| HS Code | 453541 |
| Density | 0.935 g/cm³ |
| Melt Index 190 C 2 16 Kg | 2.5 g/10 min |
| Melting Point | 124 °C |
| Vicat Softening Point | 111 °C |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 800 % |
| 1 Secant Modulus | 260 MPa |
| Film Haze | 4 % |
| Film Gloss 45 | 85 |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 500 g |
| Puncture Resistance | 60 J/cm |
| Coefficient Of Friction | 0.2 |
As an accredited Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow DOWLEX 2036A is supplied in 25 kg polyethylene bags, palletized, and optionally 1,000 kg bulk bags for shipment. |
| Container Loading (20′ FCL) | 20′ FCL: about 18 metric tons of DOWLEX™ 2036A LLDPE in 25 kg bags, typically 18 pallets, double-stacked and shrink-wrapped. |
| Shipping | DOWLEX™ 2036A is a non-hazardous LLDPE cast film resin supplied as solid pellets. Standard shipping: 25 kg polyethylene bags stacked on 1,000 kg stretch-wrapped pallets, or bulk trucks/railcars. Store in a cool, dry, ventilated area away from direct sunlight and ignition sources. |
| Storage | Store DOW DOWLEX™ 2036A in original packaging in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep bags/containers closed and off the floor to prevent moisture, dust, and contamination. Avoid excessive stacking and prolonged high temperatures. Use first-in, first-out stock rotation. Protect from UV exposure and odorous materials. Ensure good ventilation. Inspect regularly. |
| Shelf Life | Stable; no defined shelf life when stored cool, dry, in original sealed packaging, protected from direct sunlight and contamination. |
DOWLEX 2036A is processed as the core resin in coextruded cast stretch film for pallet unitization. On production-scale cast film lines equipped with 90–150 mm single-screw extruders, 30:1 L/D barrier screws, 2,500–3,500 mm coat-hanger dies, 0.5–0.8 mm die gaps, and chill-roll units maintained at 15–25 °C, the resin is typically melt-cast at 240–265 °C. The nominal density of 0.936 g/cm³ per ASTM D792 and a melt index of 2.5 g/10 min per ASTM D1238 at 190 °C under 2.16 kg load place DOWLEX 2036A in a range that balances drawability with low melt-temperature neck-in. Industrial film structures usually place DOWLEX 2036A in the core layer at 70–85 wt%, while the skin layers contain 5–15 wt% of an ultra-low density ethylene-octene plastomer or a low molecular weight polyisobutylene cling additive at 2–4 wt%. Total film thickness ranges from 12 µm to 35 µm, with the core layer occupying 50–70% of the cross-section. Mechanical evaluation follows ASTM D882 for tensile properties, ASTM D1709A for falling dart impact, ASTM D5748 for puncture resistance, and ASTM D5458 for cling. A 20 µm three-layer web based on DOWLEX 2036A typically exhibits machine-direction elongation at break between 350% and 550%, puncture resistance between 2.5 N and 4.5 N per ASTM D5748 for 23 µm film, and dart drop impact between 120 g and 200 g per ASTM D1709A. These values support pre-stretch ratios up to 300% on powered pre-stretch carriages. The cling layer must retain measurable cling force above 100 g per 25 mm strip after 24 h unwinding, measured per ASTM D5458, otherwise pallet load containment fails under transport vibration.
Powered pre-stretch equipment accelerates the film between two counter-rotating rollers; an upstream roll speed of 40 m/min and a downstream roll speed of 120 m/min produce a 3.0:1 pre-stretch ratio. The critical process window emerges above 250% pre-stretch, where retained machine-direction elongation becomes the limiting variable. At 250% pre-stretch, film exiting the pre-stretch unit typically retains 150–220% residual elongation; at 350% pre-stretch, residual elongation drops below 60% in some edge zones, producing catastrophic neck-in or film failure during wrap head acceleration. Neck-in measured at the die-to-chill-roll air gap of 100–150 mm is usually 70–110 mm for 0.7 mm lip opening at 2,500 mm die width. If line speed exceeds 650 m/min, edge draw resonance can create transverse thickness bands with amplitude above 5% of nominal thickness, as detected by online capacitance gauges. This defect is distinct from melt fracture and cannot be corrected by raising melt temperature, because melt temperatures above 285 °C accelerate oxidative gel formation and degrade cling additive performance. Processing at melt temperatures below 230 °C reduces gel formation but increases die lip build-up and causes poor molten film transfer to the chill roll. Edge trim levels of 6–12 wt% are typical; reprocessing more than 10 wt% edge trim in the core extruder without 150–250 µm melt filtration raises gel count and decreases puncture force by 10–20% per ASTM D5748. Roller stretch wrappers report film breaks when residual elongation falls below 40% at the wrap head, particularly on loads with sharp corners or uneven top boards.
In flexible packaging structures, DOWLEX 2036A serves as a 15–35 µm sealant layer in extrusion lamination to aluminium foil, metallised biaxially oriented polyethylene terephthalate, or reverse-printed biaxially oriented polypropylene. On extrusion laminators using a 90 mm single-screw extruder with 30:1 L/D, melt temperature is held at 240–275 °C; the web is cast through a 300–500 mm slot die onto a corona-treated substrate at an air gap of 80–150 mm. Substrate surface energy above 42 mN/m is verified by ASTM D2578 before the melt curtain contacts the substrate. Heat seal strength is assessed by ASTM F88 on 25 mm wide specimens with a 0.5 s dwell and 2.75 bar jaw pressure. For a 30 µm sealant web of this density class, a seal strength of 4 N/15 mm is usually achieved between 100 °C and 115 °C; below 90 °C, seal strength frequently remains below 1 N/15 mm, which is insufficient for vertical form-fill-seal lines running above 40 packages/min. Hot tack performance, measured by ASTM F1921, reaches a usable plateau above 3 N/15 mm at 105 °C; below that temperature, spring-back opens the seal before the web cools. Sealant formulations typically incorporate erucamide at 1,000–3,000 ppm and synthetic silica antiblock at 1,500–3,500 ppm. Increasing the silica above 4,000 ppm reduces kinetic coefficient of friction below 0.25 per ASTM D1894 but also decreases seal strength at 110 °C by more than 10% and raises haze above 7% per ASTM D1003. Chill-roll temperature during cast lamination is maintained at 15–25 °C; if the chill roll exceeds 35 °C, the low-density layer blocks during winding, and if it falls below 10 °C, slip additive migration to the surface is retarded, delaying stable coefficient of friction for up to 72 h.
| Jurisdiction | Reference | Verification condition |
|---|---|---|
| United States | 21 CFR 177.1520 | Olefin polymer specification, use conditions up to 121 °C for aqueous food; extractive limits per paragraph (c) |
| European Union | EU No 10/2011 Annex I | Overall migration <10 mg/dm² by EN 1186-1; specific migration limits for slip and antiblock additives as listed |
| European Union | EC No 1935/2004 | Article 3 good manufacturing practice; no transfer to food in unacceptable quantities |
| European Union | EC No 2023/2006 | GMP for materials and articles; document control for additive dosing |
| REACH | Regulation (EC) No 1907/2006, Annex XVII | No restricted phthalates or SVHC above 0.1 wt% |
That question governs structure design when DOWLEX 2036A is used as the sealing web in 25–50 µm lidding films for frozen vegetables, ready meals, and ice cream. The film must open at low seal-roll temperature because the packaging line speed is fixed by the heat-transfer rate through the seal bar; a reduction in seal initiation temperature from 100 °C to 85 °C can increase output by 15–25% on horizontal form-fill-seal equipment. Frozen lidding structures based on this grade are tested for cold-temperature impact at −20 °C using ASTM D1709A, and typical acceptance limits fall between 80 g and 160 g for 30 µm film. Haze measured by ASTM D1003 is held below 5% for top-lidding visibility; gloss at 60° per ASTM D2457 usually remains above 70 units. Anti-fog additives such as glycerol monostearate are added at 3,000–8,000 ppm, but their migration requires an amorphous surface layer. A chill-roll temperature of 15–20 °C suppresses migration and can delay anti-fog performance by 24–48 h, while a chill-roll temperature above 25 °C accelerates migration but may create plate-out on the casting roll and die lip. Moisture vapour transmission rate of a 30 µm film is typically 1.5–2.5 g/m²·day per ASTM F1249, and oxygen transmission rate is 2,000–3,500 cm³/m²·day·atm per ASTM D3985. These barrier values limit shelf life for high-fat frozen items to a few months, but remain acceptable when combined with a vacuum or modified-atmosphere outer pouch.
| Property | Test method | Acceptance range |
|---|---|---|
| Haze | ASTM D1003 | <5% |
| Dart impact at −20 °C | ASTM D1709A | 80–160 g |
| MD Elmendorf tear | ASTM D1922 | 150–350 g |
| Seal strength at 110 °C | ASTM F88 | 3.0–6.0 N/15 mm |
| WVTR at 38 °C, 90% RH | ASTM F1249 | 1.5–2.5 g/m²·day |
Converting DOWLEX 2036A into hygiene backsheet and wing films at 15–25 µm requires balancing softness, pinhole resistance, and stable high-speed web handling. Cast film lines for hygiene use the same quench-roll configuration but operate with dielectric or air-knife pinning systems because the melt curtain is thinner and more sensitive to air turbulence. Chill-roll temperatures of 18–25 °C produce a contact surface with acceptable slip and reduce blocking tendency during winding at roll diameters above 600 mm; if the chill roll is heated above 30 °C, the film softens and blocking at the core becomes statistically detectable after 24 h storage at 23 °C. Dart drop impact for a 20 µm hygiene backsheet film is commonly specified between 80 g and 150 g per ASTM D1709A, and Elmendorf tear resistance measured per ASTM D1922 falls between 150 g and 350 g in the machine direction. For lamination to polypropylene nonwovens, the film is corona-treated to 38–42 mN/m per ASTM D2578 and coated with hot-melt adhesive at 1–3 g/m². Slip additive loadings above 2,000 ppm can reduce adhesive anchorage below acceptable shear strength, measured as laminate bond strength below 1 N/25 mm per ASTM D903. On diaper lines running at 400–600 m/min, thickness variation above ±3% creates edge wrinkle and web wander at guide rolls; online thickness gauges with 1 mm transverse resolution are used to keep gauge variation within ±2%.
Agricultural bale-wrap film based on DOWLEX 2036A is produced at 25–30 µm thickness and applied in 6–8 overlapping layers on round bales. The cast film is specified for puncture resistance per ASTM D5748, with acceptance thresholds of 3.0–5.0 J for 25 µm film, and Elmendorf tear resistance per ASTM D1922 above 200 g in both machine and transverse directions. Because LLDPE has limited oxygen barrier, oxygen transmission rate at 25 µm is typically 2,000–3,000 cm³/m²·day·atm per ASTM D3985; the multi-layer wrap geometry reduces the effective transport area rather than increasing the intrinsic barrier. Water vapor transmission rate is relatively low at 1.0–2.0 g/m²·day per ASTM F1249, which assists moisture retention in silage. Film for this application usually contains hindered amine light stabilizers at 1,000–2,500 ppm and a UV absorber at 500–1,500 ppm; without these packages, tensile elongation at break after 1,000 h in accelerated xenon-arc weathering per ASTM G155 can decline by more than 50%. The major processing constraint is edge fold formation during winding on 3,000 mm wide cast film lines; winding tension above 25 N/m at the core end creates edge wrinkles that propagate into tears during bale application. Published data for this specific DOWLEX 2036A silage-wrap configuration is limited; industrial practice relies on comparative puncture and weathering data from similar octene-LLDPE cast film grades.
For industrial containment liners and surface-protection films, DOWLEX 2036A is extruded at 40–120 µm thickness on cast film lines with 2,000–3,000 mm die widths. The heavy-duty liners require puncture resistance measured per ASTM D4833 or ASTM D5748, and typical acceptance limits for 100 µm film are 300–600 g dart impact per ASTM D1709A and 600–1,200 g Elmendorf tear per ASTM D1922. When a 2–5 wt% carbon black or color masterbatch is added, dart impact can decrease by 10–25% if the masterbatch carrier polymer has poor compatibility with octene-LLDPE; concentrates based on low molecular weight polyethylene and finely ground pigments below 2 µm primary particle size minimize this loss. The film is usually corona-treated to 40–44 mN/m per ASTM D2578 before adhesive lamination or printing; wetting tension below 36 mN/m produces adhesive skip defects visible as uncoated spots under UV inspection.
Temporary surface protection of stainless steel, powder-coated appliance panels, and glass sheets uses DOWLEX 2036A films in the 40–80 µm thickness range. The cast film is coated with a low-tack acrylic or rubber-based pressure-sensitive adhesive at 5–15 g/m², and release is controlled to 0.5–3.0 N/25 mm per ASTM D3330. A critical failure mode is adhesive transfer after 28 days of outdoor ageing; this is monitored by accelerated weathering per ASTM G155 followed by peel testing per ASTM D3330. The polyethylene substrate must retain elongation above 300% per ASTM D882 during die-cutting and removal without tearing. Corona treatment above 40 mN/m per ASTM D2578 is required for anchorage of the adhesive; below this level, cohesive failure within the bond line is common. Because these films are typically not primary food-contact packaging, compliance is assessed instead under REACH and RoHS for heavy metals, with lead and mercury below 100 mg/kg and cadmium below 100 mg/kg in the colored variants.
Competitive Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DOWLEX™ 2036A Linear Low Density Polyethylene is a cast film extrusion grade supplied as free-flowing pellets and classified within the DOWLEX family of ethylene-octene copolymers. The resin is intended for cast film processes where a balance of stiffness, tear resistance, optical clarity, and drawdown stability is required. Manufacturer’s published typical resin values include a density of 0.936 g/cm³ measured in accordance with ASTM D792/ISO 1183-1 and a melt index of 2.5 g/10 min at 190 °C/2.16 kg per ASTM D1238/ISO 1133-1:2022. These values place the material in the upper density range of linear low density polyethylene, which differentiates it from blown film grades such as DOWLEX 2045G that are specified at a lower density and higher melt strength. The cast film designation indicates that the polymer is stabilized for the rapid quench and high take-off speeds of chill-roll cast film lines rather than for air-cooled blown film extrusion. Typical end uses include industrial liners, lamination films, overwrap, and food packaging structures where higher modulus and controlled elongation provide dimensional stability.
| Property | Typical value | Test method |
|---|---|---|
| Density | 0.936 g/cm³ | ASTM D792 / ISO 1183-1 |
| Melt index | 2.5 g/10 min | ASTM D1238 / ISO 1133-1:2022 |
| Vicat softening point | 118 °C | ASTM D1525 / ISO 306 |
| Melting point (DSC) | 123 °C | ASTM D3418 / ISO 11357-3 |
| Tensile stress at yield (25 µm, MD/TD) | 16 MPa / 15 MPa | ASTM D882 |
| Elongation at break (25 µm, MD/TD) | 600 % / 700 % | ASTM D882 |
| Secant modulus at 1 % (25 µm, MD/TD) | 220 MPa / 240 MPa | ASTM D882 |
| Dart drop impact F50 (25 µm) | 150 g | ASTM D1709A |
| Elmendorf tear (25 µm, MD/TD) | 80 g / 120 g | ASTM D1922 |
| Haze (25 µm) | 2.5 % | ASTM D1003 |
| Gloss 45° (25 µm) | 85 | ASTM D2457 |
Values are nominal and are not specification limits. Film data were generated on a 90 mm single-screw cast film line with 30:1 L/D, 250 mm flat die, 0.8 mm die gap, 25 °C chill-roll temperature, and 25 µm gauge. Comparative data should be obtained under the intended film gauge and line speed because quench rate and draw ratio alter tear balance and haze.
The octene comonomer distribution in DOWLEX 2036A increases tie-chain formation relative to butene-based LLDPE of equivalent density and melt index, which is observed as higher Elmendorf tear strength and dart drop impact when tested per ASTM D1922 and ASTM D1709A. Direct published comparative data for all film structures is limited; however, manufacturer resin property ranges show that replacing a butene-copolymer cast film grade with DOWLEX 2036A typically shifts the MD/TD tear balance toward higher TD tear while retaining sufficient stiffness for die-cut labels and industrial liners. The narrow molecular weight distribution of DOWLEX 2036A, typical of DOWLEX cast film grades, also improves drawdown on high-speed cast film die assemblies compared with broader-distribution autoclave low density polyethylene.
DOWLEX 2036A is specified for cast film, while DOWLEX 2045G is a blown film grade with lower density and different melt strength. The cast film designation determines stabilization level, pellet handling, and recommended die gap settings rather than simply film gauge. On a 75 mm single-screw cast line with 30:1 L/D, DOWLEX 2036A allows chill-roll temperatures between 20 °C and 40 °C without the excessive roll sticking that can occur with lower-density blown film grades when converted on cast equipment. Compared with metallocene-catalysed cast film resins, DOWLEX 2036A has a broader composition distribution, which reduces the shear stress sensitivity that can produce melt fracture at high throughput. Metallocene grades often require lower melt temperatures and optimized screw geometry to avoid melt fracture; DOWLEX 2036A can be processed on conventional single-screw cast lines with barrier screws and 30:1 L/D. The trade-off is that metallocene grades may offer lower seal initiation temperatures or lower extractables in certain food-contact uses, so converter selection must balance sealant performance against process stability.
On a cast film line configured with a 90 mm single-screw extruder with 30:1 L/D and a barrier feed section, DOWLEX 2036A is processed with barrel set points from 180 °C at the feed throat to 250 °C at the adapter, with melt temperature measured at the die between 240 °C and 270 °C. The flat die is typically set to a die gap of 0.75 mm to 1.0 mm for gauges between 15 µm and 50 µm. Chill-roll temperatures of 20 °C to 40 °C are used to control quench rate and minimize haze without excessive crystallization that can reduce dart impact. The resin’s melt index of 2.5 g/10 min allows take-off speeds from 120 m/min to 200 m/min on standard equipment, but the actual ceiling is limited by edge encapsulation, air knife positioning, and polymer flexibility after the chill roll. Excessive melt temperatures above 290 °C should be avoided because oxidative chain scission can generate gel particles detectable by optical film inspection per ASTM D6988 and reduce heat seal strength when tested per ASTM F88. Extruder back pressure is typically between 15 MPa and 25 MPa depending on screen pack arrangement; a 60/100/60 mesh screen pack is commonly used to protect the die from contamination.
High line speed operation changes the balance between optical properties and impact strength because the film undergoes uniaxial orientation before it is quenched. If a converter runs the same die gap at 200 m/min, the MD draw ratio can exceed 50:1, which increases MD orientation and reduces MD tear while potentially lowering dart impact relative to a 50 m/min line. The reduction in dart impact can be quantified by ASTM D1709A, while haze is measured per ASTM D1003. Gloss measured per ASTM D2457 is highly sensitive to chill-roll surface finish; a polished roll maintained below 0.05 µm Ra surface roughness is required to retain gloss above 80. When masterbatches containing slip and antiblocking agents are added, the total additive concentration should not exceed supplier-recommended levels because excess migratory additives increase surface haze and reduce surface tension below the 38 mN/m to 42 mN/m range required for corona-treated lamination and printing, as measured per ASTM D2578.
For direct food-contact applications, manufacturer product stewardship documentation lists compliance statements for FDA 21 CFR 177.1520 for olefin polymers and, for the European Union, Regulation (EU) No 10/2011 as amended, provided the final article meets overall migration and specific migration limits. Because DOWLEX 2036A is supplied as a base resin without colorants, processing aids, or antistatic compounds, end-users must verify that all added masterbatches and converting aids do not alter the migration profile. Heat seal strength of lamination films made from DOWLEX 2036A should be tested per ASTM F88 after converting, because seal initiation temperature is affected by film density, thickness, and corona treatment level. Published data for this specific configuration is limited; inline seal testing is required to establish a production window.
| Requirement | Applicable standard or regulation | Status |
|---|---|---|
| Olefin polymer food-contact clearance | FDA 21 CFR 177.1520 | Manufacturer statement available; end-use limitations apply |
| EU food-contact plastics | Regulation (EU) No 10/2011 | Compliance requires migration testing of final article |
| REACH registration | EC 1907/2006 | Registered by supplier; no SVHC above 0.1 % w/w by declaration |
| RoHS heavy metal restrictions | Directive 2011/65/EU | Not intentionally added; bulk polymer typically conforms |
In industrial stretch hood and cast overwrap lines, DOWLEX 2036A is frequently processed at film gauges from 25 µm to 80 µm where high puncture resistance and stiffness reduce film sag on pallet loads. Puncture resistance is characterized by ASTM D5748, and the resin’s higher density relative to conventional stretch film LLDPE increases the force required for puncture at equivalent gauge. Because the polymer does not contain cling additives as supplied, cast film producers add polyisobutylene or ultra-low density polyethylene cling masterbatches in the outer layer of three-layer coextruded structures to control unwind and shelf-load stability. The performance of such structures depends on the layer ratio and the migration behavior of the cling additive; no single cling level can be specified without a full three-layer design.
Polyethylene degradation in cast film extrusion is a function of residence time, melt temperature, and oxygen ingress. Published thermogravimetric analysis data for polyethylene under inert atmosphere generally show degradation onset above 350 °C; this is not an acceptable processing temperature because degradation begins earlier in the presence of dissolved oxygen and at long residence times. Melt temperature should be maintained below 290 °C, and screw speed should be selected to avoid more than 8 min residence time at high temperature. Frequent purging with a purging compound having a lower melt flow is recommended after shutdowns exceeding 30 min to prevent oxidized gel contamination. Black specks and fish eyes can be counted per ASTM D6988 and are direct indicators of thermal degradation or additive dispersion failure. The polymer should be kept dry before processing; while polyethylene is not hydrolytically degraded, surface condensation on pellets stored at RH > 60 % can carry water into the melt and produce steam-induced film defects.
Cast film converters running three-layer coextrusion structures commonly use DOWLEX 2036A as the core or stiffness layer, with lower-density polyethylene skin layers selected for sealing or cling performance. In such structures, the melt temperature of DOWLEX 2036A should still be constrained within the 240 °C to 270 °C range at the die to avoid viscosity mismatch that can produce interfacial flow instabilities. The viscosity mismatch between layers is assessed by comparing melt flow ratios and apparent shear viscosity on a capillary rheometer per ISO 11443. If the core layer viscosity is too low relative to the skin layer, layer inversion and gauge variation can occur at the die exit; if too high, the skin layer may not wet the chill roll uniformly. Periodic measurement of film thickness profile with a scanning beta gauge and subsequent adjustment of die bolt temperatures are required to maintain thickness tolerances of ±2 % on 25 µm gauge.