Dow Dowlex 2045g Cir Lldpe

Dow Dowlex™ 2045G CIR LLDPE

    • Product Name: Dow Dowlex™ 2045G CIR LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 755892
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Octene
    Density 0.920 g/cm³
    Meltindex 1.0 g/10 min (190°C/2.16 kg)
    Meltingpoint 122 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatyield 9 MPa
    Tensilestrengthatbreak 30 MPa
    Elongationatbreak 800%
    Flexuralmodulus 200 MPa
    Hardnessshored 50
    Thermalexpansioncoefficient 2.0E-4 /°C
    Brittlenesstemperature < -70 °C
    Dielectricconstant 2.3
    Volumeresistivity >1E16 ohm·cm
    Waterabsorption < 0.01%

    As an accredited Dow Dowlex™ 2045G CIR LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow Dowlex™ 2045G CIR LLDPE is packaged in 25 kg polyethylene bags, 55 bags per pallet (1,375 kg).
    Container Loading (20′ FCL) 20′ FCL loaded with 25 kg bags of Dow Dowlex™ 2045G CIR LLDPE, palletized, stretch-wrapped, and secured for ocean transport.
    Shipping Dow Dowlex™ 2045G CIR LLDPE ships as non-hazardous polyethylene pellets in 25 kg bags, 1,000 kg bulk bags, or bulk truck/railcars. Store dry, away from direct sunlight, moisture, and contaminants. Handle palletized loads with forklifts; avoid puncturing containers. Follow local regulations and keep packaging clean and closed during transport.
    Storage For Dow Dowlex™ 2045G CIR LLDPE resin: Store in a cool, dry, well-ventilated place away from direct sunlight, heat, and ignition sources. Keep original containers or packaging closed, off the floor, to prevent moisture pickup and contamination. Avoid prolonged UV exposure and temperatures above 50 °C. Maintain a clean, segregated area and follow good housekeeping, local regulations, and the SDS.
    Shelf Life No established shelf life; stable if stored cool, dry, sealed, away from sunlight, heat, moisture, and contamination for optimal properties.
    Application of Dow Dowlex™ 2045G CIR LLDPE

    Differential cooling across the transverse film thickness determines the crystallisation morphology of Dowlex 2045G CIR on monolayer cast stretch lines. The grade has a nominal melt index of 1.0 g/10 min at 190 °C under 2.16 kg load when measured to ASTM D1238-23 and a nominal density of 0.920 g/cm³ when measured to ASTM D1505-23. On cast stretch lines, these values place the resin in a processing bracket where draw resonance is less likely at haul-off speeds up to 600 m/min, provided the air gap is kept below 4.0 cm and the melt temperature is not pushed above 250 °C. Above 250 °C, oxidation-induced gel particles become visible in the film and can transfer to the chill roll as a sticky deposit, producing periodic transverse bands under high-speed pre-stretch. The stretch film is tested to ASTM D882-18 for tensile properties and ASTM D1709-22 Method A for dart drop, with production lot limits established by the converter rather than by the resin specification; published data for this specific configuration is limited because the final film properties depend on the chill roll temperature profile, winding tension, and the slip package.

    In monolayer cast configurations, the resin is often run at 100 wt%; in three-layer coextruded machine stretch film, the two outer skins are formulated at 70–85 wt% Dowlex 2045G CIR with 15–30 wt% of a metallocene LLDPE having a melt index of 2.0–3.0 g/10 min to modify cling and puncture behaviour. The industrial non-food boundary relies on REACH EC 1907/2006 registration and FDA 21 CFR 177.1520(c) olefin polymer status for converters that sell into food-adjacent packaging without direct food contact, with all migration responsibility transferred to the final article structure. Production equipment for this application class includes a 90–120 mm extruder with 30:1 L/D barrier screw, a coathanger slot die with internal deckle, a polished chill roll held at 21–27 °C, and a dual-turret winder with taper tension control from 15% to 25%. The melt temperature is maintained at 232–246 °C, the die gap at 0.5–0.8 mm, and the air gap at 2–4 cm. Terminal products include machine-grade stretch film of 20–23 µm for automatic pallet wrappers, hand rolls of 12–17 µm for manual overwrap, and pre-stretched rolls with applied elongation of 200–300% at the converting stage.

    Can Silage Wrap Retain Puncture Resistance at 23 µm Without Blending?

    Agricultural silage bale wrap at 23 µm nominal thickness fails not in tensile yield but in puncture energy absorption when baled forage stalks are compressed at high density. Dowlex 2045G CIR is used as the reactor-grade toughness layer in cast coextrusions where the outer skins resist stalk puncture and the core carries the tack and UV package. Under EN 14932:2007, thermoplastic stretch films for wrapping bales are qualified by elongation under load, puncture resistance, and cling retention, but the converter must separately qualify the UV stabiliser addition because this resin is not supplied with UV resistance as a standard attribute.

    The addition profile in three-layer cast silage wrap typically places 68–80 wt% Dowlex 2045G CIR across the structure, with 12–20 wt% metallocene LLDPE of melt index 2.0–4.0 g/10 min and 6–12 wt% tackifier concentrate. UV masterbatch is metered at 2–4 wt%, and pigment masterbatch at 1–2 wt%. Active polyisobutylene content above 4 wt% of total film weight causes chill roll release instability and fouling of the baler pre-stretch rollers, which appears as cyclic gauge variation across the roll width.

    Production runs on multi-layer cast film lines with melt temperature 220–250 °C, die gap 0.5–0.7 mm, and chill roll temperature 18–22 °C. Edge trim is re-fed into the core layer at 5–15 wt% provided the trim is not heavily contaminated with tackifier oxidation by-products. The finished web is slit to 500 mm and 750 mm rolls for round baler equipment, with baler pre-stretch set at 55–75% and the wound roll hardness specified to avoid telescoping during field transport. Terminal products include round bale silage wrap, haylage wrap, and high-wrap-count bale films supplied in 20–25 µm gauge.

    For heavy-duty internal liners for flexible intermediate bulk containers, the measurable combination of machine-direction Elmendorf tear propagation resistance and low-temperature drop energy when filled sacks are handled at −20 °C determines suitability. In blown film extrusion, Dowlex 2045G CIR is used below its upper blow-up ratio limit because its molecular weight distribution is sufficiently broad to stabilise the bubble at 2.0:1 to 2.5:1 without excessive gauge variation. The resin is dry-blended rather than melt-compounded in most converter plants, which preserves its tear resistance and limits additional heat history.

    Typical charge proportions are 70–90 wt% Dowlex 2045G CIR combined with 10–30 wt% high-pressure LDPE or medium-density polyethylene with melt index 0.3–1.0 g/10 min. The LDPE component reduces melt pressure and improves haul-off stability; above 30 wt% LDPE, the dart impact energy of the finished liner falls below the threshold required for 50 kg chemical powder sacks.

    Processing is performed on single- or three-layer blown film lines equipped with die diameters of 150–300 mm, die gaps of 1.8–2.4 mm, and dual-lip air rings with internal bubble cooling. Melt temperature is maintained between 195 °C and 230 °C, and frost line height is set at 600–900 mm above the die face to control TD shrink. The collapsed web is corona-treated to 38–42 mN/m before lay-flat winding.

    Compliance for FIBC liners centres on mechanical performance rather than food migration, with lot release test methods including ASTM D1709-22 Method A for dart drop, ASTM D1922-15a for Elmendorf tear, and ISO 6383-2:1983 for trouser tear on substrates above 100 µm. For containers intended to hold non-dangerous goods, the outer FIBC assembly is certified to ISO 21898:2004 for design and testing, while the inner liner is qualified as a component under the packaging certification of the specific dangerous goods pack group where applicable. Terminal products include 90–120 µm FIBC inner liners for polymer granules and fine mineral powders, 50 kg heavy-duty shipping sacks, and chemical sack liners for hygroscopic powders, with dimensions up to 2200 mm lay-flat width.

    Food-Contact Form-Fill-Seal Web and Seal Initiation Temperature

    When Dowlex 2045G CIR is coextruded as the sealant layer of a form-fill-seal packaging web, the critical control parameter is the seal initiation temperature rather than the crystalline melting peak. The resin's short-chain branching distribution permits seal initiation in the range of 85–105 °C when blended with low-density polyethylene, depending on co-monomer type and cooling rate. Compliance for direct food contact is assessed under FDA 21 CFR 177.1520(c) and EU Regulation 10/2011, with final overall migration testing carried out on the total packaging structure using food simulants and the reduced time/temperature conditions corresponding to the intended use.

    In three-layer FFS films, the sealant layer contains 60–75 wt% Dowlex 2045G CIR, 20–30 wt% autoclave or tubular LDPE with a density of 0.923–0.925 g/cm³, and 5–10 wt% EVA with vinyl acetate content of 12–18%. Slip and antiblock concentrates are added to the skins at 0.5–1.5 wt% to achieve a kinetic coefficient of friction of 0.15–0.25 under ASTM D1894-14, a range that prevents blocking during VFFS jaw cycling without excessive seal interference.

    Downstream conversion occurs on vertical form-fill-seal machines equipped with horizontal sealing jaws. The blown film line used upstream operates at blow-up ratio 2.0:1 to 2.5:1, with die gap 1.8–2.2 mm and melt temperature 190–230 °C. The web is surface-treated to 38–44 mN/m on the lamination side and kept on the opposite surface to preserve slip properties. Seal bars are set to 115–135 °C, with dwell time 0.3–0.6 s and pressure 40–60 N/cm².

    Table 1. Regulatory compliance matrix for food-contact FFS web containing Dowlex 2045G CIR.

    Regulatory referenceApplied boundaryQuantitative criterion
    FDA 21 CFR 177.1520(c)Olefin polymers in food-contact articles; end-test requirementFinal film subject to extraction limits; no single numerical release value assigned to resin alone
    EU Regulation 10/2011 Annex IPlastic multi-layer structures in direct food contactOverall migration limit 10 mg/dm² or 60 mg/kg under assigned simulant and time/temperature conditions
    REACH EC 1907/2006European Union resin import and downstream article supplySVHC communication threshold 0.1 wt% at article level

    Terminal food-contact products include frozen vegetable pouches, dry mix and cereal bags, and powder beverage sachets with seal widths of 12–18 mm, where the LLDPE-based sealant web is laminated to PET or oriented polypropylene print webs.

    When Lamination Sealant Layers Are Coextruded Rather Than Adhesive-Laminated

    In flexible packaging laminates where the sealant web is coextruded as a blown film and then adhesive-laminated to a reverse-printed PET or oriented polypropylene substrate, Dowlex 2045G CIR functions as the mechanical toughness layer behind the sealant skin. The resin's melt strength at 190 °C permits stable bubble formation at lower melt temperatures, which limits oxidative gel formation during extended runs on high-output blown film lines.

    Typical coextruded sealant web formulation comprises 75–85 wt% Dowlex 2045G CIR in the core layer and 15–25 wt% LDPE or EVA in the skin layers, with the outer skin specified for adhesion to the 2–4 g/m² polyurethane laminating system. In solventless lamination, the film surface energy is maintained at 42–46 mN/m to achieve wet-out without priming.

    The blown film line uses die diameter 200–350 mm, die gap 1.6–2.0 mm, blow-up ratio 2.2:1 to 2.6:1, and melt temperature 195–225 °C. After slitting, the web is inspected for gel count using camera-based surface inspection; gel counts above 10 gel particles per m² above 200 µm are rejected for high-gloss applications because they telegraph through the laminate surface under print.

    Food-contact status follows FDA 21 CFR 177.1520(c) and EU Regulation 10/2011, with responsibility for migration testing allocated to the laminator because the final structure includes adhesive and printing ink components not present in the sealant web. The resin layer itself is not exposed to direct food in most laminates, but the sealant skin is thinned to 5–10 µm of the total 45–60 µm sealant web, so the food-contact layer is a compounded EVA or LDPE blend rather than the pure resin. Terminal articles include stand-up pouches for dry foods, sachet laminations for powdered drink mixes, and medical device overwrap where the structure is not subjected to autoclave conditions.

    In e-commerce logistics film production using post-consumer LLDPE recyclate, a fraction of virgin Dowlex 2045G CIR is retained to restore transverse tear resistance and bubble stability that the recycled source loses after repeated heat history. In this application the resin is not used as a 100 wt% stream; its function is to widen the processing window of the recycled resin and to normalise gel content to a level acceptable for automatic bagging lines.

    A production-scale blend is typically 20–40 wt% Dowlex 2045G CIR, 50–60 wt% rLLDPE post-consumer film recyclate, and 5–10 wt% LDPE to assist bubble cooling. A processing aid masterbatch is metered at 1–2 wt% when the melt pressure upstream of the screen changer exceeds 25–30 MPa, and the screen pack is specified at 80/120/80 mesh to capture contaminants above 125 µm.

    Blown film lines with grooved feed extruders and vented single screws are used, with melt temperature limited to 190–215 °C to avoid further degradation of the recyclate fraction and to keep gel formation below the optical rejection threshold. The bubble is run at a blow-up ratio of 2.0:1 to 2.5:1, frost line height 450–700 mm, and the film is slit into mailer widths of 300–450 mm for downstream heat sealing.

    Compliance under EN 15343:2007 supports the traceability of recycled content in the final film, while REACH EC 1907/2006 Article 33 applies to substances of very high concern if the recyclate contains them above 0.1 wt%. Since the film is not food-contact, migration testing is not applicable; however, residual ink and adhesive in post-consumer flakes require the converter to qualify the recyclate supplier against its incoming lot specifications for odour and heavy metal content. Products include e-commerce mailer film, padded mailer outer webs, and logistics wrap for carton bundling where the finished thickness is 45–80 µm and the customer specification is focused on tear resistance under sorting equipment rather than optical clarity.

    Free Quote

    Competitive Dow Dowlex™ 2045G CIR LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dowlex™ 2045G CIR LLDPE is a linear low-density polyethylene resin assigned to the rotational molding segment and supplied under a certified circular feedstock program. The CIR suffix identifies a mass-balance-controlled allocation of circular feedstock; the polymer backbone, additive package, and melt rheology are maintained against the same target values as standard Dowlex 2045G. The grade is supplied as pellets and typically converted to 35-mesh powder for dry-flow rotomolding. Primary specification anchors include a melt flow index of 0.45 g/10 min determined at 190 °C under 2.16 kg piston load per ISO 1133-1:2022, and a density of 0.945 g/cm³ measured per ISO 1183-1:2019. The comonomer system is an octene-based short-chain branching architecture characteristic of the Dowlex solution polymerization platform; this topology contributes to a higher tie-chain density than butene-copolymer LLDPE at equivalent melt flow index.

    Typical mechanical values from supplier technical data include a tensile yield stress of 19 MPa per ISO 527-2:2012, elongation at break above 800% under the same standard, flexural modulus near 700 MPa per ISO 178:2019, and environmental stress crack resistance exceeding 1000 h when tested under ASTM D1693. Low-temperature brittleness is reported below -76 °C per ASTM D746, while the Vicat softening point is approximately 121 °C under ISO 306/A120. These values are typical targets and should not be interpreted as lot release specifications unless explicitly stated in the certificate of analysis.

    Typical Property Targets for Dowlex 2045G CIR LLDPE
    PropertyTest MethodTypical ValueSignificance for Rotomolding
    Melt flow indexISO 1133-1:20220.45 g/10 minSintering rate and bubble elimination
    DensityISO 1183-1:20190.945 g/cm³Stiffness and chemical barrier
    Tensile yield stressISO 527-2:201219 MPaWall design and load resistance
    Elongation at breakISO 527-2:2012>800%Ductility before fracture
    Flexural modulusISO 178:2019~700 MPaDeformation resistance under load
    Environmental stress crack resistanceASTM D1693>1000 hChemical exposure and slow crack growth
    Brittleness temperatureASTM D746< -76 °CLow-temperature service capability
    Vicat softening pointISO 306/A120121 °CUpper thermal service guidance

    How Does 2045G CIR Respond to Rotomolding Thermal Profiles and Pulverization?

    On production-scale three-arm carousel machines with direct-fired ovens and forced-air cooling, pellet-to-powder conversion is performed before mold charging. Toll pulverizers generally target a 35-mesh top cut using high-speed disk or centrifugal mills equipped with airflow classifiers; powder dry-flow behavior is then checked by funnel methods such as ASTM D1895. Molten densification requires the peak internal air temperature to reach between 204 °C and 232 °C; lower values produce incomplete sintering and residual microvoids, while higher values accelerate inner-surface oxidation, especially when the oven residence time is extended by more than 10% beyond the optimized cycle. Mold surface temperature is typically held between 260 °C and 315 °C, with the lower boundary governed by bubble dissolution and the upper boundary governed by oxidative degradation and mold-release buildup.

    Cycle design on shuttle or carousel equipment must account for wall thickness. Thick sections above 12 mm require longer oven residence but lower air recirculation velocities to avoid surface polymer degradation before the core reaches sintering temperature. Process audits on lines running 6 mm to 9 mm wall tanks show that dense outer skins form first and can insulate the inner layer; operators therefore lengthen cooling rather than elevate oven temperature to avoid post-mold warpage. Published data for this specific configuration is limited, but the practical failure modes observed are pinhole formation at gate areas and brittle inner-surface layers when the mold is pulled before internal air temperature falls below 120 °C.

    Pre-drying of pellets is not required at storage conditions below 50% RH. High-humidity powder storage may require moisture conditioning to preserve consistent dry-flow feed into the mold, because surface moisture interferes with powder flow and can create steam-induced voids during the first oven stage.

    Oxidative induction time is a useful lot-to-lot control parameter for extended oven cycles. Converters should request the antioxidant package performance value from the certificate of analysis under ISO 11357-6, because this value defines the remaining stabilizer reserve rather than the initial melt flow index alone. A reduction in oxidative induction time below the supplier-stated lower control limit typically indicates insufficient thermal stability for high-temperature rotomolding cycles above 290 °C mold surface temperature.

    Relative to butene-comonomer rotomolding LLDPE of similar melt flow index, the octene distribution in 2045G CIR modifies the tie-chain population and yields higher ESCR retention under ASTM D1693 and a lower brittle point under ASTM D746. The density of 0.945 g/cm³ places the grade above conventional low-density LLDPE and below HDPE rotomolding resins; this yields a flexural modulus near 700 MPa, which is lower than the 900–1100 MPa range typical of HDPE but adequate for medium-stiffness tanks and bins where low-temperature impact resistance carries a higher priority.

    Compared with standard Dowlex 2045G, the CIR mass-balance allocation does not require a change in molding parameters. The carbon feedstock attribution is managed through the production system; converters purchasing CIR material must maintain ISCC PLUS chain-of-custody documentation if they intend to make downstream circular content claims. Mechanical property equivalence is expected under the same certificate of analysis acceptance limits because the polymerization and finishing process remains unchanged.

    When 2045G CIR Replaces Fossil LLDPE in Low-Temperature Rotomolded Structures

    Agricultural chemical tanks, secondary containment basins, and outdoor material-handling bins are candidate structures because the polymer combines an ESCR value above 1000 h with a brittle temperature below -76 °C. In rotomolded water chlorination tanks, stress cracks from weld lines and gate areas are governed by the polymer’s slow crack growth resistance; the narrow molecular weight distribution of the solution-processed resin reduces low-molecular-weight tail content that can otherwise act as crack initiation sites. Fabricators following ASTM D1998 for stationary polyethylene tanks should verify wall-thickness distribution and drop-impact performance on the final part; the base resin’s typical properties do not substitute for part-level qualification.

    For outdoor service, the base resin does not inherently contain a UV stabilizer package sufficient for long-term UV exposure without additional formulation. Converters must specify a UV stabilizer masterbatch at supplier-recommended loading and validate weathering performance by ASTM D4329 or ISO 4892-2 exposure on rotomolded panels. Failure to stabilize adequately produces surface chalking and embrittlement before the mechanical ESCR and impact values of the base polymer can be fully utilized.

    Continuous exposure to strong oxidizing acids, aromatic solvents, and chlorinated hydrocarbons is outside the recommended service boundary. Polyethylene swells in hydrocarbon service, reducing wall thickness and joint integrity; therefore, chemical compatibility must be evaluated by immersion testing under ISO 175 or ASTM D543 using the specific chemical concentration and service temperature. Rotational molding of 2045G CIR is also not recommended for prolonged internal pressure service above 60 °C unless the part is designed with hoop stress below the material’s long-term hydrostatic strength established by ISO 9080 regression. The resin is not crosslinked; therefore, it will not provide the creep resistance of crosslinked PE under continuous stress at 80 °C or above. Published data for this specific configuration is limited.

    Food-contact suitability is not automatically conferred by the CIR designation. The base polyethylene may be evaluated under FDA 21 CFR 177.1520 and EU Regulation 10/2011 if the finished compound incorporates only compliant additives, but the converter bears responsibility for finished-part compliance including migration testing under EU Regulation 10/2011 or equivalent national legislation.

    Comparative Property and Feedstock Matrix
    ParameterDowlex 2045G CIRButene-LLDPE RotomoldingHDPE Rotomolding
    Density0.945 g/cm³0.935–0.940 g/cm³0.950–0.960 g/cm³
    Melt flow index0.45 g/10 min0.4–0.7 g/10 min0.3–0.5 g/10 min
    ESCR>1000 h200–600 h50–200 h
    Brittleness temperature< -76 °C-60 to -40 °C-40 to -20 °C
    Flexural modulus~700 MPa550–650 MPa900–1100 MPa
    Feedstock pathwayISCC PLUS mass-balance circularFossilFossil

    Representative ranges in the comparative matrix are for general-purpose rotomolding grades and vary by manufacturer. The Dowlex 2045G CIR values are supplier typical targets and should be verified against the certificate of analysis before mold trials or production release.

    Top