Dow Dowlex 2042a Linear Low Density Polyethylene Food Grade

Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade

    • Product Name: Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 437942
    Productname Dow DOWLEX 2042A Linear Low Density Polyethylene, Food Grade
    Manufacturer Dow
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer 1-Octene
    Density 0.920 g/cm3
    Meltindex 1.0 g/10 min at 190°C/2.16 kg
    Meltingpoint 122 °C
    Vicatsofteningpoint 95 °C
    Tensilestrengthatyield 10 MPa
    Tensilestrengthatbreak 30 MPa
    Elongationatbreak 800%
    Flexuralmodulus 240 MPa
    Shorehardness 50 Shore D
    Thermalconductivity 0.33 W/m·K
    Waterabsorption <0.01%
    Foodcontactcompliance FDA 21 CFR 177.1520 compliant
    Casnumber 9002-88-4
    Molecularformula (C2H4)n

    As an accredited Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene bags, palletized, for food-grade linear low density polyethylene resin handling.
    Container Loading (20′ FCL) 20' FCL: 18 MT (720 x 25 kg bags) floor loaded, without pallets, for Dow DOWLEX 2042A Food Grade.
    Shipping Shipping: Dow DOWLEX™ 2042A is supplied as free-flowing pellets in 25 kg multiwall bags or bulk packaging (boxes, octabins, bulk trucks/railcars). Non-hazardous; store/transport dry, away from heat, moisture, and odor contaminants to preserve food-grade quality. Follow local regulations and keep containers closed. Use clean, dedicated equipment when required.
    Storage Store Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade, in a cool, dry, well-ventilated, covered area away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep original packaging sealed to prevent moisture, dust, and contamination. For food-grade use, maintain hygienic handling, avoid odorous or toxic materials, and follow first-in, first-out stock rotation.
    Shelf Life Shelf life is 24 months from date of manufacture when stored unopened in a cool, dry, well-ventilated area away from sunlight.
    Application of Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade

    On mono-layer blown film lines producing 45–70 µm frozen vegetable packaging, DOWLEX™ 2042A is processed in the 190–215 °C melt temperature window because higher temperatures reduce bubble stability while lower temperatures raise backpressure above 350 bar on 24:1 L/D grooved-feed extruders. The formulation typically uses 85–100 wt% DOWLEX™ 2042A and 0–15 wt% high-pressure LDPE with a melt index of 1.8–2.5 g/10 min; slip/antiblock masterbatch is limited to 2–4 wt% to keep haze below 10% while maintaining a kinetic coefficient of friction below 0.25 when tested under ASTM D1894-14. Compliance is evaluated under FDA 21 CFR 177.1520(c) for food-contact olefin polymers and EU Regulation (EU) No 10/2011, with overall migration testing at 10 mg/dm² for aqueous and fatty food simulants as applicable. Extrusion through a 70 mm grooved-feed extruder with 30:1 L/D, die gap 1.5–2.2 mm, blow-up ratio 2.2:1–2.8:1, and frost line height 4–8 die diameters yields film slit into IQF pouches, frozen meat overwrap, and pre-portioned bakery bags.

    Palletizing Throughput Above 120 Pallets/h Pushes Cast Film Draw Resonance Boundaries

    Cast pallet stretch film operations running DOWLEX™ 2042A on 5-layer lines with 75–90 mm screw diameters and 30:1 L/D barrels are constrained less by melt temperature than by draw resonance onset and cling-force drift. At a die exit melt temperature of 240–255 °C, die gap 0.5–0.7 mm, and chill roll temperature 18–25 °C, a blend of 90–96 wt% DOWLEX™ 2042A, 1–3 wt% polyisobutylene tackifier cleared under FDA 21 CFR 177.1420, and 1–2 wt% slip/antiblock masterbatch is drawn to thicknesses of 12–20 µm. Draw resonance typically emerges when draw ratio exceeds 35:1, neck-in exceeds 90 mm total, and edge trim rises above 10%; lowering melt temperature below 230 °C worsens neck-in, while raising temperature above 260 °C accelerates tackifier volatilization and increases odour. Chill roll setpoints below 15 °C can cause condensation and gauge bands at speeds above 500 m/min. The finished machine stretch film is used for secondary packaging of food pallets, hand stretch film, and top-sheet film.

    Why Does Extrusion Coating Neck-In Depend on High-Temperature Melt Elasticity Rather Than Melt Index Alone?

    In liquid packaging board coating, DOWLEX™ 2042A is processed at the upper end of polyolefin extrusion temperatures to manage neck-in and adhesion, but oxidation and gel formation become limiting. Coating weights of 18–30 g/m² onto paperboard run with a melt temperature of 285–310 °C at the die exit, die gap 0.5–0.8 mm, air gap 120–200 mm, and cooling roll temperature 12–20 °C. The formulation blends 70–85 wt% DOWLEX™ 2042A with 15–30 wt% high-pressure LDPE of melt index 7–8 g/10 min because the LDPE raises melt elasticity and reduces neck-in below 40 mm per side; using DOWLEX™ 2042A at 100% on high-speed lines can produce neck-in above 60 mm per side and edge-bead instability. Compliance is governed by FDA 21 CFR 176.170(c) for paper and paperboard in contact with food and EU Regulation (EU) No 10/2011 for overall migration below 10 mg/dm². Adhesion to board requires corona or atmospheric plasma treatment above 42 dyn/cm, and the coated board is converted into gable-top cartons, aseptic brick sleeves, and paper cups.

    Vertical form-fill-seal packaging of snack foods and confectionery on 40–60 µm mono-layer film converts DOWLEX™ 2042A under heat-seal jaw temperatures of 125–140 °C and dwell times of 0.25–0.35 s; slip packages are adjusted to maintain a kinetic coefficient of friction below 0.30 when tested under ASTM D1894-14, because higher COF at speeds above 120 pouches/min causes film tracking drift. The product is formulated at 90–100 wt% DOWLEX™ 2042A with 0–10 wt% high-pressure LDPE to widen the hot-tack window, and the compound is stabilised to comply with FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011. Extrusion uses a 50–65 mm grooved-feed extruder with 28:1 L/D, die gap 1.8–2.2 mm, blow-up ratio 2.0:1–2.5:1, and melt temperature 195–210 °C; the finished film is slit for flow-wrap cookie packaging, pillow bags for extruded snacks, and pretzel sleeves.

    Sealant Web Requirements in Coextruded Stand-Up Pouches Under Vacuum or Modified Atmosphere

    Where DOWLEX™ 2042A serves as the sealant layer in five-layer coextruded stand-up pouches, the layer is commonly specified at 20–30% of total coextruded thickness, equivalent to 25–45 µm in a 125–150 µm structure. The sealant formulation uses 90–100 wt% DOWLEX™ 2042A with 0–10 wt% metallocene LLDPE to reduce seal initiation temperature; slip and antiblock masterbatch addition is limited to 1–2 wt% because migration of erucamide above 500 ppm can increase seal initiation temperature by 2–4 °C and reduce oxygen barrier performance in adjacent EVOH layers. Processing on a 5-layer blown film line with 25:1 L/D extruders and die temperature 210–230 °C maintains stable sealing properties; heat sealing is performed at 110–125 °C with 3–5 bar jaw pressure for 0.3–0.5 s and verified by ASTM F88/F88M-21 seal strength and ASTM F1921-18 hot tack. Compliance is established under FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011; terminal packages include vacuum pouches for frozen seafood, modified atmosphere dried fruit pouches, and pasteurisable side-gusset formats.

    Dry powder packaging of flour, starch, and milled fractions on converted tubular film lines uses DOWLEX™ 2042A in film thicknesses of 70–120 µm to resist splitting during 25 kg drop tests performed under ISO 7965-1. The blend is 80 wt% DOWLEX™ 2042A with 20 wt% high-pressure LDPE, and compliance is assessed under FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011 for dry food contact. Extrusion through a 60 mm grooved-feed extruder with 24:1 L/D, die gap 2.0 mm, blow-up ratio 2.0:1–2.5:1, and melt temperature 200–220 °C yields sealed sacks for 25 kg flour, starch, and bakery mix packaging.

    Free Quote

    Competitive Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade is a pelletized ethylene–octene copolymer produced by a solution polymerization process. The manufacturer lists density as 0.920 g/cm³ when determined according to ASTM D792 and melt index as 1.0 g/10 min when measured at 190 °C under a 2.16 kg load according to ASTM D1238. The grade belongs to the DOWLEX family of octene-based linear low-density polyethylene resins and is supplied for direct food-contact applications. The “Food Grade” designation refers to controlled formulation practices that support compliance with FDA 21 CFR 177.1520 for olefin polymers and, where the producer’s compliance statement applies, EU Regulation 10/2011. The product is not a high-pressure low-density polyethylene homopolymer; its linear backbone with controlled short-chain branching gives a different balance of melt strength, toughness, and seal response.

    What melt-phase and solid-state specifications govern extrusion and end-use performance?

    Because resin density and melt index are typical values rather than sales specification limits, purchasing decisions should be based on the manufacturer’s lot-specific specification. The table below reports representative physical properties from publicly available data sheets and should not be interpreted as a certificate of analysis.

    Representative physical properties for DOWLEX 2042A
    PropertyTest methodRepresentative value
    DensityASTM D7920.920 g/cm³
    Melt indexASTM D1238 at 190 °C/2.16 kg1.0 g/10 min
    Peak melting temperatureASTM D3418122 °C
    Vicat softening pointASTM D1525101 °C
    Tensile stress at yieldASTM D63811.0 MPa
    Tensile elongation at breakASTM D638900 %
    Flexural modulusASTM D790260 MPa

    The practical consequences of these values are a low crystalline fraction and a melting point sufficiently below standard extrusion temperatures to permit rapid melting in single-screw machines. The melt index of 1.0 g/10 min places the grade in a range that balances draw-down in cast film and melt-pressure stability. The Vicat softening point near 101 °C defines an upper temperature boundary for incidental food-contact surfaces under mechanical load; continuous service above this value may lead to deformation before the crystalline melting point is reached.

    In cast film and food-packaging lamination lines, DOWLEX 2042A is typically processed in single-screw extruders with barrier feed screws having length-to-diameter ratios from 24:1 to 30:1. Typical barrel profiles begin at 180 °C near the feed throat and increase to 240–260 °C in the metering section, with adapter and die zones held at 240–280 °C; chilled-roll temperatures between 15 °C and 25 °C are used to set film crystallinity and prevent roll blocking. The resin does not require predrying because the polyethylene backbone is not hygroscopic; however, condensed surface moisture on pellets exposed to relative humidity above 60 % can produce splay and surface defects. In such conditions, hopper drying at 60 °C for 2 h removes surface water without degrading the additive package.

    Melt temperature measured at the adapter should remain below 290 °C to limit oxidative chain scission and gel-particle formation. Production interruptions of more than 30 min require purging with a melt-index-matched low-density polyethylene or a commercial purging compound to reduce die-lip residue. On cast film lines, edge trim can be reintroduced at 10–20 wt% provided the trim is dust-free and has not been exposed to uncontrolled contamination; regrind addition beyond 30 wt% may increase gel counts and reduce optical consistency. Published data for a specific production configuration are limited; therefore, the optimum profile should be derived from screw manufacturer calculations and confirmed by melt-temperature measurement at the die.

    DOWLEX 2042A differs from butene LLDPE and high-pressure LDPE in comonomer architecture, melt strength, and film toughness

    DOWLEX 2042A is produced with octene-1 as the principal comonomer; butene-based LLDPE grades incorporate a shorter comonomer. The longer hexyl side branches generated from octene increase the concentration of tie chains between lamellae at equivalent density. The practical result is a measurable increase in Elmendorf tear strength, dart impact, and puncture resistance relative to butene-based LLDPE of the same melt index and density. These differences affect edge-tear resistance in formed food pouches and puncture resistance in lidding film over irregular tray rims.

    Compared with high-pressure LDPE, the linear backbone of DOWLEX 2042A has negligible long-chain branching. This reduces melt strength and can increase neck-in during cast film or extrusion coating; high-pressure LDPE remains the preferred choice where high melt strength, low neck-in, and high draw at elevated melt temperature are dominant processing requirements. DOWLEX 2042A compensates with greater solid-state tensile strength and higher elongation at break, which is relevant when downgauging a food-packaging film without sacrificing seal-area toughness.

    DOWLEX 2042A should not be treated as a metallocene-catalyzed plastomer. Its composition distribution is broader than that of a solution metallocene grade, which affects optical clarity and heat-seal initiation temperature. For structures requiring lower haze and lower seal initiation temperature, a metallocene or plastomer grade may be more appropriate. DOWLEX 2042A is used where a balance of stiffness, toughness, and conventional LLDPE processability is required in a food-contact resin.

    A compliance matrix for food-contact use is given below. The grade’s food-contact status is supported by the resin manufacturer’s documentation, not solely by the product name.

    Food-contact and chemical management references relevant to DOWLEX 2042A
    Regulatory referenceScope relevant to food contact
    FDA 21 CFR 177.1520Olefin polymers in articles intended for food contact, subject to conditions of use and migration limits in paragraph (c)
    EU Regulation 10/2011Plastic materials and articles intended to come into contact with food; overall migration and specific migration limits apply
    REACH (EC) No 1907/2006Registration, evaluation, authorization, and restriction of chemical substances; monomer and additive registration obligations

    Under FDA 21 CFR 177.1520, the resin may be used in contact with food types and under conditions defined in the regulation; not all food types and temperature conditions are automatically covered. Similarly, EU Regulation 10/2011 requires manufacturers of the final food-contact article to verify overall migration and specific migration limits for the finished multilayer structure, because lamination adhesives, printing inks, and tie layers can alter migration behavior. DOWLEX 2042A does not confer compliance to the final package by itself. The resin is not intended for retort sterilization above 100 °C or for long-term contact with aggressive oxidizing agents. Dry, aqueous, and fatty food applications can be supported under the regulatory conditions of use, but fatty food contact at elevated temperatures should be evaluated under EU Regulation 10/2011 migration testing because lipid-soluble low-molecular-weight fractions may migrate at measurable levels.

    In coextrusion structures, DOWLEX 2042A is placed as a sealant or skin layer; it should not be combined with unapproved recycled content in the food-contact layer unless a functional barrier is demonstrated. The resin is processable with ethylene-vinyl acetate and polyolefin plastomers, but migration characteristics of the complete structure must be confirmed by the converter. No statement in this technical note is a regulatory certification. The manufacturer’s food-contact statement and lot-specific certificate of analysis define the exact conditions of use for a specific shipment.

    Top