Dow Dowlex 2038 Linear Low Density Polyethylene

Dow DOWLEX™ 2038 Linear Low Density Polyethylene

    • Product Name: Dow DOWLEX™ 2038 Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 345892
    Density 0.935 g/cm³
    Melt Index 1.0 g/10 min (190°C/2.16 kg)
    Melting Point 124 °C
    Vicat Softening Point 109 °C
    Tensile Strength At Yield 14 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 800%
    Flexural Modulus 500 MPa
    Hardness Shore D 50
    Dart Drop Impact 200 g
    Haze 10%
    Gloss 80%

    As an accredited Dow DOWLEX™ 2038 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DOWLEX™ 2038 Linear Low Density Polyethylene is supplied in 25 kg polyethylene bags, palletized for transport and storage.
    Container Loading (20′ FCL) Standard 20′ FCL: Dow DOWLEX™ 2038 LLDPE in 25 kg bags, palletized and shrink-wrapped, securely loaded for ocean freight transport.
    Shipping Dow DOWLEX™ 2038 Linear Low Density Polyethylene is typically shipped as non-hazardous solid resin pellets in bags, octabins, boxes, or bulk trucks/railcars. It is not regulated for transport under DOT, IATA, or IMDG. Keep containers closed, dry, and away from excessive heat. Follow good industrial hygiene practices.
    Storage Store DOWLEX™ 2038 in a cool, dry, well-ventilated warehouse. Keep in original sealed packaging, palletized and off the floor. Protect from direct sunlight, UV radiation, heat, moisture, dust, and contamination. Avoid ignition sources, strong oxidizers, and excessive stacking. Maintain ambient temperatures, keep containers closed when not in use, and practice first-in, first-out stock rotation.
    Shelf Life Typically 24 months from manufacture when stored unopened in cool, dry, well-ventilated conditions, away from direct sunlight and heat.
    Application of Dow DOWLEX™ 2038 Linear Low Density Polyethylene

    On mono- and three-layer blown-film lines using grooved-feed extruders with L/D ≥ 30:1, DOWLEX 2038 is introduced at 20–40 wt% in LDPE/LLDPE heavy-duty sack formulations to raise dart impact under ASTM D1709-16a Method A and machine-direction Elmendorf tear under ASTM D1922-15. Film producers set barrel profile from feed to adapter at 180/200/215/225/230°C and keep the die zone below 238°C to limit gel oxidation; screw speeds are adjusted to produce melt temperature of 215–225°C at the die lip. Die gap ranges from 1.6–2.5 mm with blow-up ratio of 2.5:1–3.2:1 and frost-line height 700–900 mm. Because DOWLEX 2038 at 1.0 g/10 min (ASTM D1238, 190°C/2.16 kg) and nominal density 0.935 g/cm³ (ASTM D1505) has moderate melt strength, bubble stability improves when internal bubble cooling air temperature is maintained at 8–14°C. On FFS lines, side seal jaws are set at 135–155°C with dwell 0.5–1.0 s for 80–100 µm sacks, because heat seal initiation shifts upward by 4–8°C relative to a 0.920 g/cm³ LLDPE. Terminal products include woven-backed resin pellet sacks, fertilizer shipment sacks, and industrial powder sacks. Food-contact status follows FDA 21 CFR 177.1520(c)3.1a and EU Regulation 10/2011 with overall migration into 10% ethanol and 3% acetic acid simulants evaluated according to EN 1186-1.

    What Drawdown Limits Govern Extrusion Coating with 0.935 g/cm³ LLDPE?

    Air gap, chill roll temperature, and die lip opening dictate coating weight uniformity when DOWLEX 2038 is coextruded as a sealant layer on paperboard and aluminium foil laminates. Melt temperature at the die is maintained at 260–290°C to prevent draw resonance; higher melt temperature reduces extensional viscosity but increases odour and taint in the coated substrate. Air gap from die exit to nip is set at 150–250 mm, producing neck-in of 45–80 mm per edge at line speeds above 120 m/min. Die lip opening of 0.4–0.6 mm, chill roll temperature of 15–20°C, and nip pressure of 3–5 bar yield coating weights of 15–25 g/m². Bond strength to corona-treated paperboard exceeds 2 N/15 mm when substrate surface tension reaches 42–46 dyn/cm as measured by ASTM D2578. Above 150 m/min, edge tear and draw resonance appear unless 5–15 wt% LDPE is blended to lower shear viscosity and extend the drawdown window. For aqueous and fatty food contact, compliance is assessed under EU 10/2011 Annex II and FDA 21 CFR 177.1520(c)3.1a; overall migration in 10% ethanol, 3% acetic acid, and 95% ethanol simulants must not exceed 10 mg/dm².

    Geomembrane sheet extrusion and panel welding for canal liners and single-ply containment use DOWLEX 2038 at thicknesses of 1.0–2.5 mm, processed on flat-die extruders with melt temperature 220–240°C and cooling-roll temperatures of 70–90°C to balance crystallinity and sheet flatness. Hot-wedge welding at 400–450°C wedge temperature and 1.2–2.0 m/min travel speed generates lap shear strength above 80% of parent sheet when wedge gap is 0.8–1.0 mm and peel separation at the weld root is below 10 mm. Stress crack resistance is specified by ASTM D1693-21 Condition B in 10% Igepal CO-630 at 50°C; published break times for this specific configuration are limited, so factory acceptance tests typically require 500 h without failure as a batch-release gate. The higher density of 0.935 g/cm³ increases modulus over a 0.920 g/cm³ geomembrane LLDPE, but welding operators must limit moisture uptake below 2.0% at wedge entry to avoid steam porosity. Contact with ester-based PVC plasticizers or aromatic hydrocarbon backfill should be excluded because plasticizer migration reduces weld peel strength.

    When DOWLEX 2038 Replaces LDPE in Industrial Container Moulding

    At shot weights of 0.8–1.5 kg and melt temperature 210–230°C, DOWLEX 2038 fills multi-cavity industrial crate and tote moulds at injection pressure 70–100 MPa, holding pressure 50–60 MPa for 4–8 s, and back pressure 5–10 MPa. Mould cooling water at 20–30°C produces post-mould shrinkage of 1.4–2.0% measured by ASTM D955-21; ribs and bosses above 4.0 mm extend cycle time by 8–12 s unless gas-assisted injection is used. The density of 0.935 g/cm³ raises top-load strength and flexural modulus relative to a 0.918 g/cm³ LLDPE, but low-temperature impact under ISO 6603-2 at -20°C decreases when wall sections fall below 1.8 mm. Colouring at 2–4 wt% masterbatch requires a distributive screw with Maddock mixing section; no pre-drying is needed when storage relative humidity is below 60%, but surface splay appears above 70% RH and hopper drying at 70°C for 2 h is then required.

    Five-layer coextruded silage cover films integrate DOWLEX 2038 as an outer abuse layer at 15–25 wt% to increase puncture resistance under ASTM D5748-19 and tear propagation under ASTM D1938-19, while metallocene LLDPE core layers retain sealability. Blown-film equipment with dual-lip air ring and internal bubble cooling processes the structure at die gap 1.8–2.3 mm, BUR 2.0:1–2.8:1, and die temperature 218–228°C. UV stabilizer masterbatch dosing at 8–12 wt% is required for outdoor storage; unstabilised film exhibits embrittlement under ASTM G154 Cycle 1 within 300–600 h, though published data for this specific DOWLEX 2038 configuration is limited. Film thickness of 120–200 µm and sealed bag dimensions up to 2.5 m × 50 m are typical; edge fold damage during farm deployment is minimized by maintaining dart impact above 800 g at 23°C.

    Cast Web Stiffening and Edge Trim Reprocessing Limits

    Cast film lines producing industrial lamination webs run DOWLEX 2038 at melt temperature 230–250°C with chill roll temperature 18–24°C and air-knife position 5–10 mm from the die exit to suppress film edge neck-in. Film thickness of 30–70 µm exhibits tensile elongation at break above 500% in machine direction when measured by ISO 527-3 at 500 mm/min. Edge trim regrind is re-introduced at 10–20 wt% into the main feed; beyond 20 wt%, gel flecks and melt-pressure fluctuation above 5 bar appear on 75/150 mesh screen packs, requiring reduced screw speed. For food packaging laminations, cast web is tested for extractives under FDA 21 CFR 177.1520(c)3.1a and EU 10/2011; surface tension after corona treatment is maintained at 40–44 dyn/cm for subsequent adhesive lamination.

    ApplicationStandard or CodeClause / Test DesignationCondition
    Heavy-duty sacksFDA 21 CFR 177.1520(c)3.1aFood contact, all food types
    Extrusion coatingEU 10/2011Annex IIAqueous, acidic, fatty simulants
    GeomembraneASTM D1693-21Condition B10% Igepal, 50°C
    Injection mouldingISO 6603-2Puncture impact-20°C
    Agricultural filmASTM G154Cycle 1UV exposure
    Cast lamination webISO 527-3500 mm/minMD tensile elongation
    Free Quote

    Competitive Dow DOWLEX™ 2038 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2038 Linear Low Density Polyethylene is a solution-polymerized ethylene-octene-1 copolymer with a reported density of 0.935 g/cm³ per ASTM D792 and a melt index of 1.0 g/10 min per ASTM D1238 at 190 °C/2.16 kg. The octene-1 comonomer introduces hexyl side branches along the polyethylene backbone, giving a linear low-density architecture that differs from high-pressure LDPE by the near absence of long-chain branching and from butene-LLDPE by longer side-chain length. The grade is specified for cast film and selected blown film applications where stiffness, puncture resistance, and tear propagation resistance must be combined without excessive loss of sealability.

    How Does Octene-1 Comonomer Distribution Affect Dart Impact and Tear Resistance?

    In DOWLEX™ 2038, octene-1 creates hexyl side branches that disrupt crystallinity and increase tie-chain formation between lamellae. At equal density and melt index, an ethylene-octene copolymer typically exhibits higher dart drop impact per ASTM D1709 and higher Elmendorf tear per ASTM D1922 than an ethylene-butene copolymer because longer side branches are more effective at promoting inter-lamellar entanglements. Published comparative data for this specific grade are limited; therefore, film converters should verify relative tear and impact response at the target gauge and frost line height rather than extrapolating from resin density and melt index alone. The comonomer distribution also influences seal initiation temperature; differential scanning calorimetry following ASTM D3418 is used to determine the melting peak, but its correlation with seal performance depends on seal bar geometry, dwell time, and sealing pressure.

    On a cast film line with a 24:1 to 30:1 L/D single-screw extruder, a typical melt temperature window for a medium-viscosity LLDPE of 1.0 g/10 min melt index is 220–260 °C; exact setpoints depend on screw design, output rate, and die width. A general-purpose polyolefin barrier screw with a compression ratio of 2.8:1 to 3.5:1 is commonly used. The resin should be purged with a non-olefin purge compound or a lower-viscosity polyethylene when transitioning from polar materials to avoid contamination. Moisture uptake is not normally a concern for polyethylene under dry indoor storage, but resin stored at relative humidity above 60% may benefit from drying at 60–80 °C for 2–4 h using a desiccant dryer with a dew point below -20 °C to reduce surface splay.

    Oscillatory shear testing per ASTM D4440 of DOWLEX™ 2038, when available from the supplier, can be used to generate a master curve for flow simulation. In the absence of grade-specific data, capillary measurements per ISO 11443 or ASTM D3835 are recommended because melt index alone does not capture the shear-thinning slope needed to predict pressure drop in a flat die. A medium-viscosity linear polyethylene of this type typically shows apparent viscosity in the range of 102–104 Pa·s between processing and low-shear conditions at 190 °C, but the exact values are temperature- and molecular-weight-distribution dependent and must be confirmed by in-house measurement. Operators should record barrel pressure at constant output to detect gradual melt filter blockage, degradation, or regrind accumulation.

    Gauge Control and Chill Roll Conditions That Determine Film Blocking

    Because DOWLEX™ 2038 has a density of 0.935 g/cm³, its film surface is less tacky than lower-density ethylene-olefin copolymers, but thin gauges below 20 µm can still exhibit blocking under high winding tension or elevated warehouse temperatures. Cast film processing of this density typically uses a chill roll temperature between 15–30 °C and an air knife or vacuum box to hold the web against the roll. For cast film gauges between 10 and 50 µm, die gap is typically 0.5–1.0 mm; neck-in and draw resonance are controlled by molecular weight distribution and melt temperature. Film gauge uniformity is monitored by a beta gauge; variation should be held within ±5% to avoid hard bands. The resin's higher stiffness relative to DOWLEX™ 2045 (0.920 g/cm³, 1.0 g/10 min) permits down-gauging in rigid packaging if puncture resistance is not the limiting factor. Blocking force can be tested using ASTM D3354 and should be measured after 24 h conditioning at 50 °C when warehouse stacking is expected.

    Blown film bubble stability boundaries shift when the frost line is raised above the crystalline onset point.

    In blown film, DOWLEX™ 2038 requires a higher frost line than lower-density grades because the density of 0.935 g/cm³ accelerates solidification and increases modulus during bubble formation. If the frost line is set too low, the bubble may exhibit frost-line instability and variable thickness bands. A frost line height of 8–12 die diameters is typical for medium-viscosity LLDPE, but this range depends on output, ambient air temperature, and air ring configuration. Bubble stability can be tested by monitoring layflat width variation with an ultrasonic or optical gauge; a variation above ±3% often indicates insufficient cooling or excessive melt temperature. The higher density of this resin reduces bubble stretch at low blow-up ratios, so blow-up ratios below 1.8:1 are generally not recommended unless the line is specifically designed for high-stalk operation.

    For converting operations, incoming lots should be qualified by density and melt index, but film performance cannot be predicted from those two values alone. Puncture resistance is measured by ASTM D5748, dart drop impact by ASTM D1709, Elmendorf tear by ASTM D1922, tensile properties by ASTM D882, and haze and gloss by ASTM D1003 and ASTM D2457. The higher density of 0.935 g/cm³ tends to increase modulus and reduce gas permeability relative to lower-density octene grades, but the effect on tear is gauge-dependent and cannot be expressed as a single multiplier.

    DOWLEX™ 2038 is commonly dry-blended with a slip masterbatch at 1–3 wt%, an antiblock masterbatch at 1–5 wt%, and a processing aid masterbatch at 0.5–1.0 wt% depending on film gauge and line speed. These addition levels are starting points, not formulation guarantees; the active content of each masterbatch and the carrier resin melt index change final viscosity and coefficient of friction. Coefficient of friction is tested per ASTM D1894; blocking force per ASTM D3354.

    When Regrind Addition Alters Gel Levels and Optical Clarity

    Edge trim and start-up scrap from DOWLEX™ 2038 cast film can be recycled in-line at addition rates up to 20–30 wt% without systematic loss of dart impact, provided the regrind is free of degraded gel particles and the ratio of regrind to virgin resin is held constant through gravimetric blending. Gel analysis by film surface scanning or visual inspection against a lighted screen is recommended at every shift because higher regrind fractions increase the residence time distribution and can generate oxidized gels when the extruder temperature exceeds 260 °C for extended periods. If gel counts exceed the converter's internal specification, regrind addition should be reduced to 10–15 wt% or the screw speed lowered to reduce shear heating. No universal gel threshold exists across applications; acceptable levels must be tied to the end-use optical and sealing requirements.

    Thermal degradation of DOWLEX™ 2038 during extrusion follows a free-radical mechanism; prolonged residence above 260 °C can lead to chain scission, crosslinking, and gel formation. Oxidation is monitored by Fourier transform infrared spectroscopy (ASTM D5576) through absorbance in the carbonyl region between 1710–1740 cm-1. Extruders with a residence time distribution longer than 5–7 min at high melt temperature should be purged with a more thermally stable polyolefin before shutdown to avoid carbonaceous deposits on screw and die surfaces.

    Heat seal performance of DOWLEX™ 2038 films is governed by the melting range of the octene copolymer. Differential scanning calorimetry (ASTM D3418) commonly shows a primary melting endotherm in the range of 124–128 °C, making the resin suitable for form-fill-seal operations where seal bar temperatures are set above 135 °C. However, actual seal initiation temperature depends on seal dwell time, pressure, and jaw configuration. A hot-tack test per ASTM F1921 and seal strength test per ASTM F88 should be performed on the finished film, because resin density alone cannot predict seal-through-contamination performance. In comparison to a 0.920 g/cm³ octene-LLDPE such as DOWLEX™ 2045, DOWLEX™ 2038 typically requires higher seal initiation temperatures but supports higher stiffness and dead-fold in the same gauge.

    In form-fill-seal applications where caustic or dust contamination is present, the seal initiation window can narrow to 10–15 °C, requiring jaw temperature control within ±5 °C to avoid leakers or weak seals. Sealing through contamination should be evaluated with contaminated coupon tests rather than clean-film hot-tack data. A jaw dwell time of 0.2–0.5 s and jaw pressure of 0.2–0.6 MPa are typical starting points for LLDPE films, but the optimum values depend on film gauge and package geometry.

    Puncture Resistance, Slow Rate Penetration, and Load Retention in Agricultural Film

    DOWLEX™ 2038 is used in agricultural and heavy-duty industrial films where tear, puncture, and creep under load are simultaneously required. Slow rate puncture can be assessed by ASTM D5748 or a probe penetration method at 250 mm/min; film made from higher-density octene-LLDPE generally shows higher probe penetration energy than LDPE at equal gauge but lower elongation before break than lower-density LLDPE. In silage covers and greenhouse films, the resin is often blended with 5–20 wt% metallocene LLDPE or LDPE to adjust tear balance and sealability. The exact blending ratio must be optimized by measuring Elmendorf tear (ASTM D1922) and secant modulus (ASTM D882) at the specified film thickness and after UV exposure, since outdoor service introduces oxidative degradation not captured by as-extruded data.

    Relative to a butene-LLDPE of identical density and melt index, DOWLEX™ 2038 is expected to show higher dart impact and Elmendorf tear because the hexyl branch length of octene-1 is more effective at creating tie molecules than the ethyl branch length of butene-1. This difference is not linear; at very high orientation, the advantage can narrow or disappear. Relative to high-pressure LDPE at 0.935 g/cm³ and 1.0 g/10 min, DOWLEX™ 2038 has lower melt tension and lower shear sensitivity, which improves drawdown but reduces bubble stability in blown film. Relative to metallocene octene-LLDPE, DOWLEX™ 2038 typically has a broader molecular weight distribution, which can produce higher extrusion backpressure and lower optical clarity but better purge transition and less melt fracture sensitivity. The selection of DOWLEX™ 2038 over a butene-LLDPE at the same 0.935 g/cm³ density is driven primarily by tear and impact requirements, whereas the selection over a metallocene octene-LLDPE is driven by equipment compatibility and cost-to-performance in less optically demanding applications.

    Regulatory compliance for DOWLEX™ 2038 must be confirmed against the current manufacturer safety data sheet and food-contact certificate. Typical linear low-density polyethylene grades of this density are evaluated for food-contact use under FDA 21 CFR 177.1520 for olefin polymers and under EU Regulation No 10/2011 when properly formulated. The resin may also be assessed against REACH Article 33 and RoHS Directive 2011/65/EU for heavy metals; however, specific compliance status is grade- and batch-dependent and should not be assumed from chemical class alone. For medical packaging, converters should request ISO 10993 extractable data from the supplier rather than relying on olefin polymer generalizations.

    Comparative resin design data
    GradeComonomerDensity per ASTM D792Melt index per ASTM D1238Typical process
    DOWLEX™ 2038Octene-10.935 g/cm³1.0 g/10 minCast film, heavy-duty packaging
    DOWLEX™ 2045Octene-10.920 g/cm³1.0 g/10 minStretch and blown film
    Generic butene-LLDPEButene-10.935 g/cm³1.0 g/10 minGeneral-purpose film

    The resin is not intended for continuous exposure to strong oxidizing agents, aromatic or chlorinated hydrocarbons, or ultraviolet light without adequate stabilizer modification. Standard polyethylene stabilizer packages used in the grade inhibit thermo-oxidative degradation during extrusion and normal service; however, outdoor applications require additional UV stabilizer masterbatches. Continuous service temperature is generally below 80 °C for unstabilized or minimally stabilized film, and mechanical properties decline when stored at temperatures above 50 °C for extended periods due to physical aging and, in some cases, additive migration.

    Compliance evaluation matrix
    StandardScopeTypical applicability to DOWLEX™ 2038
    FDA 21 CFR 177.1520Olefin polymers for food contactConditional; verify supplier certification
    EU Regulation No 10/2011Plastic materials intended for food contactConditional; migration limits apply
    REACH Article 33Substances of very high concern reportingSupplier SDS required
    RoHS Directive 2011/65/EUHeavy metals and brominated flame retardantsNot a flame-retardant formulation
    ISO 10993-5In vitro cytotoxicity for medical packagingNot automatically implied
    Top