| HS Code | 473008 |
| Density | 0.920 g/cm³ |
| Meltindex 190c 2 16kg | 2.3 g/10 min |
| Meltflowratio I21 I2 | 30 |
| Comonomer | Octene-1 |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Meltingpoint | 124 °C |
| Vicatsofteningpoint | 108 °C |
| Tensilestrengthatyield | 11 MPa |
| Tensilestrengthatbreak | 25 MPa |
| Elongationatbreak | 800% |
| Flexuralmodulus | 240 MPa |
| Form | Pellets |
| Color | Natural |
As an accredited Dow DOWLEX™ 2047G Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DOWLEX™ 2047G is supplied in 25 kg polyethylene bags, typically 55 bags per pallet, totaling 1,375 kg. |
| Container Loading (20′ FCL) | 20′ FCL loading: Dow DOWLEX™ 2047G Linear Low Density Polyethylene, 25 kg bags, palletized, stretch-wrapped, securely stowed; approx. 20–22 MT net. |
| Shipping | Dow DOWLEX™ 2047G Linear Low Density Polyethylene is shipped as non-hazardous, free-flowing pellets in 25 kg bags on stretch-wrapped pallets, or in bulk trucks/railcars. Store in a cool, dry, ventilated area away from heat, sunlight, and ignition sources; follow SDS and local regulations. |
| Storage | Store DOWLEX™ 2047G in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and oxidizing agents. Keep original packaging closed and pallets stable; avoid excessive stacking. Protect from moisture, dust, and contamination. Maintain normal ambient temperatures and good housekeeping. Follow the supplier safety data sheet and local regulations for safe handling and storage. |
| Shelf Life | Shelf life: 24 months from manufacture when stored in original packaging in a cool, dry, well-ventilated area, away from direct sunlight. |
On high-speed cast film lines producing pallet-unitizing stretch film, DOWLEX™ 2047G is introduced as the primary resin because its octene-derived short-chain branch distribution reduces draw resonance amplitude at take-off velocities above 300 m/min. In commercial practice the formulation is not a single-component system: converters dry-blend 80–95 wt% of 2047G with 5–20 wt% of fractional-melt LDPE to suppress neck-in and improve transverse gauge uniformity, while 1.0–2.5 wt% of a cling-agent masterbatch is added at the feed throat to generate the tack layer required for pallet load retention. Extrusion is performed on a 75–120 mm single-screw extruder with a barrier-flighted screw of 30:1 L/D, a melt temperature maintained between 230 °C and 260 °C, and a flat coathanger die with 0.7–0.9 mm lip gap feeding a polished chill roll held at 15–30 °C. The air gap between die exit and chill roll surface is typically set at 15–25 mm because longer gaps increase neck-in and edge trim, while shorter gaps produce transverse flow marks on the cast web. The terminal cast stretch film is usually downgauged to 12–30 µm; however, production-side audits show that stable operation below 10 µm requires a melt temperature envelope of ±5 °C, because edge-bead thickness deviations above 3 µm initiate roll blocking and web snaps in the air gap. Compliance for food-contact pallet wrap in the EU is governed by Regulation (EU) 10/2011, and in the United States by 21 CFR 177.1520(c) for olefin polymers; mechanical property verification follows ASTM D882 for tensile modulus and tensile elongation, ASTM D5748 for puncture resistance of stretch wrap film, and ASTM D5458 for peel cling force after one unwinding cycle. Terminal finished product types include machine pallet stretch film, handwrap film, and pre-stretched wrap.
When blown film converters replace butene-based C4-LLDPE with an octene-based LLDPE such as 2047G, the frost line height and internal bubble pressure are not directly transferable parameters because the melt strength and strain-hardening response alter the bubble geometry. A practical starting formulation is 80 wt% 2047G and 20 wt% high-pressure LDPE; the blend is processed through a 250 mm spiral mandrel die with a 1.8–2.2 mm die gap, a blow-up ratio between 2.2:1 and 2.8:1, and a frost line height maintained at 500–700 mm above the air ring to balance machine-direction and transverse-direction orientation. Melt temperature is controlled at 190–215 °C, and internal bubble stabilization is achieved with a dual-lip air ring and optional internal bubble cooling. When bubble oscillation appears at high stalk heights, the formulation ratio is shifted to 70/30 2047G/LDPE; however, raising LDPE above 30 wt% lowers dart impact resistance below the threshold required for heavy-duty shipping sacks, as measured by ASTM D1709. Downstream conversion includes gusseting, surface corona treatment to 38–42 mN/m, and bottom-seal or valve-patch insertion. Terminal finished product types include industrial distributor sacks, chemical bag liners, and FIBC inner liners. Compliance obligations for non-food industrial packaging include Directive 2011/65/EU RoHS Annex II heavy-metal limits and Regulation (EC) No 1907/2006 REACH Article 33 SVHC communication; sack drop resistance is verified according to ISO 7965-2 and tear propagation according to ASTM D1922.
| Regulation / Standard | Designation or clause | Application condition |
|---|---|---|
| United States FDA food-contact olefin polymers | 21 CFR 177.1520(c) | Food-contact film, sealant layers, and coatings; end-use extractive limits apply. |
| European Union food-contact plastics | Regulation (EU) 10/2011 | Overall migration limits and specific migration limits for additives in finished articles. |
| REACH substances of very high concern | Regulation (EC) No 1907/2006 Article 33 | Supply-chain communication obligations for SVHC above 0.1 wt% article threshold. |
| RoHS heavy metals | Directive 2011/65/EU Annex II | Non-food industrial packaging and durables; maximum concentration values by weight. |
| Film tensile and tear | ASTM D882, ASTM D1922 | Tensile modulus/elongation and Elmendorf tear of thin film. |
For coextruded flexible packaging sealant webs running on vertical form-fill-seal equipment, 2047G is positioned as the heat-seal layer because the initial sealing window and hot-tack strength support jaw speeds above 40 cycles/min on polyethylene-based structures. The sealant layer typically constitutes 20–40 wt% of the total coextruded film thickness, with the remaining layers comprising tie resins, EVOH barrier, and a reverse-print skin of LDPE or HDPE; a plastomer modifier may be added at 10–20 wt% of the sealant layer to widen the hot-tack plateau, but the plastomer level is capped because higher additions reduce film stiffness. The coextrusion line is configured with three or five extruders feeding a 200–400 mm spiral die with a 1.5–2.5 mm die gap, a blow-up ratio of 2.0:1–2.5:1, and a melt temperature of 200–220 °C. Seal initiation temperature and hot-tack force are measured under ASTM F1921, and seal strength under ASTM F88/F88M; food-contact compliance is assessed under Regulation (EU) 10/2011 and 21 CFR 177.1520(c). Terminal finished product types include stand-up pouches, pillow bags for frozen food, and resealable pouch stock. Operational limitations include jaw contamination at seal-bar temperatures above 160 °C when the sealant layer is below 20 µm, which can be mitigated by raising the sealant layer thickness or reducing line dwell time.
Tandem blown film lamination lines reach the downgauging limit of 2047G when gauge uniformity and blocking tendency, not intrinsic melt strength, become the controlling variables. The resin is processed as a 100 wt% virgin stream with 0.5–1.0 wt% of a slip/antiblock masterbatch; the bubble is formed through a 1.8–2.0 mm die gap at a blow-up ratio of 2.5:1 and a melt temperature of 180–205 °C. Film below 20 µm requires a frost line height below 400 mm and a take-off speed above 50 m/min to prevent blocking on the collapsing frame. Terminal finished product types include thermal lamination film, document pouches, and book cover lamination. Compliance for these non-food applications is limited to Directive 2011/65/EU RoHS and Regulation (EC) No 1907/2006 REACH; optical quality is verified by ASTM D1003 haze and ASTM D2457 gloss measurements.
In agricultural greenhouse film production, a three-layer coextrusion line is configured with a core layer containing 60–80 wt% 2047G, 10–20 wt% high-pressure LDPE, and 8–12 wt% of a UV stabilizer masterbatch; the inner and outer skins are composed of LDPE-rich layers with anti-fog concentrate dosed at 1–3 wt% to control condensation. The bubble is extruded through a 200–350 mm die with 1.8–2.4 mm lip gap, a blow-up ratio between 2.5:1 and 3.0:1, and a melt temperature of 190–215 °C. Long-term weathering is verified according to ISO 4892-2 xenon-arc exposure, and tear resistance by ASTM D1004; European agricultural film specifications are covered by EN 13206. Published data for the exact UV retention of this specific grade in multi-season greenhouse service is limited, so converters validate additive masterbatch concentrations through outdoor weathering trials before full-scale manufacture. Terminal finished product types include single-span greenhouse covers, low-tunnel film, and mulch film backing stock.
Extrusion coaters running 2047G as the sealant skin on paperboard or aluminium foil observe that the oxidation level in the melt curtain controls adhesion strength and neck-in performance. The coating blend is formulated with 70–90 wt% 2047G and 10–30 wt% high-pressure LDPE; the LDPE fraction raises melt extensibility and reduces edge neck-in across the 500–1000 mm flat die. Processing conditions include a 90–120 mm single-screw extruder with 30:1 L/D, a melt temperature of 280–320 °C, an air gap of 150–250 mm, and line speeds of 100–300 m/min. Coating weight is typically 15–30 g/m²; below 12 g/m² the melt curtain becomes unstable and adhesion to substrates drops unless the air gap is shortened or the melt temperature is raised within the specified window. Adhesion is tested under ASTM F88/F88M for seal strength or ASTM D1876 for peel resistance; food-contact status requires 21 CFR 177.1520(c) and Regulation (EU) 10/2011. Terminal finished product types include coated paperboard for aseptic carton stock, industrial wrapping substrates, and release-liner base film.
Competitive Dow DOWLEX™ 2047G Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DOWLEX™ 2047G Linear Low Density Polyethylene is an ethylene–octene linear low density polyethylene produced by solution polymerization and supplied as uncoloured pellets. The resin is specified as a general-purpose blown film grade with a nominal density of 0.920 g/cm³ (ASTM D792) and a nominal melt index of 2.3 g/10 min (ASTM D1238, 190 °C/2.16 kg). The density value places the material within the conventional linear low density envelope of 0.915–0.925 g/cm³, while the melt index provides a balance between thin-gauge drawdown and bubble retention. The octene comonomer introduces C6 short-chain branches; by comparison, a butene-comonomer LLDPE introduces C2 branches. The longer branching architecture of the octene unit modifies interlamellar tie-molecule formation during quench cooling, which is the primary structural reason for the product’s improved dart impact and Elmendorf tear response relative to butene-copolymer LLDPE at equivalent crystallinity when tested under ASTM D1709 and ASTM D1922.
Film property comparisons for this grade require conditioning at 23 ± 2 °C and 50 ± 5% RH in accordance with ASTM D618. Tensile properties are normally determined by ASTM D882 with a jaw separation rate of 500 mm/min; Elmendorf tear is determined by ASTM D1922; and dart impact is determined by ASTM D1709 Method A using a 38.1 mm dart and a fall height of 66 cm. Published data for this specific film configuration is limited to the manufacturer’s current technical data sheet and certificate of analysis. Nominal resin values are not film performance specifications, and converter-generated data should be accompanied by gauge, blow-up ratio, frost-line height, and conditioning history.
Rheological characterisation of DOWLEX 2047G by parallel-plate oscillatory shear at 190 °C following ISO 6721-10 typically shows the expected shear-thinning behaviour of a solution LLDPE. Relative to a 1.0 g/10 min grade, the 2.3 g/10 min melt index shifts the low-shear viscosity curve downward in the 0.01–1 rad/s range and reduces the pressure required to pass the melt through a screen pack and die land. The practical consequence is lower extruder torque at the same screw speed on a given line; however, the linear backbone also provides less extensional strain hardening than autoclave LDPE, so high-stalk film lines require external cooling to maintain freeze-line height.
Processing above 240 °C or extended hold time in the die can produce oxidative gel defects; the resin should be purged at shutdown with a suitable LDPE or dedicated purging compound. Pre-drying is generally unnecessary when pellets are stored in sealed containers at 10–30 °C; if storage humidity exceeds 60% RH, surface moisture can be removed by drying at 60–70 °C for 2–4 h in a hot-air dryer.
High-stalk conversion of DOWLEX 2047G is governed by melt strength and freeze-line displacement. Because the polymer is essentially linear, it lacks the long-chain branching that gives autoclave LDPE its extensional-hardening response. A 65 mm extruder with a 24:1 L/D barrier screw and a 200 mm spiral mandrel die can be started with melt temperatures from 190 °C to 240 °C and a die gap of 1.5–2.5 mm. Die gaps below 1.2 mm raise shear stress at the lip; if the melt temperature falls below 200 °C, sharkskin melt fracture may appear as periodic surface roughness on the inner and outer bubble surfaces. The onset of this defect is a function of die-lip clean-up and output, not a single resin viscosity threshold.
Internal bubble cooling with chilled air at 10–15 °C or a dual-lip air ring is recommended when the frost line must be held at 3–8 die diameters. Insufficient cooling leads to low freeze-line height and greater bubble sag, especially in films below 50 µm. Where the line is equipped with an IBC system, the control target is usually a pressure differential of several hundred pascals; the actual setting depends on die diameter and collapsed width. Operators should monitor bubble diameter stability continuously because the relatively narrow molecular weight distribution of a solution LLDPE can produce sudden bubble breaks if the primary nip speed and blower output are not synchronized.
| Processing variable | Setting or equipment boundary | Reference condition |
|---|---|---|
| Melt temperature | 190–240 °C | Extruder zones from feed to die |
| Die gap | 1.5–2.5 mm | Spiral mandrel die |
| Blow-up ratio | 2.0:1–3.5:1 | Air ring and cage alignment |
| Frost-line height | 3–8 die diameters | IBC or dual-lip air ring |
These values are process starting conditions and are not product specification limits. A change in die diameter, screen-pack mesh, or screw design alters the shear history and requires revalidation of melt pressure and bubble cooling.
Replacement of a butene-copolymer LLDPE with DOWLEX 2047G at the same film gauge generally moves the tear–dart balance upward, provided the extrusion line is not limited by melt temperature. The C6 branch length of octene promotes a broader interlamellar amorphous layer, which increases the probability of stress transfer between crystalline lamellae. This mechanism is relevant to ASTM D1709 dart impact and ASTM D1922 Elmendorf tear results; however, the exact increment depends on quench rate, blow-up ratio, and film thickness. When a converter substitutes the resin in an existing formula, comparative testing at 25 µm and 50 µm is required because tear anisotropy in LLDPE films changes with orientation.
In contrast, butene-copolymer LLDPE at similar density and melt index may show lower puncture and tear resistance under equivalent processing conditions. The difference is not merely a function of comonomer type; it is amplified by the thermal history, die gap, and film gauge. Comparative hot-tack and seal-initiation behaviour must be tested using ASTM F1921 and ASTM F88 on the same sealing machine because differences in film cooling and ageing shift the seal curve by 5–10 °C.
Relative to DOWLEX 2045G, which has the same nominal density of 0.920 g/cm³ and a nominal melt index of 1.0 g/10 min, DOWLEX 2047G provides higher fluidity for thin-gauge film and easier drawdown, but may exhibit lower high-stalk bubble stability. The choice between the two grades is therefore equipment-dependent: extruders with limited torque or small die gaps benefit from 2047G, while high-stalk lines with tall bubble geometry may retain 2045G.
| Property | Test method | Nominal value |
|---|---|---|
| Density | ASTM D792 | 0.920 g/cm³ |
| Melt index | ASTM D1238, 190 °C/2.16 kg | 2.3 g/10 min |
Nominal values are not specification limits. Current lot certificates of analysis provide the applicable production tolerance.
Substitution of autoclave LDPE with DOWLEX 2047G requires attention to melt tension and extensional behaviour. Autoclave LDPE exhibits long-chain branching and strain hardening, whereas DOWLEX 2047G extends with limited strain hardening. In blown film, this shifts the bubble stability point upward; lines that carry a high stalk with LDPE may need a lower stalk or additional cooling with DOWLEX 2047G. In cast film, the absence of long-chain branching reduces edge neck-in but may require a higher chill-roll temperature to maintain quench and prevent surface defects. Published data for direct replacement in collation shrink film is limited; tensile properties must be compared using ASTM D882 at the same gauge.
In heavy-duty sacks and industrial liners produced at 150–200 µm, fractional-MI LLDPE grades are often selected for toughness but can limit output because of high melt pressure and motor load. DOWLEX 2047G, with a melt index of 2.3 g/10 min, permits an increase in screw speed without the corresponding pressure rise on 90–120 mm extruders equipped with 30:1 L/D barrier screws. The limiting variable shifts from extrusion pressure to bubble tension: at output rates above 1.0 kg/h per mm die circumference, the web may form wrinkles if the collapsing frame geometry and primary nip speed are not matched to the higher web velocity. A 200 mm die with a dual-lip air ring can be operated in the 0.9–1.1 kg/h per mm die circumference range when the cooling air is held at 12–18 °C; however, published data for this specific configuration is limited.
Orientation balance in such films is controlled by the blow-up ratio, not by melt index alone. A BUR of 2.5:1 is a common reference point for technical data, but actual line settings may vary from 2.0:1 to 3.5:1 depending on the desired machine-direction to transverse-direction tensile ratio. Films run at BUR 2.0:1 favour machine-direction orientation and tend to show higher MD tensile strength and lower transverse tear resistance. The correct balance should be verified with ASTM D882 tensile and ASTM D1922 tear measurements on film sampled from three positions across the lay-flat width.
When DOWLEX 2047G is substituted for a 1.0 g/10 min fractional-MI LLDPE on a 90 mm extruder with a 30:1 L/D barrier screw, the higher melt index reduces the pressure required to move the melt through the screen pack and die. The conversion does not eliminate the need for torque monitoring: the drive motor current should be recorded at the same screw speed and compared with the historical average for the previous resin. In the absence of a melt-pressure transducer, a portable pressure gauge at the breaker plate can identify pressure-drop changes greater than 10%, which usually indicate screen-pack plugging rather than resin variation. Published data for this specific equipment configuration is limited; the replacement decision should be supported by a short production trial with inline melt pressure and bubble-diameter logging.
As supplied, DOWLEX 2047G is not typically formulated as a slip-modified or antiblock-modified grade; the standard product form should be confirmed with the supplier. Converters who require a coefficient of friction below 0.2 (ISO 8295) should add an external slip/antiblock masterbatch that has been pre-dispersed on a high-shear compounding line. The addition rate is normally determined by film gauge and blocking tendency; a starting range of 500–1,500 ppm active slip is common for LLDPE films, but the exact level must be adjusted because excess slip can reduce heat-seal strength and increase haze as measured by ASTM D1003.
Seal performance is a function of jaw temperature, dwell time, and jaw pressure on the packaging machine. A starting seal characterisation can be performed on a laboratory hot-tack tester according to ASTM F1921 and on a heat-seal strength apparatus according to ASTM F88. With 50 µm monolayer film, a dwell time of 0.5 s and a sealing pressure of 0.3 N/mm² are often used as screening conditions; the actual production window must be determined at the line speed of the intended horizontal form-fill-seal or vertical form-fill-seal machine. Because the melting range of the resin is narrow, the seal temperature ladder should be run in increments of 5 °C to avoid burn-through at the upper end and weak seals at the lower end.
Regulatory conformance is end-use and formulation specific. The supplier’s current regulatory bulletin should be consulted for REACH registration, food-contact status, and residual-monomer information. Polyethylene grades of this class may be evaluated under 21 CFR 177.1520(c) for food-contact use and under European Union Directive 10/2011 when supported by migration testing; no food-contact certification is attached to the resin alone because the final article contains conversion additives, printing inks, and possibly recycled content. These additions must be included in the overall migration assessment. RoHS compliance for hazardous substances should be documented through the supplier’s material declaration.
In coextruded structures, DOWLEX 2047G is placed in the core or skin layers of ABA and ABC films to increase dart impact while maintaining surface gloss. The melt index of 2.3 g/10 min matches the viscosity of typical LDPE skins and allows the die adapter to maintain layer uniformity. If the resin is paired with a 0.5 dg/min high-density layer, the viscosity mismatch can produce layer encapsulation; a coextrusion feedblock designed with viscosity-ratio compensation is required. Layer uniformity is checked by cross-sectional microscopy and by measuring the thickness profile to within ±5% of target.
In agricultural silage and greenhouse films, DOWLEX 2047G is used in coextruded structures where puncture and tear propagation are critical field-performance parameters. Film structures at 150–200 µm are produced with internal bubble cooling and assessed for puncture resistance using ISO 7765-2 or an equivalent method tailored to agricultural film. The melt index of 2.3 g/10 min supports coextrusion with metallocene line layers when the die is designed for layer stability; the line-layer ratio must be validated with ASTM D882 and ASTM D1922 after ageing because tear resistance in thick films can decline after outdoor exposure. Accelerated weathering tests such as ISO 4892-2 are often specified by the final film producer, but the resin does not contain UV stabilisers in standard form and stabiliser masterbatches must be added for long-term outdoor exposure.