    Specifications
    HS Code 392888
    Product Name Dow DOWLEX™ 2047A Linear Low Density Polyethylene, Cast Film Grade
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Octene-1
    Density 0.917 g/cm³
    Melt Index 190 C 2 16 Kg 2.3 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 9 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 600%
    1 Secant Modulus 200 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Haze 4%
    Gloss 45 80%
    Coefficient Of Friction 0.2

    As an accredited Dow DOWLEX™ 2047A Linear Low Density Polyethylene, Cast Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DOWLEX™ 2047A Cast Film Grade is packaged in 25 kg polyethylene bags, securely palletized and wrapped for transport.
    Container Loading (20′ FCL) Dow DOWLEX™ 2047A loads 10 pallets per 20′ FCL, each 55 x 25 kg bags, totaling 13.75 MT net.
    Shipping Dow DOWLEX™ 2047A is shipped as non-hazardous polyethylene resin pellets in 25 kg moisture-barrier bags, unitized on stretch-wrapped pallets. Transport in clean, dry, covered trucks or railcars. Store in a cool, dry, ventilated area away from direct sunlight, heat, and ignition sources. Avoid puncturing bags or contaminating pellets.
    Storage Store Dow DOWLEX™ 2047A indoors in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers or bags closed to prevent moisture, dust, and contamination. Use stable, limited-height stacks on clean pallets. Avoid prolonged UV exposure and extreme temperatures. Do not stack excessively high. Follow the supplier’s SDS and local regulations for safe handling and storage.
    Shelf Life Shelf life is 24 months from manufacture when stored in original unopened packaging, dry, cool, and away from direct sunlight.
    Application of Dow DOWLEX™ 2047A Linear Low Density Polyethylene, Cast Film Grade

    Stretch pallet wrap, low-gel cast film at 300 m/min line speed

    On cast film lines equipped with 75 mm to 105 mm extruders and 36:1 L/D barrier screws, DOWLEX™ 2047A is processed at melt temperatures of 240 °C to 270 °C, with head pressures upstream of a 70/120/170 mesh screen pack commonly logged at 180 bar to 260 bar. The resin’s nominal density of 0.920 g/cm³ measured by ASTM D792 and melt flow index of 2.3 g/10 min measured by ASTM D1238 at 190 °C/2.16 kg produce the low melt strength and rapid stress relaxation required for cast stretch orientation. Because of that rheological profile, die-to-chill-roll draw distance is controlled within 8 mm to 15 mm, air gap from die lip to primary chill roll is kept at 3 mm to 8 mm, and the first chill roll surface temperature is maintained between 15 °C and 25 °C while downstream cooling rolls are held at 40 °C to 60 °C to prevent roll wrap, blocking, and uneven cold crystallization. On 2,500 mm wide lines running from 250 m/min to 600 m/min, the dominant process failure modes are edge neck-in above 12% total width reduction, die-line haze caused by oxidized polymer accumulation at the lip, and gel-induced film break below 8 µm thickness. These failures are controlled by keeping the die exit temperature 5 °C to 10 °C above the last barrel zone temperature, by reducing spool residence time below 20 min, and by excluding regrind containing polyethylene wax, paper fiber, or low-molecular-weight cling masterbatch. The formulation practice for pallet-load containment is built around the resin as the main PE phase at 80 wt% to 100 wt%, with 0 wt% to 20 wt% of a lower-MI cast film LLDPE to widen edge stability and 0.5 wt% to 5 wt% of cling masterbatch based on polyisobutylene or ethylene-vinyl acetate copolymer to generate differential unwinding force. Industrial stretch wrap is not subject to direct food-contact requirements, but logistic performance is evaluated against ASTM D5458-95(2018) for peel cling force, ASTM D5748-95(2019) for protrusion puncture resistance of stretch wrap film, and EN 14477:2004 for puncture resistance under logistic handling; when the same film is used as tertiary packaging around primary food packages, converters commonly verify EU Regulation (EC) No 1935/2004 Article 3 and Regulation (EU) No 10/2011 if transfer to the primary package is possible. The terminal finished products are machine-applied power-stretch rolls in 10 µm to 23 µm nominal thickness and pre-stretched hand-wrap rolls at 8 µm to 15 µm, supplied for pallet stabilization where load retention forces of 60 cN/25 mm to 140 cN/25 mm at 200% to 250% elongation are demanded. The upper processing boundary is defined not by screw torque or drive load but by odor generation and volatile condensate on the chill roll: above 270 °C melt temperature, low-molecular-weight oxidation products increase sufficiently to contaminate the air knife plenum and produce film surface deposits, so the practical operating window is bounded by dart impact retention and optical clarity.

    At the lower end of the thickness range, film break frequency on high-speed cast lines depends on the relationship between film puncture force and line acceleration during roll transfer. Operators observe batch-to-batch variance of ±3% to ±5% in melt flow index between production lots, which can shift draw resonance onset by 10 m/min to 20 m/min; to compensate, extruder speed is adjusted by 5 rpm to 15 rpm and the chill roll drive is biased by 0.5% to 1.5% relative speed. If a batch arrives at the upper MI limit, neck-in may increase from 45 mm to 65 mm per edge on a 2,500 mm line, requiring die deckle repositioning and potential trim waste above 6%. Published data for the exact interaction of choker-bar temperature with octene short-chain branching distribution in this specific resin is limited, so converters rely on vendor lot data and in-line optical haze measurement at 5 µm resolution rather than laboratory extraction alone.

    A monolayer cast web intended for direct food contact at subzero temperatures is run at 240 °C to 260 °C melt temperature, with a 45 °C primary chill roll, 2.0% to 5.0% primary draw, and 0.8 mm to 1.2 mm die gap. In direct food-contact use, the polyethylene phase is commonly 90 wt% to 100 wt% DOWLEX™ 2047A, with 0 wt% to 10 wt% of a high-clarity LDPE cast grade to improve tear directionality and 1.0 wt% to 3.0 wt% of silica-based antiblock masterbatch and erucamide slip masterbatch to control kinetic film-to-film coefficient of friction between 0.25 and 0.40 per ASTM D1894. The regulatory anchor for the food-contact side is FDA 21 CFR § 177.1520(c) for olefin polymers, which requires the finished article to meet the applicable extractables and density-based olefin polymer specifications, and the EU side is controlled by Regulation (EU) No 10/2011 Annex I with an overall migration limit of 10 mg/dm² and specific migration limits for approved additives. For frozen food flow wrap, a 38 dyn/cm to 44 dyn/cm corona-treated print or lamination surface is required for water-based ink adhesion; treatment is applied in-line after the secondary cooling roll and before winding, with decay from 44 dyn/cm to 36 dyn/cm over 72 h when slip masterbatch blooms to the surface. The downstream production process includes automatic gauge control across the web using beta or X-ray thickness scanning and segmented die bolts at 25 mm spacing, allowing total thickness variation below ±3% on a 30 µm target. Terminal finished product types are side-gusseted form-fill-seal flow packs for leafy greens, over-wrapped packs for frozen seafood, and pillow packs for bakery under modified atmosphere; the films are also used as heat-sealable lamination substrates to oriented polyester or biaxially oriented polypropylene. A demonstrable limitation is that the film is not suitable for high-acid tomato paste or alcohol-containing liquid foods unless an additional functional barrier layer is present, because LLDPE alone does not provide the oxygen and aroma barrier required by such products, and the heat seal range under high-speed packaging line dwell times narrows to 110 °C to 130 °C.

    What constraints govern the use of DOWLEX 2047A in cold-chain liquid liner sealant webs?

    In two-layer and three-layer bag-in-box liner coextrusions for chilled and aseptic liquid packaging, DOWLEX™ 2047A is specified for the sealant/contact layer at 60 wt% to 85 wt% of the PE-rich skin, with 10 wt% to 30 wt% of a linear low density or low density polyethylene with a lower seal initiation temperature, and 5 wt% to 15 wt% of white masterbatch for opacity in fat-containing liquid applications. The film structure is commonly a 45 µm to 90 µm cast coextrusion with a core layer of EVOH or metallized polyester as oxygen barrier, and the DOWLEX 2047A skin provides flexural crack resistance and seal integrity after repeated folding; this is evaluated by ASTM F392/F392M-20 using 10 cycles of Gelbo flex at -20 °C followed by dye penetration, with acceptance at <0.1% pinhole area. The regulatory anchor for the product-contact layer is FDA 21 CFR § 177.1520(c) for food-grade olefin polymers, supported by Regulation (EU) No 10/2011 Annex I, and for aseptic filling lines the converter must also demonstrate that migration of primary aromatic amines from polyurethane adhesives meets the specific migration limit in Regulation (EU) No 10/2011, although the DOWLEX 2047A layer is not the source of such amines. Processing on a cast line is performed at 250 °C to 265 °C melt temperature; the skin layer is separated from the hot die by a short 10 mm to 20 mm air gap onto a 18 °C to 22 °C matte chill roll to reduce ethylene-vinyl acetate volatilization and to build a fine crystal structure that resists environmental stress cracking. Terminal finished product types are 1 L to 10 L bag-in-box liners for liquid egg, dairy cream, edible oil, and cold-chain coffee extract, where seal strength is required to exceed 1.8 kgf/15 mm at 85 °C seal bar temperature per ASTM F88/F88M-21. A significant process conflict is the balance between high-seal-integrity surface cooling and low-gel build-up: raising chill roll temperature above 25 °C improves seal strength but increases blocking, while lowering it below 15 °C raises seal initiation temperature by 5 °C to 8 °C. Converters therefore often run a dual-zone chill roll at 18 °C first zone and 40 °C second zone to control crystallinity at the sealant face.

    Extraction testing for such structures generally follows Regulation (EU) No 10/2011 food simulant selection rules, with 10 days at 40 °C for long-term chilled contact or 2 h at 70 °C for short-term hot-fill conditions, but published data for this specific DOWLEX 2047A thickness and white masterbatch loading is limited. The practical formulation ceiling for white masterbatch is governed by flex crack resistance rather than processability: above 15 wt% masterbatch, filler loading creates stress concentration sites that can reduce Gelbo flex performance by 20% to 30% relative to the unfilled skin. The use of DOWLEX 2047A in this application is therefore bounded by seal initiation temperature, pinhole generation after flexing, and compliance documentation from the supplier covering the approval status of antioxidant and slip packages for fatty food contact.

    Coextruded surface-protection webs based on DOWLEX™ 2047A are produced on multi-roll stack cast lines with a 900 mm to 1,800 mm coat-hanger die, a 0.8 mm die gap, and a matte-finish chill roll at 20 °C to 30 °C followed by an embossing nip at 50 °C to 80 °C. In a two-layer construction, the bulk and front skin layer is formulated with 70 wt% to 90 wt% DOWLEX™ 2047A blended with 10 wt% to 30 wt% of a lower-modulus linear low density polyethylene or polyolefin plastomer to control conformability on curved substrates, while a reverse-side pressure-sensitive adhesive layer may be coextruded or solvent-coated. The base film is corona-treated to 40 dyn/cm to 46 dyn/cm before coating so that the water-based acrylic or rubber-based removal adhesive wets without pinholes; peel adhesion is adjusted to 0.2 N/25 mm to 2.5 N/25 mm by altering adhesive coat weight, and the film is tested for 24 h and 7 d peel evolution on PMMA, polycarbonate, and grade 304 stainless steel coupons. Compliance for this non-food industrial application falls under REACH Regulation (EC) No 1907/2006 Annex XVII restricted substances and, when the protected article is an electrical or electronic component, Directive 2011/65/EU RoHS Annex II; no direct food-contact declaration is generated unless the film is also evaluated under FDA 21 CFR § 177.1520(c). The terminal finished product types are temporary protective films in 40 µm to 80 µm thickness supplied in roll widths of 1,000 mm to 2,200 mm for acrylic sheet, polycarbonate glazing, pre-painted metal coil, and flat glass during fabrication and installation. The primary processing bottleneck is optical clarity after removal: if the base film contains high-gel particles from resin or regrind, the adhesive surface shows pressure-transfer defects on glossy acrylic; therefore, the extrusion line uses 100/120/170 mesh filtration and limits regrind to <15% of the virgin resin feed. Published data for the specific tackifier migration coefficient between the adhesive and DOWLEX 2047A skin is limited, so converter trials are required for long-term plasticizer resistance on polycarbonate.

    When a 0.920 g/cm³ cast film resin is specified for low-temperature puncture resistance

    Heavy-duty cast liners for drum and gaylord applications are extruded at 220 °C to 250 °C melt temperature on single-flite screw lines with 30:1 to 36:1 L/D and a screen changer containing 70/120/170 mesh packs, because higher melt temperatures increase the risk of gel formation from recycled content. The blend formula uses 65 wt% to 85 wt% DOWLEX™ 2047A as the virgin film-grade phase, 15 wt% to 35 wt% of clean post-industrial LLDPE regrind, and 0.5 wt% to 2.0 wt% of a UV stabilizer masterbatch when outdoor storage is intended. Low-temperature performance is measured by ASTM D1709-16a drop dart impact at -18 °C after 48 h conditioning, with reported converter values for a 50 µm cast film generally between 150 g and 350 g depending on regrind fraction and chill roll conditions; published data for this specific resin grade at this thickness is limited. Tear resistance is assessed by ASTM D1922-09(2015) Elmendorf tear in machine direction and transverse direction, where cast orientation lowers machine-direction tear but raises transverse-direction tear relative to blown film. Compliance for non-food industrial containment is governed by REACH Regulation (EC) No 1907/2006 and, for reusable transport packaging, ISO 14021:2016 for recycled content claims when post-industrial regrind is included; if the liner is used for chemical powders, the converter verifies that the regrind stream is free of residues under Directive 2008/98/EC waste framework compliance declarations. The downstream production process includes lay-flat tubing or bottom-seal bag conversion with ultrasonic or impulse sealing at 130 °C to 150 °C; cast film from DOWLEX 2047A seals through contamination more effectively than blown film with heavy additive loading. Terminal finished product types are open-top and valve-style liners for 200 L drums, gaylord liners up to 1,200 kg capacity, and collation shrink overwrap for engineered polymer granules. The critical processing limit is the use of high levels of post-industrial regrind: above 35%, melt flow index may shift upward by 10% to 20% depending on prior heat history, narrowing the cast line’s neck-in window and increasing edge trim failure; batch consistency is therefore maintained by melt filtration and by testing each regrind lot for melt flow index per ISO 1133-1:2022 and density per ASTM D792.

    For a 35 µm to 60 µm sealant web laminated to oriented polyester or biaxially oriented polypropylene in dry food and medical device pouches, DOWLEX™ 2047A is run as the inner skin layer at 70 wt% to 90 wt% of the PE skin, with 10 wt% to 30 wt% of a lower-seal-initiation LLDPE or EVA copolymer to allow sealing through powder contamination. The film is produced on a two-layer cast coextrusion line with a 1,000 mm die, 0.7 mm to 0.9 mm die gap, and 25 °C to 35 °C first chill roll, with the second cooling roll at 45 °C to 55 °C so that the non-seal side retains 38 dyn/cm to 42 dyn/cm corona treatment for lamination adhesion. Seal strength is required to reach 2.0 kgf/25 mm to 3.5 kgf/25 mm at 95 °C to 125 °C seal bar setpoints, measured by ASTM F88/F88M-21, while the unsealed web is tested for grammage profile uniformity using a non-contact beta gauge at ±3%. Compliance in dry food is anchored to FDA 21 CFR § 177.1520(c) and Regulation (EU) No 10/2011 Annex I with total migration 10 mg/dm²; medical device pouch applications require ISO 11607-1:2019 for sterile barrier packaging validation, where the DOWLEX 2047A layer contributes seal integrity but not sterile barrier performance unless combined with Tyvek or another microbial barrier substrate. The downstream conversion process includes lamination with a two-component solvent-free polyurethane adhesive at 0.8 g/m² to 1.8 g/m² coat weight, followed by slitting into 150 mm to 600 mm reels for horizontal form-fill-seal machines. Terminal finished product types are pharmaceutical blister lidding, dry beverage stick pack laminates, and peelable pouch structures for medical instruments. A notable boundary is that DOWLEX™ 2047A is not recommended for repeated steam sterilization above 121 °C in unstressed pouch form without dimensional distortion; converters use the resin for ethylene oxide or gamma-sterilized packages only when the seal layer is protected by a higher-temperature outer web and the sterilant dose does not exceed 25 kGy to 50 kGy per cycle.

    Free Quote

    Competitive Dow DOWLEX™ 2047A Linear Low Density Polyethylene, Cast Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2047A Linear Low Density Polyethylene is supplied as a pelletized cast film resin with a typical density of 0.920 g/cm³ when determined by ISO 1183-1 or ASTM D792-20, and a melt flow rate of 1.0 g/10 min at 190°C/2.16 kg using ISO 1133-1:2022 or ASTM D1238-20. The resin is an octene-comonomer linear low density polyethylene produced in a solution process, and it is intended for chill-roll cast film extrusion rather than blown film extrusion. In cast film conversion, the melt is extruded through a flat die and quenched against a polished chill roll, producing rapid solidification and controlled thickness when the line is balanced. The product is used in monolayer and coextruded structures for industrial liners, overwrap, laminating webs, and protective packaging. Suitability for a specific structure must be confirmed by the converter because final film performance depends on die gap, melt temperature, chill-roll temperature, line speed, and winding tension.

    Representative properties from supplier technical literature are listed in Table 1. These values are typical laboratory data for cast film, not specification limits. Lot-specific certificates of analysis should be consulted for release criteria.

    Table 1. Representative cast film property profile for DOWLEX 2047A
    PropertyTest methodTypical value
    DensityASTM D792-20 / ISO 1183-10.920 g/cm³
    Melt flow rateASTM D1238-20 / ISO 1133-1:20221.0 g/10 min
    Melting temperatureASTM D3418-21 / ISO 11357-3122°C
    Vicat softening pointASTM D1525-17 / ISO 306107°C
    Tensile strength at break MD/TDASTM D882-1852/42 MPa
    Elongation at break MD/TDASTM D882-18620/780%
    Dart impact strengthASTM D1709-16a130 g
    Elmendorf tear MD/TDASTM D1922-09350/500 gf
    HazeASTM D1003-213.0%
    Gloss at 45°ASTM D2457-2175

    The primary lot-release characteristics used to confirm resin consistency are melt flow rate and density. Film tensile and tear values vary with film thickness, draw ratio, and cast-film orientation. For a 25 µm monolayer film, the balance of MD and TD properties reflects the uniaxial orientation introduced by the chill-roll draw. A higher draw ratio increases MD orientation and typically lowers MD tear resistance under ASTM D1922, while improving gauge uniformity. Draw ratios on cast film lines are commonly between 5:1 and 20:1, though published data for this specific grade on narrow-gap high-speed lines is limited.

    On a coextrusion cast line built around a 90 mm main extruder with 30:1 L/D and two satellite extruders of 45 mm diameter, the resin is typically run at melt temperatures between 240°C and 280°C, with die zones held near 250°C. The flat-die gap is usually set at 0.4–0.8 mm, and the air gap from die lip to chill roll is kept at 10–50 mm to manage neck-in and edge profile. Chill-roll temperatures are maintained between 20°C and 40°C, depending on gauge and optical requirements. A 0.4 mm die gap can generate backpressure in the range of 20–35 MPa on a 90 mm extruder, but the value is screw-specific and must be recorded during initial production runs. If melt temperature exceeds 290°C, thermo-oxidative degradation can form gel particles and increase odour. Residence time above 280°C should therefore be minimized. The feed throat should remain below 50°C to avoid premature pellet softening. Pre-drying is not normally required unless the resin has been stored open at relative humidity above 60%. At start-up and shutdown, purging with a lower-viscosity polyethylene grade is standard practice to flush hold-up zones and reduce die-lip accumulation.

    Melt filtration with screen packs of 60–120 mesh is common before the flat die to remove gel and contamination. A shorter air gap of 10 mm tends to reduce neck-in but may increase melt mark defects; a longer gap of 50 mm can improve chill-roll contact but increases edge draw and draw resonance risk. The selected air gap should be recorded together with melt temperature and line speed because changes in these three variables interact. Cast film produced from LLDPE is uniaxially oriented in the machine direction, so MD tear strength is frequently lower than TD tear strength under ASTM D1922. On high-speed lines running thin films below 20 µm, edge stability and winding quality require line-specific optimization rather than direct transfer of parameters from thicker gauge production.

    How Does 2047A Differ from LDPE, Butene LLDPE, and Metallocene LLDPE?

    The structural difference between 2047A and high-pressure LDPE is the absence of long-chain branching. This produces a lower degree of shear thinning and a different extensional viscosity response; on a cast film line, that difference commonly appears as higher extruder torque at equivalent melt flow rate and a stronger tendency toward neck-in if die gap and air gap are not optimized. Compared with butene-based LLDPE, the octene short-chain branches in 2047A generally provide higher energy absorption under ASTM D1709 dart impact and higher ASTM D1922 tear values at equivalent density and melt flow rate. Against metallocene-catalyzed LLDPE grades designed for narrow composition distribution, 2047A may exhibit a broader molecular weight distribution, which can reduce clarity and gloss under ASTM D1003 and ASTM D2457 while improving extrusion stability and reducing melt-pressure fluctuation.

    Within the DOWLEX cast film range, 2047A is differentiated by its 1.0 g/10 min melt flow rate and 0.920 g/cm³ density. A lower melt flow rate grade would normally require higher melt temperature and may generate higher backpressure; a higher melt flow rate grade would process with lower torque but may sacrifice some toughness. The choice between 2047A and other polyethylene families depends on the balance between processability, optics, seal performance, and abuse resistance in the finished film. In coextruded sealant layers, 2047A is often blended with LDPE or mLLDPE to balance seal initiation temperature and hot tack. The blend ratio must be determined on the target cast line because the optimum depends on die width, cooling capacity, and downstream packaging speed.

    Published comparative data for this specific configuration is limited. General structure-property relationships indicate that the octene comonomer in 2047A shifts the balance toward higher puncture and tear resistance relative to butene-based grades of equivalent density. Processors replacing an LDPE-rich formulation with 2047A may need to adjust screw speed and temperature profile because the melt viscosity has a different shear response. On lines originally designed for LDPE, the screw may require modification or the temperature profile may need to be raised to avoid excessive torque and melt-pressure variability.

    When Melt Temperature Exceeds 270°C, Degradation Indicators Appear

    Thermo-oxidative stability of linear low density polyethylene is influenced by antioxidant package, residence time, and melt temperature. In cast film conversion, gel formation is the primary visible indicator of degradation; gel counts may be assessed by ASTM D3596 or equivalent optical inspection systems. If the melt remains above 270°C for extended periods or above 290°C for any period, the resin may generate oxidized gel particles that appear as specks in thin film and reduce tear resistance under ASTM D1922. Processors should avoid hold-up zones in adapters and screen changers, and should not use copper or copper-alloy components in melt contact because copper ions catalyze polyethylene oxidation.

    Scrap containing metal contamination, high-acid polymers, or amine-based antifog additives should be evaluated before blending because such additives can accelerate degradation and plate-out. The antioxidant package is often assessed by oxidative induction time using ISO 11357-6 or ASTM D3895; lot-specific data may be requested from the supplier. If the resin is stored in humid conditions above 60% relative humidity, moisture uptake is generally low for polyolefins, but surface moisture can introduce bubbles or surface defects in the cast film. Under such conditions, pre-drying with a desiccant hopper at 60–80°C for 2–4 h is a conservative corrective action. These are starting points, not validated limits for every line.

    Compliance Cannot Be Inferred from Resin Grade Alone

    Food-contact status is use-dependent. The base resin may satisfy the compositional requirements of FDA 21 CFR 177.1520(c) for olefin polymers and the overall migration limits of Commission Regulation (EU) No 10/2011 as amended, but only a supplier-issued food-contact certificate can confirm a specific lot. For packaging sold in the European Union, the converter must verify that the finished film, including all masterbatch and processing aids, meets overall migration and specific migration limits under Commission Regulation (EU) No 10/2011. For electrical and electronic packaging, RoHS Directive 2011/65/EU and REACH SVHC declarations must be obtained from the resin supplier or compounder.

    Medical packaging applications may require additional final-article testing to ISO 10993-1 or USP <661.1>; the resin manufacturer’s food-contact or medical-grade statement does not replace finished-device biocompatibility assessment. No compliance statement should be considered valid beyond the conditions of use explicitly listed in the supplier certificate. Downstream converters are responsible for documenting that additives, regrind, and processing conditions do not alter the regulatory status of the finished article.

    Top