| HS Code | 345502 |
| Density | 0.920 g/cm³ |
| Melt Index | 1.0 g/10 min |
| Comonomer | 1-Octene |
| Melting Point | 122 °C |
| Vicat Softening Point | 101 °C |
| Tensile Strength At Yield Md | 10.3 MPa |
| Tensile Strength At Yield Td | 10.3 MPa |
| Tensile Strength At Break Md | 31.0 MPa |
| Tensile Strength At Break Td | 27.6 MPa |
| Elongation At Break Md | 700% |
| Elongation At Break Td | 800% |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 400 g |
| Dart Drop Impact | 180 g |
| Haze | 12% |
| Gloss | 60 |
As an accredited Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade is packaged in 25 kg polyethylene bags for industrial use. |
| Container Loading (20′ FCL) | Dow DOWLEX™ 2045.11 LLDPE Heavy Duty Film Grade: 20' FCL holds 25 MT net, 1,000 x 25 kg bags, floor-loaded. |
| Shipping | Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade, is shipped as non-hazardous polymer pellets in sealed 25 kg bags, palletized and stretch-wrapped, or in bulk octabins/trucks. Transport in clean, dry vehicles; avoid heat, sunlight, moisture, and contamination. Keep packaging closed and labeled, and follow local regulations and the SDS. |
| Storage | Store DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade, in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers closed and pallets intact to prevent moisture, dust, and contamination. Avoid excessive stacking or physical damage. Rotate stock first-in, first-out. No special temperature control is normally required; follow the supplier’s SDS. |
| Shelf Life | Shelf life: Typically 24 months when stored dry, in original sealed packaging, at moderate temperatures, away from direct sunlight, heat, and contaminants. |
On monolayer blown film lines operating with a 90 mm extruder at an L/D ratio of 30:1, DOWLEX 2045.11 is processed as a heavy-duty sack resin for dry bulk shipping sacks, fertiliser packaging, and polymer granule bags. The resin is run against a nominal density of 0.920 g/cm³ and a melt mass-flow rate of 1.0 g/10 min at 190 °C under 2.16 kg load per ISO 1133-1:2022, placing it within the viscosity window that supports heavy-gauge blown film without excessive backpressure on conventional barrier screws. A barrel temperature profile of 180 °C to 210 °C is maintained, while adapter and die zones are held at 210–220 °C. Die gaps from 2.0 mm to 2.4 mm are preferred because gaps below 1.6 mm increase die pressure and shear heating, which can initiate sharkskin on linear resin at high line speeds. In the 180–220 µm thickness range, the bubble is operated at a blow-up ratio of 2.5:1 to 3.0:1; ratios below 2.0:1 produce machine-direction-dominant orientation and reduce transverse-direction tear resistance when measured by ASTM D1922. Frost line height is controlled at 4–6 times the die diameter because an elevated frost line increases quench-induced orientation and can reduce impact toughness. The use of internal bubble cooling reduces stalk surface temperature by 10–15 °C and permits output gains of 20–30 % on a 300 mm die at equivalent bubble stability. Melt pressure transducers at the die are monitored during production; sustained readings above 350 bar indicate the need to widen the die gap or reduce screw speed before melt fracture propagates across the web.
Tensile and impact data for heavy-duty sack film are generated after specimens are conditioned for 48 h at 23 °C ± 2 °C and 50 % ± 5 % relative humidity. Under ISO 527-3, machine-direction and transverse-direction tensile strength at break for a 200 µm monolayer film commonly fall in the 35–45 MPa range, with elongation at break above 600 %. These values shift with bubble geometry: at 3.0:1 blow-up ratio, transverse-direction tensile strength can exceed machine-direction tensile strength by 5–10 %, while at 2.0:1 the reverse orientation dominates. Dart impact is tested according to ASTM D1709-16a; for 180 µm sack film used in 25 kg granular polymer or fertiliser bags, purchaser specifications commonly set dart impact above 700 g using Method A. Puncture resistance is measured by ASTM D5748; a 200 µm film intended for high-abrasion bulk fill is often specified above 90 N probe puncture force, although the exact threshold is set by the end-user loading test. In three-layer coextrusion, 2045.11 is placed in the core at 50–70 wt% of the total structure, while outer layers are a lower-density metallocene plastomer or LDPE sealant. This construction lowers seal initiation to 105–115 °C at 0.8–1.2 s dwell; seal strength is validated by ASTM F88/F88M using a 25 mm width specimen and 250 mm/min jaw separation. Seal values below 6 N/15 mm after sealing at 120 °C indicate insufficient melting of the sealant skin. For freezer-grade shipping sacks, low-temperature dart impact at -18 °C is measured after 48 h conditioning; retention of 70–80 % of ambient impact is used as a practical quality gate for downstream cold-chain filling.
Aggressive industrial liner films fabricated from 2045.11 are used where hydrocarbon process oils, heavy-metal carboxylates, or oxygenated cleaning agents contact the polymer surface during waste consolidation, chemical transfer, or roll-off box service. The primary failure mode is not instantaneous tensile rupture but seal peeling and environmental stress-crack propagation at fold lines after the liner is loaded. Because LLDPE is semicrystalline and has a relatively narrow thermal seal window, seal strength depends on precise control of jaw temperature, jaw pressure, and dwell. When a 150 µm liner includes a sealant layer of metallocene plastomer or EVA at 10–15 wt% of total formulation, seal initiation is lowered to approximately 105–115 °C. Seal strength is tested by ASTM F88/F88M; seals produced at 135 °C and 1.0 s dwell with 250 mm/min grip separation typically fall in the 10–14 N/15 mm range before filling. Oily or solvent-containing contents can reduce post-fill seal strength, so preliminary immersion screening is required. The filled liner material is exposed to the actual chemical or process oil for 7 days at 40 °C using ASTM D543-20; acceptance is based on mass change below 3 % and tensile retention above 80 % of the original value. Published data for 2045.11 in specific hydrocarbon streams is limited; therefore the ASTM D543 screen is treated as a minimum requirement rather than a substitute for field testing.
Coextrusion die design affects layer uniformity and seal thickness in aggressive liner structures. A 5-layer die with a 1.8–2.2 mm die gap is used to avoid interfacial instability caused by rheological mismatch between 2045.11 and lower-melting seal resins. In production, the core layer may be 60–70 % of total gauge, with the seal skin at 15–20 % and the opposite skin containing slip and antiblock. Because erucamide slip migrates slowly through linear low-density polyethylene, coefficient of friction measured by ISO 8295 may remain above 0.4 for the first 24 h after extrusion. Converters compensate with a thicker antiblock-loaded outer skin or with corona treatment to improve winding and bag insertion. If the liner is intended for peroxide-containing waste, the stabiliser package is augmented with phosphite and lactone antioxidants; otherwise chain scission at processing temperatures above 230 °C degrades melt strength, and the film tears during haul-off in high-speed bag-making. Equipment specifications for this application often include a barrier screw with a Maddock mixing section and a 100–150 mesh screen pack; pressure drop across the screen pack above 120 bar indicates unacceptable gel or contaminant accumulation.
Because silage covers and reinforced agricultural films are deployed in direct contact with acidic fermentation leachate and long-term solar radiation, the selection of 2045.11 as a base resin requires additive and extrusion decisions that differ from dry-bulk packaging. The acid level in silage leachate is commonly between pH 3.8 and 4.5, which extracts phenolic antioxidants and accelerates oxidative embrittlement at film edges and fold lines. For a 180 µm monolayer cover, a high-molecular-weight hindered amine light stabiliser package at 0.25 % to 0.45 % and a tris(2,4-di-tert-butylphenyl) phosphite processing stabiliser at 0.08 % to 0.12 % are incorporated at the hopper. Carbon black at 2.0 % to 2.5 % improves UV durability but raises melt pressure and film surface temperature; line speed is reduced by 10–15 % compared with unpigmented LLDPE at the same screw speed. A gear pump is fitted to maintain output uniformity because carbon black masterbatch may vary in melt index by up to 20 % from the base resin. The die gap is held at 2.2–2.4 mm for black films to prevent excessive die pressure, and the screen pack is maintained at 80–100 mesh to reduce carbon black agglomerate defects.
Field performance of silage covers is evaluated with accelerated weathering per ASTM G154 cycle 1 or ASTM D4329; a 180 µm film retaining 80 % of initial elongation after 2,000 h is considered adequate for a 12–18 month silage cover service interval. Puncture from forage stems is measured by ASTM D5748 probe puncture; targets above 70 N at 125 µm are common, but the actual value is determined by forage type and bale density. Sealing of silage covers to silo walls is performed with pressure-sensitive tapes; adhesion is affected by erucamide migration, so the film is corona-treated to 38–42 dyn/cm before taping. In black films, a surface treatment above 44 dyn/cm can increase surface oxidation and make tape adhesion irregular; surface energy is measured by ASTM D2578. The film is laid with 50 mm overlaps and mechanically anchored at the base; failure at an overlap results in oxygen ingress that accelerates fermentation spoilage and defeats the oxygen-limiting function of the cover.
Construction-side applications for 2045.11 include concrete curing covers, temporary enclosures, and below-slab vapour retarders where the film is installed at 100 µm to 250 µm gauge. The primary technical requirement is water vapour transmission resistance, which is measured by ASTM E96/E96M desiccant method at 23 °C and 50 % relative humidity. A 200 µm LLDPE vapour retarder typically exhibits a WVTR below 1.0 g/(m²·day); thinner 100 µm film is closer to 2.0–2.5 g/(m²·day), so specifications for below-slab use often require 250 µm to compensate for construction-site damage. Concrete curing covers are specified under ASTM C171; the film must retain moisture during the curing period and must not tear when walked on or stretched over reinforcing bars. LLDPE film provides higher puncture resistance than LDPE at similar gauge; puncture is measured by ASTM D1709-16a or ASTM D5748 depending on whether falling-dart or probe loading is specified. Temporary enclosure films may require flame-retardant masterbatch addition; inclusion of 15–25 wt% brominated or intumescent masterbatch reduces tensile strength by 15–25 % and increases die pressure, so the extrusion profile is shifted downward by 5–10 °C to avoid decomposition of the flame-retardant package.
| Heavy-duty sack film | dart impact | ASTM D1709-16a | falling dart, Method A or B, 20 specimens |
| Construction vapour retarder | water vapour transmission | ASTM E96/E96M | desiccant method, 23 °C, 50 % RH |
| Silage cover | accelerated weathering | ASTM G154 | UVA-340, cycle 1 |
| Industrial liner | seal strength | ASTM F88/F88M | constant-rate tensile tester, 250 mm/min |
| Low-temperature food liner | low-temperature dart impact | ASTM D1709-16a | conditioned at -18 °C, 48 h |
Below-slab vapour retarders are inspected for puncture and tear resistance before concrete placement because hidden damage after slab installation cannot be remediated. Elongation at break measured by ISO 527-3 should exceed 500 % at 23 °C; at -10 °C the film should retain at least 50 % of ambient elongation to survive winter construction. Lap joints use pressure-sensitive acrylic tapes, and shear resistance is tested by ASTM D3654; a minimum average shear of 4 N/25 mm is often specified for 24 h dwell. If the film is used as a temporary façade or scaffold enclosure, wind-load performance is evaluated under the applicable building-code load combination rather than a polymer test standard. Corners and clamped edges are the primary failure zones; production-scale fabrication therefore includes folded-edge hems and grommet reinforcement at 300–450 mm spacing, with grommet pullout tested by ASTM D638-14 on a 25 mm punched strip to ensure that the film survives handling before the enclosure is tensioned.
When 2045.11 is used as a core layer in low-temperature bulk food liners, the objective is to retain puncture resistance and flex-crack resistance during freezer storage at -18 °C to -30 °C while shifting the seal function to a lower-melting skin layer. The core layer of a 120 µm three-layer film may be 60–70 % of total thickness; this arrangement exposes the core to flexural stresses while the skins provide seal and coefficient-of-friction control. Low-temperature performance is assessed by conditioning film for 48 h at -18 °C and then performing ASTM D1709-16a dart impact or ISO 7765-2; retention of at least 60–70 % of ambient dart impact is expected for a properly formulated structure. Flex-crack resistance is evaluated by the Gelbo flex test ASTM F392; for a frozen-food liner, a pinhole count below 5 after 20,000 cycles at -20 °C is often targeted, but exact pass-fail criteria are purchaser-specific. The sealant skin is typically a metallocene plastomer or a low-melting LDPE blend at 15–20 % of total thickness; its seal initiation temperature of 105–115 °C allows lower sealing temperature and reduces thermal exposure to the frozen product.
Regulatory status must be confirmed against 21 CFR 177.1520(c) for olefin polymers and any applicable food-contact premarket authorizations in destination markets such as EU 10/2011. The base resin supplier may provide a food-contact compliance certificate for 2045.11, but the final film formulation, including slip, antiblock, and sealant layers, must be tested for overall migration according to EU 10/2011 Annex III and 21 CFR 176.170(c) if fatty contact is intended. For dry frozen products, fatty-food simulants may not be required; for packaged processed meats or bakery goods, the converter must run 10-day/40 °C migration tests using the prescribed simulant. No direct food-contact claim for the finished film can be assumed from the base resin compliance statement alone. In production, processing temperatures above 240 °C should be avoided to limit organoleptic volatiles; film samples can be screened for odor and taste by ASTM E1870 or sensory panel per ISO 13301. The sealant layer is monitored for gel formation because recycled sealant edge trim can carry degraded EVA that appears as hard spots in the seal area at 120–130 °C sealing temperatures.
Competitive Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene is a solution-process ethylene/1-octene copolymer supplied as free-flowing pellets for heavy-duty blown film. The material is assigned to the 2045 series with a nominal density of 0.920 g/cm³ and a nominal melt flow index of 1.0 g/10 min measured at 190°C under a 2.16 kg load according to ASTM D1238. The octene-derived short-chain branching distribution gives a broader tie-chain population relative to butene-based linear low density polyethylene at equivalent crystallinity, a feature that governs rapid crack propagation resistance and dart impact performance in heavy-gauge films. The product is targeted at industrial liners, heavy-duty shipping sacks, construction films, and agricultural silage covers where downgauging and tear strength are specified together with standard haul-off and converting performance.
Resin qualification normally begins with melt flow index and density because these two parameters control processability and stiffness. Melt flow index should be measured according to ASTM D1238 method A at 190°C/2.16 kg; density is determined by ASTM D1505 or ASTM D792. The heavy-duty film grade’s low melt flow index of 1.0 g/10 min corresponds to high molecular weight, requiring higher extruder torque and providing the extensional stress needed for bubble stability. A density of 0.920 g/cm³ balances stiffness and toughness; lower density would reduce crystallinity and increase impact but reduce yield stress, while higher density would raise modulus and reduce puncture resistance.
Film properties are not intrinsic; they are produced by the orientation state of the bubble. Machine-direction and transverse-direction tear imbalances are used to diagnose bubble geometry. Tensile properties are measured per ASTM D882, Elmendorf tear per ASTM D1922, dart drop impact per ASTM D1709, and slow-rate puncture per ASTM D5748 or ASTM D2582. A ratio of transverse-direction tear to machine-direction tear greater than approximately 2.5:1 may be acceptable for heavy-duty liners but must be confirmed against final application requirements. Published data for specific configurations are limited; conversion of resin density and melt flow index into a guaranteed film property requires constant temperature profile, die gap, blow-up ratio, frost-line height, and air-ring volume.
Processing on conventional blown film lines proceeds with a grooved-feed or smooth-bore extruder having a barrier screw and L/D of 24:1 to 30:1. Melt temperatures are typically maintained between 190°C and 230°C. Below the lower limit, sharkskin melt fracture may appear at the die lip, especially at high screw speeds; above the upper limit, oxidative chain scission can generate gels and reduce dart impact. The die gap for heavy-duty film is generally 1.5 mm to 2.5 mm, with the wider gap reserved for gauges above 100 µm because it lowers shear stress at the die lip and stabilizes the bubble. Blow-up ratios of 2.0:1 to 3.0:1 are common; higher ratios improve transverse mechanical strength but reduce bubble stability when the frost-line height is too low. Frost-line height is often set at 4 to 8 die diameters to balance orientation and cooling. Dual-lip air rings and internal bubble cooling are preferred on long-run production lines because they raise output while controlling bubble diameter variation.
Because linear low density polyethylene has narrower molecular weight distribution than high-pressure LDPE and exhibits shear thinning, die pressure at a given output is higher than LDPE of the same melt flow index. Dies designed for LDPE may have short lands and narrow gaps; those geometries create excessive shear heating and melt fracture with DOWLEX 2045.11. A die land length of 10 to 20 times the die gap is generally recommended for LLDPE, and the melt pressure is monitored at the die inlet. Gauge uniformity is improved by rotating or oscillating haul-off geometry; randomizing film thickness during winding minimizes hard bands and roll blocking. On production lines, typical gauge variation of ±10% around nominal is considered acceptable for heavy-duty film, although critical liners may require tighter control.
Unlike high-pressure LDPE, the resin does not exhibit pronounced strain-hardening in extensional flow; melt strength is achieved through high molecular weight rather than long-chain branching. This affects bubble stability on high-stalk configurations: a stable bubble is more sensitive to air-ring turbulence and wind-up speed variation. The melt viscosity at processing shear rates of 10²–10³ s⁻¹ remains pseudoplastic, and the material may require higher motor torque than LDPE of equivalent melt flow index. Batch-to-batch variation in melt flow index should be tracked against extruder motor load; a decrease of 0.2 g/10 min from nominal can increase melt pressure by a detectable amount and alter gauge profile.
In heavy-duty industrial liner service, the film is evaluated for puncture propagation resistance under ASTM D5748 and slow-rate tear under ASTM D1938, rather than tensile yield alone. In heavy-duty shipping sack constructions, the film is commonly combined with LDPE or recycled polyethylene layers to optimize sack drop-test performance and sealing. The DOWLEX 2045.11 layer is positioned as the load-bearing core because its octene comonomer increases slow-rate penetration resistance. Industrial liners for bulk chemical packaging require low gel count and pinhole resistance; film qualification includes gel-count inspection and water-bath pinhole tests in addition to ASTM D1709 dart impact. Agricultural films based on this resin may require a UV-stabilizer masterbatch; the base resin is not inherently UV-stabilized. Construction and temporary enclosure films are evaluated for tear propagation under site conditions, where machine-direction tear may be the limiting variable.
Compared with high-pressure LDPE of equivalent melt flow index, DOWLEX 2045.11 has a primarily linear molecular structure with short-chain branching rather than long-chain branching. This gives lower melt strength, less shear thinning, and usually higher extrusion back-pressure. The benefit appears in dart impact, puncture, and tear; the penalty is bubble stability and optical clarity. LDPE typically produces haze below 10% in thin films, whereas LLDPE may exhibit higher haze and lower gloss. However, heavy-duty grades prioritize toughness over optics. A change from LDPE to DOWLEX 2045.11 may permit gauge reduction at equal dart impact performance, though final values must be established by packaging performance testing rather than resin comparison alone.
Compared with butene-copolymer LLDPE of the same density and melt flow index, the octene short-chain branching in DOWLEX 2045.11 provides a more efficient entanglement network. At equivalent dart impact, the octene resin may provide lower thickness or higher slow-rate puncture. Butene grades often have a cost advantage but lower Elmendorf tear at high line speeds because the shorter branches do not distribute tie chains as effectively across the crystalline lamellae. Compared to single-site metallocene LLDPE, DOWLEX 2045.11 may exhibit broader molecular weight and comonomer distribution. Metallocene grades often provide better optics and dart impact at lower film gauge, but may show lower melt strength and higher extrusion torque. DOWLEX 2045.11 is selected where conventional equipment compatibility and high back-pressure tolerance are decisive.
Heat-seal properties are assessed using ASTM F88 or ASTM F1921 for hot-tack; the seal initiation temperature of LLDPE in this density range is typically lower than high-pressure LDPE and depends on seal bar geometry. In heavy-duty sacks, final package strength after sealing is influenced by cooling rate and film thickness. Seal strength measured by ASTM F88 should be interpreted together with dart impact and tear because seal failure in heavy-duty service often initiates at local thickness variations. Conditioning of specimens is performed at 23°C and 50% RH according to ASTM D618 before mechanical testing.
Compliance for food-contact packaging is assessed under 21 CFR 177.1520 for polyolefin articles and EU 10/2011 for plastic materials intended for food contact. The resin does not contain intentionally added cadmium, lead, mercury, or hexavalent chromium; RoHS declarations for packaging are typically prepared from the material safety data sheet and supplier certification. The grade is not flame-retardant and should not be processed in systems that require UL 94 V-0 without flame-retardant compounding. For outdoor service, the base resin requires ultraviolet stabilizer addition; unstabilized film will embrittle after prolonged exposure.
The material is not hygroscopic; pre-drying is not required unless surface condensation is visible after storage in high-relative-humidity environments. If surface moisture is present, a hopper dryer at 60°C for 2–4 h may be used. Pellets should be protected from direct sunlight and stored below 45°C to minimize oxidation of the antioxidant package. Regrind containing high levels of pro-oxidant or metal stearate residues should be limited because such contaminants can destabilize the antioxidant system and reduce long-term film toughness. The base resin is not inherently UV-stabilized; outdoor service without a compounded UV package leads to embrittlement and rapid reduction in elongation at break measured by ASTM D882.