under EC 1907/2006 and is assessed against RoHS Directive 2011/65/EU for restricted substances. Food-contact suitability is use-specific; converters must validate the finished article under end-use temperature, simulant, and contact time because additives in the final formulation may alter migration behavior.

    Storage should be in dry conditions below 50 °C. Polyethylene does not normally require predrying, but condensation on pellet surfaces must be avoided if the resin is transferred from cold storage into humid processing areas. Regrind addition up to 20 wt% is generally tolerated if the regrind is clean and dry; higher levels may reduce dart impact and increase gel count. Production-scale detection of gels uses inline camera systems or visual inspection after winding.

    Operational boundaries include loss of bubble stability at high output on high-stalk lines if LDPE is not added, sharkskin melt fracture at narrow die gaps or low melt temperatures, and reduced seal performance if the film is contaminated during regrind handling. The resin is not designed for sustained service above its crystalline melting point, and applications requiring high-temperature resistance should use a different polymer class. Downgauging below the critical thickness specified for a given application should be validated by end-use abuse testing, because laboratory film properties do not capture distribution-cycle loads.

    Top