Dow Dowlex 2045 02ac Linear Low Density Polyethylene Blown Film Grade

Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade

    • Product Name: Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 455975
    Comonomer 1-Octene
    Density 0.920 g/cm³
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Melt Flow Ratio I21 I2 30
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield Md 10.3 MPa
    Tensile Strength At Yield Td 10.3 MPa
    Tensile Strength At Break Md 32.4 MPa
    Tensile Strength At Break Td 27.6 MPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    1 Secant Modulus Md 207 MPa
    1 Secant Modulus Td 234 MPa
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 500 g
    Haze 10%
    Gloss 45 60%
    Low Temperature Brittleness -70 °C
    Heat Seal Initiation Temperature 110 °C
    Antiblock Yes

    As an accredited Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DOWLEX™ 2045.02AC is supplied in 25 kg bags, 40 bags per pallet, or 1,000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL: 16 pallets, 25 kg bags, 55 bags/pallet; approximately 22 MT net Dow DOWLEX™ 2045.02AC LLDPE blown film grade.
    Shipping Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade, ships as non-hazardous resin pellets in 25 kg polyethylene bags, palletized and stretch-wrapped. Transport in clean, dry, covered trucks or containers at ambient temperature. Protect from moisture, contamination, punctures, and excessive heat; typically not regulated as dangerous goods.
    Storage Store in a cool, dry, well-ventilated warehouse, keeping Dow DOWLEX™ 2045.02AC in original unopened bags or packaging. Palletize off the floor, away from direct sunlight, moisture, heat, ignition sources, and strong oxidizers. Maintain ambient temperature, avoid excessive stacking, and follow first-in, first-out stock rotation.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in original packaging in a cool, dry, well-ventilated area.
    Application of Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade

    On three-layer blown film lines producing heavy-duty flexible intermediate bulk container liners, DOWLEX 2045.02AC with a melt mass-flow rate of 1.0 g/10 min at 190 °C/2.16 kg per ISO 1133-1 and a base density of 0.920 g/cm³ per ISO 1183-1 is processed at a melt temperature of 210–230 °C, a die gap of 2.0–2.5 mm, and a blow-up ratio of 2.0–2.5. In liner stock at 80–200 µm thickness, the octene-1 comonomer distribution reduces interlamellar tie-molecule scission at the fold lines generated during filling of woven polypropylene outer FIBCs. On lines with screw length-to-diameter ratios of 24:1 to 30:1 and no internal bubble cooling, increasing the blow-up ratio beyond 2.5 at melt temperatures below 205 °C produces frost-line height oscillation and transverse thickness bands measured by capacitance gauging at ±4 µm on a nominal 150 µm film. The defect is attributed to insufficient extensional viscosity under high stalk tension; it is corrected by adding 10–30 wt% of a LDPE homopolymer with a melt mass-flow rate of 0.25–2.0 g/10 min. The final polymer fraction for heavy-duty sack stock therefore comprises 70–90 wt% DOWLEX 2045.02AC and 10–30 wt% LDPE, with a non-amine hindered phenolic stabilizer masterbatch at 1–3 wt% where the liner contacts alkaline mineral fillers or cementitious powders.

    Mandatory compliance for dangerous goods liners follows UN Model Regulations Chapter 6.5 for 13H2, 13H3, and 13H4 flexible intermediate bulk container types; non-dangerous FIBC liners are assessed under ISO 21898, and food-contact variants require FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011. Mechanical acceptance is anchored to dart drop impact per ISO 7765-1 and ASTM D1709, Elmendorf tear propagation per ISO 6383-2, and tensile elongation at break per ISO 527-3. Terminal product types include UN-rated inner liners for woven polypropylene FIBCs, valve sacks for polymer resins, open-mouth sacks for carbon black and titanium dioxide, and lay-flat tubular liners for mineral wool insulation. DOWLEX 2045.02AC is not the sole barrier layer where the liner is exposed to aromatic solvents above 40 °C; a coextruded polyamide or EVOH layer is required.

    What Limits LLDPE Addition in High-Shrink Collation Film?

    Additions of DOWLEX 2045.02AC above 40 wt% in LDPE-based collation shrink formulations raise machine-direction shrink force to a level that distorts low-caliper tray corners during hot-air tunnel shrinkage. Typical collation film formulations for beverage multipacks contain 20–40 wt% DOWLEX 2045.02AC and 60–80 wt% of a LDPE shrink base with a melt mass-flow rate of 0.3–0.5 g/10 min. At 30 wt% LLDPE, the dart drop impact improves from a LDPE-only value of 150 g to a range of 260–340 g at 40 µm film thickness when tested per ISO 7765-1, but the free shrink at 120 °C in a hot-air bath may fall from 55% to 42% in machine direction under ASTM D2732 if the frost-line height is not raised. Film production uses high-stalk blown film lines with die diameters of 150–400 mm, die gaps of 1.0–1.5 mm, melt temperatures of 180–210 °C, and blow-up ratios of 3.5–4.5. Stalk height is held at 8–10 die diameters to delay crystallization, and frost-line height control is maintained within ±50 mm. When LLDPE content exceeds 35 wt%, line speed is reduced by 10–15% to avoid melt fracture at the die lip and to maintain bubble symmetry. Compliance for food-contact collation film falls under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, with overall migration limited to 10 mg/dm². Terminal product types include 6-can beverage collation packs, 12-packs of PET bottled water, canned food tray bundling, and pharmaceutical carton unitization. DOWLEX 2045.02AC is not suitable for high-clarity sleeve labels where light transmission above 90% and haze below 5% are required.

    Thermal Stabilizer Package Limits during Silage Film Conversion

    During conversion of agricultural silage blown film, DOWLEX 2045.02AC is formulated at 65–85 wt% with 15–35 wt% of a polyolefin elastomer or EVA for sealability and cling consistency; a HALS-based UV stabilizer masterbatch is added at 3–8 wt%, and polyisobutylene tackifier is present at 1–4 wt% only in the cling outer layer. The addition of PIB in the outer layer reduces dart drop impact after 14 days of warehouse aging at 35 °C because surface migration alters the coefficient of friction; slip/antiblock levels are rebalanced with a coefficient of friction target of 0.30–0.50 under ASTM D1894. Extrusion is performed on three-layer blown film lines with die gaps of 2.0–2.4 mm, melt temperatures of 200–225 °C, and blow-up ratios of 2.2–3.0, producing film at 25–80 µm. Lines without internal bubble cooling show output losses of 8–12% when the BUR is raised above 2.8. Regulatory references for silage stretch film include EN 13206 for bale wrap mechanical requirements, ISO 527-3 for tensile properties, ISO 6383-2 for tear strength, and ISO 4892-2 for accelerated weathering of greenhouse films. Published data for multi-year greenhouse exposure using this specific grade is limited; UV stabilizer loading should be validated under site-specific irradiation. Terminal products include round bale silage wrap, maize silage bags, greenhouse covering film, and silage pit covers. DOWLEX 2045.02AC should not be specified for greenhouse films requiring more than 24 months of continuous UV exposure unless the HALS package is raised beyond the formulation range above.

    Vertical form-fill-seal machines running IQF vegetable packaging utilize DOWLEX 2045.02AC in the inner sealing layer of three-layer blown film structures at 100% resin or with 5–10 wt% of a slip/antiblock masterbatch to prevent blocking on the film roll and to maintain seal jaw release at 115–135 °C. The blown film line is configured with a die gap of 1.8–2.2 mm, melt temperatures of 190–220 °C, and a blow-up ratio of 2.2–2.8; film thickness is held between 25 µm and 70 µm to maintain seal-response time below 1.5 s on rotary sealing jaws. Hot-tack strength is measured per ASTM F1921 as a function of seal temperature and delay; DOWLEX 2045.02AC maintains a seal initiation temperature below 105 °C because the octene-1 short-chain branches lower the onset temperature for interlayer chain diffusion. At thickness above 70 µm, seal bar dwell time must be increased or the heat-seal strength under ASTM F88 falls below 4 N/15 mm at 120 °C. For food-contact compliance, the layer is evaluated under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, with overall migration limited to 10 mg/dm². Terminal product types include IQF vegetable bags, frozen fruit pouches, frozen seafood pillow packs, and ice cream overwrap film. DOWLEX 2045.02AC does not provide sufficient oxygen barrier for long-term frozen meat storage; EVOH or polyamide must be included in the core layer.

    Laminating Sealant Web Melt Strength and Hot-Tack Thresholds

    For laminating sealant webs in sachet and stand-up pouch structures, DOWLEX 2045.02AC is employed as the blown film sealant layer at 85–100 wt%, with 0–15 wt% of a LDPE homopolymer added to lower seal initiation temperature when a higher melt-flow core layer is present. The sealant web is coextruded with tie layers and an EVOH or polyamide core at a die gap of 1.8–2.3 mm, melt temperatures of 195–225 °C, and a blow-up ratio of 2.0–2.5; film thickness is specified at 20–50 µm. The melt strength of DOWLEX 2045.02AC is sufficient to maintain bubble stability over an 8-hour production run, but adding more than 15 wt% LDPE lowers dart drop impact and reduces the interlayer adhesion at the tie interface after solventless lamination and 35–45 °C curing for 24–48 h. Seal strength is measured per ASTM F88, with a minimum requirement of 6 N/15 mm for medium-fast packaging lines; hot-tack initiation is measured per ASTM F1921. Regulatory compliance includes FDA 21 CFR 177.1520(c), Regulation (EU) No 10/2011, and REACH 1907/2006. Terminal product types include dry-food sachet laminates, pharmaceutical unit-dose overwrap, aluminium foil sachet sealant film, and stand-up pouch inner webs for granular powders. DOWLEX 2045.02AC is not recommended for retort pouches requiring sterilization above 121 °C, because the sealant layer softens and may fail under internal steam pressure.

    If Pallet Load Stabilization Requires Stretch Hood Puncture Resistance

    Pallet stretch-hood lines processing DOWLEX 2045.02AC at 70–90 wt% with 10–30 wt% VLDPE or butene-based plastomer benefit from the octene-1 LLDPE puncture resistance when films are stretched over sharp pallet corners. Stretch hood film is produced on three-layer blown film equipment with die gaps of 2.0–2.5 mm, melt temperatures of 195–225 °C, and blow-up ratios of 2.5–3.5, yielding a film thickness of 60–120 µm. The film is applied at 50–120% stretch on stretch-hood machines with corner folding devices; films must maintain a minimum puncture resistance of 200 N per ISO 7765-1 at 80 µm to avoid failure when the load is transported. Cling is measured as peel cling per ASTM D5458, and tensile properties are validated per ISO 527-3. Compliance for non-food industrial pallet loads falls under REACH 1907/2006; when the film contacts packaged food, the corresponding layer must comply with FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011. Terminal product types include pallet load stabilization for construction materials, household chemical multipacks, beverage pallet unitization, and large appliances. DOWLEX 2045.02AC should not be formulated with high levels of amine-based antistats because surface migration can reduce print adhesion and alter peel cling.

    Free Quote

    Competitive Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2045.02AC is a linear low density polyethylene blown film grade produced via solution polymerization with octene as the alpha-olefin comonomer. The resin has a density of 0.920 g/cm³ under ASTM D792 and a melt index of 1.0 g/10 min under ASTM D1238 at 190°C and 2.16 kg. The AC suffix identifies a pre-dispersed slip and antiblock additive package. Typical structures include monolayer and coextruded heavy-duty sacks, industrial liners, frozen food packaging, carrier bags, and agricultural wrap. The product differs from non-AC DOWLEX 2045.02 grades not in base resin density or melt index but in the presence of the additive system, eliminating separate masterbatch dosing at the extruder.

    What governs melt temperature and screw speed limits in blown film extrusion of DOWLEX 2045.02AC?

    The resin imposes a workable melt temperature range of 199°C to 232°C in conventional single-screw extruders with 24:1 length-to-diameter ratio. At melt temperatures below 190°C, incomplete plastication of the high-molecular-weight fraction causes gel streaks at the frost line. Above 240°C, the slip additive undergoes oxidative degradation, which increases odor and can lower film dart impact. Barrel temperature profiles are typically set from 160°C at the feed zone to 200°C at the metering zone, with die zones at 205–215°C.

    Bubble geometry is the primary control variable. A blow-up ratio of 2.2:1 to 2.8:1 and a frost line height of 8 to 12 die diameters balance machine-direction and transverse-direction orientation. Narrower die gaps below 1.8 mm increase shear rate and can trigger shark-skin melt fracture at lower output; a die gap of 2.0–2.5 mm is recommended for film thicknesses below 50 µm. In a 90 mm extruder with a 250 mm die, screw speed is typically maintained between 40 and 80 rpm, corresponding to outputs of 150–250 kg/h; higher output requires internal bubble cooling and a dual-lip air ring to suppress bubble respiration. Published data for the maximum stable output on a specific production line is limited because the threshold depends on die diameter, air ring geometry, and ambient conditions.

    The resin’s melt viscosity is more shear-thinning than high-pressure LDPE; at die shear rates of 100–1000 s⁻¹, it flows with lower pressure drop at equivalent output. However, this shear-thinning behavior reduces melt tension, and excessive drawdown or high frost line can cause bubble sag and gauge variation. A vented or grooved-feed extruder is not required, but screen packs of 40/80/40 mesh are used to remove incidental contaminants and build backpressure. A barrier screw with a Maddock mixing section is preferred for consistent melt homogeneity.

    Typical physical properties of DOWLEX 2045.02AC measured on 25 µm blown film produced at 2.5:1 blow-up ratio
    PropertyTest methodTypical valueUnit
    DensityASTM D7920.920g/cm³
    Melt indexASTM D12381.0g/10 min
    Tensile strength at break MDASTM D88245MPa
    Tensile strength at break TDASTM D88236MPa
    Elongation at break MDASTM D882500%
    Elongation at break TDASTM D882700%
    Dart drop impact F50ASTM D1709A150g
    Elmendorf tear MDASTM D1922150g
    Elmendorf tear TDASTM D1922380g
    HazeASTM D100313%
    Gloss at 60°ASTM D245770-
    Seal initiation temperatureASTM F88100°C

    Comparative performance against butene-based LLDPE and high-pressure LDPE in heavy-gauge film

    At equivalent density and melt index, DOWLEX 2045.02AC provides higher dart impact and Elmendorf tear than butene-copolymer LLDPE because octene short-chain branches create an increased tie-molecule population during quench cooling. In 25 µm film, the resin exhibits a dart drop impact of approximately 150 g under ASTM D1709A and transverse-direction Elmendorf tear of 380 g under ASTM D1922. Butene-based LLDPE of the same 0.920 g/cm³ density and 1.0 g/10 min melt index typically has lower puncture and tear values; exact differences depend on film fabrication conditions and additive packages. Compared with high-pressure LDPE, the resin has lower melt extension hardening and lower melt strength, which narrows the stable operating window at high blow-up ratios but improves tensile strength and puncture resistance at equivalent thickness.

    The addition of 10–30 wt% high-pressure LDPE is a standard converter practice to improve bubble stability and dart impact in thick films. The LDPE phase adds melt strength and allows higher frost lines without bubble flapping. Blends are processed at the same melt temperatures, but die pressure increases with LDPE content due to the higher viscosity of LDPE at typical die shear rates. The seal initiation temperature of the blend shifts upward by approximately 2–5°C relative to pure LLDPE; the exact shift depends on LDPE density and molecular weight distribution.

    Low-temperature impact performance is also differentiated by comonomer type. Octene-based DOWLEX 2045.02AC retains dart impact below -20°C, whereas some butene-based grades show a sharp loss in impact below -10°C. This characteristic supports selection of the product for frozen food packaging and ice bags. Puncture resistance measured with a 0.75 mm radius probe at 250 mm/min is typically 60–80 N on 50 µm film, depending on orientation and additive content. Comparative testing should be conducted under ASTM D5748 for puncture and ASTM D1709 for dart impact because film age and additive bloom influence results.

    Seal initiation temperature of DOWLEX 2045.02AC is approximately 100°C under ASTM F88 on 25 µm film. Hot tack strength develops above 110°C, supporting vertical form-fill-seal equipment with seal bar temperatures of 110–140°C and dwell times of 0.3–0.8 s. However, after extended storage above 40°C, migration of the slip additive to the seal surface can reduce seal strength; converters should qualify seal performance after aging at 50°C for 7 days before approving final packaging.

    The pre-dispersed slip and antiblock additive package produces a kinetic coefficient of friction of 0.10–0.20 under ASTM D1894. The antiblock component, typically synthetic silica with a median particle size of 2–4 µm, creates surface micro-roughness that reduces blocking under roll stacking. Film-to-film blocking force is generally below 10 g/cm when measured under ASTM D3354, enabling unwind speeds above 200 m/min on horizontal form-fill-seal machines. For converters that have historically used non-AC DOWLEX 2045.02 grades, the AC product eliminates the need for separate dosing of 2–5 wt% silica or erucamide masterbatch and reduces additive dispersion variance across production lots.

    When slip migration retards corona treatment on lamination films

    Surface treatment of films containing slip and antiblock packages must account for additive bloom. Erucamide-type slip additives migrate to the film surface over 24–72 h, reducing surface energy. If the film is corona-treated before bloom is complete, subsequent slip migration lowers the surface energy from an initial value above 40 mN/m to below 38 mN/m as measured by ASTM D2578. Laminators using solventless adhesives should specify a minimum surface energy of 38 mN/m and re-treat film if storage exceeds 30 days at 23°C.

    During corona treatment, the generated ozone and reactive species oxidize the polyethylene surface. The presence of slip additive can suppress oxidation because the additive competes for reactive sites. Higher corona power density of 10–15 W·min/m² may be required relative to untreated LLDPE. In-line treatment immediately before coating or lamination is preferred over off-line treatment for this grade. When treatment is performed off-line, the time-to-use should be limited because the additive bloom will continue to lower surface energy.

    Regulatory compliance matrix for DOWLEX 2045.02AC
    Standard or regulationReferenceCondition or end-use limitation
    U.S. FDA21 CFR 177.1520Food-contact olefin polymer, subject to finished article compliance and intended use conditions
    EU plastics regulationRegulation (EU) No 10/2011Overall migration limit 10 mg/dm²; specific migration limits for additives must be verified
    REACHRegulation (EC) No 1907/2006Substances of very high concern not intentionally added above 0.1% w/w
    RoHSDirective 2011/65/EUPackaging excluded from electrical and electronic equipment scope; no restricted substances intentionally added

    For agricultural silage wrap and frozen food packaging, the product is processed with a frost line height that maximizes transverse orientation. In a 3-layer coextrusion line, the skin layers often contain DOWLEX 2045.02AC for sealability and puncture resistance, while the core layer contains LDPE for bubble stability. The product should not be combined with high levels of amine-based antifog or antistatic additives unless compatibility with the slip and antiblock package has been verified; such combinations can lead to plate-out on die lips and reduced film clarity. Pre-drying is generally not required, but if sacks or gaylords have been stored above 70% relative humidity, surface moisture should be removed by drying at 60°C for 2 h to avoid steam bubbles in the melt. Extruder purge after processing HDPE with this grade requires a transition of at least 5 barrel volumes of LLDPE to remove high-melting-point residues and prevent gels.