| HS Code | 298985 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.920 g/cm³ |
| Melt Index 190 C 2 16 Kg | 0.80 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Point | 96 °C |
| Tensile Strength At Break Md | 32 MPa |
| Tensile Strength At Break Td | 30 MPa |
| Elongation At Break Md | 700 % |
| Elongation At Break Td | 800 % |
| Dart Drop Impact F50 | 200 g |
| Elmendorf Tear Strength Md | 300 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 10 % |
| Gloss 45 | 60 % |
| Secant Modulus 1 | 200 MPa |
| Hardness Shore D | 50 |
| Flexural Modulus | 240 MPa |
| Coefficient Of Friction | 0.2 |
| Heat Seal Initiation Temperature | 110 °C |
| Low Temperature Brittleness | < -70 °C |
As an accredited Dow DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DOWLEX™ 2056 Heavy Duty Film Grade is supplied in 25 kg polyethylene bags, 55 bags per pallet, totaling 1,375 kg. |
| Container Loading (20′ FCL) | 20' FCL loading: Dow DOWLEX™ 2056 LLDPE Heavy Duty Film Grade, 25 kg bags, palletized, shrink-wrapped, secured for ocean transport. |
| Shipping | DOWLEX™ 2056 is shipped as free-flowing polyethylene pellets in 25 kg bags or 500–1000 kg FIBCs, palletized and stretch-wrapped. Transport by truck or rail under dry, clean, ambient conditions. Store away from direct sunlight, moisture, and contamination. Not classified as dangerous goods. |
| Storage | Store DOWLEX™ 2056 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers sealed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid excessive stacking and prolonged high temperatures. Store away from food, water, and incompatible materials. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is indefinite when stored in original packaging, cool, dry, ventilated, away from sunlight, heat, moisture, and ignition sources. |
Gusseted tubing for free-flowing polyolefin regrind and mineral filler shipment places simultaneous demands on dart impact, Elmendorf tear, and seal integrity at automated filling rates of 20–30 sacks/min. In monolayer heavy-duty chemical shipping sacks, DOWLEX 2056 is processed at 100 wt% for non-contact industrial fillers, while bubble-stable blends use 70–85 wt% DOWLEX 2056 with 15–30 wt% high-pressure LDPE having a melt index of 0.2–0.8 g/10 min and 0.5–2.5 wt% slip/antiblock masterbatch. The resin is an ethylene-octene copolymer with nominal melt index 1.0 g/10 min at 190°C/2.16 kg under ISO 1133-1:2022 and nominal density 0.920 g/cm³ under ISO 1183-1:2019. The blown film process for this application is run with a barrier screw at 30:1 L/D, die diameter 200–350 mm, die gap 1.6–2.2 mm, and melt temperature at the die of 215–232°C; neck height is held at 5–8 die diameters with a blow-up ratio of 2.0:1–2.5:1. A dual-lip air ring with internal bubble cooling is required when layflat width exceeds 1,800 mm because gauge variation at the crease otherwise moves above ±4%. Output is slit into single-wound or center-fold sheeting and converted into valve sacks, open-mouth sacks with heat-sealed or sewn closures, FIBC liners, and dust-tight cavity liners for box fillers. Compliance anchors are ISO 527-3:2018 for tensile properties of films, ASTM D1709A for dart drop impact, ASTM D1922 for Elmendorf tear, and 21 CFR 177.1520(c) where incidental food contact is required. UN Model Regulations Part 6 performance testing applies only if the sack is declared as dangerous goods outer packaging; DOWLEX 2056 alone is not a barrier for aggressive solvent liquids and must be fluorinated or laminated when such service is specified.
| ASTM D1709A | Dart drop impact, F50 failure mass, 38.1 mm tup, 127 mm drop height |
| ASTM D1922 | Elmendorf tear resistance, machine and transverse directions |
| ISO 527-3:2018 | Tensile properties of polyethylene films, dumbbell specimen type 5, 200 mm/min |
| 21 CFR 177.1520(c) | Olefin polymer clearance where food contact is incidental |
| UN Model Regulations Part 6 | Performance test framework when the sack is declared as dangerous goods outer packaging |
Bunker silo covers do not function as sealed packages; they operate as tensioned membranes over fermenting forage, subject to gas pressure, UV radiation, and repeated foot traffic at feed-out. DOWLEX 2056 is compounded at 88–96 wt% with 2–4 wt% carbon black/UV-stabilizer masterbatch and 0.5–1.5 wt% processing stabilizer; a white/black coextruded cover uses DOWLEX 2056 in the black core and a white LLDPE/LDPE skin on the exposed face. Gauge is normally 150–250 µm, and the limiting property after 12 months of service is puncture after UV embrittlement rather than initial tensile yield. The film is blown on a monolayer line with die gap 1.8–2.4 mm, melt temperature 210–225°C, blow-up ratio 2.2:1–3.0:1, and oscillating haul-off; layflat widths up to 6 m require internal bubble cooling and corona treatment on one side for later seam welding. Terminal products include bunker silo covers, clamp films, temporary grain storage sheets, and fermentation tarps. Feed-contact clearance under EU Regulation 10/2011 Annex I is application-dependent; where silage film is intended for direct contact with whole-crop feed, the complete structure including tie layers and color masterbatches must be migration-tested under the relevant simulant conditions. DOWLEX 2056 should not be used below 80 wt% in the core if winter flexibility below −30°C is specified, because dilution with higher-density LLDPE raises the ductile-to-brittle transition temperature.
Because stretch hood films are applied at film consumption rates of 250–450 kg/h per pallet line, the cast or blown film must combine low machine-direction permanent set with controlled cling aging. In a three-layer cast structure, DOWLEX 2056 is used at 35–60 wt% overall, typically 40–70 wt% of the cling layer and 20–50 wt% of the core, with the balance composed of metallocene LLDPE or high-pressure LDPE. The cling layer contains 1–3 wt% polyisobutylene or proprietary cling additive; the outer slip layer carries 1–2 wt% erucamide or similar slip agent to prevent blocking on the mill roll. Thickness is normally 50–100 µm. Cast film is produced on a 3-layer feedblock/multi-manifold die line with extruder L/D 30:1, chill roll surface temperature 18–25°C, and line speed 250–400 m/min. Blown versions use a 2.0:1–2.5:1 blow-up ratio and die gap 1.4–2.0 mm. The application machine draws the tube at 1.5:1–1.8:1 circumferential stretch. Terminals are stretch hood films for palletized bagged resin, cement, fertilizer, and IBC cages up to 1200 mm × 1000 mm load footprint. Compliance uses ASTM D5459-95(2020) for elastic recovery and permanent set, ASTM D5748-95(2019) for cling stretch film, and ASTM D882 for tensile properties. If DOWLEX 2056 exceeds 70 wt% in the cling layer, coefficient of friction may fall below 0.2 after 48 h aging, causing load instability in high-bay racking; cling level must be revalidated after warehouse storage above 30°C.
Under concrete placement, a sub-slab vapor retarder is exposed to aggregate puncture, rebar traffic, and tensile stress over soil settlement rather than to hydrostatic water pressure alone. DOWLEX 2056 is incorporated at 80–100 wt% in a blown membrane, with 2–5 wt% carbon black or grey masterbatch and optionally 10–20 wt% MDPE/HDPE to raise creep resistance; films below 200 µm are generally insufficient for rebar traffic unless protected by a geotextile. The membrane is extruded at 250–500 µm thickness using a die gap of 2.0–2.8 mm, melt temperature 215–235°C, blow-up ratio 2.0:1–2.5:1, and air ring air temperature 12–18°C. Site installation uses hot wedge welding or extrusion fillet welding; seam peel adhesion is verified by ASTM D1876, and the installed membrane is classified by ASTM E1745-17 for water vapor retarders in contact with soil. ASTM D1434 and ASTM E96/E96M are used for permeance measurement, with Class A under ASTM E1745-17 requiring water vapor permeance ≤0.1 perm. Terminal products are underslab vapor retarders, crawl space membranes, and temporary interior partition barriers. DOWLEX 2056 alone is not an oxygen barrier and should not be specified for methane or radon soil-gas service without an additional foil or EVOH layer.
Sub-zero flexural brittleness in institutional frozen block liners and ice bags is controlled by comonomer distribution rather than by melt index alone. DOWLEX 2056, as an ethylene-octene copolymer with density 0.920 g/cm³, is used at 60–75 wt% with 20–30 wt% LDPE or metallocene LLDPE for seal initiation and 2–5 wt% slip/antiblock masterbatch; an additional 3–6 wt% white masterbatch may be included for opacity. The film is blown at 75–100 µm gauge using die gap 1.5–2.0 mm, melt temperature 200–220°C, blow-up ratio 2.0:1–3.0:1, and a frost line height not exceeding 7 die diameters to avoid excessive machine-direction tear. Conversion on vertical packaging machines uses impulse or ultrasonic sealing at jaw temperatures 120–140°C and dwell times 0.3–0.8 s; the seal must withstand −40°C flexing without stress whitening. Terminal items include frozen seafood block liners, ice bags, cold-chain cushioning films, and institutional freezer pouches. Food-contact compliance is governed by 21 CFR 177.1520(c) and EU Regulation 10/2011 Annex I, with overall migration not exceeding 10 mg/dm² under the assigned food simulant conditions in Annex V; EC 1935/2004 Article 3 also applies to the converter’s finished article. The unsupported film is not suitable for autoclaving or liquid nitrogen immersion, because dimensional stability is lost above 80°C.
LLDPE geomembrane specifications for secondary containment under chemical storage tanks require elongation at break above 600% and stress crack resistance rather than high modulus. DOWLEX 2056 is used at 70–100 wt% of the LLDPE component, with 2–3 wt% carbon black masterbatch and 0.5–1.5 wt% UV stabilizer; 10–25 wt% HDPE or higher-density LLDPE is added when tensile modulus must be raised for anchor trench stability. Sheet gauge is 500–1000 µm, produced on a flat die extrusion line with gear pump, screen changer, and calendar stack at melt temperature 200–225°C; sheet width is controlled by roll stand gap rather than bubble blow-up ratio. Field joining uses hot wedge or extrusion fillet welding, with destructive seam peel testing under ASTM D6392. Terminal products are secondary containment liners under chemical storage tanks, temporary rain covers for soil stockpiles, and floating covers for open tanks. Applicable specifications include GRI-GM17 for LLDPE geomembranes, ASTM D6693-20 for tensile properties, ASTM D4833 for puncture, and ASTM D1004 for tear. DOWLEX 2056 is not a primary barrier for chlorinated solvents or highly aromatic hydrocarbons; for these media, permeation testing under EN 14150 or a fluorinated barrier is required before membrane selection.
Competitive Dow DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade, is a solution-process ethylene/α-olefin copolymer supplied by Dow. The resin is specified primarily by a nominal melt index of 0.95 g/10 min measured under a 2.16 kg load at 190°C per ASTM D1238 and a nominal density of 0.920 g/cm³ per ASTM D792 or ISO 1183-1:2019. These two values place the product in the low-flow, medium-density segment of linear low density polyethylene film resins. The heavy duty film grade designation is associated with monolayer and coextruded structures intended for industrial bags, shipping sacks, agricultural films, pond liners, and temporary containment membranes. Because the material is an α-olefin copolymer with short-chain branches along a predominantly linear backbone, its solidified film develops a greater population of tie molecules than high-pressure low density polyethylene at equivalent density. That molecular architecture is the basis for higher dart impact and puncture resistance at comparable gauge.
| Property | Method | Typical nominal value |
|---|---|---|
| Melt index | ASTM D1238 at 190°C/2.16 kg | 0.95 g/10 min |
| Density | ASTM D792 | 0.920 g/cm³ |
| Base comonomer architecture | Internal structural data | Ethylene/α-olefin with short-chain branching |
| Typical blown film die gap | Production practice | 2.0–2.5 mm |
| Typical blow-up ratio | Production practice | 2.0:1–3.0:1 |
Published film-property data for DOWLEX 2056 are limited to the manufacturer’s technical data sheet and converter-generated data; the values above are nominal resin properties, not finished film specifications. Finished film values depend on die gap, blow-up ratio, frost line height, gauge, and additive masterbatch loading.
The melt index of 0.95 g/10 min produces a melt viscosity that is higher than that of typical 1.0–2.0 g/10 min LLDPE film grades. In a blown film extruder with an L/D ratio of 24:1 to 30:1, this viscosity can increase die pressure at constant output. Single-screw extruders processing 2056 commonly run with barrel zones from 180°C to 210°C and an adapter/die zone at 210–225°C. Die gaps below 1.8 mm may promote melt fracture in high-output lines, while die gaps of 2.0–2.5 mm are used to reduce shear stress at the die lip. Frost line height, blow-up ratio, and internal bubble cooling must be held constant during film qualification because the linear resin has lower melt strength than high-pressure LDPE and can exhibit bubble instability if the frost line is too high or internal bubble pressure varies. Batch-to-batch melt index variation is normally controlled within the manufacturer’s published specification window, often expressed as ±0.05 g/10 min or tighter for this flow range; converters should monitor die pressure and motor load because small viscosity shifts can change film gauge profiles.
Capillary rheometry per ISO 11443 can be used to compare the shear viscosity function of DOWLEX 2056 with higher-melt-index resins. At a shear rate of 100 s⁻¹ and 190°C, linear low density polyethylene of this melt index typically shows an apparent viscosity in the range of 350–500 Pa·s; at 10 s⁻¹ the apparent viscosity can exceed 1,500 Pa·s. These values are not universal because solution-process resins differ in molecular weight distribution. The shear-thinning behavior of the resin permits higher output at the die lips while maintaining enough low-shear viscosity for bubble stability. The high low-shear viscosity also means that the resin can develop wall slip or sharkskin if die exit velocity exceeds the critical shear stress of the melt. A die-lip coating or a wider die gap is used to reduce surface defects.
Polyethylene is not hygroscopic; pre-drying is not normally required at ambient relative humidity below 60%. Surface moisture from outdoor storage or condensation should be removed through hopper blending with warm air if visual moisture is present. If outdoor silo storage is used below dew point conditions, pre-drying at 50–60°C for 2–4 h may be applied. Bulk handling systems should be cleaned to remove high-melt-index polyolefin fines because mixing 2056 with high-melt-index LLDPE can change the apparent melt index of the blend.
In heavy-duty shipping sacks, film thicknesses typically range from 75 μm to 200 μm. Converters qualify material through ASTM D1709 dart drop impact, ASTM D1922 Elmendorf tear resistance, ASTM D5748 puncture propagation resistance, and ASTM D882 tensile properties. A variation in blow-up ratio from 2.2:1 to 2.6:1 can change the machine-direction/transverse-direction tear balance by more than 20%, so acceptance values must be tied to a fixed processing history. The resin can be used in monolayer sacks or as a core layer in three-layer coextrusions where the skin layers provide seal initiation and coefficient of friction control. Skin-layer slip and antiblock levels are selected by measuring coefficient of friction per ASTM D1894. Stacked-sack drop performance is frequently the final qualification method; film property tests alone do not capture failures caused by seam folding, corner stress concentration, or pallet strapping.
Agricultural silage covers and greenhouse films use DOWLEX 2056 at gauges from 150 μm to 250 μm. The linear backbone provides low-temperature ductility; however, the neat resin is not UV-stabilized. Outdoor films must include a UV stabilizer masterbatch, and the stabilizer package must be tested by accelerated weathering per ISO 4892-2 or equivalent. Under coextrusion conditions, 2056 may be paired with lower density polyethylenes to reduce water vapor transmission; the layer ratio must be recorded because changing the 2056 core thickness by 10% of total gauge can shift tear initiation by more than 15%. Accumulation of low molecular weight species on the die lip can increase during long runs, so die lip cleaning schedules may be shorter than for high-pressure LDPE.
At the same nominal density of 0.920 g/cm³, high-pressure LDPE contains long-chain branching, which increases melt strength and strain-hardening but restricts crystallization into a morphology with fewer tie chains. The linear backbone of DOWLEX 2056, built with short-chain branches from α-olefin comonomer, permits a more uniform lamellar structure. In a dart drop test under ASTM D1709, the LLDPE film can consume greater fracture energy than LDPE of equal density and thickness. The difference is not a density effect alone; it is a molecular architecture effect. Tensile strain at break values measured by ASTM D882 are typically higher for LLDPE than for high-pressure LDPE, but high-pressure LDPE can be easier to process in large-bubble heavy-duty lines because its long-chain branching stabilizes the bubble at low shear rates.
Compared with a higher-melt-index DOWLEX film grade near 1.0 g/10 min, the 0.95 g/10 min version gives a measurable increase in shear viscosity. This can lead to higher extruder head pressure at equivalent screw speed but improves thick-gauge bubble stability and lowers the incidence of sagging in wide-web films. The density of 0.920 g/cm³ is common across several DOWLEX film grades; therefore melt index and additive package become the main selection variables. High-melt-index LLDPE grades are generally easier to extrude at high throughput but may show more gauge variation in films above 100 μm. In coextruded structures, 2056 is frequently placed in the core layer, while a lower viscosity skin resin is used to fill the die at lower pressure and provide sealant performance.
| Resin class | Melt index | Density | Molecular architecture | Processing implication |
|---|---|---|---|---|
| DOWLEX 2056 | 0.95 g/10 min per ASTM D1238 | 0.920 g/cm³ per ASTM D792 | Linear LLDPE with short-chain branching | Higher viscosity; stable thick-gauge bubble; moderate melt strength |
| High-pressure LDPE film grade | 0.3–2.0 g/10 min | 0.918–0.930 g/cm³ | Long-chain branched | High melt strength; easier large-bubble stability; lower dart impact at equal gauge |
| Higher-melt-index DOWLEX LLDPE | 1.0 g/10 min | 0.920 g/cm³ | Linear LLDPE with short-chain branching | Lower head pressure; higher output potential; may show more sag in thick film |
Sealing performance of DOWLEX 2056 differs from high-pressure LDPE because the linear resin typically has a higher seal initiation temperature. When the grade is used in a monolayer film for heavy-duty sacks, the heat seal bar must be set 10–20°C higher than for an LDPE film of comparable density. Hot-tack measurements per ASTM F1921 should be included when the sack line runs at high sealing speeds. On rotary sealing machines, the higher melting point and narrower sealing window can cause leakers if jaw temperature is not adjusted; operators should map the heat seal curve before changing from LDPE to LLDPE.
Downgauging from high-pressure LDPE to DOWLEX 2056 can be evaluated by comparing puncture resistance per unit thickness. A converter may reduce film thickness from 150 μm to 125 μm if the LLDPE film retains the required dart impact and tear resistance under ASTM D1709 and ASTM D1922. The downgauging limit is not set by tensile strength alone; orientation can shift with changes in blow-up ratio, frost line height, and die gap. A shift in blow-up ratio of 0.2:1 can alter Elmendorf tear values by more than 20%. Automatic gauge control and bubble diameter sensors are used to maintain thickness variation within ±5% of target on coextrusion lines. If the film is converted into sacks on bottom-seal or side-seal machines, the heat seal window and hot-tack response must be re-mapped because LLDPE seal behavior differs from high-pressure LDPE.
During transfer of 2056 from a monolayer line to a three-layer coextrusion line, operators may observe instability at the layer interface if the skin resin has a melt index above 2.0 g/10 min. The viscosity ratio between layers should be maintained within the die manufacturer’s recommended range. External bubble cooling air should be adjusted to prevent bubble wobble; a frost line that oscillates by more than ±50 mm can produce film with transverse gauge bands. Melt temperatures above 240°C should be avoided for long residence times because thermal degradation lowers melt strength and increases gel formation. If gels accumulate on the die lip, the die lip should be cleaned and the screen pack inspected. Screen combinations of 40–80 mesh are typical for heavy-duty film extrusion; screen selection depends on extruder pressure limits and the gel count specification of the final product.
For food-contact applications, the applicability of 21 CFR 177.1520(c) must be verified with the manufacturer’s compliance letter for the specific formulation and use condition. Under European Union REACH, the polymer substance requires registration by the manufacturer; fabricated articles are generally not subject to RoHS restrictions unless heavy-metal-based colorants or additives are incorporated downstream. The resin is not formulated with slip or antiblock unless specified in a grade suffix; converters must add masterbatches to control coefficient of friction and blocking. Additive masterbatches based on LDPE carriers can reduce melt viscosity and shift tear balance, so the addition level should be recorded and the film re-qualified under the same test methods.