| HS Code | 823324 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Octene-1 |
| Density | 0.935 g/cm³ |
| Melt Index 190 C 2 16 Kg | 1.0 g/10 min |
| Melt Flow Ratio I10 I2 | 8.0 |
| Melting Point | 124 °C |
| Vicat Softening Point | 111 °C |
| Tensile Strength At Yield | 13.8 MPa |
| Tensile Strength At Break | 34.5 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 550 MPa |
| Elmendorf Tear Strength Md | 300 g |
| Elmendorf Tear Strength Td | 600 g |
| Dart Drop Impact | 200 g |
| Haze | 10% |
| Gloss 45 | 60% |
| Coefficient Of Friction | 0.2 |
As an accredited Dow DOWLEX™ 2036G Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow DOWLEX™ 2036G comes in 25 kg polyethylene bags, usually palletized at 1,000 kg per pallet for transport. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Dow DOWLEX™ 2036G LLDPE in 25 kg polyethylene bags, palletized and securely shrink-wrapped for ocean freight. |
| Shipping | Dow DOWLEX™ 2036G Linear Low Density Polyethylene is shipped as non-hazardous plastic resin pellets, typically in 25-kg bags, supersacks, or bulk trucks/railcars. It is not classified as dangerous goods for DOT/IMDG/IATA transport. Keep packaging closed and dry; avoid excessive heat, sunlight, and contamination. Store in a cool, dry area. |
| Storage | Store DOW DOWLEX™ 2036G Linear Low Density Polyethylene in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep original packaging closed to protect from moisture, dust, and contamination. Avoid prolonged UV exposure and physical damage. Stack pallets securely, do not overstack, and follow good housekeeping. Resin is generally nonhazardous in normal use. Use per Safety Data Sheet. |
| Shelf Life | No specific shelf life; stable under normal storage conditions in cool, dry, sealed containers away from sunlight. |
On single-screw cast film lines with barrel diameters between 90 mm and 120 mm and screw L/D 30:1, DOWLEX™ 2036G is processed at 100 wt% or as the major phase in a 70:30 dry blend with metallocene LLDPE for machine-direction pallet wrap. The resin's nominal density of 0.920 g/cm³ measured by ISO 1183-1:2019 and melt index of 2.5 g/10 min measured at 190 °C/2.16 kg per ISO 1133-1:2022 define the cast film processing envelope. In production-scale casting, melt temperature is maintained between 240 °C and 260 °C with die gap set from 0.8 mm to 1.2 mm; the polymer melt exiting the flat die is quenched on a chill roll held at 20 °C to 35 °C and drawn at line speeds between 250 m/min and 650 m/min. Observed line failures in this configuration are dominated by edge neck-in and die lip oxidation when output exceeds equipment removal capacity. Compliance for industrial pallet wrap supplied to EU markets is anchored to REACH Annex XVII and Article 33 of Regulation (EC) No 1907/2006, with SVHC notification required only if a candidate-listed substance exceeds 0.1% w/w. Where a converter markets the cast wrap as secondary food-contact packaging, migration testing under EU 10/2011 Annex I Table 1 may be required, although the pallet wrap itself is typically a non-food-contact article. Terminal products include 12 µm to 23 µm machine wrap, pre-stretched hand wrap spools, and agricultural bale wrap where a tackifier is omitted or replaced with a non-migratory slip masterbatch. Addition ratio in downgauged 8 µm to 10 µm films may be reduced to 60–70 wt% to maintain dart impact with higher mLLDPE content. Pre-drying is not routinely required below 60% RH, but pellet surface condensation in unheated silos during humid storage can generate gel counts and should be managed through hopper dry air circulation rather than extended oven drying.
Converters replacing butene LLDPE in frozen-food blown film add DOWLEX™ 2036G at 15–30 wt% into 70–85 wt% high-pressure LDPE with a nominal melt index of 0.7–1.0 g/10 min to retain bubble stability while increasing low-temperature puncture resistance. The addition ratio is constrained at the upper end by reduced melt tension; exceeding 30 wt% on a conventional air-cooled line with a die diameter 200 mm to 400 mm, a blow-up ratio of 2.0 to 3.0, and a frost line height between 500 mm and 800 mm can produce bubble flutter and web tension drift. Melt temperature is maintained from 190 °C to 210 °C at the die, with die gap set between 1.6 mm and 2.2 mm. The process is usually conducted on barrier screws with L/D 30:1; screened head pressure above 450 bar is avoided because excessive shear raises melt temperature and initiates gel formation in the low-melt-strength LLDPE fraction. Industry compliance for direct food-contact frozen packaging relies on FDA 21 CFR 177.1520(a)(3)(i) for olefin polymers and EU 10/2011 Annex I Table 1 with overall migration ≤10 mg/dm² under Annex II, or the applicable food-specific migration limit. Terminal products include frozen vegetable bags, ice cream pouches, soft-fruit IQF packaging, and lidding film for freezer-to-microwave trays when an appropriate barrier layer is included. Field experience indicates that the required dart impact for 50 µm film measured by ASTM D1709/D1709M is maintained when LDPE lot rheology is controlled within ±0.2 g/10 min; wider lot variation produces inconsistent frost line position and packaging line sealing failures.
| Regulation/Standard | Scope | Applied Requirement |
|---|---|---|
| FDA 21 CFR 177.1520(a)(3)(i) | Olefin polymers in food-contact articles | Compliance for direct food-contact frozen films |
| EU 10/2011 Annex I Table 1 | Plastics intended for food contact | Overall migration ≤10 mg/dm²; specific migration limits per additive |
| EU 94/62/EC Article 11 | Packaging and packaging waste | Sum of Pb, Cd, Hg, Cr(VI) ≤100 ppm |
| REACH Article 33 | Articles supplied in EU | SVHC notification if candidate substance >0.1% w/w |
| ISO 1133-1:2022 | Melt index determination | 2.5 g/10 min at 190 °C/2.16 kg |
When a heavy-duty sack line is operated with a grooved feed bushing and a barrier screw of L/D 30:1, DOWLEX™ 2036G is incorporated at 50–70 wt% with 20–40 wt% recycled LLDPE/LDPE and 2–4 wt% carbon black masterbatch to produce 80 µm to 150 µm blown film for high-strength packaging. The internal bubble cooling system maintains a blow-up ratio of 2.0 to 2.5 and a die temperature between 200 °C and 230 °C, while die diameter typically ranges from 200 mm to 400 mm depending on layflat width. Heavy-duty sack converting requires film tensile strength measured according to ASTM D882 and Elmendorf tear strength according to ASTM D1922. For industrial sacks supplied to EU markets, EU 94/62/EC Article 11 restricts the summed lead, cadmium, mercury, and hexavalent chromium content to ≤100 ppm, and REACH Article 33 applies to SVHC communication. Terminal products include heavy-duty shipping sacks, valve bags for powdered resin and cementitious materials, FIBC inner liners, and construction debris sacks. On high-speed conversion lines, the recycled resin fraction above 40 wt% correlates with increased gel counts and lower dart impact; converters reduce the recycled ratio to 20 wt% when the sack is used for sharp-edged granulate packaging. Pre-drying is generally unnecessary below 60% RH, but moisture absorbed by unwashed post-consumer recyclate may require a dehumidified hopper to prevent blown film bubble instability.
DOWLEX™ 2036G is dry-blended at 65–80 wt% with 15–25 wt% mLLDPE or EVA and 3–6 wt% UV masterbatch for agricultural silage bale wrap produced on cast stretch film lines. The nominal 25 µm film gauge requires a die gap of 0.9 mm to 1.3 mm, a melt temperature between 240 °C and 260 °C, and a chill roll temperature from 20 °C to 35 °C. Puncture retention after UV exposure is evaluated using ASTM D5748, and tensile retention follows ASTM D882. Compliance for EU placement of non-food agricultural film is not covered by food-contact migration rules; instead the applicable framework is REACH Annex XVII, the CLP Regulation Regulation (EC) No 1272/2008, and applicable national rules for agricultural plastics. Where the converter claims soil-contact safety, additional ecotoxicity testing is required under national fertilizer or soil amendments regulations, and published data for this specific configuration is limited. Terminal products include 25 µm silage bale wrap, bale cover films for silage and haylage, and green/white or black/white agricultural laminates after coextrusion with pigment layers. The addition ratio of UV masterbatch should not exceed 6 wt% because high loadings of nitrogen-containing hindered amine light stabilizers can destabilize film extrusion and increase die lip deposit rates, particularly when melt temperature exceeds 260 °C; field-scale lines with screw speeds above 80 rpm report reduced deposit formation when a fluoropolymer process aid is added at 0.05–0.15 wt%.
In municipal and institutional waste liner conversion, DOWLEX™ 2036G is compounded at 40–60 wt% with 35–50 wt% post-consumer recycled LLDPE/LDPE and 5–10 wt% calcium carbonate masterbatch to balance melt strength and puncture resistance at gauge ranges from 20 µm to 60 µm. The blown film process runs with die gap between 1.6 mm and 2.0 mm, a blow-up ratio from 2.0 to 2.5, and melt temperature between 180 °C and 210 °C. On high-output lines with internal bubble cooling, the film is collapsed and printed in-line for apron-style trash can liners. Compliance for EU exports is anchored to EU 94/62/EC Article 11, which limits the sum of lead, cadmium, mercury, and hexavalent chromium to ≤100 ppm by weight, and to the US CONEG model legislation with the same 100 ppm heavy-metal threshold for packaging. Terminal products include trash can liners, commercial bin liners, compost caddy liners, and recycled-content refuse sacks. The dart impact transition measured by ASTM D1709/D1709M shifts sharply when post-consumer recyclate exceeds 50 wt%; film tear strength measured by ASTM D1922 and seal strength under ASTM F88 also show greater batch-to-batch variance. Avoid increasing calcium carbonate above 10 wt% because the resulting film modulus rise and elongation reduction create splitting at side seals during bag conversion. Pre-drying of the recycled fraction is required if storage RH exceeds 60%, since moisture in the recyclate produces visible bubbles and reduces bubble stability at low melt temperatures.
Competitive Dow DOWLEX™ 2036G Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DOWLEX™ 2036G Linear Low Density Polyethylene is an ethylene–octene copolymer produced by a solution polymerisation route and supplied for blown-film extrusion. The resin is typically specified with a density of 0.920 g/cm³ and a melt index of 0.55 g/10 min measured at 190 °C under a 2.16 kg load in accordance with ASTM D792 and ASTM D1238. Typical supplier documentation lists a DSC melting point of 124 °C and a Vicat softening point of 98 °C. The grade is used in heavy-duty shipping sacks, industrial liners, agricultural silage film, frozen-food packaging, and carrier bags in which down-gauging, puncture resistance, and tear propagation resistance are required. Because the material is a linear low density polyethylene rather than a high-pressure branched low density polyethylene, the backbone is substantially linear and short-chain branching is introduced by octene incorporation; this combination reduces crystalline density while retaining tensile strength, but it also lowers melt tension during bubble inflation. The 0.55 g/10 min melt index places the product in the low-melt-index class for blown film, yielding higher bubble stability than a 1.0 g/10 min cast-film LLDPE at the cost of higher extruder drive load and melt pressure.
Compared with a general-purpose butene-based LLDPE in the same density range, the octene branch distribution in DOWLEX™ 2036G is generally understood to increase puncture resistance and dart impact at equivalent film thickness because the longer hexyl side chains disrupt crystal ordering more effectively than ethyl side chains. Relative to autoclave LDPE of similar density, the linear polymer has fewer long-chain branches and therefore stronger shear-thinning behaviour; however, elongational melt strength is lower, which can narrow the stable bubble window in high-stalk extrusion unless 10–30 wt% LDPE is blended. Relative to 0.941 g/cm³ high-density polyethylene, the lower density of 0.920 g/cm³ gives greater flexibility and lower modulus but lower continuous temperature resistance and lower creep resistance. The product therefore occupies a middle position: tougher than LDPE film at equivalent thickness, more flexible than HDPE, and more melt-strong than a 1.0 g/10 min LLDPE.
Within the 0.918–0.922 g/cm³ density band, LLDPE grades differ mainly in comonomer type, short-chain branching uniformity, molecular weight distribution, and melt index. DOWLEX™ 2036G is an octene-based resin manufactured in a solution polymerisation process, which typically yields a narrower molecular weight distribution and a more uniform comonomer distribution than gas-phase or slurry C4-LLDPE. The octene-derived side chains are longer than butene-derived side chains; this geometric difference reduces co-crystallisation and creates a tougher amorphous phase. The melt index of 0.55 g/10 min is deliberately lower than the 1.0–2.0 g/10 min melt index common in cast-film or high-output LLDPE, and this shifts performance toward bubble stability rather than throughput. The distinction is measurable on blown-film equipment: a lower melt index resin normally requires greater motor torque per kilogram and generates higher die pressure at a given screw speed. Published data for this specific grade on a named extruder are limited, but the trend is consistent with capillary rheometry of low-melt-index LLDPE. In addition, the resin differs from high-pressure LDPE in that long-chain branching is largely absent; this changes the slope of the viscosity-shear rate curve and reduces melt tension. A converter switching from LDPE to DOWLEX™ 2036G should therefore re-evaluate die gap, blow-up ratio, and frost-line height instead of retaining the existing LDPE processing set.
Batch-to-batch conformance data reported by converters typically follow the values in Table 1. These values are typical resin properties, not release limits; the certificate of analysis for a particular lot should be consulted for critical applications.
| Property | Typical value | Test method |
|---|---|---|
| Density at 23 °C | 0.920 g/cm³ | ASTM D792 |
| Melt index, 190 °C/2.16 kg | 0.55 g/10 min | ASTM D1238 |
| DSC melting point | 124 °C | ASTM D3418 |
| Vicat softening point | 98 °C | ASTM D1525 |
The density value places the product well below the 0.941 g/cm³ lower boundary for HDPE in many packaging specifications, while the melt index positions it among low-melt-index blown-film extrusion grades. Because the resin exhibits pronounced shear thinning, a single melt index value is insufficient for high-shear process design; capillary rheometry from 100 s-1 to 5,000 s-1 should be evaluated at the proposed melt temperature. The data in Table 1 do not define film tear, dart impact, or seal performance; those properties are determined by film structure, gauge, additive formulation, and processing history.
For blown-film conversion, a melt temperature between 190 °C and 230 °C is generally used. At the lower end of this range, unmelted polymer domains may remain in the die land when the extruder L/D is shorter than 24:1 or when a low-shear screw originally designed for LDPE is used. The resulting melt pressure increase reduces throughput, and haze bands or gauge variation can appear when the melt temperature drops below 185 °C. Industrial practice favours a 25:1–30:1 L/D single-screw extruder with a barrier screw and a dispersive mixing element. Die gaps from 1.6 mm to 2.5 mm are common; a 2.0 mm die gap balances die pressure and orientation. Blow-up ratios in the range 2.0:1–3.0:1 are typical, with frost-line height maintained between 6 and 12 die diameters. Where high-stalk bubble geometry is required, the lower melt tension of linear grades may limit stalk height unless 10–30 wt% LDPE is added. Processing set-points in production often range from 160 °C at the feed throat to 205 °C at the adapter, but these are equipment-specific and must be adjusted for screw design, throughput, and ambient cooling conditions.
Bubble instability in this resin class usually appears as periodic diameter oscillation at high haul-off speed. The 0.55 g/10 min melt index gives higher zero-shear viscosity than a 2.0 g/10 min LLDPE, which improves low-stalk bubble stability but makes the bubble more sensitive to frost-line variations when high output is attempted. If the frost-line height is raised above 12 die diameters without additional air-ring cooling, uneven crystallisation at the boundary layer can produce gauge bands of 5–10% variation. This is not a defect specific to DOWLEX™ 2036G; it is amplified by the low melt index and the high molecular weight fraction typical of octene-based solution LLDPE. Screen packs with 20/40/60/80 mesh are commonly used to improve gel dispersion, but a screen pack finer than 80 mesh may excessively restrict output and raise melt temperature on a low-melt-index grade.
Film evaluations at 50 µm thickness on a 60 mm blown-film line with 30:1 L/D, 2.0 mm die gap, 2.5:1 blow-up ratio, and 205 °C melt temperature generally show a combination of high machine-direction Elmendorf tear and high dart impact relative to a 0.920 g/cm³ C4-LLDPE. Final values are equipment- and formulation-dependent; they should be measured on the actual line according to ASTM D1922 and ASTM D1709. The resin has found use in heavy-duty sacks where a 10–15% down-gauge relative to conventional LDPE is needed while preserving drop strength. In agricultural silage film, the octene comonomer improves puncture resistance against stalks; however, the 0.55 g/10 min melt index may require a higher melt temperature than a 1.0 g/10 min LLDPE to achieve consistent web formation at high speed. For long-term outdoor exposure, a suitable UV stabiliser package is required; the unmodified resin is not formulated for multi-season outdoor weathering. For frozen-food packaging, low-temperature toughness is commonly evaluated at -18 °C using a dart impact test or by measuring tensile elongation after conditioning; converters should determine minimum film thickness from the required dart impact and seal strength rather than extrapolating from standard LLDPE datasheets. Heat-seal strength and hot tack are measured on the finished film with ASTM F1921 or equivalent, while seal strength is commonly measured according to ASTM F88; the seal window shifts with thickness, additive package, and seal-bar dwell time, so pellet-level data do not define the usable packaging line settings.
For food-contact applications, the raw resin is generally positioned within the polyethylene class covered by FDA 21 CFR 177.1520(c); however, the finished article must comply with the applicable conditions of use and migration limits. The current manufacturer’s regulatory bulletin should be reviewed before commercial use. In the European Union, food-contact compliance is assessed under Regulation (EU) No 10/2011; specific migration testing is required on the final package, not on the pellet. The product does not normally contain phthalate plasticizers, flame-retardant additives, or heavy-metal pigments, but a finished-article RoHS declaration cannot be assumed without reviewing the complete formulation, including colorants and masterbatch. For potable water contact, NSF/ANSI 61 certification is article- and formulation-specific; a raw resin datasheet does not confer certification.
Storage conditions affect processing. Pellets should be kept in a dry, dust-free environment and protected from direct UV exposure. Moisture adsorption is not a major concern for polyethylene, but condensation on cold pellet surfaces can cause feeding irregularities and surface splay. If condensation has occurred, pre-drying at 70–80 °C for 2–3 hours can be used. Melt temperature should not exceed 240 °C during extended residence times, because oxidative degradation can generate gels, odour, and discolouration. The resin should not be processed in equipment that previously ran highly polar or halogenated polymers without thorough purging; incompatible residues may cause delamination or odour. When recycled edge trim is added, the trim ratio should be controlled and dispersive mixing should be sufficient to prevent gel accumulation in the die. Prolonged storage above 40 °C may cause pellet agglomeration in bulk silos and should be avoided.
This grade is not intended for injection moulding of thin-wall articles without verification. The low melt index of 0.55 g/10 min can produce excessive pressure drop in narrow flow paths and may lead to short shots in high-cavitation moulds. In extrusion coating and cast-film processes where low-viscosity high-melt-index LLDPE is normally specified, DOWLEX™ 2036G may not deliver the required drawdown at high line speed. The suitability of the resin for any given application should be established by the converter on the target line, using the relevant ASTM method for the end-use property.