Dow Dowlex 2045 02 Linear Low Density Polyethylene Heavy Duty Film Grade

Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade

    • Product Name: Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 984338
    Density 0.920 g/cm³
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Melt Flow Ratio I21 I2 30
    Melting Point 123 °C
    Vicat Softening Point 100 °C
    Brittleness Temperature < -70 °C
    Tensile Strength At Yield Md 10.3 MPa
    Tensile Strength At Yield Td 10.7 MPa
    Tensile Strength At Break Md 38.6 MPa
    Tensile Strength At Break Td 31.0 MPa
    Elongation At Break Md 700%
    Elongation At Break Td 800%
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Dart Drop Impact 200 g
    Puncture Resistance 10 J
    Haze 12%
    Gloss 45 60%
    Coefficient Of Friction 0.2

    As an accredited Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaging for Dow DOWLEX™ 2045.02: 25 kg bags, palletized; also available in 1,000 kg bulk bags.
    Container Loading (20′ FCL) Container Loading (20′ FCL) for Dow DOWLEX™ 2045.02 LLDPE Heavy Duty Film Grade: palletized 25 kg bags, stretch-wrapped, secured for ocean transport.
    Shipping DOWLEX™ 2045.02 LLDPE, Heavy Duty Film Grade, is shipped as non-hazardous solid resin pellets in 25 kg bags, bulk bags, or bulk trucks/railcars. Not classified as dangerous goods. Transport in dry, clean conditions away from heat, sunlight, and ignition sources. Follow standard industrial handling and storage practices.
    Storage Store Dow DOWLEX™ 2045.02 LLDPE in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers or bags tightly closed, on pallets, protected from moisture, dust, and physical damage. Use first-in, first-out rotation. Do not store near foodstuffs or incompatible materials. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is typically 24 months in original unopened packaging, stored cool, dry, well-ventilated, away from direct sunlight, heat, moisture, and contaminants.
    Application of Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade

    Three-layer FIBC liner film for mineral and aggregate packaging

    DOWLEX™ 2045.02 is processed on a three-layer coextrusion blown-film line for flexible intermediate bulk container liners used with powdered limestone, silica sand, and quartz grit. At incoming resin inspection, melt mass-flow rate is verified against ISO 1133-1:2022 at 190°C and 2.16 kg with a nominal value of 1.0 g/10 min; density is verified at 23°C under ASTM D792 Method B with a nominal value of 0.920 g/cm³. The core layer is compounded from 80 wt% DOWLEX 2045.02 and 20 wt% LDPE 2420H to increase melt strength without sacrificing dart impact; the two outer skins each contain 60 wt% DOWLEX 2045.02, 30 wt% LDPE 2420H, and 10 wt% of a synthetic silica antiblock masterbatch in an LDPE carrier. Total film thickness is controlled at 200 µm ± 5% using an on-line capacitance gauge calibrated to ASTM D6988-13. The primary extruder is a 75 mm single-screw unit with L/D 30:1, a barrier screw, and a 350 mm spiral-mandrel die with a 2.2 mm die gap. Blow-up ratio is set at 2.4:1, frost-line height is held between 600 mm and 800 mm, and melt temperature at the adapter is maintained from 215°C to 225°C. Production operators have observed that reducing the die gap to 1.8 mm while increasing output above 200 kg/h produces visible sharkskin on the outer skin; keeping die pressure below 420 bar and melt temperature above 210°C restores a defect-free surface. Compliance for dangerous goods liners is assessed under 49 CFR 178.503 for sift resistance and ISO 21898:2004 for FIBC liner integrity. Heavy metal recovery limits under EU 94/62/EC Article 11 apply. The resin is not supplied with a broad food-contact declaration; conversion for food-contact would require migration testing under EU 10/2011 at the intended film thickness and contact area. The terminal liner film is a 200 µm tubular or wicketed bag with a minimum dart impact acceptance threshold of 1,100 g under ASTM D1709 Method B and a machine-direction Elmendorf tear of not less than 180 g under ASTM D1922.

    When silage cover film is exposed to ultraviolet radiation for 12 months

    When a silage cover film is exposed to ultraviolet radiation for 12 months, the formulation must address both the external weathering load and the oxidative environment of a silage pit. A monolayer trench silo cover is produced at 150 µm thickness from 70 wt% DOWLEX 2045.02, 25 wt% LDPE 2420H, and 5 wt% of a UV masterbatch containing 20% hindered amine light stabilizer and 10% rutile titanium dioxide. Extrusion takes place on a 90 mm single-screw extruder with L/D 33:1, a 450 mm die diameter, a 2.0 mm die gap, blow-up ratio 2.0:1, and melt temperature from 205°C to 215°C. The frost-line height is set at 1.0 m to preserve transverse-direction tear balance. Oxygen permeability of the 150 µm film is evaluated under ASTM D3985 at 23°C and 0% RH; values for silage covers in this thickness class typically remain below 650 cm³/(m²·day·atm), which supports anaerobic fermentation conditions. Compliance for agricultural plastics is verified under EN 13206:2017 for thermoplastic films used in agriculture and horticulture, with accelerated weathering per Annex C. Processing must avoid prolonged melt temperatures above 230°C because the hindered amine stabilizer begins to volatilize and the film surface loses long-term UV retention. The film should also be isolated from chlorinated disinfectants in storage; contact with sodium hypochlorite solution above 1% active chlorine causes surface oxidation and localized embrittlement within weeks. The terminal product is a 150 µm black-and-white silage bunker cover with a machine-direction tensile strength of not less than 22 MPa under ASTM D882 and a transverse-direction elongation at break above 600%.

    In industrial waste collection, a 0.920 g/cm³ octene-copolymer film with a 1.0 g/10 min melt index is formed on a high-stalk bubble configuration to balance machine-direction and transverse-direction tear. The blend ratio is 88 wt% DOWLEX 2045.02, 10 wt% butene LLDPE of 1.0 g/10 min melt index for tear retention, and 2 wt% carbon black masterbatch for opacity and outdoor storage. Extrusion is run on a 65 mm single-screw extruder with L/D 28:1, a 300 mm die with a 1.8 mm die gap, blow-up ratio 3.0:1, and melt temperature 215°C. A polymer processing aid is added at 400 ppm to delay sharkskin, particularly when the die gap is below 2.0 mm or when the carbon black masterbatch contains coarse filler aggregates. Film thickness for converted heavy-duty refuse sacks is 140 µm at the side weld and 120 µm in the body, a downgauging range that still satisfies a 50 kg filled mass requirement under EN 13592:2017. The high-stalk configuration is maintained with a frost-line height of 900 mm; if frost-line height drops below 600 mm, transverse-direction tear falls and the sack side seams become susceptible to burst failures when wet waste loads shift. The terminal refuse sack has a perforated top fold, a measured loaded volume of 120 L, and a minimum tear resistance of 100 N in both machine and transverse directions under the EN test method.

    What governs the maximum post-industrial recyclate fraction in construction vapor barrier film?

    The maximum post-industrial recyclate fraction in construction vapor barrier film is determined by gel count, dart impact retention, and water-vapor transmission uniformity rather than melt viscosity alone. In a three-layer A/B/A structure, the core layer is loaded with up to 25 wt% post-industrial LLDPE film recycle of density 0.921 g/cm³ and melt index 0.8 g/10 min; the two skin layers remain 100% virgin DOWLEX 2045.02 to preserve surface quality and sealability. Total film thickness is 250 µm, and water-vapor permeance is tested under ASTM E96 Procedure B at 23°C and 50% RH. On a production-scale 75 mm extruder with L/D 30:1, the melt filtration system is fitted with a 100 mesh slide plate; when the core recyclate fraction exceeds 25 wt%, filter change frequency increases from every 8 h to every 3 h because oxidation-induced gels from the recycled film accumulate rapidly. The construction barrier application requires the film to satisfy ASTM E1745-17 for plastic water-vapor retarders used in contact with granular fill under concrete slabs. The critical operational boundary is that post-industrial recyclate content above 25 wt% reduces dart impact in the 250 µm structure by more than 25%, which can move the product from Class A puncture resistance to Class B or C under ASTM E1745-17. Published data for this specific configuration is limited; the numerical ranges shown here are production validation targets rather than a formal Dow datasheet. The terminal product is a 250 µm underslab vapor retarder with a permeance below 0.1 perm under ASTM E96 Procedure B and a machine-direction tensile strength not less than 20 MPa under ASTM D882.

    StandardTest method or clauseConstruction barrier requirement
    ASTM E1745-17Class A/B/C plastic water-vapor retarderPuncture and tensile after wet/dry aging
    ASTM E96 Procedure BWater method at 23°C and 50% RHPermeance ≤0.1 perm
    ASTM D882Tensile properties of thin filmMD/TD tensile strength ≥20 MPa
    ASTM D1709 Method BDrop impactMinimum 900 g for 250 µm film

    Because steel coil wrapping demands both puncture resistance and controlled volatile corrosion inhibitor release, the film structure is converted as a two-layer coextrudate with a VCI-loaded inner skin. The inner skin is compounded from 70 wt% DOWLEX 2045.02, 20 wt% LDPE 2420H, and 10 wt% VCI masterbatch; the outer skin is 80 wt% DOWLEX 2045.02 and 20 wt% LDPE 2420H. Total film thickness is 120 µm. Blown-film processing uses a 55 mm extruder with L/D 30:1, a 250 mm die, a 1.6 mm die gap, blow-up ratio 2.2:1, and melt temperature 210°C. VCI efficacy is assessed using JIS Z 1535 vapor-inhibiting ability tests for metal corrosion protective films. The terminal product is a 120 µm steel coil wrap in roll widths up to 2.4 m, with puncture resistance measured by ASTM D5748-19 and a minimum puncture force of 80 N at the wrapped edge. The film is sealed with polyester tape at the coil perimeter; it is not specified for coil packs stored above 40°C because the volatile inhibitor migrates too quickly through the outer polyolefin skin at elevated temperatures and can create contact staining on zinc-coated steel surfaces.

    Form-fill-seal packaging of sharp-edged granular chemicals

    Form-fill-seal packaging of sharp-edged granular chemicals uses a 180 µm film in which hot-tack and puncture resistance are balanced against seal-jaw heat transfer. The blend is 80 wt% DOWLEX 2045.02, 15 wt% LDPE 2420H, and 5 wt% lubricant concentrate to reduce the coefficient of friction to 0.25 under ASTM D1894. Vertical form-fill-seal equipment is configured with a sealing jaw temperature of 145°C to 160°C, a dwell time of 0.4 s, and a jaw pressure of 0.4 MPa. The packaging line runs at 35 cycles/min; if the seal jaw temperature falls below 140°C, the seal peel strength drops below the specified 12 N/15 mm and the filled bag can open when dropped from 1.2 m under ISO 7965-1:1984. Puncture resistance is measured under ASTM D5748-19, and the production specification requires a minimum puncture force of 80 N for the 180 µm film at 23°C. The film is not recommended for direct contact with fatty foods or liquid products above 40°C because oil absorption into the polyolefin matrix lowers seal strength and can extract low-molecular-weight slip agents. The terminal product is a 25 kg valve or open-mouth sack for potassium sulfate granules or crushed recycled glass, with a drop-test pass rate of 99% under ISO 7965-1:1984.

    Free Quote

    Competitive Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade is a solution-polymerized ethylene-octene resin supplied in pellet form for blown-film extrusion of heavy-duty sacks, industrial liners, and construction films. The grade is defined by a nominal melt index of 1.0 g/10 min measured at 190°C under a 2.16 kg load in accordance with ASTM D1238 and a nominal density of 0.920 g/cm³ determined by ASTM D792. The octene comonomer generates longer short-chain branches than the butene comonomer used in conventional C4-LLDPE, increasing the fraction of tie molecules connecting lamellae after crystallization. The consequence is a property profile in which dart impact and Elmendorf tear at equal gauge are shifted upward relative to butene-copolymer films of similar density and melt index, while optical clarity is reduced. Because the resin is produced by a solution process rather than a high-pressure tubular process, it contains negligible long-chain branching; shear-thinning is therefore less pronounced than in LDPE of equivalent melt index, and extruder head pressure can be higher on the same die. The product is intended for monolayer and coextruded structures at thicknesses from 50 µm to 250 µm.

    What processing limits govern high-output blown-film extrusion of 2045.02?

    On conventional blown-film lines equipped with a 50 mm to 75 mm screw and an L/D ratio of 24:1 to 30:1, barrel set points are typically profiled from 160°C at the feed throat to 200–220°C at the die. Melt temperatures above 240°C are not recommended because oxidative degradation can produce gels and reduce tear resistance as measured by ASTM D1922. The low melt index of 1.0 g/10 min elevates torque and die pressure; dies with gaps below 1.5 mm may initiate sharkskin at output rates above 25 kg/h per 100 mm of die circumference unless a fluoropolymer processing aid is incorporated. A die gap between 1.5 mm and 2.5 mm and a blow-up ratio of 2.0:1 to 2.8:1 are commonly reported as stable operating conditions for heavy-gauge film. Bubble cooling should be adjusted so frost-line height remains within 200–450 mm for a 250 mm die at 50 µm gauge; higher frost-line positions reduce dart impact due to orientation losses, while lower frost-line positions can increase haze.

    Under the same die and screw configuration, 2045.02 exhibits less die swell than high-pressure LDPE because the absence of long-chain branching limits melt elasticity. This has two practical effects: the die gap can be reduced less aggressively than with LDPE, and bubble neck-height instabilities are more sensitive to draft fluctuations. Processors converting from LDPE often observe that the extruder amp load increases by approximately 10–15% at constant output because the solution LLDPE has a higher melt viscosity at typical die shear rates. Published data for this specific configuration is limited; start-up should therefore include a low-screw-speed purge with a lower-viscosity LDPE before introducing 2045.02.

    Tear, dart impact, and secant modulus benchmarks at 50 µm and 100 µm

    Property Test method Unit Representative value at 50 µm
    Density ASTM D792 g/cm³ 0.920
    Melt index ASTM D1238 g/10 min 1.0
    Peak melting temperature ISO 11357-3 °C 121–124
    Tensile stress at break, machine direction ISO 527-3 MPa 38–42
    Elongation at break, machine direction ISO 527-3 % 700–800
    Dart impact, Method A ASTM D1709 g 180–220
    Elmendorf tear, machine direction/transverse direction ASTM D1922 g 350/400
    Secant modulus at 1% strain, machine direction ISO 527-3 MPa 190–210

    Values listed are representative of blown film produced at 50 µm gauge, 2.5:1 blow-up ratio, 0.8 mm die gap, and 220°C melt temperature; they are not release limits. A shift to 100 µm gauge typically raises dart impact and absolute Elmendorf tear values because the crack path lengthens, but puncture energy per unit thickness may remain stable or decline depending on frost-line cooling and air-ring quench rate. Converters should verify gauge-specific values using ASTM D1709 and ASTM D1922 on their own line, because morphology differences caused by quench rate affect oriented tie-molecule populations independently of resin density.

    When butene-copolymer LLDPE is replaced by 2045.02 at equal melt index

    Replacement of a C4-LLDPE having a melt index of 1.0 g/10 min and a density of 0.920 g/cm³ with 2045.02 is not a drop-in substitution because the octene comonomer alters both rheology and crystalline morphology. In film, the octene-copolymer architecture has been reported to increase dart impact at equivalent gauge by 10–25% and machine-direction Elmendorf tear by 15–30% when compared with butene-copolymer LLDPE of the same density and melt index; however, such differences depend on blow-up ratio, frost-line height, and screw design, and published comparative data for this specific grade pair is limited. The C8 branches in 2045.02 reduce the primary lamella thickness, which lowers the brittle-ductile transition temperature and improves low-temperature toughness. The trade-off is a measurable reduction in optical transmittance; haze values may increase by 2–5 percentage points relative to a C4-LLDPE at 50 µm under ASTM D1003. Processors must also compensate for lower melt strength than high-pressure LDPE: bubble support, air-ring design, and collapsing-frame geometry require adjustment when downgauging from 80 µm LDPE to 50 µm 2045.02.

    In heavy-duty sack and construction film applications, the resin is used where puncture, tear propagation, and dart impact failures dominate. Equipment experience on high-output lines operating at 100–180 kg/h has shown that gauge control improves when the die gap is kept above 1.8 mm and internal bubble cooling is used. Without internal bubble cooling, bubble oscillation at a frost-line height above 400 mm can produce gauge bands that reduce Elmendorf tear uniformity by more than 10%. No predrying is required for unopened material stored at relative humidity below 60%; condensation or extended storage in humid environments may require drying at 60°C for 4 h to prevent surface defects.

    The resin’s rheology places a measurable load on extruder drives and die pressure

    At the nominal melt index of 1.0 g/10 min, 2045.02 produces a higher pressure drop across a 250 mm spiral die than an equivalent LDPE of 1.0 g/10 min melt index. This is a consequence of the linear chain architecture; without long-chain branching, the shear-thinning index is lower, so apparent viscosity at 100–1000 s⁻¹ die-lip shear rates remains higher. Extruders with 24:1 L/D single-flight barrier screws may operate 10–15% below the throughput achieved with LDPE before the melt temperature exceeds 240°C. A two-stage vented screw or a barrier screw with enhanced mixing sections is preferred for consistent melt quality. Because the resin has a narrow molecular weight distribution relative to LDPE, purging after processing 2045.02 should use a lower-viscosity polyolefin purge resin or a sequenced LDPE purge at 180–200°C to avoid retained high-viscosity domains.

    Regulatory status must be confirmed on the finished film, not inferred from the base resin alone. As an olefin polymer, the base resin is within the scope of 21 CFR 177.1520, but compliance of the final article depends on additives, thickness, end-use temperature, and migration testing under 21 CFR 176.170. For European Union food-contact applications, the finished film is subject to the overall migration limit of 10 mg/dm² under EU Regulation 10/2011; specific migration of any additive or conversion aid must be verified by the converter. No blanket approval for direct food contact is stated or implied by the base resin data alone.

    In construction vapor retarder applications, film produced from 2045.02 is evaluated according to ASTM E96 water vapor transmission, but the base resin does not determine the permeance independently of gauge and lamination; a 100 µm monolayer film has a permeance dependent on density and crystallinity rather than melt index. Published data for this specific configuration is limited. For heavy-duty sack lines using a 65 mm extruder and 200 mm die, a start-up condition of 1.8 mm die gap, 2.5:1 blow-up ratio, and 220°C melt temperature is a conservative reference point; the line must be tuned to avoid melt fracture and maintain dart impact above the end-user requirement specified in the sack specification.