Dow Dowlex 2037 Linear Low Density Polyethylene Cast Film Grade

Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade

    • Product Name: Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 227115
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Octene-1
    Grade Cast Film Grade
    Density 0.935 g/cm³
    Meltindex 2.5 g/10 min
    Meltingpoint 124 °C
    Vicatsofteningpoint 111 °C
    Tensilestrengthatyield 12.1 MPa
    Tensilestrengthatbreak 31.0 MPa
    Ultimateelongation 700%
    Dartdropimpact 120 g
    Elmendorftearmd 250 g
    Elmendorfteartd 500 g
    Haze 2.0%
    Gloss45 90
    Coefficientoffriction 0.15
    Heatsealinitiationtemperature 95 °C
    Recommendedfilmthickness 1 mil

    As an accredited Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DOWLEX 2037 is supplied in 25 kg polyethylene-lined paper bags, 40 bags per pallet (1,000 kg total).
    Container Loading (20′ FCL) Dow DOWLEX™ 2037 LLDPE Cast Film Grade: 20′ FCL, palletized 25 kg bags, shrink-wrapped, about 18–20 MT net, loaded floor-to-ceiling.
    Shipping Dow DOWLEX™ 2037 LLDPE Cast Film Grade ships as non-hazardous polyethylene pellets. Typical packaging: 25 kg moisture-barrier bags or 1,000 kg bulk bags/octabins. Not DOT, IMDG, IATA, or UN regulated. Transport by standard truck, rail, or container. Store dry, ambient, away from heat; handle with normal industrial PPE.
    Storage Store DOWLEX™ 2037 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed, clean, and clearly labeled. Protect from moisture, dust, and contamination. Stack pallets safely to prevent damage. Observe first-in, first-out inventory. Avoid prolonged exposure to high temperatures or UV radiation. Store separately from food and drinking water.
    Shelf Life No fixed shelf life; store in cool, dry, ventilated area away from direct sunlight, heat, moisture, and ignition sources.
    Application of Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade

    What Restricts Migration Compliance in Sub-20 µm Cast Produce Wrap?

    Food-contact cast film produced with DOWLEX™ 2037 at 0.935 g/cm³ density falls under FDA 21 CFR 177.1520(a)(3)(i) for olefin polymers in direct food contact, conditional upon end-testing for overall migration under EU Regulation 10/2011 Annex III with an overall migration limit of 10 mg/dm². The resin does not intrinsically carry a food-contact declaration; compliance is achieved through formulation discipline and downstream conversion monitoring. Typical formulation loading for fresh-produce wrap is 85–95 wt% DOWLEX™ 2037 with 2–5 wt% slip/antiblock masterbatch (erucamide or oleamide slip, synthetic silica antiblock at 1000–3000 ppm active loading) and 0–10 wt% LDPE for machinability adjustment during high-speed bag conversion. The cast film process for sub-20 µm produce wrap employs a single-screw extruder with L/D 30:1–36:1, barrier screw geometry, melt temperature 240–270°C, flat die with flex-lip adjusting bolts and a die gap of 0.4–0.6 mm. Chill roll temperature is maintained at 15–25°C using polished chrome-plated rolls with surface finish Ra ≤ 0.1 µm; haze below 4% (ASTM D1003-13) and gloss above 70 GU at 60° angle (ASTM D2457-13) are the operational targets. The higher 0.935 g/cm³ density of DOWLEX™ 2037 relative to conventional 0.918 g/cm³ film-grade LLDPE elevates tensile modulus in the machine direction, which reduces bag-sag on vertical form-fill-seal equipment. The end-product matrix includes fresh-cut produce bags, bakery display film, frozen-food overwrap, and tamper-evident retail packaging where dart impact (ASTM D1709-16a, Method A) above 150 g at 25 µm is required. The operational boundary: melt temperatures above 280°C initiate oxidative degradation evidenced by carbonyl index increase, gel formation in the die lip, and loss of cling performance in downstream conversion. Published data for specific slip surfactant bloom rates on 0.935 g/cm³ LLDPE cast film at sub-20 µm thickness is limited, requiring internal migration kinetics testing per film structure.

    Industrial Liner Extrusion and Puncture Propagation Resistance at 0.935 g/cm³

    Industrial liner and construction film production using DOWLEX™ 2037 targets puncture propagation resistance under ASTM D5748-95 (now withdrawn, but referenced in procurement specifications) and tensile properties per ASTM D882-18. Formulation loading is 70–100 wt% DOWLEX™ 2037, with 0–30 wt% recycled linear-low-density polyethylene (rLLDPE) post-industrial resin where cost-driven specifications permit; calcium carbonate masterbatch at 5–15 wt% is introduced only for moisture-barrier underlayment films where opacity and basis weight are prioritized over tensile strength. The downstream cast film process for industrial liner runs at film thicknesses of 50–150 µm with a die gap of 0.6–1.0 mm, melt temperature 250–285°C, and chill roll temperature 18–28°C. Failures observed on production lines include edge-bead thickness exceeding ±5% gauge tolerance when the die lip is not thermally controlled across the width, and winder tension oscillation above ±10 N causing telescoped rolls. The 0.935 g/cm³ density contributes to Elmendorf tear resistance in the cross direction (ASTM D1922-15) exceeding 400 g at 100 µm, which is a critical parameter for construction grade membranes that must resist wind tear during installation. End-product types include concrete-curing membranes, temporary wall sheathing, pipe protection wrap, moisture vapour retarders under slab, and construction debris containment. Where flame-retardant compliance is required, the building code pathway is EN 13501-1 for reaction-to-fire classification; however, the polyethylene substrate without halogenated or intumescent additives is rated Class E, and published data for achieving Class B or higher with DOWLEX™ 2037 is limited. This scenario does not require food-contact or medical-grade documentation, and no surface treatment above 38 dyn/cm corona discharge (ASTM D2578-17) is needed for construction tape adhesion.

    When ISO 11607 Sterile Barrier Requirements Dictate Cast Film Layer Architecture

    Medical device packaging films built on DOWLEX™ 2037 must satisfy ISO 11607-1:2019 clause 5.2 for material performance and clause 5.3 for seal-integrity verification in terminally sterilized barrier systems. Production occurs in an ISO 14644-1 Class 8 clean room minimum, with ISO 13485:2016 quality management governing batch traceability and change control; the material supplier must issue a certificate of analysis per ASTM D1238-20 (melt index 2.5 g/10 min at 190°C/2.16 kg) and ASTM D792-20 (density 0.935 g/cm³) for each lot. Formulation loading in medical lidding and header bag film is 80–100 wt% DOWLEX™ 2037, with 0–20 wt% metallocene LLDPE for seal initiation temperature reduction to 95–110°C and seal-peel transition control; antiblock masterbatch loading is capped at 2000 ppm to avoid particulate migration into the sterile field. The cast film line for medical barriers employs a vented single-screw extruder with L/D 32:1 and a downstream melt filter stack with screen pack 100/120/100 mesh for gel particle removal; die gap is held at 0.5–0.8 mm, chill roll temperature at 12–18°C, and line speed is typically 80–200 m/min for film thicknesses of 40–80 µm. Peel strength per ASTM F88/F88M-15 must fall within 3–8 N/15 mm for chevron pouch seals and 2–6 N/15 mm for Tyvek lidding film seals; seal failure in production often traces to polymer degradation at the die lip creating micro-gels that interrupt the seal interface. End-product types include peelable lidding film for thermoformed trays, header bags for single- and double-pouch configurations, chevron pouches for surgical kits, and back-web for form-fill-seal sterile packaging. The operational boundary is strict: ethylene oxide sterilization cycles at 50–60°C and gamma irradiation at 25–50 kGy both induce measurable molecular weight reduction in the 0.935 g/cm³ LLDPE; post-sterilization seal strength must be verified per ISO 11607-2:2019 clause 6.2 with a minimum retained seal strength of 1.5 N/15 mm after accelerated aging at 60°C/70% RH for 14 days.At densities above 0.930 g/cm³, machine stretch film production with DOWLEX™ 2037 shifts the mechanical balance between pre-stretch propagation and load retention in pallet unitization. The resin is typically introduced into the core layer of a 5-layer cast film line at 60–80 wt%, while skin layers receive a lower-density LLDPE or metallocene PE at 0.918–0.922 g/cm³ in 10–20 wt% per skin for cling development via ISO 527-3 tensile modulus differential. Polyisobutylene (PIB) tackifier at 0.5–2.0 wt% is injected into the skin layers via liquid pump downstream of the primary extruder at a melt temperature of 220–240°C to minimize thermal degradation. The five-layer cast line for stretch film operates with independent extruders at L/D 30:1–36:1, feedblock distribution of 10%/25%/30%/25%/10% or similar split, flat die gap 0.4–0.7 mm, and a chill roll at 15–25°C with air knife assistance for edge pinning. Gauge reduction trials on commercial lines reveal that pre-stretch ratios above 250% often trigger transverse-direction tearing at the film edge when DOWLEX™ 2037 loading in the core exceeds 80 wt%, evidenced by fracture morphology oriented perpendicular to machine direction. Dart impact per ASTM D1709-16a Method A is typically 180–250 g at 23 µm, while ultimate elongation in the machine direction per ASTM D882-18 exceeds 700% prior to catastrophic failure; these values support transport-stability loads above 500 kg for single-pass pallet wrapping. End-product types include hand stretch film at 12–20 µm, machine stretch film at 17–35 µm, pre-stretched film at 8–15 µm, and vented pallet wrap. The dominant processing failure mode is cling reduction caused by migration of erucamide from core-layer recycled content competing with PIB at the skin surface, a batch-to-batch variance documented in production logs with cling force falling below 200 g/cm under ASTM D5458-95.For applications where silage bale and grain storage films demand UV-stabilized barrier performance without food-contact documentation, DOWLEX™ 2037 serves as an extrusion base at 70–90 wt% with hindered amine light stabilizer (HALS) masterbatch at 3–8 wt% and carbon black masterbatch at 2–5 wt% where opacity is specified. Compliance for silage films is governed by CEN/EN 13207:2018 for thermoplastic silage films, which sets requirements for oxygen transmission rate above 600 cm³/m²·day·atm only in non-sealed wrap configurations; the actual airtight sealing in bale wrap is achieved by film-to-film cling through a PIB-tackified surface layer. The cast film process for agricultural barrier film typically uses a single-screw extruder at L/D 28:1–32:1, die gap 0.6–0.9 mm, and melt temperature 240–270°C. One critical operational boundary: UV masterbatches containing HALS at loadings above 8 wt% reduce melt viscosity and can cause die-lip build-up (fogging) on cast film lines, requiring periodic die wipe cycles that interrupt continuous runs of 8–12 hours. End-product types include round-bale stretch wrap at 25–35 µm, clamp silage covers at 80–120 µm, grain storage fumigation barrier films at 100–150 µm, and greenhouse liner outer sheeting. Published data for specific DOWLEX™ 2037 agricultural film weatherability under outdoor exposure exceeding 12 months is limited; laboratory accelerated UV aging per ISO 4892-2 with UVA-340 lamps at 0.76 W/m² irradiance and 60°C black-panel temperature is the standard verification route for customer-specific formulations.

    Extrusion Lamination Core Architecture and Sealant Interlayer Behavior

    In flexible packaging lamination, DOWLEX™ 2037 is deployed primarily as an extrusion lamination tie layer or sealant interlayer rather than as a surface print web, due to its 0.935 g/cm³ density delivering elevated stiffness in unsupported structures. Formulation loading is 50–80 wt% DOWLEX™ 2037 with 20–50 wt% metallocene LLDPE or EVA for seal initiation temperature reduction to 80–95°C in cold-seal alternatives; anhydride-grafted LLDPE tie resin may constitute 5–10 wt% of the blend for laminate adhesion to aluminium foil or biaxially oriented polyester. Compliance is anchored to ASTM D1876-08 (T-peel resistance of adhesives) for bond strength measurement and ASTM F88/F88M-15 for seal strength verification; for flexible food packaging, EU Regulation 10/2011 and FDA 21 CFR 177.1520 remain the food-contact reference points. The downstream process is extrusion lamination on a tandem line where the DOWLEX™ 2037 blend is melted at 280–320°C—notably higher than cast film extrusion—to promote oxidative adhesion to the primary web. The melt is delivered through a flat die with a die gap of 0.3–0.5 mm into the nip between a chill roll at 10–18°C and a pressure roll at 3–5 N/mm nip force. Failure modes at production scale include neck-in exceeding 30% when melt temperature drops below 280°C, causing edge-thinning and web break at line speeds above 120 m/min. End-product types include stand-up pouch sealant layers, retortable pouch interlayers, frozen-food laminate cores, and insulation backing laminates for construction. The operational boundary is specific: DOWLEX™ 2037 exposed to temperatures above 320°C for extended residence times in the extruder barrel (> 6 min) develops oxidative gels that interrupt the thin melt curtain and create visual defects in the laminated structure. For sterilizable retort pouch applications, autoclave conditions at 121°C/15 psi for 30 min require sealant interlayer thickness above 35 µm to prevent delamination from the aluminium foil barrier.
    Formulation Gradient Study for 5-Layer Machine Stretch Film with DOWLEX™ 2037 Core
    Core Layer Loading (wt%)Skin Layer Density (g/cm³)Film Thickness (µm)MD Elongation (%) ASTM D882-18Dart Impact (g) ASTM D1709-16aPre-stretch Ratio Before TD Fracture (%)
    500.91820650160220
    650.91820720195260
    800.92023740230280
    900.92223760245300
    Compliance Standards Matrix for Downstream Applications of DOWLEX™ 2037 Cast Film
    ApplicationPrimary StandardTest Method DesignationCritical Parameter
    Food-contact produce wrapFDA 21 CFR 177.1520(a)(3)(i)EU 10/2011 Annex IIIOverall migration ≤ 10 mg/dm²
    Machine stretch filmASTM D5748-95ASTM D5458-95Puncture propagation ≥ 100 N/mm
    Medical sterile barrierISO 11607-1:2019ASTM F88/F88M-15Seal strength 3–8 N/15 mm
    Industrial linerASTM D882-18ASTM D1922-15CD Elmendorf tear ≥ 400 g
    Agricultural silageCEN/EN 13207:2018ISO 4892-2UV exposure durability
    Extrusion laminationASTM D1876-08ASTM F88/F88M-15Peel bond strength ≥ 5 N/15 mm
    Free Quote

    Competitive Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DOWLEX™ 2037 Linear Low Density Polyethylene is a solution-polymerized ethylene–octene copolymer supplied for cast film conversion. The resin is characterized by a nominal density of 0.935 g/cm³ when measured under ASTM D792-20 and a nominal melt mass-flow rate of 2.5 g/10 min under ASTM D1238-20 at 190 °C and 2.16 kg. The octene comonomer generates a linear backbone with a short-chain branch distribution that is structurally distinct from the long-chain branching architecture of high-pressure low-density polyethylene and from the shorter butene branch structure of conventional Ziegler-Natta butene-LLDPE. This difference controls solid-state density, crystallization kinetics, and melt relaxation behavior in cast film cooling. The product is supplied as pellets and is intended for monolayer and coextruded cast film applications where a balance of stiffness, drawdown, and tear resistance is required at film gauges commonly between 12 µm and 80 µm.

    Representative physical property data for DOWLEX™ 2037
    PropertyMethodRepresentative value
    DensityASTM D792-20 / ISO 1183-1:20190.935 g/cm³
    Melt mass-flow rateASTM D1238-20 / ISO 1133-1:2022, 190 °C/2.16 kg2.5 g/10 min
    DSC peak melting temperatureASTM D3418-15124 °C
    Vicat softening temperatureASTM D1525-17e1, Rate A, 10 N121 °C

    These values are representative material-selection data and not specification limits. Lot-specific certificates of analysis control the commercial release of DOWLEX™ 2037, and converters should verify the current values before die design or final film qualification. The resin is not hygroscopically sensitive when packaging is intact, but sacks exposed to relative humidity above 60% RH should be pre-dried at 80 °C for 2–4 h to avoid surface moisture entering the feed throat and generating melt-pressure fluctuation. Antioxidant and processing stabilizer packages are incorporated to protect the resin during melt processing; they are not intended to replace UV stabilizers in the final film. If outdoor exposure is required, a separate UV stabilizer masterbatch must be added at levels determined by weathering requirements under ISO 4892-2 or ASTM G154.

    What limits draw resonance in 0.935 g/cm³ octene-LLDPE cast film extrusion?

    Draw resonance in cast film is a periodic thickness oscillation generated by the interaction of melt relaxation time, draw ratio, and the distance between the die exit and the freezeline imposed by the chill-roll, air knife, or vacuum box. For DOWLEX™ 2037, the higher density of 0.935 g/cm³ raises the quench crystallization temperature relative to 0.918 g/cm³ butene-LLDPE, which enables the web to sustain a higher draw ratio before sustained oscillation when the chill-roll temperature is held between 15 °C and 20 °C. However, the elevated density also increases melting enthalpy and zero-shear viscosity at equivalent melt temperature; die melt temperature should be maintained at 240–280 °C to keep apparent shear viscosity within the range required for stable die-lip filling without excessive thermo-oxidative gel formation.

    Single-screw extruders with L/D ≥ 24:1, grooved feed sections, barrier flights, and Maddock mixing sections are typically required because the higher melting enthalpy of 0.935 g/cm³ LLDPE demands additional specific energy input per kilogram of melt. Die gap is normally set between 0.6 mm and 0.8 mm; the draw ratio from die gap to final film gauge is governed by the air-knife or vacuum-box position. If the freezeline is allowed to wander beyond 15 mm from the die lip, gauge uniformity at 12 µm can deteriorate and draw resonance may appear at lower line speeds. Melt temperature should not exceed 290 °C, because residence-time-dependent oxidation above this threshold can generate crosslinked gel particles that appear as fisheyes in thin-gauge cast film. Processors running DOWLEX™ 2037 on lines originally designed for butene-LLDPE often need to increase barrel temperatures in the transition zone by 5–10 °C to complete melting before the metering zone.

    Chill-roll temperature also affects blocking and release. A polished roll at 15 °C reduces haze and improves gauge stability, but too low a roll temperature can produce condensation at high humidity and must be balanced against web release. A matte roll at 30 °C may produce higher haze but can improve downstream handling. The choice of air knife versus vacuum box depends on die-to-roll distance and line speed; vacuum-box systems generally allow higher line speeds and thinner gauge because they force the melt curtain onto the chill roll more rapidly, but they require more precise die-lip adjustment. Published data for a specific line configuration is limited; controlled line trials are required to determine the maximum stable draw ratio.

    Film tensile properties are measured under ASTM D882-18; dart impact resistance under ASTM D1709-16a; Elmendorf tear under ASTM D1922-15; puncture resistance under ASTM D5748; haze under ASTM D1003-13; and specular gloss under ASTM D2457-13. In monolayer cast film at 25 µm, the higher density of DOWLEX™ 2037 shifts tensile yield stress upward relative to 0.920 g/cm³ octene-LLDPE when run under identical quench conditions; the size of the shift depends on chill-roll temperature and film orientation. Dart impact and puncture resistance remain gauge-dependent, with films below 15 µm showing reduced energy absorption because the rapidly quenched crystallite network limits plastic deformation before failure. Optical haze is controlled primarily by the chill-roll surface finish and by melt-temperature uniformity. A polished chill roll at 15 °C typically yields lower haze than a matte roll at 30 °C, but the specific configuration must be qualified on the production line because cooling-roll finish and vacuum-box design interact with resin crystallization rate.

    Corona treatment of DOWLEX™ 2037 cast film is generally performed in-line at discharge power levels adjusted to achieve surface energies between 38 mN/m and 44 mN/m for lamination or printing. The higher density of 0.935 g/cm³ may require a slightly higher discharge energy than a 0.918 g/cm³ LDPE to reach the same surface energy because the polymer has lower fractional free volume and lower initial surface polarity. Surface energy should be verified with dyne solutions conforming to ASTM D2578 or with contact-angle measurement using ISO 19403. Untreated film is not recommended for laminating or printing because low surface energy prevents adequate ink and adhesive wetting.

    Comparative stiffness and seal response are governed by comonomer selection and density.

    Relative to 0.918 g/cm³ high-pressure LDPE and 0.920 g/cm³ octene-LLDPE, DOWLEX™ 2037 increases the crystalline mass fraction and raises the storage modulus below the alpha transition. In coextruded cast film, the grade is therefore used as a stiffening skin layer rather than as a sealant layer when low seal initiation temperature is required. The octene comonomer reduces the concentration of highly regular short branches typical of butene-LLDPE, which lowers the tendency for lamellar thinning and improves the tear balance measured under ASTM D1922-15. Direct substitution of butene-LLDPE by DOWLEX™ 2037 at equal gauge and output generally increases tensile modulus, puncture resistance, and clarity, but the higher density also reduces fractional free volume and can shift water vapor transmission rate performance; converters should revalidate barrier data under the intended package shelf-life conditions.

    Comparative nominal properties of selected polyethylene film resins
    ResinDensity (ASTM D792-20)Melt index (ASTM D1238-20)Polymer architecture
    DOWLEX™ 20370.935 g/cm³2.5 g/10 minoctene solution LLDPE
    DOWLEX™ 2045G0.920 g/cm³1.0 g/10 minoctene solution LLDPE
    DOW LDPE 7220.918 g/cm³8.0 g/10 minhigh-pressure autoclave LDPE

    The nominal data in the table show that DOWLEX™ 2037 is not a direct replacement for 8.0 g/10 min LDPE extrusion-coating grades such as DOW LDPE 722, which are selected for low-viscosity web stability at very high line speeds. DOWLEX™ 2037 is positioned for cast film structures in which higher stiffness and moderate melt strength are required. DOWLEX™ 2045G at 0.920 g/cm³ and 1.0 g/10 min is typically used where lower density and higher melt strength are favored for seal-peel or blown film conversion. The grade 2037 is also differentiated from butene-LLDPE cast film resins of similar melt index by its higher density and octene comonomer, which alter the balance between modulus and low-temperature toughness. Those differences become more pronounced at thin gauges below 15 µm, where crystalline orientation and cooling-rate gradients control the final property profile.

    Regulatory status and food-contact compliance matrix

    Compliance statements for DOWLEX™ 2037 should be obtained from the manufacturer’s product regulatory bulletin and the food-contact certificate. The resin is commonly covered by FDA 21 CFR 177.1520(c) for olefin polymers used in food-contact articles; the applicable subparagraph, density and extractable limitations, and end-use restrictions are lot-specific and must be documented in the certificate of compliance. Under EU Regulation (EU) No 10/2011, food-contact articles made with DOWLEX™ 2037 must meet the overall migration limit of 10 mg/dm² using the food simulants and time-temperature conditions assigned to the intended contact category. The resin is subject to registration under REACH Regulation (EC) No 1907/2006. No halogenated flame retardants, heavy-metal stabilizers, or ortho-phthalate plasticizers are intentionally added. Compliance with RoHS Directive 2011/65/EU is not applicable to packaging film by default but may be declared for articles used in electronics packaging when supported by a written supplier statement. Converters should also verify that additives or concentrates blended downstream do not change the regulatory status of the finished article.

    When DOWLEX™ 2037 replaces butene-copolymer LLDPE in high-speed stretch film lines

    Substitution trials on cast stretch-film lines running 13–17 µm film at 200 m/min line speed show that DOWLEX™ 2037 can be processed without changing the screw when the melt temperature is raised by 5–10 °C to compensate for the higher melting enthalpy. The 0.935 g/cm³ density and octene comonomer structure produce a stiffer film that maintains pre-stretch at higher draw ratios; however, the ultimate pre-stretch ratio before film break may be lower than that of a 0.920 g/cm³ octene LLDPE depending on the pre-stretch gearing and ambient temperature. Puncture retention under ASTM D5748 improves relative to butene-LLDPE at equal gauge, while edge tear under ASTM D1922 becomes more anisotropic; slitter performance and roll hardness should be evaluated before the formulation is locked. Published data for this specific substitution in a given machine configuration is limited, so controlled line trials are required.

    In cast lamination film for flexible packaging, DOWLEX™ 2037 is used where a stiff outer layer is required to improve machinability and reduce film elongation under tension. The higher density can also reduce blocking in film-to-film contact because the harder surface has a lower contact area. In hygiene and industrial film, the grade may be blended with lower-density LLDPE or LDPE to adjust modulus, dart impact, and tear balance. The allowable blend ratio is limited by compatibility and by the minimum seal or tough layer requirements of the structure; no single blend ratio applies across all coextrusion lines. Processing should be validated under ISO 2813 for gloss or ASTM D1003-13 for haze when visual quality is critical.

    DOWLEX™ 2037 should not be processed at melt temperatures above 290 °C for prolonged residence times because thermo-oxidative chain scission produces gel particles. It is incompatible with strong oxidizing agents, aromatic and chlorinated solvents at elevated temperatures, and should not be blended with high levels of ionomer or acid-functional polymers without prior dispersion testing due to potential interfacial instability in coextrusion. Storage above 50 °C can increase pellet blocking; sacks should be protected from UV exposure during outdoor storage to avoid surface oxidation that raises gel count. The resin is not intended for implantable medical devices, and no USP Class VI or ISO 10993 certification should be assumed without a written letter from the manufacturer.

    Top