| HS Code | 927668 |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Grade | Heavy Duty Film Grade |
| Comonomer | 1-Octene |
| Density | 0.920 g/cm³ |
| Meltindex | 0.85 g/10 min |
| Meltingpoint | 122 °C |
| Vicatsofteningpoint | 102 °C |
| Tensilestrengthatyield | 10.3 MPa |
| Tensilestrengthatbreak | 29.6 MPa |
| Ultimateelongation | 800% |
| Flexuralmodulus | 241 MPa |
| Dartimpactstrength | 200 g |
| Elmendorftearmd | 250 g |
| Elmendorfteartd | 400 g |
| Haze | 11% |
| Gloss45degree | 75 |
| Coefficientoffriction | 0.2 |
| Heatsealinitiationtemperature | 105 °C |
| Lowtemperaturebrittleness | < -70 °C |
| Hardnessshored | 50 |
| Waterabsorption | <0.01% |
As an accredited Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DOWLEX™ 2056A is packaged in 25 kg polyethylene-lined bags, 40 bags per pallet, totaling 1,000 kg net. |
| Container Loading (20′ FCL) | 20' FCL: DOWLEX 2056A supplied in 25 kg bags; floor-loaded, approximately 20–22 metric tons net, subject to palletization and weight limits. |
| Shipping | DOWLEX 2056A is non-hazardous polyethylene resin, supplied in 25 kg bags, 1,000 kg bulk bags, or bulk trucks/railcars. Not regulated as dangerous goods. Ship and store dry, clean, away from heat, sunlight, and moisture; use standard handling equipment and avoid bag damage or contamination. |
| Storage | Store DOWLEX™ 2056A in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original containers or bags closed to prevent moisture, dust, and contamination. Avoid excessive stacking and physical damage. Protect from UV light and moisture. Store indoors. Maintain clean, labeled stock and follow first-in, first-out rotation. Use within the recommended shelf life. |
| Shelf Life | No specific shelf life; stable under recommended cool, dry, sealed storage away from heat, sunlight, and ignition sources. |
Blown film lines converting DOWLEX 2056A into heavy-duty shipping sacks for granular fertiliser, polymer pellets, and mineral aggregates are typically configured with a 90 mm grooved-feed extruder, a 30:1 L/D barrier screw, and a 350 mm spiral mandrel die having a 2.2 mm die gap. The resin’s nominal density of 0.920 g/cm³ (ASTM D792) and melt index of 0.45 g/10 min (ASTM D1238 / ISO 1133-1, 190 °C / 2.16 kg) position it for thick-gauge film where low-temperature toughness and high dart impact retention are required. The octene short-chain branching distribution provides a higher concentration of tie molecules than conventional butene LLDPE at equivalent density, which improves crack propagation resistance under filled-sack stacking loads. On a high-output line running 100% virgin 2056A, the adiabatic melt temperature at the die lip is held between 204 °C and 232 °C, the blow-up ratio is typically set from 2.2:1 to 2.8:1, and frost line height is maintained at 550–800 mm to produce film from 125 µm to 250 µm. At 15 wt% high-pressure LDPE addition, bubble stability improves sufficiently to sustain BUR 3.0:1, but converter data consistently show a directional loss in machine-direction tear and dart impact relative to the unmodified resin, typically 10–15% lower dart impact under ASTM D1709 Method A; therefore converters blend LDPE into the core or outer layer of coextruded structures rather than sacrificing the entire film. The finished sacks are typically filled with 25–50 kg of free-flowing solids and are qualified by ASTM D1709 Method A for dart impact, ASTM D882 for tensile yield and break, and ASTM D1922 for Elmendorf tear. Where food-contact use is required, the olefin polymer clearance under FDA 21 CFR 177.1520 applies, and the converter must verify that all additives in the formulation meet the same regulation. The main processing constraint is melt-pressure sensitivity to regrind: incorporation of 10 wt% post-industrial reprocessed film without stabilizer adjustment produces melt pressure fluctuations of ±5% on 30:1 extruders, which can appear as gauge bands unless the die gap is adjusted or the regrind fraction is held constant.
| Parameter | Range or setting | Process note |
|---|---|---|
| Melt temperature at die lip | 204–232 °C | Lower end improves impact; upper end reduces melt pressure |
| Die gap | 2.0–2.5 mm | Thicker die gap reduces orientation in mono-layer heavy-gauge film |
| Blow-up ratio | 2.2:1–3.0:1 | Higher BUR improves TD tear and dart impact, reduces MD tear and bubble stability |
| Frost line height | 550–900 mm | Controls crystalline orientation and sack stiffness |
| Extruder L/D | 24:1–30:1 | Barrier screw lowers melt temperature variability |
| Output per die circumference | 0.8–0.9 kg/h/mm | Upper limit is set by internal bubble cooling capacity and melt-pressure stability |
Vertical form-fill-seal equipment running 80–125 µm tubular film at 28–32 cycles/min imposes a narrower seal window than pre-made open-mouth sacks because seal jaws close while the product column drops. In a three-layer coextrusion with an EVA sealant skin, the 2056A core or non-seal layer contributes puncture resistance and hot-tack after sealing; the EVA skin shifts heat seal initiation to 105–115 °C, while a 100% 2056A seal layer generally requires 120–130 °C jaw temperature for equivalent seal strength at 0.8–1.2 s dwell. Seal strength is evaluated by ASTM F88/F88M at a separation speed of 200 mm/min, and hot-tack force is measured by ASTM F1921 over 0.2–0.5 s cooling times. The pouch puncture mode in pet-food and dry-cement fills is better characterised by ASTM D3420 or drop testing with product-filled bags than by a slow tensile test, because the failure occurs under shock loading of sharp granules. On a horizontal FFS line filling 20–25 kg pet-food bags, film made with 85 wt% 2056A and 15 wt% LDPE in the core has sufficient dart impact at 150 µm gauge to survive product drop from 1.2 m; however, published data for this exact configuration are limited and converter-specific filled-bag drop tests according to internal protocols are required before release. The main operational limitation is that seal jaw temperature must be raised as ambient relative humidity exceeds 60% because surface moisture on film from chilled storage condenses and delays sealing; pre-conditioning at warehouse temperature for 4–6 h reduces such variability.
Low-temperature converting of IQF vegetables, frozen seafood, and meat parts uses 2056A-rich blown film where the failure criterion is not room-temperature tensile yield but resistance to crack propagation at freezer temperatures. The blend structure normally contains 70–80 wt% 2056A and 20–30 wt% of a metallocene LLDPE or polyolefin plastomer with lower melt index; the plastomer increases low-temperature impact but reduces film stiffness, so converters limit plastomer addition to 30 wt% unless the bag is unsupported. Melt temperature is reduced to 199–215 °C, blow-up ratio is held at 2.5:1–3.0:1, and film gauge is kept between 75 µm and 100 µm to reduce heat capacity while retaining puncture resistance. The finished bags are flexographic-printed on the outer surface and are typically sealed on one side; food contact compliance follows EU Regulation (EC) 10/2011 and FDA 21 CFR 177.1520, with the additive masterbatch vendor responsible for providing dual-listed antioxidant and slip packages. Low-temperature impact data generated by ASTM D1709 at 23 °C do not replace freezer-conditioned tests; the converter should expose specimens at −20 °C or −30 °C for 24 h and subject them to the same dart test or a specified bag-drop protocol. Published data for 2056A at −40 °C under ASTM D746 or ISO 974 remain limited, so operational release should be based on filled-bag freezer trials rather than nominal resin data.
Silage clamp covers and multi-year greenhouse side sheets produced from 2056A demand a separate UV-stabilisation strategy from monolayer sack film because the film must withstand solar irradiance, chemical contact with silage leachate, and repeated mechanical handling without surface fogging. In a three-layer coextruded cover, 2056A is placed in the outer layer or core at 70–85 wt%, with a UV masterbatch based on hindered amine light stabilisers and a UV absorber added at 5–10 wt%; the inner layer may contain 1–2 wt% of an anti-fogging concentrate to prevent condensate droplets from reducing light transmission. The extrusion line uses a 2.0–2.5 mm die gap, BUR 2.8:1–3.2:1, and a melt temperature of 205–225 °C; film gauge is normally 150–200 µm for silage covers and 180–220 µm for multi-season greenhouse film. High BUR increases transverse-direction tear and balances the high machine-direction orientation from high frost line; however, it also increases shrink, so downstream winders must operate with controlled tension below 5 N/100 mm at the nip. The finished cover is typically welded into 6–12 m sheets with hot-air welders; seam strength is checked against the farm film specification, while tensile properties of the cover are tested under ASTM D882. Where the film is used as silage cover, EN 13206:2017 provides requirements for mechanical strength and elongation; animal-feed contact is not subject to food-contact plastics regulation, but the converter must ensure the masterbatch is compliant with REACH registration and does not contain substances listed in REACH Annex XIV. The primary incompatibility is over-dosing UV masterbatch above 10 wt%, which can generate agglomerates at the die lip and reduce dart impact by forming stress risers.
Temporary construction enclosures, slab underlayment membranes, and remediation containments employ thick-film panels produced from 2056A-rich blends where conformability and weldability outweigh long-term chemical exposure. Panels are extruded at 200–500 µm gauge on blown film lines with die gaps of 2.5–3.0 mm and BUR 2.0:1–2.5:1; the larger die gap prevents coarse melt fracture at high viscosity and the lower BUR retains machine-direction tensile strength for installation on sharp aggregate. Blends commonly include 15–30 wt% high-pressure LDPE to widen the hot-air welding window and reduce modulus, although this addition lowers chemical resistance compared with the 100% 2056A baseline when evaluated by ASTM D543 mass change. Field seams are made with hot-air wedge welders at 350–450 °C using a 30 mm/min travel speed; welded seam strength is measured as a percentage of parent material tensile strength under ASTM D882, with a common acceptance threshold of 85% of parent yield. The resin’s sub-ambient brittleness temperature and low modulus allow panels to remain flexible during installation at 0–10 °C, but specifiers should not treat 2056A as a primary geomembrane for long-term BTEX or chlorinated solvent containment; chemical resistance must be confirmed by ASTM D543 immersion for the site-specific fluid. Temporary containment systems are commonly installed as 6 m-wide panels with prefabricated seams, and the film is overlapped and welded to prevent groundwater intrusion. Published data for this specific product in landfill capping service are limited, so long-term performance should be validated against GRI GM13 or equivalent site-specific flexible membrane liner requirements rather than relying on polyethylene density alone.
Extrusion coating of 2056A onto woven polypropylene fabric for fertiliser sacks, salt bags, and FIBC outer layers requires melt draw stability and low neck-in, which are not automatically delivered by a 0.45 g/10 min LLDPE run at heavy-duty film conditions. For coating weights between 15 g/m² and 30 g/m², the blend usually contains 20–40 wt% high-pressure LDPE to raise melt elasticity, reduce neck-in and permit an air gap of 150–250 mm between the flat die exit and the chill roll; 100% 2056A at 120–180 m/min line speed shows audible edge instability and gauge thinning at the web edges. The melt temperature is raised to 230–260 °C to promote oxidation of the polyethylene at the corona-treated woven PP surface, and the substrate is treated to a minimum surface energy of 42–46 dyn/cm immediately before lamination. Adhesion between nonpolar LLDPE and woven PP is insufficient without either a thin maleic anhydride-grafted polyethylene tie layer or blending 3–5 wt% of an anhydride-modified concentrate; peel adhesion is then measured by a T-peel method according to ASTM D1876 at 180° and 100 mm/min crosshead speed, with typical acceptance values of ≥2.5 N/15 mm for heavy-duty sack construction. Chill roll temperature is held at 15–25 °C to reduce crystallinity and improve interlayer peel after slitting. The laminated fabric is subsequently cut and stitched into bags; when the bag is used as a flexible intermediate bulk container, ISO 21898 requires safety factor verification but the LDPE/LLDPE lamination contributes moisture protection rather than primary load-bearing strength. A key limitation is melt-swell-induced edge bead; line operators control it by lip adjustment and reduce draw ratio below 80:1 to prevent pinhole formation in the coating.
| Application | Standard designation | Property or test |
|---|---|---|
| Heavy-duty shipping sacks | ASTM D1709 Method A | Dart impact at 23 °C |
| Heavy-duty shipping sacks | ASTM D1922 | Elmendorf tear resistance |
| Vertical FFS bags | ASTM F88/F88M | Seal strength |
| Vertical FFS bags | ASTM F1921 | Hot-tack force |
| Frozen food packaging | EU 10/2011, FDA 21 CFR 177.1520 | Food contact compliance |
| Silage cover | EN 13206:2017 | Mechanical requirements for bale-wrap films |
| Construction containment | ASTM D543 | Chemical compatibility |
| Extrusion-laminated FIBC | ISO 21898 | Flexible intermediate bulk container safety factor |
Competitive Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DOWLEX™ 2056A Linear Low Density Polyethylene is a solution-polymerized LLDPE resin supplied as pelletized feedstock for heavy-duty blown film extrusion. The product is categorized as a heavy-duty film grade because its nominal property set is specified for load-bearing sacks, industrial liners, agricultural films, and coextruded structures where gauge reduction is evaluated against retained impact strength and tear resistance. The nominal density is 0.920 g/cm³ and the nominal melt index is 0.95 g/10 min when measured at 190°C/2.16 kg in accordance with ASTM D1238 and ISO 1133-1:2022. The density value places the material below medium-density polyethylene and above very-low-density ethylene copolymers, resulting in a semicrystalline morphology that supplies tensile strength while retaining enough amorphous phase for slow crack propagation resistance and low-temperature impact. The product is not a high-pressure low-density polyethylene; its linear backbone and controlled comonomer placement produce a different balance of melt rheology, puncture resistance, and drawdown. In practice, the resin is used in monolayer and multilayer structures, often as a core layer to increase dart impact while thin LDPE or EVA skin layers control heat sealing and surface friction. Because the base stabilization package is not formulated with high slip or antiblock levels, surface coefficient-of-friction and blocking behavior are adjusted with masterbatches on the converting line. The grade should be selected only after comparing the target film gauge, internal bubble cooling capacity, and downstream bag-filling speed against the current Dow technical datasheet and lot-specific certificate of analysis.
| Property | Test method | Typical nominal value |
|---|---|---|
| Melt index (190°C/2.16 kg) | ASTM D1238, ISO 1133-1 | 0.95 g/10 min |
| Density | ASTM D792, ISO 1183-1 | 0.920 g/cm³ |
| Vicat softening temperature | ASTM D1525, ISO 306 | 103°C |
| Melting peak temperature (DSC) | ASTM D3418, ISO 11357-3 | 124°C |
Film mechanical values are intentionally omitted from the table because they are gauge-dependent and vary with blow-up ratio, frost-line height, and die gap. Converter qualification should reference the current Dow technical datasheet for the exact method and film gauge. Heavy-duty film evaluation for this grade typically requires ASTM D1709A dart impact, ASTM D1922 Elmendorf tear, and ASTM D882 tensile elongation at the specified final gauge; acceptance thresholds are converter-specific and depend on orientation state. Published data for every gauge and equipment configuration is limited; pilot-film values should not be treated as production guarantees.
Bubble instability in LLDPE heavy-duty film is governed by the interaction of melt relaxation time, internal bubble pressure, and cooling air distribution. For DOWLEX 2056A, the melt index of 0.95 g/10 min produces a higher extensional melt strength than a comparable 2.0 g/10 min LLDPE but a lower melt strength than high-pressure LDPE used in conventional film lines. On high-stalk configurations, the bubble is drawn upward through a stalk before expansion; the stalk is typically maintained at 4–7 die diameters in height when the die gap is 1.5–2.5 mm and the blow-up ratio is between 2.0:1 and 3.0:1. Operation outside this window increases edge flutter and causes asymmetric frost line movement. Internal bubble cooling lowers the air temperature at the bubble interior and stabilizes the frost line, but excessive IBC air velocity creates low-frequency bubble breathing. Melt temperature is commonly held at 205–240°C; temperatures below 205°C can produce unmelts and screw torque fluctuations on single-screw extruders with barrier elements, while temperatures above 240°C increase the risk of oxidative gel formation and reduce bubble load-bearing capacity. Frost line height is maintained by adjusting air ring and IBC air flow rather than by increasing melt temperature. Line operators monitor bubble diameter via ultrasonic sensors and adjust internal pressure to hold diameter within ±2% of target; deviations beyond this range correlate with gauge variation and poor roll conformation. The die gap should not be reduced below 1.2 mm for this melt index range because sharkskin melt fracture appears at the die lip and persists through the film as surface haze. If sharkskin is encountered, increasing the die lip temperature or widening the gap to 1.5 mm restores smooth film. These processing limits matter because heavy-duty sack lines run at high output, and bubble instability in an unoptimized set-up translates into dart impact variation across the web.
In heavy-duty sack production, DOWLEX 2056A is evaluated against high-pressure LDPE, butene-based LLDPE, and higher-density polyethylene grades. The differentiation is not a single property but a response across impact, tear, and stiffness. At equal film gauge, a high-pressure LDPE typically provides lower dart impact and lower Elmendorf tear than DOWLEX 2056A, but it contributes higher melt strength and easier bubble processing. High-pressure LDPE crystalline structure also yields a lower heat seal initiation temperature, which is why many converters co-extrude LDPE skins over a DOWLEX 2056A core. Compared with a butene-based LLDPE of similar 0.918–0.920 g/cm³ density and 1.0 g/10 min melt index, DOWLEX 2056A benefits from its solution-process comonomer distribution, which is associated with increased tie-molecule concentration and improved dart impact and Elmendorf tear. However, this same architecture raises melt elasticity and may require a wider die gap or lower haul-off speed than an equivalent butene grade. Against higher-density DOWLEX grades, such as those in the 0.926–0.930 g/cm³ range, DOWLEX 2056A has lower stiffness and tensile yield but higher dart impact and tear resistance at equivalent gauge. Therefore, a heavy-duty sack may use a higher-density layer for stiffness and a 0.920 g/cm³ layer for impact, with the final structure determined by seal requirements and filling-line abuse.
Replacement of high-pressure LDPE with DOWLEX 2056A in a co-extruded heavy-duty sack or liner is not a direct drop-in change. The LLDPE resin produces higher extensional viscosity at low shear and lower shear thinning than LDPE, so the same screw speed and extruder profile generate higher melt pressure and motor load. On a 24:1–30:1 L/D grooved-feed extruder with a barrier screw, the expected melt pressure increase is converter-specific, but the practical response is to raise the die temperature by 10–20°C and increase the die gap to 1.5–2.5 mm. High-pressure LDPE often runs with a die gap of 1.0–1.2 mm, but that gap is below the stable range for DOWLEX 2056A. Bubble cooling must be rebalanced because the LLDPE bubble is less resistant to high-stalk oscillation. Internal bubble cooling and a dual-lip air ring are recommended to maintain bubble diameter. Heat seal performance changes: DOWLEX 2056A has a higher seal initiation temperature than high-pressure LDPE and may require a seal bar temperature increase of 10–20°C; if seal initiation is critical, co-extruded EVA or LDPE seal skins are retained. Dart impact of the total structure typically improves at equal gauge, while film modulus may decrease, which is offset by increasing thickness or adding a higher-density layer. The replacement is most effective when the failure mode of the existing LDPE film is impact puncture rather than stiffness or seal strength.
Extended operation with solution-polymerized LLDPE can generate gel particles and die-lip buildup if melt temperature and residence time are not controlled. The stabilizer package in DOWLEX 2056A is formulated for typical blown film extrusion, but it does not eliminate oxidation indefinitely. Melt temperatures above 250°C are generally outside the intended processing window for this density and melt index; if thermocouple readings exceed 250°C at the die, the risk of antioxidant depletion and gel formation increases with residence time. Production lines use barrel profiles that ramp from 180°C at the feed zone to 220–240°C at the die, with the die temperature adjusted independently to manage melt fracture. Start-up and shutdown procedures should minimize oxygen ingress by purging with nitrogen or by keeping the screw filled and idle time short. Light-induced degradation is not a primary processing concern, but outdoor film applications require UV stabilizer masterbatch addition because the base resin does not contain sufficient UV protection for long-term weathering. In storage, the pellets should be protected from direct sunlight and moisture; although polyethylene is not hygroscopic, surface condensation in high-humidity environments can introduce steam bubbles during extrusion. The grade should not be processed on equipment with excessive melt temperature overrides because thermal degradation shifts film color and reduces tear strength. Foaming or bubble defects near the die are often a sign of moisture from condensation or additive degradation; the remedy is raw material conditioning and barrel-temperature adjustment, not increasing screw speed.
On 90 mm grooved-feed extruders operating above 180 kg/h, the typical failure modes observed are melt fracture, bubble instability, and web gauge variation. These are not resin defects but processing mismatches. Melt fracture appears as fine surface ridges at the die lip and indicates excessive shear stress; the response is to widen the die gap to 1.8 mm or reduce melt temperature to 215°C, not to increase haul-off speed. Gauge variation across the web often traces to uneven air ring distribution or a frost line that is too low. If the frost line is below 2 die diameters, the film quenches before molecular orientation is stabilized, reducing tear in the machine direction. If the frost line is above 7 die diameters, the bubble loses mechanical support and oscillates, producing thick-thin bands. Mills running the resin in monolayer heavy-duty sacks frequently set a blow-up ratio of 2.5:1 and a die gap of 1.6 mm, but these are starting points and not specification limits.
Industrial liners made from DOWLEX 2056A are exposed to surfactants, mild oxidizers, and solvent vapors during service. Environmental stress crack resistance of the resin is governed by density and comonomer distribution. At densities near 0.920 g/cm³, ESCR is generally better than that of medium- or high-density polyethylene grades. However, strong oxidizers, aromatic solvents, and chlorinated hydrocarbons degrade polyethylene by swelling and oxidative attack; the product is not rated for long-term contact with such media unless barrier liner testing demonstrates fitness. ASTM D1693 ESCR testing in 10% Igepal CO-630 at 50°C is commonly used as a comparative test, but field failure data from actual production-scale sack lines should be used to set acceptance thresholds. Published data for specific aggressive chemical exposure of this product is limited; end-use qualification under filled-container storage conditions is required before specifying the grade for chemical packaging.
Documentation for heavy-duty packaging and industrial film often requires confirmation of regional chemical regulations and food-contact status. DOWLEX 2056A is an olefin polymer and is typically covered by the manufacturer’s food-contact statements under the conditions specified in those documents; the statements are application-specific and temperature-dependent. The following table summarizes the standards commonly referenced in certificates of compliance for films based on this grade. The applicability of each entry must be verified against the intended food type, contact time, and processing history. No single regulatory statement covers all converters or all end uses.
| Standard or regulation | Typical relevance to DOWLEX 2056A film |
|---|---|
| FDA 21 CFR 177.1520(c) 3.2a | Olefin polymer provisions; require application-specific temperature and food-type confirmation |
| EU Regulation (EU) No 10/2011 | Plastic food-contact migration limits; compliance depends on layer structure and food simulant |
| REACH (EC) No 1907/2006 | Substance registration and SVHC communication obligations |
| RoHS Directive 2011/65/EU | Heavy metal and brominated flame retardant restrictions; relevant if film enters electrical and electronic equipment packaging scope |
| ASTM D1693 | Environmental stress crack resistance in surfactant solution |