| HS Code | 724547 |
| Density | 0.920 g/cm³ |
| Melt Index 190 C 2 16 Kg | 1.0 g/10 min |
| Melt Flow Ratio I10 I2 | 8.0 |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 26.2 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 248 MPa |
| Vicat Softening Point | 100°C |
| Melting Point | 122°C |
| Hardness Shore D | 50 |
As an accredited Dow Dowlex™ 2046G LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow Dowlex™ 2046G LLDPE is packaged in 25 kg polyethylene-lined bags, palletized and stretch-wrapped for industrial shipping. |
| Container Loading (20′ FCL) | 20′ FCL: Dow Dowlex™ 2046G LLDPE in 25 kg bags, palletized, shrink-wrapped, approx. 20 MT net, securely stowed for export. |
| Shipping | Dow Dowlex™ 2046G LLDPE is shipped as non-hazardous polyethylene resin pellets in 25-kg bags, 1,000-kg octabins, or bulk trucks/railcars. Store in a dry, cool, ventilated area away from direct sunlight, heat, and ignition sources. Protect packaging from moisture and damage. No special transport placarding required. |
| Storage | Store Dowlex™ 2046G LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep containers or bags sealed to prevent moisture, dust, and contamination. Use pallets, avoid floor contact, and stack safely to prevent deformation. Protect from prolonged UV exposure. Store at ambient temperature. Keep clean. Follow local regulations and the manufacturer’s SDS. |
| Shelf Life | Dowlex 2046G LLDPE has a shelf life of 2 years when stored in a cool, dry area in original packaging. |
In silage clamp cover and bunker silo cover film production, Dowlex 2046G is metered as the primary film resin at 85–100 wt%, with a HALS-based UV-stabilizer masterbatch supplied at 1.0–2.5 wt%; where long-term black film is specified, a carbon black masterbatch at 2.0–4.0 wt% is used to achieve a minimum carbon black content of 2.0 wt% in the finished film. The base resin is characterized by a nominal density of 0.920 g/cm³ and a melt flow rate of 1.0 g/10 min under ISO 1133-1:2022 at 190 °C/2.16 kg. Compliance under EN 13207:2018 requires retention of specified tensile strength and elongation after artificial weathering, while REACH (EC) No 1907/2006 requires SVHC content below 0.1 wt% per article for EU import. Conversion is performed on a mono-layer or three-layer blown film line with a single-screw extruder of L/D 30:1–36:1, a barrier screw with mixing sections, and a 60/100/60 mesh screen pack to trap carbon black agglomerates. Melt temperature at the die is held at 195–220 °C; die diameter ranges from 200 mm to 450 mm, die gap 1.8–2.4 mm, blow-up ratio 2.2:1–2.8:1, and frost line height 8–10 times the die gap. With internal bubble cooling, chilled air is delivered at 10–20 °C; without IBC, haul-off speeds above 80 m/min can produce gauge bands exceeding ±7% and increase blocking tendency in the wound roll. Final film thickness is 120–250 µm. Terminal finished products include silage clamp covers, bunker silo covers, temporary grain storage liners, and agricultural fumigation sheets.
Coextruded frozen food packaging structures rely on the sealant layer to provide both low-temperature puncture resistance and seal integrity. In a three-layer A/B/C film, the sealant layer contains 60–80 wt% Dowlex 2046G and 20–40 wt% metallocene LLDPE or LDPE; the blend ratio is adjusted within this range based on seal initiation performance measured under ASTM F2029-16 and dart impact retention under ASTM D1709-20. The skin layer receives 2–4 wt% slip/anti-block masterbatch based on layer mass, while the core layer remains unfilled to avoid reducing Elmendorf tear under ASTM D1922-19. Food-contact conformance is documented under the matrix shown below.
| Standard or regulation | Scope | Test method or limit |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers in food contact articles | Extractables testing under conditions of use E or G; compliance with food-type migration limitations |
| Commission Regulation (EU) No 10/2011 | Plastic food contact materials | Overall migration 10 mg/dm² per EN 1186-1; specific migration limits in Annex II |
| REACH (EC) No 1907/2006 | Chemical safety and SVHC reporting | SVHC content 0.1 wt% per article; Annex XVII restrictions |
| GB 9685-2016 | China food contact additives | Positive-list use levels and migration limits per national sanitary standard |
Production is performed on a three-layer coextrusion blown film line with three extruders, the largest screw diameter specified at 75–100 mm for the core. Melt temperature at the die is 200–225 °C; die gap 1.8–2.4 mm, blow-up ratio 2.0:1–2.5:1, dual-lip air ring with chilled air at 8–12 °C, and in-line corona treatment to 38–42 mN/m. Film thickness is 40–80 µm. At start-up, if the frost line is set below 4 times the die gap, bubble instability can produce transverse gauge bands and uneven seal thickness; if the frost line is too high, low film temperature at the nip promotes blocking. Terminal finished products include IQF vegetable pouches, frozen seafood liners, ice cream pouches, and lidding film for frozen ready meals.
On heavy-duty sack and FIBC liner lines equipped with internal bubble cooling and oscillating haul-off, gauge variation is maintained within ±5% at haul-off speeds above 120 m/min by blending Dowlex 2046G with 15–30 wt% LDPE or re-pelletized edge trim. Where regrind levels exceed 30 wt%, a 120/80/120 mesh screen pack is used to remove oxidized gels; without such filtration, visible gel counts increase and dart impact under ASTM D1709-20 degrades at the gusset fold. Slip/anti-block masterbatch is limited to 1.0–2.0 wt% because higher loadings depress seal strength in automatic filling operations; a polymer processing aid is dosed at 0.5–1.0 wt% only when sharkskin melt fracture appears at the mandrel side. For dangerous goods inner packaging, drop and stack tests under UN Model Regulations 6.1.4 and ADR 6.1.4 apply, and leakproofness is verified before filling; mechanical acceptance follows ASTM D1922-19 for tear and ISO 527-3:2018 for tensile properties. REACH (EC) No 1907/2006 controls SVHC content below 0.1 wt% per article. Conversion is performed on a mono-layer or three-layer blown film line with a single-screw extruder of L/D 30:1–36:1, die diameter 250–600 mm, die gap 1.6–2.6 mm, blow-up ratio 1.8:1–2.4:1, and melt temperature 200–230 °C. Final film thickness ranges from 100 µm for box liners to 250 µm for FIBC liners; in-line gusseting and center-surface winding produce flat, fold-resistant rolls. At relative humidity above 60%, pellets and regrind are dried at 70–80 °C for 2–4 h; surface moisture produces splay and pinholes in the outer layers. Terminal finished products include form-fit liners for FIBCs, box liners for mineral and chemical powders, heavy-duty shipping sacks for granular resins, and compression packaging for insulation wool.
Five-layer cast stretch film lines process Dowlex 2046G as the core layer at 70–85 wt%; the cling layer is modified with 3–8 wt% polyisobutylene concentrate based on layer weight, while the release layer receives 0.5–1.5 wt% slip/anti-block masterbatch. The total film basis weight is 15–23 g/m², equivalent to 15–23 µm for unpigmented polyethylene. Cling force and unwind behavior are evaluated under ASTM D5458-95; pre-stretch elongation is limited to 200–300% and verified by encoder speed ratio; tensile modulus and yield under ASTM D882-18; puncture resistance under ASTM D5748-95; and tensile properties for thin films under ISO 527-3:2018. Production is performed on a five-layer cast film line with die width 2,000–3,500 mm, melt temperature 230–260 °C, air gap 10–25 cm, chill roll temperature 15–25 °C, and winding speed up to 600–900 m/min. Melt draw resonance, which appears as transverse thickness bands at high line speed, is suppressed by maintaining melt temperature and by using an air knife to stabilize the film edge; die lip build-up of polyisobutylene can cause tiger stripes and is controlled by scheduled cleaning of the die lips at 4–8 h intervals. Chill roll condensation at relative humidity above 60% causes localized haze and surface defects, requiring dehumidification of the casting area. Terminal finished products include hand stretch wrap, machine stretch wrap, pre-stretched pallet film, and bundling film for glass bottles and beverage multipacks.
For high-speed HFFS laminate structures, the PE sealant web incorporates 65–85 wt% Dowlex 2046G with 15–35 wt% LDPE or mLLDPE; anti-block masterbatch is added at 1–3 wt% to the outer skin and erucamide slip at 500–1,000 ppm in the sealant layer to control coefficient of friction. Seal strength is tested according to ASTM F2029-16, static and kinetic COF according to ISO 8295:1995, and food-contact conformance under FDA 21 CFR 177.1520 and Commission Regulation (EU) No 10/2011. The sealant web is produced on a three-layer blown or cast film line at 30–60 µm thickness and surface tension 38–42 mN/m for adhesive lamination; the lamination adhesive is applied at 1.2–2.5 g/m² and cured 24–48 h at 35–40 °C before slitting and pouching. At slip levels below 500 ppm, static COF can exceed 0.40 and cause drag on HFFS forming collars; at slip levels above 1,000 ppm, erucamide migration can reduce lamination bond strength and create delamination at seal areas. Terminal finished products include inner sealant webs for stand-up pouches, HFFS wrap for snack bars, lidding film for dairy and produce trays, and multi-wall bag liners.
Competitive Dow Dowlex™ 2046G LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dowlex™ 2046G is a linear low-density polyethylene produced by solution polymerization with 1-octene as the primary short-chain branching comonomer. The resin is specified with a nominal density of 0.920 g/cm³ under ASTM D792 or ISO 1183-1, and a nominal melt flow rate of 1.0 g/10 min at 190°C/2.16 kg under ASTM D1238 or ISO 1133-1. These coordinates place the grade in the low-density portion of linear polyethylene film resins, where molecular weight is high enough for bubble stability while density remains low enough to allow extensional deformation and puncture energy absorption. Dowlex™ 2046G is intended for blown-film extrusion, with commercial use in heavy-duty sacks, industrial liners, agricultural films, and coextruded laminating webs. The octene-derived C6 branch structure differentiates the product from butene-copolymer LLDPE of the same nominal density, because the longer branch is more effective in generating load-bearing tie chains under film orientation. This distinction is most visible in tear-propagation and dart-impact data rather than in pellet appearance or melt-flow specification.
At 0.920 g/cm³ and 1.0 g/10 min, a butene-based Ziegler-Natta LLDPE and Dowlex™ 2046G can appear identical on a purchasing specification. The difference arises from comonomer chemistry and comonomer placement. Butene introduces C2 branches, while 1-octene introduces C6 branches. Longer branches contribute more effectively to tie-molecule formation between lamellae without increasing the total branch count, and solution polymerization typically yields more uniform comonomer distribution across the molecular weight distribution. In film tests, this shifts the balance of ASTM D1922 Elmendorf tear and ASTM D1709 dart impact upward relative to butene copolymers of similar melt index. The improvement is not a fixed multiple; it depends on frost-line height, die gap, blow-up ratio, film thickness, and regrind level. The grade is also distinct from high-pressure LDPE. LDPE has long-chain branching that provides high shear thinning and substantial bubble stability, but its lower tensile strength and tear resistance at comparable density limit downgauging. In blends, Dowlex™ 2046G can increase puncture resistance while LDPE improves extensional strain at break and bubble consistency.
Heavy-duty sack applications place simultaneous demands on tensile strength, puncture resistance, and seal integrity when filled with abrasive or dense powders. Tubular film made from Dowlex™ 2046G is often specified where the sack is exposed to drop loading and side-wall bulge stresses. Industrial liners use the resin for its resistance to stress cracking and tear propagation. In agricultural film, the resin is typically converted into silage covers, greenhouse films, or similar structures requiring toughness under wind load and handling. Agricultural specifications must be considered separately from standard packaging specifications because ultraviolet exposure and multi-season weathering require additional stabilization. The base resin itself does not contain a complete long-term UV package.
On blown-film lines with 45 mm to 75 mm grooved-feed extruders and 24:1 to 30:1 L/D barrier screws, the resin is typically run with die lip gaps of 1.8 mm to 2.5 mm and blow-up ratios between 2.0 and 3.0. Melt temperatures are held between 190°C and 230°C. Operation above 230°C can consume the antioxidant package, increase odor and gel formation, and raise the probability of melt fracture. Operation below 190°C may increase motor load and produce poorly homogenized film with gauge bands. Because the resin is not formulated with added slip or antiblock, high-speed packaging operations may require separate slip/antiblock masterbatch addition. A line that normally processes a 2.0 g/10 min butene LLDPE will typically see higher die pressure and extruder motor load when changing to Dowlex™ 2046G; screw speed and screen-pack configuration should be adjusted so that the maximum allowable barrel and die pressure is not exceeded. Predrying is not routinely required. If pellets are stored in an unheated warehouse at relative humidity above 80%, surface moisture can generate bubble defects and should be removed with a 60°C hopper dryer for approximately 2 h.
Low-melt-index LLDPE resins such as Dowlex™ 2046G have a relatively narrow processing window on high-output lines. The onset of sharkskin is commonly observed at die-lip shear rates above 300 s⁻¹ to 500 s⁻¹, depending on die geometry and melt temperature. If surface melt fracture appears, the first control action is to raise melt temperature or reduce output. Fluoropolymer processing aids may be added at 200–1000 ppm to increase the critical shear rate, but the final film must be checked for seal-strength changes under ASTM F88 because some processing aids can migrate to the surface. Bubble stability is governed by the balance between melt strength, crystallization rate, cooling-air impingement, and internal bubble air exchange. On high-stalk lines using internal bubble cooling, the frost-line height is typically set between 450 mm and 800 mm, but this range is machine-specific. If the frost line is too low, rapid cooling can increase haze and reduce transverse-direction tear. If it is too high, the bubble may oscillate and generate thickness variation. These boundaries must be validated by on-line thickness profiling and tear testing rather than by visual inspection alone.
Die gap and air-ring performance affect film gauge distribution and mechanical properties. A larger die gap of 2.5 mm can reduce melt fracture but may reduce orientation and increase downgauging limitations. A smaller die gap of 1.8 mm can increase transverse-direction tensile strength but may raise die pressure and melt fracture. Dual-lip air rings provide better cooling control than single-lip designs when running low-MI LLDPE at high output. The air-ring lip angle and air velocity should be adjusted to stabilize the bubble at the desired frost-line height. These adjustments are interaction effects; changing one parameter without recording die pressure and thickness profile can create a new failure mode.
| Parameter | Method or source | Value / range |
|---|---|---|
| Melt flow rate | ASTM D1238 / ISO 1133-1 | 1.0 g/10 min at 190°C/2.16 kg |
| Density | ASTM D792 / ISO 1183-1 | 0.920 g/cm³ |
| Comonomer | Manufacturer solution process | 1-octene, C6 branches |
| Slip additive | Manufacturer formulation | Not added |
| Antiblock additive | Manufacturer formulation | Not added |
| Melt temperature | Production blown-film lines | 190°C–230°C |
| Blow-up ratio | Production blown-film lines | 2.0–3.0 |
| Die gap | Production blown-film lines | 1.8 mm–2.5 mm |
| Predrying | Handling guideline | Not normally required; dry at 60°C for 2 h if pellet surface condensation is present |
Heavy-duty sack and liner specifications are written around dart impact, tear propagation, tensile properties, and seal strength, not pellet density alone. Film qualification often includes tensile tests under ASTM D882 with a crosshead speed of 500 mm/min, Elmendorf tear under ASTM D1922, dart impact under ASTM D1709, slow-rate puncture under ASTM D5748, heat-seal strength under ASTM F88, and hot tack under ASTM F1921. Samples are conditioned at 23°C and 50% RH according to ASTM D618. For agricultural film, oxidative-induction time under ASTM D3895 or ISO 11357-6 is used to verify that the base stabilizer package remains active after compounding with UV stabilizer and color masterbatch. The results are not transferable across different bubble geometries. A high-stalk process with a long frost line orients the film differently from a low-stalk process; the former may favor machine-direction tear while the latter may favor transverse-direction tear. Converters should not use density and melt-flow data to predict absolute film property values.
The addition of regrind influences rheology, gel counts, and film appearance. Because Dowlex™ 2046G is a linear polymer with relatively low shear thinning, increasing regrind content tends to raise screw motor load and die pressure more than the same regrind level in LDPE. Film scrap should be ground with screen sizes suitable for the feed throat, typically 5–8 mm, and blended with virgin pellets before the feed throat rather than added as a separate stream. Regrind levels of 20–30 wt% are common in industrial film operations, but higher levels require vacuum degassing, screen changers, and melt filtration to control black specks and gel particles. If the resin is compounded with amine-containing additives, the thermal stabilizer system may be degraded more rapidly; such formulations should be tested for oxidative-induction time under ASTM D3895 before production.
The stabilizer package is designed for normal blown-film processing. At melt temperatures above 230°C, oxidative degradation can produce carbonyl species that increase odor and color. Repeated extrusion cycles, as encountered with high regrind ratios, consume the stabilizer package and lower oxidative-induction time. A film that passes initial tensile testing may still fail after 3 or more extrusion cycles if additional stabilizer is not added. The use of a nitrogen blanket on the feed hopper is generally not required; however, high-temperature processing with long screw residence times may justify inert-gas blanketing to protect the melt.
In heavy-duty sack and industrial liner applications, film downgauging from LDPE to Dowlex™ 2046G is typically confirmed through a structured trial plan rather than a single formulation change. A converter may first run a 50 µm LDPE film and measure dart impact under ASTM D1709, tear under ASTM D1922, and seal strength under ASTM F88. After substituting or blending Dowlex™ 2046G, the same tests are repeated at reduced gauge, often in 5 µm decrements, until the acceptance limits are reached. Because polyethylene film properties are not additive by weight fraction, blend ratios with LDPE should be determined empirically. In multilayer structures, the resin may be placed in the core layer to increase tear resistance or in the outer layer to improve puncture performance. Published data for this specific grade in complete commercial laminates is limited, and final fitness must be demonstrated on the converter’s line at representative output rates and temperature profiles.
Compared with a metallocene-catalyzed LLDPE of equivalent density, Dowlex™ 2046G may exhibit broader molecular weight distribution and lower melt elasticity. That broader distribution generally improves extruder throughput and bubble stability on conventional spiral annular dies, but it may reduce ultimate dart impact and clarity at high quench rates. When high haze is unacceptable, the converter may place a metallocene-catalyzed or high-clarity LDPE layer on the outside and retain Dowlex™ 2046G in the core. Haze is measured under ASTM D1003; LLDPE films with no antiblock can have haze values that vary with die gap, quench rate, and film thickness.
Heat-seal performance is critical in sack and liner applications because a seal failure can cause the entire package to burst. Low-density LLDPE films typically exhibit a seal-initiation temperature above low-pressure LDPE but below high-density polyethylene. Seal strength is measured under ASTM F88 at a specified jaw temperature, dwell time, and pressure. Hot tack is measured under ASTM F1921. Because the resin contains no antiblock, films may stick to themselves at high rewind tension or elevated storage temperatures; converters can address blocking by adding silica or zeolite antiblock masterbatch. The required addition level depends on roll diameter, film gauge, and storage temperature, and should be optimized against haze and seal strength.
For food-contact applications in the United States, Dowlex™ 2046G is typically considered as an olefin polymer under FDA 21 CFR 177.1520. The citation covers olefin polymers, but the finished fabricated article must meet extraction and end-use limitations. A resin compliance statement does not replace converter migration testing. In the European Union, the final article is assessed under Regulation (EU) No 10/2011 on plastic materials intended to come into contact with food. Overall migration and specific migration of additives must be evaluated with the food simulant and time–temperature conditions assigned to the food type. The resin is not supplied for medical-device implant or parenteral contact. For outdoor agricultural film, long-term UV stabilizers must be added separately because the base resin contains only processing antioxidants. Storage temperatures above 40°C for extended periods can induce pellet blocking and additive bloom. Avoid strong oxidizing agents, and provide local exhaust ventilation during high-temperature processing to control decomposition products.