Dow Dowlex 2049 Linear Low Density Polyethylene Food Grade

Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade

    • Product Name: Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 905255
    Productname Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade
    Chemicalfamily Linear Low Density Polyethylene (LLDPE)
    Density 0.920 g/cm³
    Meltindex 0.85 g/10 min at 190°C/2.16 kg
    Meltingpoint 122 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatyield 10.3 MPa
    Tensilestrengthatbreak 29.0 MPa
    Ultimateelongation 850%
    Flexuralmodulus 207 MPa
    Hardnessshored 50
    Foodcontactcompliance Complies with FDA 21 CFR 177.1520 and EU 10/2011 for food contact

    As an accredited Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg (55 lb) food-grade polyethylene bags, palletized and stretch-wrapped for safe industrial transport.
    Container Loading (20′ FCL) 20′ FCL: DOWLEX™ 2049 LLDPE food-grade resin, 25 kg bags, palletized and stretch-wrapped; approx. 20 MT net; dry container.
    Shipping DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade is typically shipped in 25-kg polyethylene bags or 1000-kg bulk bags, palletized and stretch-wrapped. Transport in clean, dry, covered vehicles at ambient temperature, protected from moisture, contamination, UV, and odors. Comply with food-grade handling and local transport regulations.
    Storage Store DOWLEX™ 2049 in a dry, clean, well-ventilated area away from direct sunlight, heat, ignition sources, and oxidizing agents. Keep original bags or containers sealed on pallets to prevent moisture, dust, and contamination. Avoid temperatures above 50°C (122°F). Protect from UV and physical damage. Use first-in, first-out rotation and maintain food-grade hygiene.
    Shelf Life DOWLEX™ 2049 food-grade LLDPE has no defined shelf life if stored cool, dry, sealed, away from sunlight and moisture.
    Application of Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade

    Blown Film Frost Line Positioning at 80 wt% DOWLEX 2049 in Primary Dry-Food Packaging

    Blown-film primary packaging for dry foods represents the highest-volume use of DOWLEX 2049 in food-contact flexible packaging. The resin’s manufacturer-published density of 0.926 g/cm³ and melt index of 1.0 g/10 min (ISO 1183-1:2019; ISO 1133-1:2022) impose a narrow processing window when the grade is run as the dominant ethylene-α-olefin component. In FDA-regulated dry-food pouches, the olefin polymer clause FDA 21 CFR 177.1520(c) applies when the resin is manufactured under GMP and the finished film is tested for migration under conditions of use; for EU destinations, Regulation (EU) No 10/2011 Annex I and Annex II set an overall migration limit of 10 mg/dm². For the Chinese market, GB 4806.7-2016 requires total migration ≤10 mg/dm² when tested per GB 31604.8-2016. The formulation on a typical 65 mm single-screw blown-film line is 70 wt% to 85 wt% DOWLEX 2049, 15 wt% to 30 wt% LDPE for bubble stability, and 0.5 wt% to 2.0 wt% slip/antiblock masterbatch; a fluoropolymer processing aid at 0.02 wt% to 0.1 wt% is introduced only when die pressure exceeds 45 MPa or when sharkskin surface defects appear at line speeds above 120 m/min.

    Downstream, the process is blown-film extrusion through a spiral mandrel die with a die gap of 1.8 mm to 2.5 mm, a die diameter of 250 mm to 350 mm, and blow-up ratio of 2.2:1 to 3.0:1. Melt temperature at the die is held between 190°C and 225°C; barrel zones are profiled from 170°C at zone 1 to 220°C at the adapter. Frost line height is maintained at 450 mm to 700 mm above the die face. When frost line height drops below 350 mm, transverse-direction gauge variation increases above ±8% due to insufficient crystallinity; when it exceeds 750 mm, bubble flutter produces inconsistent film impact. Batch-to-batch melt-index variation within the supplier’s certificate band shifts frost line position by roughly 50 mm on the same barrel profile, so converters compensate with adapter temperature adjustment rather than screw speed changes. Terminal products include cereal liner bags, cracker pillow packs, rice pouches, and dry pet-food bags. On production-scale lines, the primary failure mode is bubble instability when LLDPE loading exceeds 85 wt%, because the low shear melt strength of DOWLEX 2049 cannot sustain a 1.8 m bubble at an output of 150 kg/h without LDPE dilution.

    At coating weights above 18 g/m², extrusion lamination with DOWLEX 2049 becomes a heat-seal alternative to LDPE coating on paperboard cupstock and flexible lidding. In this process, the resin is not pre-dried unless surface condensation occurs at relative humidity above 75%; otherwise, melt-phase moisture uptake is negligible. Regulatory compliance for EU and US food-contact laminates relies on FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011, with migration testing conducted using EN 1186-1:2002 and EN 1186-14:2002 for coated board; overall migration must not exceed 10 mg/dm². The extrusion coating formulation is either 100 wt% DOWLEX 2049 or 85 wt% DOWLEX 2049 blended with 15 wt% LDPE to reduce neck-in. Coating weight is set between 18 g/m² and 30 g/m² for barrier lidding, while tie-resin coextrusion feedblock layers account for 3 g/m² to 5 g/m² when bonding to ethylene-vinyl alcohol or aluminium foil.

    On a 90 mm extruder with L/D 30:1 and a 0.6 mm slot die, melt temperature is held at 280°C to 305°C; below 270°C, neck-in increases to more than 15 cm per side, and above 320°C, oxidation gel accumulation on the die lip requires line stoppage within 6 h. The ozone treatment unit at the chill roll interface doses 0.04 mg/L to 0.08 mg/L to raise surface energy of the melt curtain from 28 mN/m to 38 mN/m for adhesion to paperboard. Chill roll temperature is maintained at 15°C to 20°C, and line speed ranges from 80 m/min to 150 m/min. Finished product types include heat-seal lidding for dairy cups, coated paperboard for quick-service food trays, and foil-laminated sachet stock for powdered beverage mixes.

    Food-contact compliance matrix for DOWLEX 2049 primary and secondary applications
    JurisdictionRegulationTest methodLimit/criterion
    United StatesFDA 21 CFR 177.1520(c)Extraction per 21 CFR 177.1520(d) under intended conditions of useOlefin polymer produced with authorised catalysts; GMP extractives control
    European UnionRegulation (EU) No 10/2011 Annex I, Annex IIEN 1186-1:2002, EN 1186-2:2002, EN 1186-14:2002Overall migration 10 mg/dm² or 60 mg/kg for infant food
    ChinaGB 4806.7-2016GB 31604.8-2016 total migrationTotal migration ≤10 mg/dm²

    What Chill Roll Temperature Range Minimizes Blocking in Cast Produce Overwrap at 120 m/min?

    For cast film overwrap of fresh produce and bakery items, DOWLEX 2049 is processed at film gauges between 15 µm and 25 µm. At this thickness, slip and antiblock masterbatch loadings are constrained by food-contact additive restrictions: erucamide slip is typically added at 0.3 wt% to 0.6 wt% and synthetic silica antiblock at 0.8 wt% to 1.5 wt%, because higher loadings reduce optical clarity below the 90% transmittance threshold accepted in retail overwrap. The resin complies with FDA 21 CFR 177.1520 for olefin polymers and with Regulation (EU) No 10/2011 overall migration limit of 10 mg/dm²; in China, GB 4806.7-2016 applies. A 75 mm extruder with L/D 30:1, barrier feed section, and 1.4 m slot die is used. Die gap is set at 0.3 mm to 0.5 mm, melt temperature at 200°C to 230°C, and air-knife pressure at 0.02 MPa to 0.05 MPa to pin the melt curtain to the polished chill roll.

    Chill roll temperature is the critical variable. At 18°C to 24°C, the cast film releases cleanly and blocking is absent; above 28°C, the film wraps on the roll and surface defects called re-weld marks appear. Line speed at 100 m/min to 180 m/min is achievable when the die lip gap is uniform within ±0.02 mm. Terminal products include perforated produce bags, oversize bakery-bread overwrap, and transparent food-wrap rolls for delicatessen use. On production lines, the dominant failure is edge curl from uneven quench, corrected by increasing chill roll contact from 180° to 240° of wrap angle and maintaining roll surface roughness at Ra 0.1 µm to 0.3 µm.

    Two-layer bag-in-box liners for liquid foodservice syrups are produced from DOWLEX 2049 on a 65 mm coextrusion blown-film line with a 250 mm spiral die and a die gap of 2.0 mm to 2.4 mm. In this structure, the food-contact inner layer contains 80 wt% DOWLEX 2049 and 20 wt% LDPE, while the outer layer is 70 wt% LDPE and 30 wt% DOWLEX 2049 to increase heat-seal window separation; an EVOH barrier layer inserted as 8 wt% to 10 wt% of the total 70 µm to 110 µm structure requires a maleic-anhydride tie resin at 4 wt% to 6 wt% on both sides. Compliance is established under FDA 21 CFR 177.1520, Regulation (EU) No 10/2011 Annex I and Annex II, and GB 4806.7-2016; for aqueous and acidic liquid foods, EU migration testing follows EN 1186-2:2002 and EN 1186-3:2002 with 10% ethanol and 3% acetic acid simulants, respectively, with overall migration ≤10 mg/dm².

    Processing conditions are melt temperature 205°C to 225°C, blow-up ratio 2.0:1 to 2.5:1, frost line 350 mm to 500 mm, and output 80 kg/h to 110 kg/h. The coextrusion feedblock and die must be purged after every 24 h of continuous run because EVOH degradation products accumulate at the layer interface when idle temperatures exceed 230°C. Terminal product types include 3 L to 10 L bag-in-box liners for dairy creamer, post-mix beverage syrup, and liquid egg yolk for foodservice. The limiting operational boundary is seal contamination from inner-layer migration of slip additive above 0.8 wt%; at higher loadings, heat-seal strength measured by ASTM F88/F88M-21 falls below 15 N/25 mm at 110°C seal jaw temperature.

    When Collation Shrink Film Targets an MD Shrinkage of 55%, Blend Limits for DOWLEX 2049 Are Narrower

    In collation shrink bundling for canned foods and beverage multipacks, DOWLEX 2049 is used as a secondary packaging layer that may transiently contact primary labels and closures. The applicable compliance for US and EU destinations is FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011; since the film is not intended for direct food contact, organoleptic and overall migration testing is still conducted when the film is printed and stacked against primary packaging. The formulation is 60 wt% to 80 wt% DOWLEX 2049 diluted with 20 wt% to 40 wt% LDPE, with slip masterbatch at 0.2 wt% to 0.5 wt% to maintain a kinetic coefficient of friction below 0.35 (ISO 8295:1995). Film thickness is set at 35 µm to 60 µm, and the target machine-direction shrinkage at 150°C is 50% to 55%, while transverse-direction shrinkage is held at 30% to 40%.

    Production on a high-stalk blown-film line uses a die gap of 1.6 mm to 2.2 mm, blow-up ratio of 3.5:1 to 5.0:1, frost line at 700 mm to 1100 mm, and melt temperature of 190°C to 215°C. The high stalk imparts orientation before the bubble reaches the frost line; if the frost line drifts below 600 mm, MD shrinkage drops below 45% and the film cannot recover from tray compression. Shrink force measured by ISO 14616:1997 confirms the processing boundary: DOWLEX 2049 loadings above 80 wt% produce excessive transverse-direction shrink force that deforms lightweight corrugated tray sidewalls; below 60 wt%, the shrink tension is insufficient to hold 12-can corrugate trays during palletising. Terminal finished products include shrink-wrapped slabs of canned tomato paste, multipack beverage bottles, and bakery tray bundling.

    Freezer-grade pouches for IQF vegetables and frozen poultry demand a DOWLEX 2049 film gauge of 60 µm to 100 µm, because the resin’s low-temperature toughness is the controlling technical property. Under FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011, frozen-food applications are tested with food simulant E or 95% ethanol under time–temperature conditions corresponding to long-term storage at -18°C; overall migration remains subject to 10 mg/dm². The formulation is 80 wt% to 100 wt% DOWLEX 2049, with LDPE at 0 wt% to 20 wt%, and slip/antiblock masterbatch at 0.4 wt% to 1.0 wt%. On a 70 mm single-screw blown-film extruder with L/D 28:1, melt temperature is 190°C to 215°C, die gap is 2.0 mm to 2.4 mm, blow-up ratio is 2.5:1 to 3.0:1, and frost line height is 500 mm to 800 mm.

    Seal integrity after -20°C storage is measured by ASTM F88/F88M-21; seal jaw temperature at the converter is set between 115°C and 135°C, with a dwell time of 0.5 s to 1.0 s. The product types include IQF vegetable bags, frozen poultry shrinkable bags, and ice cream pouch stock. Field experience on vertical form-fill-seal machines shows that film stiffness increases when film temperature drops below -18°C, requiring servo-driven sealing jaws rated for 35 N/mm² jaw pressure; lower jaw pressure produces channel leaks at the gusset folds. The material should not be used in direct contact with high-fat frozen sauces at temperatures above 100°C, because the additive package in standard food-contact DOWLEX 2049 is not stabilised for retort or roasting conditions.

    Free Quote

    Competitive Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade, is an ethylene-octene copolymer produced via solution polymerization and supplied as free-flowing pellets. The grade has a nominal density of 0.926 g/cm³ (ASTM D792) and a nominal melt index of 1.0 g/10 min (ASTM D1238, 190 °C/2.16 kg). The octene comonomer provides C8 short-chain branching that increases tie-molecule density relative to commodity butene-based linear-low-density grades of the same melt index. This structural feature becomes important in frozen food packaging because it shifts failure from brittle puncture or tear propagation toward ductile deformation at temperatures approaching -20 °C. The food-grade classification is documented under U.S. FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011, subject to migration testing on the finished package rather than the pellet alone. The grade contains antioxidant and processing stabilizer additions; the specific formulations are disclosed in lot-specific documentation and are selected to avoid interference with seal strength or organoleptic transfer in dry, moist, and fatty food contact. Primary application contexts include frozen food bags, cereal liners, liquid pouch films, produce packaging, and high-output form-fill-seal structures produced on single-layer or coextruded film lines.

    Under FDA 21 CFR 177.1520(c), an olefin polymer of this density class is evaluated by hexane or xylene extractables according to the specifications for polyethylene; the exact limit depends on the density grouping and the stated end-use temperature. A lot-specific certificate of analysis should therefore be consulted, because pellet compliance alone does not establish finished article compliance when inks, adhesives, or coextruded layers are introduced downstream. Under Regulation (EU) No 10/2011, overall migration must not exceed 10 mg/dm² of the finished package surface area, and specific migration for primary antioxidants such as pentaerythritol tetrakis[3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate] (CAS 6683-19-8) is limited to 15 mg/kg when that substance is present.

    What Distinguishes DOWLEX 2049 from Butene- and Hexene-Based LLDPE Grades?

    The main difference is comonomer chain length and its effect on the amorphous phase. Butene-modified LLDPE inserts C4 branches into the polyethylene backbone; a fraction of these branches can co-crystallize into the lamellae, which reduces their efficiency in forming load-bearing tie chains between crystal domains. Hexene-based LLDPE represents an intermediate structure. Octene-based DOWLEX 2049 achieves the target density with a lower molar fraction of comonomer and produces longer amorphous segments between crystallites. The practical consequence is that a film fabricated at 25 µm thickness on a 40 mm blown film line with a 2.5:1 blow-up ratio can show higher dart drop impact (ASTM D1709A) and Elmendorf tear (ASTM D1922) relative to a butene grade of equivalent melt index. The resin is not a metallocene polyolefin; its molecular weight distribution is broader than that of a constrained-geometry-catalyst product, which yields higher melt strength but often lower gloss and higher haze. A converter replacing a metallocene LLDPE with DOWLEX 2049 should expect higher die pressure at the same output and increased seal initiation temperature. The choice between the two families is governed by target optics, seal window, and available extrusion equipment.

    Resin characterization matrix for DOWLEX 2049
    ParameterTest StandardTypical Value
    DensityASTM D7920.926 g/cm³
    Melt indexASTM D1238 (190 °C/2.16 kg)1.0 g/10 min
    ComonomerManufacturer specificationOctene
    Melting peakISO 11357-3122 °C
    Vicat softening pointASTM D1525102 °C

    Typical values in the matrix are not guaranteed limits and must be verified against the lot-specific certificate of analysis before equipment validation.

    On single-layer blown film extrusion lines with screw diameters between 40 mm and 90 mm and length-to-diameter ratios of 24:1–30:1, DOWLEX 2049 is normally processed at melt temperatures of 205–230 °C and die temperatures of 210–225 °C. The die gap should be maintained between 1.8 mm and 2.5 mm. Linear low density polyethylene does not exhibit the pronounced shear thinning of branched LDPE, so narrow die gaps below 1.5 mm can generate high die pressure and increase the risk of melt fracture. Blow-up ratios from 2.0 to 3.0 are typical; lower BUR values improve machine-direction tear while penalizing transverse-direction tear. Frost line height must be positioned high enough to permit bubble cooling but not so high that excessive crystalline orientation at the free surface reduces dart impact. Screen packs of 40/80/40 mesh are commonly used to protect the die from gel contamination. If the storage environment exceeds 60% relative humidity, surface moisture on the pellets can produce bubble defects, and a hopper purge with dry air at 40–50 °C is required before extrusion.

    Melt temperature excursions greater than ±5 °C from the set point can generate bubble instability because the resin’s melt tension is temperature-sensitive. In practice, thermocouple drift in barrel zones above 230 °C can cause gel formation and reduced film impact properties. The maximum allowable back pressure at the breaker plate should be set in the range of 150–300 bar to avoid excessive shear heating. At screw speeds above 120 rpm, the melt temperature may rise faster than the barrel set point, and the use of a barrel cooling blower in the transition zone is often necessary to maintain a stable viscosity.

    When High-Speed Form-Fill-Seal Equipment Demands Seal Integrity

    Seal failure is a critical defect in horizontal and vertical form-fill-seal lines. The seal performance of DOWLEX 2049 is determined by the heat transfer through the film, the polyethylene crystallization rate, and the cooling rate in the seal jaw. On horizontal lines running laminated structures at 60–120 packages/min, seal jaw pressure is commonly set from 0.4 N/mm² to 0.8 N/mm² with dwell times of 0.3–0.6 s. Under these conditions, the resin must reach a molten seal interface without excessive flow from the seal edge; grades with broad molecular weight distribution tolerate higher seal temperatures without squeeze-out. The seal initiation temperature of DOWLEX 2049 on a 25 µm cast film at 100 °C jaw temperature is in the range 95–105 °C; the exact value must be confirmed for the specific film structure because coextruded skins, slip agents, and antiblock particles change the heat transfer. Hot tack is lower for film quenched on a cold chill roll because small spherulites remelt rapidly; slow cooling on a blown film bubble produces larger crystallites that can hold sealing stress over a wider temperature window. The food-grade additive package must not contain migratory amides that exceed the specific migration limit for fatty food simulants under Regulation (EU) No 10/2011.

    Package validation should include ASTM F88 seal strength tests and ASTM F1921 hot-tack measurements on the actual film, because seal strength scales with film thickness. A seal that is 12 N/15 mm at 50 µm may fall below 6 N/15 mm at 25 µm; therefore down-gauging requires separate sealing and abuse testing.

    Melt Rheology and Screw Design Parameters

    The shear viscosity of DOWLEX 2049 at 190 °C and 100 s⁻¹ is expected to fall near 1,000 Pa·s, based on its melt index of 1.0 g/10 min. It exhibits lower shear thinning than autoclave LDPE, so extruder screw designs selected for LDPE may not deliver stable melt temperature under high back pressure. Barrier screws with a continuous spiral barrier flight and a Maddock mixer of 5–8 flight diameters are preferred for LLDPE. The compression ratio should be between 3.0:1 and 4.0:1, and the feed section should be cooled only enough to prevent pellet bridging. The critical shear rate at which sharkskin melt fracture begins depends on melt temperature and die land geometry; for linear grades, increasing die land length from 10:1 to 15:1 relative to the die gap allows the melt to relax and reduces surface defects. On cast film lines with 90 mm extruders and barrier screws, the melt pump may be operated at 10–30 bar suction pressure to damp output variation. The resin does not require drying unless wet; if moisture is present, a dry-air hopper temperature of 40–50 °C for 2–4 h is sufficient.

    Rheometric data generated by a capillary rheometer at 190 °C show shear thinning across the 10–1,000 s⁻¹ range; the power-law index for this resin is reported to be in the range of 0.45–0.60, consistent with linear polyethylene of moderate molecular weight distribution. The melt strength measured by a Göttfert Rheotens device is lower than that of a branched LDPE at the same melt index. This imposes a bubble diameter control requirement on blown film lines; the internal bubble cooling air pressure must be maintained within ±5 Pa at high output to avoid diameter fluctuation and gauge banding.

    Unlike autoclave LDPE, which derives melt strength from long-chain branching, DOWLEX 2049 relies on high molecular weight and a broader molecular weight distribution to stabilize the melt web. As a result, its neck-in and draw resonance behavior in cast film differ from LDPE-rich formulations. In coextrusions where an LDPE-rich skin is used to control neck-in, DOWLEX 2049 can be used in the core or sealant layer. The addition of 10–30 wt% LDPE to DOWLEX 2049 reduces melt fracture and improves bubble stability, but it also raises haze and lowers dart impact relative to the pure LLDPE film. Compared with metallocene LLDPE grades of the same density, DOWLEX 2049 typically shows higher seal initiation temperature and lower clarity; however, the wider molecular weight distribution allows it to be processed on conventional low-pressure dies that would show melt fracture with narrow-distribution resins. The differences therefore are not simple property upgrades but trade-offs involving equipment capability, seal window, and optical targets. Published data for all possible blend configurations is limited, and package performance should be confirmed by ASTM D882 tensile, ASTM D1922 tear, and ASTM D1709A impact testing on the exact film.

    For frozen food packaging, low-temperature brittleness is often characterized by ASTM D746 or by dart impact at -20 °C; DOWLEX 2049 is generally selected where the failure mode must remain ductile rather than brittle at negative temperatures. This is a property of the octene comonomer and the resulting tie-molecule network, not of the melt index alone.

    Down-Gauging Increases the Sensitivity of Food Films to Gauge Variation

    When a food film is down-gauged from 50 µm to 25 µm, the local stress concentration at thin spots becomes dominant. A gauge variation of ±5% at 50 µm may be tolerable, but the same percentage variation at 25 µm can create seal failure and puncture defects because heat transfer and load-bearing capacity are thickness-dependent. On cast film lines with 0.8–1.2 m die widths and chill roll temperatures of 6–10 °C, DOWLEX 2049 can be drawn at high rates, but draw resonance must be controlled by maintaining a stable air gap and die temperature. For cereal liners and frozen food pouches, a thickness of 30–35 µm is often the lower practical limit for this resin when the package must survive distribution at -20 °C. At lower thickness, the seal dwell time is often reduced from 0.5–1.0 s to 0.3–0.6 s; this is possible only if the form-fill-seal machine uses precise temperature control with a variation of ±3 °C at the jaw face. The food contact status is not diminished by down-gauging, but the overall migration value may increase relative to package mass because the surface-to-volume ratio increases; compliance testing should be based on the final thickness and intended food simulant.

    Food-contact compliance for DOWLEX 2049 is not a single worldwide approval. The resin itself must be listed, and the finished structure must satisfy migration limits specific to the food type and use temperature. The matrix below summarizes the principal compliance instruments and their mandatory test or condition.

    Food-contact compliance matrix for DOWLEX 2049
    Regulation/StandardScopeMandatory Condition or Test
    U.S. FDA 21 CFR 177.1520Olefin polymers for food contactComply with density, extractables, and food-type/use-temperature limitations; verify finished article under end-use conditions.
    Regulation (EU) No 10/2011Plastic materials and articles intended for food contactOverall migration limit 10 mg/dm²; specific migration limits apply to additives based on simulants A, B, C, D1, D2, E.
    Canadian Food and Drugs Act, Division 23Polyethylene for food packagingBase polymer positive list; additives must meet Division 23 limits.
    China GB 9685-2016Additives permitted in food contact materialsPermitted additive positive list and specific migration limits.
    REACH (EC) No 1907/2006Registration and SVHC communicationArticle 33 communication if candidate list substance exceeds 0.1 wt%.