| HS Code | 955180 |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Octene-1 |
| Density | 0.938 g/cm3 |
| Meltindex | 0.85 g/10 min (190°C/2.16 kg) |
| Meltingpoint | 124 °C |
| Vicatsofteningpoint | 108 °C |
| Tensilestrengthatyield | 11 MPa |
| Tensilestrengthatbreak | 31 MPa |
| Elongationatbreak | 700% |
| Flexuralmodulus | 300 MPa |
| Hardnessshored | 50 |
| Dartdropimpact | 120 g |
As an accredited Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene is supplied in 25 kg polyethylene bags, 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with 25 kg bags of DOWLEX™ 2038.68G LLDPE, palletized, stretch-wrapped, approximately 13.75 MT net. |
| Shipping | Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene ships as non-hazardous polymer resin pellets. It is not DOT/IMDG/IATA regulated, requiring no UN number, hazard class, or placards. Typically transported in 25-kg bags, octabins, or bulk trucks/railcars. Keep dry, cool, and clean; avoid excessive heat and contamination. |
| Storage | Store Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep original packaging tightly closed and pallets off the floor to prevent moisture pickup and contamination. Avoid prolonged high temperatures, UV light, and strong oxidizing agents. Maintain FIFO rotation and good housekeeping. Follow the SDS and local regulations. |
| Shelf Life | Typically no fixed shelf life; stable LLDPE resin if stored sealed, dry, cool, and protected from UV, moisture, and contaminants. |
DOWLEX™ 2038.68G is an ethylene/octene linear low-density polyethylene with a nominal density of 0.935 g/cm³ (ASTM D792) and a melt index of 1.0 g/10 min (ASTM D1238, 190 °C/2.16 kg). In heavy-duty shipping sack extrusion, the resin is processed on upward blown film lines; equipment configurations commonly use grooved-feed extruders with L/D 24:1–30:1, barrier screws with Maddock mixing elements, and die gaps from 2.0 mm to 2.5 mm. The blow-up ratio is maintained between 2.2:1 and 2.8:1, with frost line height 2.5–4.0 die diameters and melt temperature 200–230 °C. The formulation window for a three-layer ABA structure is 70–100 wt% DOWLEX 2038.68G in the core layer, 0–30 wt% high-pressure LDPE with melt index 0.25–0.75 g/10 min for bubble stability, and 1–3 wt% slip/antiblock masterbatch only when blocking is detected during slitting.
The critical process failure modes are bubble flutter at BUR above 2.8:1 when the frost line is below 2.5 die diameters and seal-bar overpenetration when the outer skin contains more than 30 wt% LDPE, which reduces dart impact measured by ASTM D1709 and Elmendorf tear measured by ASTM D1922. Compliance for non-food industrial sacks is evaluated under the Packaging and Packaging Waste Directive 94/62/EC, with total heavy-metal content not exceeding 100 mg/kg, and under REACH Article 33 with an SVHC threshold of 0.1 wt%. Food-contact dry-bulk sacks require olefin polymer clearance under FDA 21 CFR 177.1520(c) and, for the EU, end-use migration testing under EU Regulation 10/2011 including overall migration limit 10 mg/dm². Terminal finished product types include 25 kg and 50 kg chemical granule sacks, resin export bags, mineral-filler bags, and mill-roll liners.
| Downstream sector | Primary compliance or test standard | Acceptance criterion or property |
|---|---|---|
| Heavy-duty shipping sacks | 94/62/EC; REACH Article 33 | Sum of Pb, Cd, Hg, Cr(VI) < 100 mg/kg; SVHC < 0.1 wt% |
| Extrusion lamination sealant web | EU Regulation 10/2011; FDA 21 CFR 177.1520(c) | Overall migration limit 10 mg/dm²; end-use conditions apply |
| Agricultural silage cover film | EN 13206; REACH | Weathering and tensile retention classification |
| Stretch-hood film | ISO 527-3; ASTM D5459 | Tensile curve and holding-force recovery |
| FFS chemical powder packaging | 94/62/EC; EU Regulation 10/2011 | Heavy metals < 100 mg/kg; migration testing by contents |
| Heavy-duty refuse sacks | EN 13592 | Puncture and tear classification |
In extrusion lamination of woven polypropylene and kraft paper substrates, DOWLEX 2038.68G is used as a sealant web because the 0.935 g/cm³ density reduces penetration of granular materials through pinholed coatings. The flat-die extrusion coating process is run at melt temperature 280–310 °C, air gap 120–200 mm, and coating weight 15–30 g/m²; neck-in is controlled by adding 10–20 wt% LDPE to the sealant layer or by coextruding a low-density skin. The chill roll is maintained between 15 °C and 25 °C; deviations outside this band create inconsistent coating gloss and seal-strength variation. DOWLEX 2038.68G is specified at 80–100 wt% of the sealant layer. Food-contact laminates require migration testing of the finished composite under EU Regulation 10/2011 with overall migration limit 10 mg/dm², and for U.S. applications, the olefin polymer component must meet FDA 21 CFR 177.1520(c). Terminal finished product types include woven PP fertilizer sacks, paper-plastic valve bags, pet-food multilayer pouches, and mineral-filler bag liners.
Agricultural silage cover film from DOWLEX 2038.68G is run as monolayer or three-layer blown film at thickness 100–200 µm, blow-up ratio 2.5:1–3.2:1, and melt temperature 200–230 °C. The octene short-chain branching distribution shifts the Elmendorf tear after weathering, but the bubble stability window narrows when BUR exceeds 3.2:1 at melt temperatures below 200 °C; this is the central process conflict on high-output lines. Formulation is typically 88–96 wt% DOWLEX 2038.68G, 4–8 wt% carbon-black masterbatch or TiO₂ white masterbatch for opacity, and 1–3 wt% UV/HALS masterbatch. Combined masterbatch above 12 wt% reduces tear and increases gel-count variation.
Compliance is assessed under EN 13206 for covering films used in agriculture and horticulture, with additional EU REACH SVHC threshold 0.1 wt%. No food-contact migration claim applies unless the specific ensiled feed contact is tested under EU Regulation 10/2011. Terminal finished product types include silage clamp covers, silage bags, round-bale silage wrap, and greenhouse ground covers.
For stretch-hood film formulations with a density of 0.935 g/cm³, DOWLEX 2038.68G is blended with metallocene LLDPE to balance elongation at break and holding force. The addition ratio for DOWLEX 2038.68G in stretch-hood film is commonly 40–70 wt%, with 30–60 wt% metallocene ethylene/octene LLDPE with density 0.915–0.925 g/cm³; slip and anti-block masterbatches are omitted from the core layer. The process requires three-extruder cast film lines with die gap 0.6–1.0 mm, chill roll temperature 15–25 °C, and line speeds above 150 m/min. At DOWLEX 2038.68G content above 70 wt%, machine-direction Elmendorf tear measured by ASTM D1922 typically declines, and cold-climate puncture energy measured by ISO 7765-2 requires monitoring. Mechanical compliance is evaluated by ISO 527-3 and ASTM D5459; the film is not a food-contact article unless tested under EU Regulation 10/2011. Terminal finished product types include pallet stretch hoods for construction materials, appliance stretch hoods, beverage multipack covers, and export pallet protection.
In vertical form-fill-seal packaging for cementitious powders, grouts, and detergents, DOWLEX 2038.68G provides higher seal strength measured by ASTM F88 than a 0.918 g/cm³ LLDPE at filling temperatures above 60 °C. The FFS process operates at 20–40 bags/min, with seal-bar temperature 150–180 °C and dwell 0.4–1.0 s; film gauge is 80–150 µm. Formulation is 85–100 wt% DOWLEX 2038.68G, 0–15 wt% LDPE or mLLDPE to lower seal initiation, and 1–2 wt% silica or calcium carbonate anti-block masterbatch when high-friction formers are used. Compliance includes heavy-metal limits under 94/62/EC, REACH SVHC threshold 0.1 wt%, and for detergent or food-powder contact, migration testing under EU Regulation 10/2011 according to fill temperature and fat content. Terminal finished products include 20–30 kg cementitious adhesive bags, grout pouches, detergent refill bags, and powdered resin export sacks.
Heavy-duty refuse sacks made from DOWLEX 2038.68G are produced at 70–100 wt% resin with 0–30 wt% post-consumer recycled LDPE and 1–2 wt% processing aid or anti-block masterbatch; the standard monolayer blown film process uses melt temperature 190–220 °C, BUR 2.0:1–2.5:1, and thickness 50–120 µm. Compliance is evaluated under EN 13592 for plastic refuse sacks, including tensile and puncture classification; terminal finished products include building rubble sacks, industrial waste liners, and heavy-duty household refuse sacks.
Competitive Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene is a solution-polymerized ethylene/1-octene copolymer with nominal density 0.935 g/cm³ (ASTM D792; ISO 1183-1:2019) and melt index 1.0 g/10 min (ASTM D1238; ISO 1133-1:2022 at 190 °C/2.16 kg). The product is composed of a linear backbone with short-chain branches introduced by the octene comonomer; this structure distinguishes it from high-pressure low-density polyethylene and from butene-based linear low-density polyethylene grades. The resin is used in heavy-duty film conversion where stiffness, impact toughness, and tear propagation resistance are specified. Target applications include industrial liners, agricultural greenhouse and silage films, heavy-duty shipping sacks, and carrier layers in coextruded barrier structures.
The values cited in this document are representative physical property data used for process setup and are not intended as release specifications. Density and melt index measurements are performed on conditioned samples at 23 ± 2 °C and 50 ± 5% relative humidity in accordance with the conditioning clauses of ASTM D618 and ISO 291. The grade is supplied as free-flowing pellets; storage should be in closed hoppers or containers at temperatures below 50 °C to prevent pellet blocking. For food-contact and health-related compliance, the final converted article must be evaluated separately because additives, colorants, and processing aids may alter the regulatory profile of the base polymer.
| Property | Test method | Representative value |
|---|---|---|
| Melt index (190 °C/2.16 kg) | ASTM D1238; ISO 1133-1:2022 | 1.0 g/10 min |
| Density | ASTM D792; ISO 1183-1:2019 | 0.935 g/cm³ |
| DSC peak melting temperature | ISO 11357-3 | 124 °C |
| Vicat softening point | ASTM D1525; ISO 306 | 122 °C |
The melt index of 1.0 g/10 min establishes a moderate-viscosity processing window. It is lower than general-purpose film grades in the 2.0–6.0 g/10 min range, so head pressure and motor load are higher, but the resin retains sufficient drawdown for cast film and for blown film in the 20–150 µm thickness interval. The density of 0.935 g/cm³ is higher than typical film LLDPE and produces a measurable increase in secant modulus and a reduction in gas transmission coefficient when compared with 0.920 g/cm³ octene grades at the same gauge. The DSC peak at 124 °C is not a direct indication of seal initiation temperature; seal initiation on film surfaces is influenced by thermal diffusion, pressure, and dwell time and should be determined on the finished film using a heat-seal tester according to ASTM F2029 or equivalent.
Processing behavior on single-screw extruders has been characterized on 45 mm to 90 mm grooved-barrel machines with 24:1 to 30:1 L/D. Barrier-flighted screws with Maddock-type mixing sections are preferred because the melting behavior of linear low-density polyethylene creates a solid-bed disruption risk in conventional three-zone screws. A die gap of 0.8–1.5 mm is common for blown film; narrower gaps raise die shear stress and may initiate sharkskin melt fracture at lower specific output. Blow-up ratios between 2.0:1 and 3.5:1 orient the film for balanced machine-direction and transverse-direction tear. Frost line height is maintained at 4–8 die diameters. Adapter melt temperatures are set between 190 °C and 230 °C for blown film; melt temperatures above 250 °C should be avoided because residence-time-dependent oxidation can produce gel defects and screen-pack plugging.
For cast film, melt temperatures of 240–290 °C and die gaps of 0.5–0.8 mm lower the viscosity at high shear and improve drawdown onto the chill roll. Chill roll temperatures of 15–30 °C are used with an air knife or vacuum box for edge pinning. The resin has lower melt strength than high-pressure LDPE at comparable melt index; therefore, draw resonance and neck-in become limiting when downgauging below 20 µm. Maintaining a short die-to-chill-roll distance and increasing chill roll speed relative to melt output are standard countermeasures. At thicknesses below 15 µm, process stability is highly sensitive to die lip cleanliness, melt temperature uniformity, and polymer lot-to-lot variation; published film data for this specific configuration is limited.
Pre-drying is not generally required for polyolefin film extrusion. If pellet surface condensation occurs during storage or conveying at relative humidity above 60%, drying at 60–80 °C for 2–4 h in a desiccant-bed or hot-air drier removes surface moisture before extrusion. Fluoropolymer processing-aid masterbatches are used at 200–800 ppm to suppress die lip build-up and delay the onset of sharkskin. Concentrations above 1000 ppm may create plate-out on downstream rolls and should not be used without line-specific confirmation. The resin is incompatible with polyvinyl chloride in melt processing; accidental PVC contamination releases hydrogen chloride and corrodes tooling. Purge with a higher-melt-index LDPE or HDPE after shutdowns to remove stagnated resin from the die lip, spiral channels, and screen pack.
Melt-pressure variations at the die are a more sensitive indicator of process instability than melt temperature alone. On a 75 mm barrier-screw extruder, pressure fluctuations greater than 0.5–1.0 MPa at constant screw speed suggest inconsistent solids conveying or screw wear. Melt filtration with screen packs of 40–80 mesh is typical for film lines; finer screens increase backpressure and are not recommended unless melt temperature is reduced to compensate. For cast film, die lip adjustment should be performed in 10–20 µm increments to control transverse gauge variation; automatic or manual die bolts require thermal expansion allowance before final gauge readings are recorded.
Internal bubble cooling and automatic air rings have two distinct control functions: internal bubble cooling controls frost line height by adjusting internal air temperature and flow, while the external air ring controls bubble shape and gauge uniformity at the die. For this grade, internal bubble cooling is recommended when output exceeds 2.0–2.5 kg/h per mm of die circumference; below that threshold, external air ring control is usually sufficient. Excessive external air velocity can create unstable bubble flutter in the tentering cone and should be balanced against the required frost line height.
The octene comonomer in DOWLEX 2038.68G produces longer short-chain branching than butene-based LLDPE. At comparable density and melt index, the octene structure generally increases the number of tie molecules between crystal lamellae, which raises dart impact energy and slow crack growth resistance. Comparative testing should follow ASTM D1709 for dart impact, ASTM D1922 for Elmendorf tear, and ASTM D5748 for puncture resistance. The magnitude of improvement is dependent on film gauge, blow-up ratio, frost line height, and extrusion thermal history; values obtained on a laboratory blown-film line may not transfer directly to production equipment.
Relative to high-pressure LDPE with a melt index of 0.8–2.0 g/10 min, the resin has higher tensile strength at break and higher elongation at break when measured according to ASTM D882, but lower melt strength. This creates a processing trade-off: LDPE stabilizes the bubble at high blow-up ratios and low gauge, while 2038.68G contributes stiffness and puncture resistance. In heavy-duty sack formulations, converters often blend 20–40 wt% LDPE to restore bubble stability. The blend ratio is not a specification; it must be set according to die diameter, air ring design, and internal bubble cooling capability.
Compared with DOWLEX 2045G, which carries a nominal density of 0.920 g/cm³ and melt index of 1.0 g/10 min, 2038.68G raises the density to 0.935 g/cm³. The consequence is higher secant modulus and lower oxygen permeability at equal film thickness, but also a slightly higher seal initiation temperature and reduced low-temperature impact. Compared with DOWLEX 2035G, nominal 0.919 g/cm³ density and 6.0 g/10 min melt index, 2038.68G is significantly more viscous at extrusion shear rates; it is more suited to thick-gauge film and less suited to thin-gauge cast stretch film. Selection among these grades is governed by the target stiffness, permeability, and process line speed.
For film downgauging, the thickness reduction is not linear with density change. Because film failure is initiated by local stress concentrations, the retained dart impact and tear resistance must be measured at each target gauge. A practical evaluation protocol uses a three-gauge series around the incumbent thickness, for example 80 µm, 70 µm, and 60 µm, with at least 20 dart impact specimens per gauge according to ASTM D1709. Only if the lower-gauge film meets the same lower specification limit as the incumbent can downgauging be considered robust; otherwise the stiffness gain from higher density is not sufficient to compensate for thickness reduction.
Antioxidant and stabilizer consumption is coupled to processing temperature and residence time. Repeated extrusion at 240 °C or above consumes phenolic antioxidants faster than at 200 °C; film produced from regrind should be limited to 15–25 wt% unless oxidative induction time testing per ISO 11357-6 confirms retained stabilization. Excessive regrind fractions above 30 wt% may increase gel content and reduce bubble stability on high-output lines.
Food-contact and regulatory status applies only to the unreinforced base polymer and to formulations that have not been modified with non-compliant additives. The resin is generally covered by the manufacturer’s food-contact statement under FDA 21 CFR 177.1520(c) for olefin polymers, subject to the conditions of use and food types set out in 21 CFR 176.170. In the European Union, compliance is assessed under Regulation (EU) No 10/2011 for plastic materials and articles intended to come into contact with food; overall migration should be verified on the final article using EN 1186 series test methods. The base polymer does not contain intentionally added perfluoroalkyl substances and should be evaluated for REACH Candidate List substances only after all additives are included.
| Framework | Designation | Verification basis |
|---|---|---|
| U.S. food-contact olefin polymers | FDA 21 CFR 177.1520(c) | Compliance of base polymer and final extraction under 21 CFR 176.170 use conditions |
| EU plastic food-contact materials | Regulation (EU) No 10/2011 | Overall migration 10 mg/dm² for general contact; specific migration limits apply to additives |
| REACH SVHC | Regulation (EC) No 1907/2006 | Candidate List substance concentration 0.1 wt% per article |
| RoHS | Directive 2011/65/EU | Lead 1000 ppm, cadmium 100 ppm, mercury 1000 ppm, hexavalent chromium 1000 ppm in homogeneous materials for EEE applications |
The resin is not supplied with medical-grade certification unless explicitly agreed in writing. For hot-fill or retort applications, the final article must be tested for deformation and migration under the intended temperature profile. The Vicat softening point of 122 °C does not by itself guarantee dimensional stability under load; creep and shrinkage behavior must be assessed by ASTM D2990 or equivalent part-level testing.
In coextruded films, the resin is placed in outer or internal layers where higher modulus and tear resistance are required. Viscosity matching with adjacent LDPE or EVA layers is necessary to avoid interfacial waviness; a melt-index difference greater than 0.5–1.0 g/10 min between layers may require melt temperature adjustments or die design changes. Typical structures pair the resin with high-pressure LDPE in the core at 40–60 wt% and an EVA or metallocene plastomer sealing layer at 10–20 wt%. Such ratios are equipment-dependent and must be optimized through actual line trials. Direct adhesion to EVOH or polyamide is insufficient; a maleated polyolefin tie layer is required.
Agricultural film applications require UV stabilization. The base resin does not contain UV stabilizers unless incorporated by the converter; accelerated weathering should be performed per ASTM D4329 or ISO 4892-2 on the final film. In silage and greenhouse films, the higher density of 0.935 g/cm³ improves tensile strength under wind load but may reduce low-temperature flexibility compared with 0.920 g/cm³ LLDPE grades; anti-fog and anti-drip additives must be evaluated for their effect on surface energy and migration kinetics. Converters should compare tensile modulus per ASTM D882, puncture resistance per ASTM D5748, and tear propagation per ASTM D1922 on samples produced under identical blow-up ratio, frost line height, and chill roll temperature before committing to a downgauging program. Laboratory values generated on a 50 mm line may not transfer to production-scale equipment without scale-up trials.