Dow Dowlex 2045g Linear Low Density Polyethylene

Dow DOWLEX™ 2045G Linear Low Density Polyethylene

    • Product Name: Dow DOWLEX™ 2045G Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 786244
    Comonomer 1-Octene
    Density 0.920 g/cm³
    Melt Index 1.0 g/10 min
    Melt Flow Ratio 8.0
    Melting Point 124 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 35.2 MPa
    Elongation At Break 600%
    1 Secant Modulus 200 MPa
    Flexural Modulus 240 MPa
    Hardness Shore D 53
    Dart Drop Impact 140 g
    Elmendorf Tear Md 300 g
    Elmendorf Tear Td 500 g
    Haze 10%
    Gloss 45 60%
    Coefficient Of Friction 0.2
    Low Temperature Brittleness < -70 °C
    Environmental Stress Crack Resistance >1000 h

    As an accredited Dow DOWLEX™ 2045G Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DOWLEX™ 2045G Linear Low Density Polyethylene resin supplied in 25-kg polyethylene bags, palletized as resin pellets for industrial handling.
    Container Loading (20′ FCL) A 20′ FCL typically loads 20–22 MT of Dow DOWLEX™ 2045G LLDPE pellets in 25 kg bags, palletized or floor-loaded.
    Shipping Dow DOWLEX™ 2045G LLDPE ships as non-hazardous polymer pellets in 25 kg bags, octabins, or bulk containers. Transport in clean, dry trucks or railcars; protect from moisture, heat, and UV. No special dangerous goods placards required. Store cool and dry.
    Storage Store Dow DOWLEX™ 2045G Linear Low Density Polyethylene in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or containers closed to prevent moisture and dust contamination. Avoid static buildup. Maintain good housekeeping and follow first-in, first-out stock rotation. Consult the SDS and local regulations for specific requirements.
    Shelf Life Stable under normal storage conditions; no specific shelf life. Store in a cool, dry, well-ventilated area away from heat sources.
    Application of Dow DOWLEX™ 2045G Linear Low Density Polyethylene

    On a three-layer cast film line configured with 45 mm, 65 mm, and 45 mm extruders, each with 30:1 L/D barrier screws, DOWLEX 2045G is processed as the core and non-cling skin at a combined output of 420 kg/h to 480 kg/h across a 2200 mm die width. The die temperature is held at 240 °C to 255 °C, while the adapter melt temperature measured before the feedblock is maintained at 244 °C to 252 °C. The primary chill roll runs at 22 °C to 28 °C, and the secondary chill roll is kept below 18 °C to remove residual heat before the film enters the winder. A polyisobutylene-based tackifier masterbatch is injected into the core layer at 0.8 wt% to 1.5 wt%, targeting a cling force of 60 g to 130 g per 25 mm width when tested per ASTM D5458. Slip and antiblock additives are incorporated in the non-cling skin at 1.5 wt% to 2.5 wt% masterbatch dilution to maintain a kinetic coefficient of friction below 0.35 per ASTM D1894. Film thickness ranges from 15 μm to 38 μm, with the 17 μm machine-grade product running at 300 m/min to 420 m/min. Edge neck-in is a recognized production defect because the 1.0 g/10 min melt index of DOWLEX 2045G does not provide the melt tension of a branched low-density polyethylene; vacuum boxes and flexible edge pinners are therefore set to keep total neck-in below 40 mm. At low gauge, draw resonance can appear as transverse thickness bands when the die gap is closed below 0.55 mm; opening the slot to 0.75 mm and increasing air-knife impingement distance to 25 mm reduces the instability without raising thickness variation beyond 3 %. Dent and puncture resistance of the wound pallet wrap is checked on the production floor using ASTM D5748; published data for this specific grade in that test is limited. The finished pallet wrap is not intended for direct food contact, so the relevant compliance path is REACH Regulation (EC) No 1907/2006 for imported tackifier and slip masterbatches and California Proposition 65 for residual mineral oil. End products include manual and machine pallet wrap, heavy-gauge agricultural transportation film, and bundling film for construction profiles.

    Why Does Frost Line Height Govern Dart Impact Retention in Heavy-Duty Sack Film?

    A blown film line producing heavy-duty shipping sacks from DOWLEX 2045G typically uses a 120 mm grooved-feed extruder with 28:1 L/D, a 400 mm die, and a 1.8 mm to 2.2 mm die gap. The resin is run at a blow-up ratio of 2.0:1 to 2.8:1, giving a layflat width of 1250 mm to 1750 mm. The melt temperature at the die is controlled between 205 °C and 225 °C to retain bubble strength; lower melt temperatures reduce dart impact and increase gel-like flow defects, while higher temperatures cause bubble sagging and melt fracture on the die lip. The frost line height is maintained with a dual-lip air ring and internal bubble cooling at 250 mm to 350 mm above the die face, approximately 6 to 9 die diameters. If the frost line is allowed to rise beyond 10 die diameters, the film develops excessive longitudinal orientation in the amorphous region before crystallization; this is observed as a reduction in ASTM D1709 dart impact and an increase in directional tear imbalance when compared with the same film tested per ASTM D1922. The conversion to heavy-duty sacks requires a gauge of 100 μm to 180 μm, usually in a 3-layer structure where DOWLEX 2045G occupies the core and skin layers. To meet tear and seal requirements, a metallocene-catalysed LLDPE with higher melt strength may be blended at 10 wt% to 25 wt% in the outer layer; published data for this specific DOWLEX 2045G blend in ASTM D1709 is limited, so production-scale trials are required to set the blend ratio. Failure modes observed on sack lines include bubble flapping at high blow-up ratio, creasing in the collapsing frame, and gusset weld misalignment caused by differential shrink after slitting. Where the sack is used for dangerous goods packaging, the finished article must meet the applicable drop and stack test requirements under the UN Model Regulations. End products include valve sacks for polymer resins, intermediate bulk container liners, and compression-pack bags for textile fibres.

    When a 3-Layer Coextrusion Line Deploys DOWLEX 2045G as the Sealant Skin

    Flexible packaging films for dry foods and frozen goods are coextruded with a sealant skin containing DOWLEX 2045G at 10 % to 30 % of total film thickness, typically 8 μm to 15 μm in a 60 μm structure. The core layer is polypropylene or a higher-modulus LLDPE, and the outer layer is a printable HDPE or LDPE. The seal initiation temperature of the finished film is measured by making heat seals at 0.5 s dwell and 0.3 MPa jaw pressure, then recording the temperature at which seal strength reaches 0.5 N/15 mm; for DOWLEX 2045G, production lines generally observe this threshold between 108 °C and 122 °C, but the value shifts with film thickness, seal bar configuration, and additive package. Hot-tack strength is measured per ASTM F1921, and because DOWLEX 2045G has a 0.920 g/cm³ density, the hot-tack plateau is narrower than that of lower-density metallocene sealants. Packaging converters should not assume performance interchangeability when replacing a metallocene resin with DOWLEX 2045G without retesting at the same gauge. Compliance is anchored to FDA 21 CFR 177.1520(c) for olefin polymers used in contact with food, subject to end-use temperature and food type limitations. For European Union applications, the final film must comply with Regulation (EU) No 10/2011, including overall migration below 10 mg/dm² using the appropriate food simulant for the intended contact. Additive migration from slip and antiblock masterbatches must be included in the overall migration calculation; therefore the masterbatch must be chosen from an approved supplier and dosed at the lowest level that achieves the required coefficient of friction. End products include form-fill-seal pouches for frozen vegetables, cereal liners, and dry snack bags where a reliable seal through product contamination is required.

    JurisdictionStandard or RegulationTest or ClauseApplication Condition
    United StatesFDA 21 CFR 177.1520Olefin polymer specificationNeat or blended DOWLEX 2045G in food-contact films; end-use extraction tests apply
    European UnionRegulation (EU) No 10/2011Overall migration 10 mg/dm²Finished film with additives; simulant selection per Annex III
    Global melt flowASTM D1238190 °C, 2.16 kgNominal 1.0 g/10 min for incoming resin control
    Global densityASTM D79223 °C immersionNominal 0.920 g/cm³ for layer calculations

    Silage conversion lines feed DOWLEX 2045G as a structural skin in 5-layer blown film structures designed for round bale wrap and clamp sheets. Total film thickness ranges from 150 μm to 250 μm, with DOWLEX 2045G occupying 20 % to 35 % of the layer distribution on both outer skins to provide puncture resistance and sealability, while a metallocene-catalysed plastomer or ethyl vinyl acetate copolymer is used in the core to reduce oxygen transmission. The bubble is run at a blow-up ratio of 2.5:1 to 3.2:1, and the frost line is kept high enough to generate balanced orientation; however, an excessive frost line above 350 mm from the die can destabilize the bubble when wind gusts or ambient temperature fluctuations exceed 5 °C. UV stabilisation is achieved with a hindered amine light stabilizer masterbatch at 0.5 wt% to 1.0 wt% total formulation, plus a 0.2 wt% to 0.4 wt% carbon black concentrate in the outer skin. The film is tested for tear resistance per ASTM D1004, dart impact per ASTM D1709, and puncture propagation per ASTM D5748; agricultural convertors usually specify retained dart impact and tear after 12 months of outdoor stacking, although published data for this exact DOWLEX 2045G formulation is limited. The main processing bottleneck on silage film lines is the trade-off between low film weight and puncture survival on baled grass with sharp stalks; this is managed by raising the DOWLEX 2045G skin thickness and lowering the core plastomer content when punctures exceed the agreed value. The UV masterbatch and carbon black concentrate are selected to comply with REACH Regulation (EC) No 1907/2006; no food-contact listing is required unless the silage film is later repurposed for feed packaging. End products include wrapped round bales, square bale in-line tubes, and reusable silage clamp covers.

    Injection Moulding of Thick-Walled Industrial Stoppers and Closure Liners

    For applications outside film extrusion, DOWLEX 2045G is moulded into thick-walled industrial stoppers, drum closure liners, and gaskets where its 0.920 g/cm³ density and 1.0 g/10 min melt index are acceptable because flow length is short and wall thickness exceeds 2 mm. Injection moulding machines with clamp force above 800 kN and melt temperatures between 210 °C and 240 °C are used; mould temperatures are kept at 25 °C to 40 °C to allow stable part ejection. Because the melt index is low, a high injection speed and a nozzle tip with a minimum bore of 2.5 mm are required to avoid short shots when filling multiple cavities. The part should be cooled below 60 °C before ejection to prevent post-mould shrinkage exceeding 2 % of the drawing dimension. This application is not recommended when the wall thickness falls below 1.2 mm or when the flow length exceeds 150 mm; published data for this specific resin in spiral flow testing is limited, so simulation and actual tool trials are required. Industrial stoppers and liners used with non-regulated chemicals are outside FDA 21 CFR; if the closure contacts food or drug products, the moulded part must meet USP <661.1> or Regulation (EU) No 10/2011 as appropriate. End products include agricultural chemical closures, industrial container liners, and temporary protection caps requiring flexibility and chemical resistance.

    Free Quote

    Competitive Dow DOWLEX™ 2045G Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2045G Linear Low Density Polyethylene is a pelletized ethylene/1-octene copolymer produced via solution polymerization and intended for film extrusion. The grade is specified around a nominal density of 0.920 g/cm³ (ISO 1183-1:2019 / ASTM D792) and a nominal melt index of 1.0 g/10 min (ISO 1133-1:2022 / ASTM D1238, 190 °C, 2.16 kg). The term “linear low density polyethylene” describes a predominantly linear backbone with controlled short-chain branches; in DOWLEX™ 2045G the branches are longer than those in butene-based LLDPE, which alters tie-molecule formation and solid-state toughness. The product is used in blown and cast film structures where puncture resistance, tear resistance, seal performance, and low-temperature impact strength are controlling design variables. Applications include heavy-duty sacks, industrial liners, lamination films, agricultural film, and food packaging subject to regional compliance. The resin is not a direct substitute for high-pressure LDPE or narrow-composition metallocene LLDPE; substitution requires revalidation of extrusion, sealing, and film toughness behavior on the target line.

    Resin Architecture and Specification Parameters

    The density and melt-flow-rate pair defines the processing class. Density is measured after conditioning at 23 °C and reflects the mass per unit volume of the annealed polymer. Melt index is a single-point capillary flow value and does not describe the full shear-viscosity curve. For die design and extruder screw selection, capillary viscosity per ISO 11443:2021 at 210 °C and apparent shear rates between 100 s⁻¹ and 1000 s⁻¹ is recommended. A melt index of 1.0 g/10 min places the grade in the low-flow film class, which generally produces higher head pressure than cast-film grades with melt indices above 3.0 g/10 min but lower head pressure than fractional-melt LLDPE. The density and cooling rate jointly determine crystallinity. Rapid cooling from the melt reduces crystallinity and increases amorphous tie-molecule content, whereas slow annealing increases lamellar thickness; therefore values generated on laboratory plaques may differ from those measured on film.

    Table 1. Published typical properties for DOWLEX™ 2045G.
    PropertyTest methodTypical value
    Melt index (190 °C/2.16 kg)ISO 1133-1:2022 / ASTM D12381.0 g/10 min
    Density (23 °C)ISO 1183-1:2019 / ASTM D7920.920 g/cm³
    Vicat softening temperature (A50, 10 N)ISO 306:2022 / ASTM D152595–100 °C
    Peak melting temperature (DSC, 10 K/min)ISO 11357-3:2018121–123 °C
    Water absorption (24 h, 23 °C)ISO 62:2008 / ASTM D570<0.01%

    Typical values are not batch-certificate specification limits. The resin architecture is defined by comonomer length, branch distribution, molecular weight distribution, and stabilization package. The solution process used for DOWLEX™ 2045G allows 1-octene incorporation with a branch length of 6 carbons. This longer branch disrupts crystallinity but increases the probability of load-bearing tie molecules in the amorphous regions at equivalent density. The practical effect is measurable in slow crack growth, instrumented puncture, and low-temperature impact tests. Melt-state behavior is also affected: the linear backbone provides less melt elasticity than high-pressure LDPE, while the broader molecular weight distribution provides lower extruder pressure than metallocene LLDPE of equal melt index.

    On a production blown-film line equipped with a smooth-bore or grooved-feed single-screw extruder of 25:1 to 30:1 L/D and die diameter from 100 mm to 400 mm, melt temperatures between 180 °C and 210 °C are typical. The die body and die lip are maintained above 210 °C to reduce melt fracture. Head pressure at the screen changer is monitored as an indirect indicator of melt homogeneity and gel formation; the acceptable peak-to-peak variation is line-specific and should be established from the die manufacturer’s pressure rating and the screw design. At melt temperatures above 240 °C, oxidative degradation can generate visible gel particles and reduce film impact strength. During shutdowns longer than 15 min, the screw should be kept rotating at low speed or purged. Pre-drying is not normally required if the pellets are stored below 60% relative humidity. If surface condensation is present, surface moisture can be removed with dehumidified air at 60 °C for 2 h without melting the pellets. The resin is not universally formulated with slip and antiblock; if coefficient-of-friction targets below 0.30 are required, the converter must validate a suitable slip/antiblock masterbatch.

    Cast-film conversion with this density and melt index typically uses melt temperatures of 220–230 °C and chill-roll temperatures between 15 °C and 30 °C. The lower melt index may require a die gap between 0.5 mm and 0.8 mm to maintain line speed while controlling neck-in. The addition of 10–30 wt% high-pressure LDPE is a common industrial method to improve melt curtain stability and reduce draw resonance, although this dilution reduces the tearing resistance and puncture performance of the final structure.

    What Distinguishes DOWLEX™ 2045G from Butene-Based LLDPE and High-Pressure LDPE?

    The principal molecular distinction is comonomer length. Butene-based LLDPE grades carry ethyl branches from 1-butene, whereas DOWLEX™ 2045G carries hexyl branches from 1-octene. At equal density and crystallinity, the longer octene branch increases the number of tie molecules linking crystalline lamellae. This difference is observed as higher puncture toughness and better low-temperature resistance in film. Relevant test anchors include ISO 6603-2 / ASTM D3763 for instrumented puncture, ISO 7765-1 / ASTM D1709 for dart drop, and ISO 6383-2 / ASTM D1922 for Elmendorf tear. The magnitude of the improvement is not a fixed material constant; it depends on blow-up ratio, drawdown, cooling rate, and film thickness. Published data for cross-line comparisons are limited, and grade-specific substitution trials are required.

    High-pressure LDPE is a long-chain-branched polymer, whereas DOWLEX™ 2045G has a linear backbone with short-chain branching. The long-chain branching in LDPE produces strain hardening in extensional flow and a broader crystallization exotherm, which yields higher melt strength and better bubble stability in high-stalk blown film. DOWLEX™ 2045G lacks that long-chain branching; its melt strength is lower and its neck-in in cast extrusion is greater. Conversely, the LLDPE grade typically provides higher tensile yield stress, higher elongation at break, and better environmental stress crack resistance than LDPE of similar density. Tensile properties are measured by ISO 527-1/-3 or ASTM D638; environmental stress cracking is assessed by ASTM D1693 or ISO 22088-3. These differences explain why DOWLEX™ 2045G is blended with LDPE on many film lines: LDPE improves process stability, while the LLDPE fraction retains toughness.

    Compared with metallocene-catalyzed LLDPE of comparable density and melt index, DOWLEX™ 2045G generally exhibits a broader molecular weight distribution. This characteristic reduces extruder pressure at equal screw speed and improves melt strength in thicker gauge film, but it can increase haze and reduce dart impact in very thin film. Haze is measured by ASTM D1003 or ISO 14782, and dart impact by ASTM D1709. The selection between Ziegler-Natta solution grades such as DOWLEX™ 2045G and metallocene LLDPE should therefore be based on the relative weight of optical specifications, extrusion throughput, and toughness requirements.

    For converters who need higher dart impact in thick film, a fractional-melt LLDPE of the same density may offer superior toughness but at reduced output. For converters who need higher line speed in thin cast film, a melt index of 2.3–3.5 g/10 min may be preferred. DOWLEX™ 2045G occupies the intermediate melt-index range where blown-film bubble stability, extrusion head pressure, and solid-state toughness are balanced.

    When Food-Contact and Article-Use Compliance Are Required

    For food-contact use in the United States, DOWLEX™ 2045G is generally covered by 21 CFR § 177.1520(c)3.2a, provided the finished article meets the extractives and end-use limitations of that regulation. In the European Union, the finished plastic article must comply with Commission Regulation (EU) No 10/2011. For plastic materials intended for food contact, the overall migration limit is 10 mg/dm² of food-contact surface area, and specific migration limits apply to additives, monomers, and conversion aids. A base-resin food-contact statement does not by itself clear the finished package because printing inks, laminating adhesives, colorants, and regrind may introduce additional migrating species. Migration testing must be conducted under the intended food simulant and time-temperature condition.

    For electrical and electronic applications, the material must be assessed under the Restriction of Hazardous Substances Directive 2011/65/EU when the final article is placed on the market as electrical or electronic equipment. Polyolefin resins of this grade do not require halogenated flame retardants, but cadmium, lead, mercury, and hexavalent chromium contents should be verified from the supplier’s certificate for RoHS compliance. Under REACH, the polymer itself is not subject to registration, but imported articles with intentionally released substances or with substances of very high concern above 0.1% by weight must be evaluated. The resin is not intended for medical implant applications; food-contact status does not establish USP Class or ISO 10993 biocompatibility.

    The grade is not suitable for continuous exposure to strong oxidizing acids, aromatic hydrocarbons, or chlorinated solvents at elevated temperatures. Swelling in xylene or toluene is expected. For any nonaqueous chemical-contact application, compatibility should be tested per ISO 175 or ASTM D543. The Vicat softening range of 95–100 °C does not define a maximum continuous service temperature because stiffness loss under load occurs below the softening point. For load-bearing applications, heat deflection temperature under load should be evaluated per ISO 75-2 method B at 0.45 MPa, and long-term creep behavior should be considered.

    Storage and handling conditions influence downstream processing. The pellets should be stored indoors at 23 °C and 50% relative humidity in sealed containers. Under these conditions, the oxidative stabilization package is generally effective for 12 months from the production date. After prolonged storage, melt-flow stability and yellowness index should be checked before use. The resin is not biodegradable under composting conditions and is not designed for marine-degradable applications. Unintended exposure to sunlight and condensate should be avoided because ultraviolet radiation can initiate surface oxidation even at ambient temperature.

    Top