| HS Code | 680139 |
| Product Name | DOWLEX™ 2045.11G Linear Low Density Polyethylene |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Octene-1 |
| Density | 0.920 g/cm³ |
| Melt Index | 1.0 g/10 min (190°C/2.16 kg) |
| Melt Flow Ratio | 27 (I21/I2) |
| Tensile Strength At Yield | 9.7 MPa |
| Tensile Strength At Break | 24.1 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 241 MPa |
| Vicat Softening Point | 100 °C |
| Melting Point | 122 °C |
| Crystallization Temperature | 104 °C |
| Hardness Shore D | 50 |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Md | 300 g |
| Elmendorf Tear Td | 500 g |
| Haze | 10% |
| Gloss | 60% |
As an accredited Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DOWLEX™ 2045.11G Linear Low Density Polyethylene in 25 kg polyethylene-lined bags, 55 bags per pallet (1,375 kg). |
| Container Loading (20′ FCL) | 20′ FCL: 25 kg bags, 55 bags per pallet, 20 pallets, totaling 1,100 bags / 27.5 MT Dow DOWLEX™ 2045.11G LLDPE. |
| Shipping | DOWLEX™ 2045.11G LLDPE ships as a non-hazardous, non-DG thermoplastic solid in 25 kg polyethylene bags, typically 1,000 kg per pallet, or in bulk containers. Not regulated for transport. Keep dry, away from heat, sunlight, and contamination. Use standard warehouse, truck, or rail handling. |
| Storage | Store DOWLEX™ 2045.11G indoors at ambient temperature in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and strong oxidizers. Keep original containers closed to prevent moisture, dust, and contamination. Use clean pallets, avoid excessive stacking, and maintain good housekeeping to prevent pellet spills and slipping. Consult the SDS for specific storage requirements. |
| Shelf Life | DOWLEX 2045.11G shelf life is typically 24 months when stored cool, dry, in sealed original packaging, protected from sunlight. |
In blown film extrusion of heavy-duty shipping sacks in the 100 µm to 200 µm gauge range, DOWLEX 2045.11G is processed on a single-screw extruder with a grooved feed section and an L/D ratio of 25:1 to 30:1. The resin has a nominal density of 0.920 g/cm³ when tested to ASTM D792 and a melt index of 1.0 g/10 min under 2.16 kg at 190 °C when tested to ASTM D1238. Melt temperature is maintained between 199 °C and 232 °C to avoid unmelted gels at the lower boundary and oxidative gel formation above 240 °C during start-up interruptions. Die gap is held between 1.5 mm and 2.5 mm because LLDPE melts of this density retain high extensional viscosity at the die entry; gaps below 1.5 mm can initiate sharkskin when extruder output exceeds 80 kg/h. Blow-up ratio is set from 2.0:1 to 3.0:1. At 2.0:1, machine-direction tear measured by ASTM D1922 becomes anisotropic and may fall below converter targets for filled sacks, while settings above 3.2:1 can produce bubble oscillation on low-stalk lines and gauge variation of ±8% to ±15%. Frost line height is maintained at 6 to 12 die diameters. A 150 µm sack produced under these conditions is typically welded at seal bar temperatures of 105 °C to 125 °C and then tested for drop impact by ASTM D1709/A and seal strength by ASTM F88/F88M; many converters establish a minimum seal strength of 4–7 N/15 mm depending on fill weight and drop height, but the resin supplier does not assign a universal pass value. When the finished sack is intended for food contact, the article must comply with FDA 21 CFR 177.1520(c) 3.2a and EU Regulation (EU) No 10/2011 with associated migration limits, because compliance is a function of the complete film structure rather than the raw resin alone. No pre-drying is required for sealed pellet containers at relative humidity below 60%; however, surface condensation on cold pellets fed directly into the hopper can cause steam-induced bubble defects. On extended runs, die lip buildup from low-molecular-weight fractions can worsen gauge scatter, and operators typically purge with HDPE at 210 °C or reduce die exit temperature by 5 °C to manage the condition.
At carbon black letdown ratios above 5 wt% in silage cover film, the dominant failure risk shifts from processing instability to loss of tear resistance in the black outer layer. Silage covers based on 2045.11G are commonly run as three-layer coextrusions with the base resin in the core at 60–70 wt% and carbon black concentrate in the skins at 3–5 wt%. The concentrate should use a carrier LLDPE with a melt index within 0.5–2.0 g/10 min of the base resin; carrier mismatch above 2.0 g/10 min can produce black specking after 4–6 h of continuous extrusion because the lower-viscosity carrier migrates to the die wall ahead of the pigment. In 100–150 µm silage covers, the black layer suppresses solar irradiance and limits heating of the ensiled crop, while an inner white layer containing 6–10 wt% titanium dioxide masterbatch can reduce inner surface temperature by 5–10 °C under direct solar load. Weathering performance is evaluated after 1000 h and 2000 h of accelerated exposure by tear retention using ASTM D1922 and tensile elongation at break using ASTM D882; no universal specification exists for the base resin because additive packages are converter-compounded. Oxygen transmission is measured at 23 °C and 0% RH by ASTM D3985; a 125 µm three-layer structure generally requires oxygen transmission below 2500 cm³/m²·day·atm, but the achievable value depends on carbon black loading, layer ratio, and cooling rate. If the film is stored in contact with fermented feed, the converter must verify that the stabilizer package does not extract into the aqueous phase under acidic conditions; published data for this specific configuration is limited, so final film qualification must include a migration study under the intended use conditions. The resin itself is not a ready-to-use silage formulation, and failure to add a carbon black concentrate with sufficient ultraviolet stabilization leads to edge-initiated cracking after one season in exposed locations.
Frozen food liners and pillow pouches converted from 2045.11G in the 50 µm to 90 µm gauge range are tested for seal initiation, hot-tack, and puncture propagation because the packaging line is exposed to cyclic thermal stress at pack-off temperatures down to -20 °C. The seal initiation temperature for LLDPE with a density of 0.920 g/cm³ typically falls between 95 °C and 110 °C, allowing reciprocating-film seal jaws to operate at up to 50 cycles/min without excessive dwell. Hot-tack performance is assessed by ASTM F1921, and the usable hot-tack window is commonly 15–25 °C above seal initiation; processors must avoid upper seal jaw temperatures above 140 °C because edge thinning reduces weld integrity. Seal strength after 24 h of storage at -20 °C is measured per ASTM F88/F88M; a loss of more than 20% compared with room-temperature seals generally indicates inadequate jaw pressure, which should be maintained at 350–500 N/cm² for full surface wet-out. High-speed puncture resistance is evaluated by ASTM D5748 to simulate sharp frozen-product corners, while full-bag drop impact is assessed by ASTM D1709/A. Because the grade is supplied without a slip package, coefficient of friction values above 0.45 per ASTM D1894 are common, and a slip masterbatch at 1.0–2.5 wt% is required if packaging speed exceeds 45 packs/min. Over-addition above 3 wt% of erucamide-based slip can reduce seal strength by migration to the weld interface; seal integrity must be re-verified because the additive bloom can act as a contaminant. On vertical form-fill-seal machines, the film path temperature is kept below 30 °C to prevent blocking, and converters should establish a seal-strength minimum against ASTM F88/F88M under their specific bag geometry rather than relying on resin density alone.
On high-output 50–75 mm grooved-feed extruders producing 25–40 µm ice bags and thin retail produce film, DOWLEX 2045.11G is run with a die gap of 2.0 mm and blow-up ratio of 2.5:1 to 3.5:1. The primary processing constraint is melt fracture on the die land rather than extruder capacity; screw speed is often limited to 60–80 rpm because excessive shear heating in the barrier section can raise melt temperature above 240 °C and initiate oxidation, evidenced by yellowing of the film core and a loss of extractable antioxidants. Thin-gauge film is tested for Elmendorf tear in both directions using ASTM D1922 and tensile elongation at break using ASTM D882; transverse direction tear values can show a ratio of 1.3:1 to 2.0:1 relative to machine direction at low blow-up ratios, and this anisotropy can create splitting failures at bag side seals. Ice bags require low-temperature flexibility, but the exact performance threshold must be established by the converter because seal geometry and bag size dominate the failure mode. After surface treatment for flexographic printing, in-line corona treatment at 35–42 mN/m is applied; however, treatment decay can occur within 24 h under high ambient humidity. Plants operating at relative humidity above 70% should store pellets in sealed containers above 15 °C to prevent surface moisture, because water entrainment into the feed throat can decrease output by 5–10% and increase back pressure fluctuation. On high-stalk lines, neck height is maintained at 8–10 die diameters for this gauge range; internal bubble cooling with exhaust air at 15–25 °C improves stability, but if plant dew point exceeds 20 °C, condensation marks can form on the inner surface and later reduce seal strength under ASTM F88/F88M.
Post-industrial edge trim and printed sack regrind are routinely combined with virgin 2045.11G in the core layer of heavy-duty sack films at recycle additions of 20–35 wt%. Above 20 wt%, oxidative induction time measured by ASTM D3895 at 200 °C can fall below 20 min if the regrind has undergone multiple heat histories, especially when the scrap stream contains paper label fragments or nylon film fragments from mixed waste sources. The consequence is not immediate film failure but a narrowing of the safe extrusion temperature window; core extruder melt temperature should then be limited to 199–215 °C, and screw cooling must be checked for localized hot spots above 220 °C. Screen packs of 40/80/100 mesh are inserted ahead of the breaker plate because contaminant particles above 200 µm can produce die lines that fail tear testing under ASTM D1922. Polypropylene contamination at levels above 5 wt% creates hard translucent islands in the film because of the melting point difference; these defects reduce dart impact under ASTM D1709/A and cannot be eliminated by additional mixing at normal LLDPE melt temperatures. Melt pressure fluctuation above ±10 bar during regrind runs indicates feed-zone bridging or regrind bulk-density change; screw speed should be reduced by 10–15% or feed temperature increased by 5–10 °C before returning to rated output. If the finished sack is exported, the converter must also confirm that the regrind stream does not introduce substances restricted by EU Directive 2011/65/EU RoHS or REACH candidate list obligations, because raw resin compliance does not automatically extend to articles containing post-consumer fractions.
The coefficient of friction and haze of 2045.11G thin films are modified by synthetic silica antiblock masterbatch with a typical particle size distribution centered at 4–8 µm. Addition at 0.5–1.5 wt% reduces blocking but increases haze by approximately 1–3 percentage points per 0.5 wt% addition when measured by ASTM D1003; the exact shift depends on particle agglomeration during extrusion and screw shear history. When the antiblock is added only to the skin layer, surface roughness rises and coefficient of friction falls to 0.15–0.25 under ASTM D1894, but the core remains transparent; this configuration is used for frozen food films where bag movement on inclined metal surfaces must not exceed 25°. In contrast, addition of antiblock to the core is less effective for surface slip and can create internal voids that reduce puncture resistance under ASTM D5748. Migration kinetics must be considered before setting a coefficient of friction target: erucamide-based slip agents bloom over 24–72 h and are sensitive to storage temperatures above 35 °C, whereas inorganic antiblock functions immediately but is not self-replenishing after surface wear. Published data for this specific configuration is limited, so final film qualification should use ASTM D1003, ASTM D1894, and ASTM D1922 after the film has been aged for 7 days at 23 °C to allow migration equilibrium. The converter should avoid combining amine-based processing aids with this grade in thin-gauge film without verifying stabilizer package compatibility; such combinations can shift melt stability and generate plate-out on downstream rolls.
Competitive Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DOWLEX™ 2045.11G Linear Low Density Polyethylene is a solution-process ethylene/1-octene copolymer supplied as pellets for cast and blown film extrusion. The nominal density is 0.920 g/cm³ when tested according to ASTM D792, and the melt index is 1.0 g/10 min at 190°C and 2.16 kg as defined by ASTM D1238. These two values establish the resin’s position in the LLDPE film-extrusion range: density controls crystallinity-dependent stiffness and permeation onset, while melt index governs extruder throughput and head pressure. The product is used in heavy-duty film structures where gauge reduction, dart impact resistance, and tear propagation control are converted into industrial liners, agricultural films, and packaging overwrap. The designation “linear” refers to the absence of long-chain branching in the backbone; short-chain branches introduced by the octene comonomer determine solid-state morphology after bubble cooling.
The 2045.11G suffix identifies an additive package that is typically selected for film surface handling and high-speed converting. Exact slip and antiblock loadings should be confirmed against the supplier’s lot documentation because additive concentration affects coefficient of friction, film-to-metal drag, and heat-seal jaw release. The resin is not intended for injection molding or rotational molding; film extrusion and film-converting operations define the primary processing envelope.
The melt viscosity at low shear and the shear-thinning behavior are not characterized by melt index alone. For this resin class, a higher high-load melt index relative to the 2.16 kg condition indicates broad molecular weight distribution, which supports bubble stability and reduces melt fracture at high output. Processing windows published for DOWLEX™ 2045.11G generally place the melt temperature between 190°C and 230°C. Exceeding 240°C increases oxidative gel formation and can generate pinholes in thin film. The Vicat softening point, typically near 104°C under ASTM D1525, defines the upper service temperature for contact applications, while the crystalline melting point measured by differential scanning calorimetry is typically near 122°C under ISO 11357-3. Density and melt index should be re-verified at incoming quality control using ASTM D792 and ASTM D1238 because batch-to-batch variation in comonomer incorporation and additive loading can shift draw-down behavior on high-speed lines.
Rheological measurements on similar linear low density polyethylene grades show pronounced shear thinning above 100 s⁻¹, which is relevant in spiral mandrel dies and narrow die gaps. Melt pressure should be monitored at the die adapter rather than at the screw tip because pressure transducers in the adapter provide a more direct indication of die-lip shear stress. Excessive shear stress can produce sharkskin melt fracture at the die exit; increasing the die temperature or widening the die gap reduces the critical shear stress at the lip. However, widening the die gap beyond 2.5 mm reduces orientation and lowers film tensile strength.
On production-scale blown film lines, DOWLEX™ 2045.11G is typically run on single-screw extruders with barrier mixing sections and an L/D ratio of at least 24:1. The die gap is usually set between 2.0 mm and 2.5 mm, and the blow-up ratio is commonly held in the 2.5:1 to 3.0:1 range. Bubble cooling configuration is more decisive than screw design for this resin: dual-lip air rings and internal bubble cooling stabilize the bubble when output exceeds the melt strength limit. Operators observe that the limiting factor is rarely melting capacity but bubble flutter and draw resonance, particularly at frost-line heights below 1.5 die diameters. In such conditions, reducing the melt temperature within the allowed window increases bubble stiffness and permits higher take-off speeds. Moisture on pellet surfaces is not a hydrolysis concern, but condensation can create surface defects and haze; if storage conditions exceed 60% relative humidity, pre-drying at 80°C for 2–4 h is applied before extrusion. The resin should not be dry-blended with polypropylene or high-pressure LDPE at high concentrations without evaluating seal uniformity and film optics, because immiscible domains can reduce tear resistance under ASTM D1922.
On high-output cast film lines, the same resin is processed with flat dies and chill-roll temperatures between 20°C and 40°C. Cast film produced from this grade typically exhibits more balanced MD/TD orientation than blown film, but lower dart impact and tear strength at equivalent gauge. The selection between blown and cast processes is therefore dictated by the end-use requirement: heavy-duty sacks usually favor blown film for impact resistance, while stretch overwrap and lamination film favor cast process speed and gauge uniformity.
Representative values from supplier technical data for 25 µm blown film are shown below. The values are typical, not specification limits, and they vary with gauge, blow-up ratio, frost-line height, and film-converting conditions.
| Property | Test method | Typical value | Unit |
|---|---|---|---|
| Density | ASTM D792 | 0.920 | g/cm³ |
| Melt index, 190°C/2.16 kg | ASTM D1238 | 1.0 | g/10 min |
| Vicat softening point | ASTM D1525 | 104 | °C |
| Melting point, DSC | ISO 11357-3 | 122 | °C |
| Tensile strength at break, MD | ASTM D882 | 38 | MPa |
| Tensile strength at break, TD | ASTM D882 | 32 | MPa |
| Elongation at break, MD/TD | ASTM D882 | 650/750 | % |
| Dart drop impact, F50 | ASTM D1709 | 140 | g |
| Elmendorf tear, MD/TD | ASTM D1922 | 300/450 | g |
The dart drop impact of 140 g under ASTM D1709 is a central purchasing specification for heavy-duty sack applications because it correlates with film toughness under sharp impact at ambient temperature. The MD/TD tear imbalance, typically 300 g and 450 g under ASTM D1922, is a consequence of blown film orientation and must be accounted for when sealing or stacking the film. Tensile values are determined at 25 µm and 500 mm/min per ASTM D882; lower gauge film reports higher gauge-normalized values in some protocols but lower absolute fracture force. Haze and gloss are not the primary selection criteria for this grade, but surface additive package contributes to handling performance in high-speed bag-making equipment.
The primary technical differences between DOWLEX™ 2045.11G and high-pressure LDPE of similar density arise from molecular architecture. High-pressure LDPE contains long-chain branches that provide high melt strength and stable bubble geometry, but the same branching reduces ultimate tensile strength and dart impact when tested side-by-side per ASTM D882 and ASTM D1709. In contrast, the linear backbone of DOWLEX™ 2045.11G supports higher orientation-induced tensile strength but reduces melt strength; bubble stability must therefore be managed with air-ring design rather than by increasing melt temperature. Against butene-based LLDPE grades of the same 0.920 g/cm³ density and 1.0 g/10 min melt index, the octene-based DOWLEX™ 2045.11G typically gives higher dart impact and tear resistance because the longer short-chain branches distribute tie-molecule formation more effectively during crystallization. This distinction is most visible in thin-gauge film below 25 µm, where dart impact and Elmendorf tear values become sensitive to comonomer type. Processing differences are smaller but measurable: the octene grade may require a slightly lower extruder head pressure and lower melt temperature to avoid surface haze caused by higher shear sensitivity.
Compared with metallocene-catalyzed LLDPE of similar density, DOWLEX™ 2045.11G tends to process with lower head pressure and broader operating latitude, but it may not match the dart impact and clarity of some metallocene grades in coextruded structures. The choice between these materials is therefore controlled by the film line’s bubble cooling capacity and the target seal and tear balance. In high-speed form-fill-seal operations, seal initiation temperature and hot-tack strength must be measured according to ASTM F1921 or ASTM F2622 because comonomer type and additive migration shift the sealing window independently of density and melt index.
For food-contact applications, regulatory status must be verified against FDA 21 CFR 177.1520(c) for olefin polymers used in direct contact with food, and against Commission Regulation (EU) No 10/2011 for plastic materials and articles intended to come into contact with food. Compliance under these frameworks is use- and migration-dependent; the raw resin supplier documentation should be consulted for specific overall migration limits and temperature restrictions. The product may be used as supplied or in blends, but any change in additive masterbatch or recycled content must be re-evaluated under the same standards. Storage should avoid direct sunlight, temperatures above 40°C, and proximity to strong oxidizing agents. Pellets stored in unheated warehouses during winter should be allowed to equilibrate to ambient temperature before opening to prevent condensation on the cold pellet surface. Incompatible melt streams include PVC, nylons, and polycarbonate at processing temperatures; cross-contamination with these polymers can generate carbonized inclusions and film defects.
| Regulatory reference | Scope | Verification requirement |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Olefin polymers for direct food contact | Supplier food-contact statement and migration limits |
| (EU) No 10/2011 | Plastic materials and articles in contact with food | Overall migration and specific migration limits |
| REACH | Chemical substances in the European Union | Registration status and SVHC declaration |
| RoHS | Restriction of hazardous substances | Heavy metal and restricted substance verification |
Published data for the exact film performance of this grade in coextruded high-barrier structures is limited; therefore, pilot-scale trials on the target line are required to establish final gauge, dart impact, and seal strength specifications. Any substitution of DOWLEX™ 2045.11G for another LLDPE grade should be accompanied by re-qualification of tear resistance under ASTM D1922, dart impact under ASTM D1709, and seal strength under ASTM F88 because density and melt index alone do not predict film performance in all converting operations.