Dow Dowlex 2045 Linear Low Density Polyethylene Heavy Duty Film Grade

Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade

    • Product Name: Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 939826
    Product Name DOW DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade
    Manufacturer Dow
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Density 0.920 g/cm³
    Melt Index I2 1.0 g/10 min
    Melting Point 124 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Break Md 38.6 MPa
    Tensile Strength At Break Td 34.5 MPa
    Ultimate Elongation Md 800%
    Ultimate Elongation Td 900%
    1 Secant Modulus Md 200 MPa
    1 Secant Modulus Td 240 MPa
    Elmendorf Tear Strength Md 120 g
    Elmendorf Tear Strength Td 300 g
    Dart Drop Impact 120 g
    Haze 12%
    Gloss 45 55
    Coefficient Of Friction 0.2

    As an accredited Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DOWLEX™ 2045 is supplied in 25 kg polyethylene-lined multiwall paper bags, palletized; also available in 1,000 kg bulk bags.
    Container Loading (20′ FCL) Container Loading (20′ FCL): DOWLEX™ 2045 LLDPE Heavy Duty Film Grade in 25 kg bags, palletized, stretch-wrapped; approx. 20 MT.
    Shipping DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade, is shipped as polyethylene pellets in moisture-resistant bags, bulk bags, trucks, or railcars. It is not DOT/IMDG/IATA regulated, with no UN number, hazard class, or packing group. Store cool, dry, away from direct sunlight and ignition sources.
    Storage Store DOWLEX™ 2045 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed to prevent moisture and contamination. Maintain clean, labeled packaging; avoid dust generation and static discharge. Store away from strong oxidizers. Protect from prolonged moisture exposure and UV radiation. Use first-in, first-out stock rotation. Do not store near odorous materials.
    Shelf Life Recommended shelf life is 24 months when stored unopened in a cool, dry place away from direct sunlight and moisture.
    Application of Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade

    On a high-speed form-fill-seal converting line running DOWLEX™ 2045 at film thicknesses from 80 µm to 120 µm, the web is subjected to impulse seal-bar temperatures of 125–140 °C, dwell times of 0.5–1.0 s, and vertical drop loads exceeding 30 kg per sack. The resin is not pre-dried unless storage relative humidity exceeds 50 %, because moisture uptake above that threshold can generate micro-bubble surface defects in the melt film and reduce seal consistency. The formulation for this segment is typically 100.0 wt% DOWLEX 2045 as the base polymer, with 2.0–3.0 wt% titanium dioxide white masterbatch for opacity and UV opacity during outdoor warehousing, 0.5–1.0 wt% slip/antiblock concentrate, and 0.05–0.2 wt% polymer processing aid to suppress die deposits on long campaigns. Excess inorganic masterbatch above 3.0 wt% repeatedly depresses Dart impact below the required handling threshold, so the addition ratio is maintained within this band unless a converter has generated comparable data under ASTM D1709-16a. Compliance is verified against ASTM D1709-16a for free-falling dart impact, ASTM D1922-09 for Elmendorf tear propagation, and ISO 527-3:2018 for machine-direction and transverse-direction tensile properties; melt flow rate is controlled to 1.0 g/10 min under 190 °C and 2.16 kg load by ASTM D1238-10. On a 75 mm single-screw extruder with 30:1 L/D grooved feed section, the process window is 205–225 °C melt temperature, 2.0 mm annular die gap, 2.2:1–2.4:1 blow-up ratio, and 550–750 mm frost line height. At melt temperatures below 200 °C, die pressure oscillation becomes audible on the barrel and film gauge bands fluctuate beyond ±8 %, producing sack side-seam weaknesses. The terminal products are valve sacks and open-mouth sacks for 25 kg to 50 kg granular fertilizers, pelleted resins, and non-volatile chemical solids, where the gusseted tube is cut, impulse-sealed, and discharged through a rotary packing station.

    When Silage Covers Must Combine Oxygen Ingress Control and Multi-Season UV Ageing Resistance

    The silage cover segment uses DOWLEX 2045 not as a transient packaging film but as a weathering component that must retain mechanical integrity after repeated handling by tractor-mounted blocks, livestock contact, and wind-driven mechanical flexing. Formulation for this sector typically consists of 100.0 wt% DOWLEX 2045 plus 3.0–5.0 wt% hindered amine light stabilizer masterbatch, 1.0–2.0 wt% anti-fog surfactant concentrate to reduce interior condensation on fermented forage, and 1.0–2.0 wt% carbon black masterbatch when the clamp face demands extended UV shielding. HALS addition above 5.0 wt% can lower interlayer weld strength in three-layer structures and plate out on the die lip during extended runs, so the upper ratio is treated as a maximum under EN 13207:2018 silage film performance classification. Downstream production uses a three-layer coextruded blown film line with 1.6–2.0 mm die gap, 2.0:1 blow-up ratio, and melt temperature between 190 °C and 210 °C; the high molecular weight and long-chain branching resistance of DOWLEX 2045 allow frost line heights of 600–800 mm without destabilizing the bubble. Film thicknesses run from 25 µm for round bale stretch wraps to 150 µm for pit clamp covers. Terminal finished products are round bale silage wrap, square bale stretch film, and silage clamp cover sheets. Published data for the exact multi-season UV retention of DOWLEX 2045 in this specific configuration is limited, so converters should perform accelerated weathering screening under ASTM G154-16 before issuing a performance guarantee.

    What Governs Seal Integrity and Creep Resistance in Flexible Intermediate Bulk Container Liner Webs?

    When FIBC liner film is extruded from DOWLEX 2045, the dominant failure modes are creep rupture near the bottom spout weld and puncture propagation when powders are discharged under pressure from aeration pads. The liner formulation is typically 100.0 wt% DOWLEX 2045 with 0.3–0.6 wt% slip/antiblock concentrate and 0.05–0.1 wt% processing aid, because softer slip packages above 0.6 wt% can reduce heat-seal peel strength below the value required for hydrostatic head tests under ISO 21898:2021. Compliance is further assessed by ASTM D1709-16a for impact after filling and ISO 527-3:2018 for tensile yield behavior at 50 mm/min crosshead speed. The downstream process is blown film coextrusion on a large-diameter die, commonly 400–600 mm, with internal bubble cooling and automated air ring control to hold thickness variation within ±5 %. Melt temperature is maintained at 200–215 °C, die gap at 2.0 mm, and blow-up ratio at 2.0:1–2.2:1, producing layflat widths from 1,200 mm to 2,600 mm. Film thickness for FIBC liners generally ranges from 80 µm to 120 µm, depending on the bulk density and particle shape of the fill. Terminal products are seamless tubular liners inserted inside woven polypropylene FIBCs for 1,000 kg shipments of polymer powders, fine chemicals, and mineral fillers.

    In below-slab vapor retarder manufacture, DOWLEX 2045 is evaluated not only by standard film tensile tests but also by water vapor permeance and puncture resistance under construction loading, because the installed film must survive direct contact with sharp gravel, rebar chairs, and wheelbarrow traffic before the concrete pour. The single-ply film is typically extruded at 100.0 wt% DOWLEX 2045 with 2.0–3.0 wt% carbon black masterbatch for opacity and UV resistance during exposed staging periods, and 0.05–0.1 wt% processing aid. The governing compliance standard is ASTM E1745-17, which classifies vapor retarders into Class A, B, and C based on water vapor permeance, puncture resistance, and tensile strength; DOWLEX 2045 film above 250 µm thickness is assessed for permeance by ASTM E96/E96M-16 desiccant method and for impact by ASTM D1709-16a. Downstream processing uses high-output blown film lines with 2.2:1 blow-up ratio, 2.0 mm die gap, and melt temperature of 205–220 °C, producing layflat widths up to 6.0 m. The terminal product is a below-slab vapor retarder or radon barrier sheet installed under concrete slabs in commercial and residential construction. The operational boundary is that carbon black loading above 3.0 wt% significantly depresses low-temperature impact performance, so this formulation is not interchangeable with HDPE geomembrane compounds designed for 500 µm or thicker landfill liner service.

    Sizing a Cast Film Line for Heavy-Duty Stretch Hoods Without Sacrificing Gauge Uniformity

    The cast film route for heavy-duty stretch hoods uses DOWLEX 2045 as the puncture-resistant toughening component in a polymer blend rather than as the sole polymer, because a 100.0 wt% LLDPE hood film would develop excessive machine-direction elongation and insufficient transverse recovery. A representative formulation for this application is 45.0 wt% DOWLEX 2045, 30.0 wt% low-density polyethylene, and 25.0 wt% metallocene LLDPE, with 0.5–1.0 wt% cling additive and 0.05–0.1 wt% processing aid. The film is evaluated under ASTM D882-18 for tensile elongation in both directions, ASTM D1709-16a for drop-impact toughness, and ASTM D4649-20 for selection criteria relevant to stretch hood containment. Downstream processing on a five-layer cast coextrusion line uses a 3,000 mm coat-hanger die, 240 °C melt temperature, 18–22 °C primary chill roll temperature, and line speeds up to 350 m/min. The main processing conflict is gauge uniformity at high line speed: if winder tension exceeds 80 N/m, neck-in becomes unstable and edge-bead thickness rises above ±5 % of nominal. Terminal finished products are heavy-duty stretch hoods applied by automated pallet wrapping machines for building materials, bagged mineral products, and chemical drums. Published data for this exact DOWLEX 2045 / mLLDPE / LDPE blend at full industrial width is limited, so pilot-line trials with the intended die gap and chill roll configuration are required before commercial qualification.

    Puncture Propagation and Low-Temperature Flexibility in Frozen Food Block Packaging Without Ethylene-Vinyl Acetate

    DOWLEX 2045 is converted into frozen food block packaging where the critical requirement is resistance to puncture by bone fragments, ice shards, and hard-frozen product edges at temperatures as low as -30 °C. Unlike ethylene-vinyl acetate based structures, the resin avoids vinyl acetate monomer migration concerns and maintains a simpler food contact statement under FDA 21 CFR 177.1520(c) 3.1a and 3.2, as well as Regulation (EU) No 10/2011 Annex I for multilayer olefin films. The formulation is 100.0 wt% DOWLEX 2045 with 0.8–1.0 wt% slip/antiblock masterbatch and no EVA; seal initiation is achieved through impulse or hot-bar sealing with PTFE-coated seal bars, but sealing through ice deposits requires increasing dwell time by 0.2–0.4 s relative to dry film. Mechanical compliance is verified by ASTM D1709-16a at room temperature and product-conditioning trials at -20 °C, plus ISO 527-3:2018 tensile elongation at 500 mm/min. Downstream production is blown film coextrusion with a 2.0 mm die gap, 2.0:1–2.2:1 blow-up ratio, 205–215 °C melt temperature, and film thickness maintained between 75 µm and 100 µm for heavy-duty frozen food bags. The terminal products are frozen meat, seafood, and vegetable block bags used in high-speed vertical form-fill-seal lines. The operational boundary is that film thickness below 50 µm is not recommended for sharp-edged frozen products because transverse-direction Elmendorf tear retention drops under ASTM D1922-09 after freezer conditioning.

    Free Quote

    Competitive Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2045 Linear Low Density Polyethylene is a heavy-duty film grade supplied by The Dow Chemical Company for blown film extrusion. The resin is produced by a solution polymerisation process that yields a linear polyethylene backbone with controlled short-chain branching. Supplier-published typical values list a density of 0.920 g/cm³ when measured in accordance with ASTM D792 and a melt index of 1.0 g/10 min at 190°C under a 2.16 kg load when measured in accordance with ASTM D1238. These values place DOWLEX 2045 in the low-density segment, but the linear architecture separates its melt rheology and solid-state toughness from high-pressure low-density polyethylene homopolymers of equivalent density. Primary conversion is by air-cooled or internal-bubble-cooled blown film lines producing industrial liners, heavy-duty shipping sacks, agricultural silage covers, and construction sheeting. The resin is also used in coextruded structures as a toughness layer. The supplier’s technical data sheet states that typical values are not specification limits; lot-specific certificate-of-analysis data govern final acceptance. No pre-drying is required under normal storage conditions, but condensation from storage below the dew point can introduce surface moisture that reduces bubble stability.

    What Distinguishes DOWLEX 2045 from Conventional Butene LLDPE Resins?

    The principal architectural difference is comonomer type. DOWLEX 2045 is an octene-copolymer linear low-density polyethylene, whereas many general-purpose LLDPE grades use butene as the short-chain branching monomer. In an octene copolymer, the branch length is six carbon atoms, which influences tie-molecule formation and resistance to slow crack growth in film. Under dart impact loading per ASTM D1709, an octene LLDPE of equivalent density and melt index typically develops higher puncture energy than a butene copolymer at the same gauge because the longer branches permit more efficient stress transfer through the amorphous phase. Elmendorf tear resistance per ASTM D1922 often shows a similar ranking, although machine-direction tear and cross-direction tear respond differently to blow-up ratio and frost line height. The replacement of butene with octene may also reduce heat seal initiation temperature in many formulations, but the magnitude is resin-specific and must be verified on a given film line. DOWLEX 2045 should not be selected when the primary target is maximum tensile modulus or stiffness, because higher-density bimodal polyethylene grades exceed it in this property. On air-cooled lines without internal bubble cooling, converters report that octene grades may run at slightly lower melt temperatures than butene equivalents to avoid bubble sag, but published data for this specific configuration is limited.

    On grooved-feed single-screw extruders with length-to-diameter ratios between 24:1 and 30:1, DOWLEX 2045 is conventionally staged with a flat reverse temperature profile. Recommended melt temperatures for bubble stability range from 190°C to 225°C. Barrel temperatures are typically set from 160°C in the feed zone to 210°C at the adapter, while the die is maintained between 190°C and 210°C. A die gap of 1.8 mm to 2.5 mm and a blow-up ratio between 2.0:1 and 3.0:1 provide a workable balance between transverse mechanical properties and output. Excessively narrow die gaps below 1.5 mm can raise shear stress and trigger melt fracture, while gaps above 3.0 mm may reduce melt strength and destabilise the bubble. Frost line height is normally maintained between 2 and 6 die diameters, depending on film gauge and cooling air velocity; lowering the frost line increases quench rate and improves optical clarity but may reduce dart impact. Internal bubble cooling lowers melt temperature more rapidly and allows higher output, but the additional cooling can induce gauge bands if air distribution is asymmetric.

    Tear Resistance, Dart Impact, and Gauge Interaction in Finished Film

    Mechanical performance of DOWLEX 2045 film is highly gauge-dependent. Dart impact values reported under ASTM D1709 are not normalised to unit thickness; therefore a 25 µm film will show lower absolute dart impact than a 100 µm film of the same resin. Specification sheets that omit film gauge are incomplete for comparative purposes. Elmendorf tear resistance per ASTM D1922 also depends on gauge, orientation, and blow-up ratio. Increasing blow-up ratio raises cross-direction orientation and can improve cross-direction tear while lowering machine-direction tear. Puncture resistance per ASTM D5748 is frequently used for agricultural and construction films because it applies biaxial deformation at low strain rates, but it does not correlate linearly with high-speed dart impact. For heavy-duty sack applications, the critical failure mode is commonly puncture by sharp granular contents rather than pure tensile loading; converters should therefore specify dart impact and slow-rate puncture together rather than relying on tensile yield strength alone. In biaxial orientation, DOWLEX 2045 shows lower stiffness than high-density grades but higher elongation at break, which delays brittle fracture at fold lines and gusset edges.

    Heavy-duty shipping sacks produced from DOWLEX 2045 are commonly fabricated by blown film extrusion followed by bottom sealing. Seal strength is measured according to ASTM F88, and hot tack is measured according to ASTM F1921. The resin’s linear architecture provides a low seal initiation temperature relative to high-pressure LDPE, but exact sealing curves must be developed with the specific sealing bar profile, dwell time, and film temperature. In gusseted sacks, high machine-direction tear resistance reduces failure at the crease line during drop testing, while dart impact resistance controls puncture from sharp granular contents. Films are often surface-treated by corona discharge to reach a wetting tension of 38 mN/m to 42 mN/m before printing or lamination. Treatment level decays with storage, so use within 24 h to 48 h is typical for this grade. Additive packages may include slip and antiblock levels that affect coefficient of friction; ASTM D1894 is used to quantify static and kinetic coefficient of friction. Converters evaluating DOWLEX 2045 for silage wrap must test oxygen permeability and UV additive persistence under actual field exposure, because these properties depend on additive masterbatch and film thickness rather than on the polyethylene base resin alone.

    When Coextrusion Pairs DOWLEX 2045 with HDPE or MDPE, What Changes?

    In multi-layer heavy-duty film, DOWLEX 2045 is positioned as a tie-adjacent toughness layer or as an outer skin over high-density polyethylene or medium-density polyethylene core layers. The linear backbones of DOWLEX 2045 and HDPE share similar processing windows, but the lower density of the LLDPE skin reduces overall film stiffness; total structure modulus can be modelled by layer volume fraction and tensile modulus of each layer according to ISO 527-3. Adhesion between layers is governed by melt temperature at the die and interfacial residence time; insufficient feed-block residence can produce delamination. In coextrusion blow-up ratios above 2.5:1, gauge distribution between layers can shift if the melt viscosities are not matched. DOWLEX 2045 at 190°C has a lower viscosity than many HDPE grades at equivalent shear, which can cause the LLDPE skin to migrate to regions of lower die resistance. The resulting thickness variation must be measured by gravimetric or optical gauge profiling. When a high-stiffness outer layer is required, converters often reduce the LLDPE layer to less than 20% of the total structure to preserve overall modulus while retaining puncture resistance.

    Regulatory status for food-contact applications is commonly assessed under FDA 21 CFR 177.1520 for olefin polymers and EU Regulation No 10/2011. Specific migration limits depend on film thickness, temperature, and food simulant. DOWLEX 2045 does not contain intentionally added per- and polyfluoroalkyl substances, but converters must verify compliance declarations against the supplier’s current product stewardship bulletin. Under REACH, the resin is a polymer and is generally exempt from registration as a substance, but monomers and additives require registration. For agricultural film, soil-biodegradable claims do not apply to this grade; disposal must follow local plastics recycling or energy recovery routes. Heavy metal content and phthalate content are not expected to exceed standard packaging thresholds, but lot-specific documentation should be requested when the end market requires compliance with EU Directive 94/62/EC packaging waste limits.

    Property Test Method Typical Value
    Density ASTM D792 0.920 g/cm³
    Melt Index ASTM D1238, 190°C/2.16 kg 1.0 g/10 min
    Comonomer Type Supplier documentation Octene-1
    Film Dart Impact ASTM D1709 Gauge-dependent
    Elmendorf Tear ASTM D1922 Gauge- and orientation-dependent
    Processing Parameter Recommended Range
    Melt temperature 190°C–225°C
    Die temperature 190°C–210°C
    Die gap 1.8 mm–2.5 mm
    Blow-up ratio 2.0:1–3.0:1
    Frost line height 2–6 die diameters
    Screw L/D ratio 24:1–30:1

    On production-scale lines, bubble instability in DOWLEX 2045 is most often observed when the melt temperature falls below 180°C or when the die gap is reduced below 1.5 mm without a corresponding reduction in output. Typical failure modes include vertical gauge bands, oscillating frost line height, and intermittent bubble collapse at high stalk heights. These are distinct from moisture-induced defects, which appear as random pinholes or irregular bubble diameter. Gauge bands are frequently corrected by improving die lip parallelism and by increasing internal bubble cooling air exchange. Oscillating frost line height is often linked to insufficient melt strength at high draw ratios; reducing the stalk height or increasing the melt temperature by 5°C to 10°C stabilises the bubble. On lines with twin-screw feeding, batch-to-batch melt index variation above ±0.1 g/10 min can shift bubble geometry and require adjustment of air ring velocity. These operational boundaries are more important than resin grade alone because heavy-duty film lines operate near the upper limit of bubble stability to maximise output.