Dow Dowlex 2035 Linear Low Density Polyethylene Cast Film Grade

Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade

    • Product Name: Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 373892
    Density 0.919 g/cm³
    Melt Index 2.0 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 94 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 700%
    1 Secant Modulus 200 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 400 g
    Haze 4%
    Gloss 45 80
    Coefficient Of Friction 0.2

    As an accredited Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing DOWLEX™ 2035 is supplied in 25 kg polyethylene bags, 40 bags per pallet, totaling 1,000 kg.
    Container Loading (20′ FCL) 20-foot FCL loaded with palletized 25 kg bags of Dow DOWLEX™ 2035 LLDPE cast film grade, stretch-wrapped and secured.
    Shipping DOWLEX 2035 LLDPE cast film grade ships as nonhazardous polyethylene pellets, typically in 25 kg bags on pallets or in bulk trucks/railcars. Keep packaging dry, intact, and clean; avoid heat, moisture, and contamination. No DOT/IMDG special shipping classification—follow local rules and Dow’s SDS.
    Storage Store DOWLEX™ 2035 Linear Low Density Polyethylene in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep containers tightly closed to prevent moisture and contamination. Avoid contact with strong oxidizing agents. Maintain normal ambient temperatures; protect from UV exposure. Follow manufacturer's SDS and local regulations for safe handling and storage.
    Shelf Life DOWLEX 2035 has no defined shelf life; store properly cool, dry, sealed, away from direct sunlight and ignition sources.
    Application of Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade

    In pallet unitization film between 20 µm and 25 µm, the dominant cast film extrusion constraint is the interaction between neck-in and transverse orientation. DOWLEX™ 2035 is processed on conventional cast film lines with a 90 mm single-screw extruder at an L/D of 30:1, using a barrier screw with a Maddock mixing section to maintain melt temperature uniformity. The melt temperature at the die exit is normally held between 240°C and 260°C, with a coat-hanger die gap of 0.8 mm to 1.0 mm for monolayer pallet wrap. Under these conditions, neck-in is typically observed at 2% to 4% per side, and edge trim is maintained below 8% of total web width. The web is pinned to a matte-finish chill roll at 18°C to 25°C using an air knife and a vacuum box in sequence, because edge lift on the chill roll produces gauge bands that transfer directly into stretch force variation downstream. Stretch force at 200% elongation is evaluated per ASTM D5459, but for pallet wrap the more practical measurement is wrap force retention on a rotary stretch wrapper. The film must retain sufficient elastic recovery after 200% pre-stretch without inducing load shift on a pallet. Blends are typically formulated with 70 wt% to 85 wt% DOWLEX™ 2035, 10 wt% to 20 wt% metallocene polyethylene for dart impact improvement, and 3 wt% to 6 wt% cling masterbatch. Slip and antiblock packages are kept low, usually below 1.5 wt%, because excessive erucamide migration reduces the cling force below the minimum safe level for a 15 kg hand-wrap roll. The main process conflict is that raising chill roll temperature to improve cling surface smoothness reduces the cooling rate and increases film blocking on the roll. Conversely, lowering chill roll temperature to 10°C prevents blocking but raises haze and reduces the conformability of the film on irregular pallet corners. Batch-to-batch variance in tackifier melt flow can produce cling force swings from 0.8 N to 1.6 N per 50 mm width when measured against a steel plate at 23°C. For high-speed automatic wrappers, the film must maintain a coefficient of friction below 0.25 on the unwind side, measured per ASTM D1894, while the cling side must remain above 0.40 against an identical film surface. This asymmetry is achieved by differential chill roll surface finish and a kiss-roll application of cling promoter rather than by increasing the bulk tackifier concentration. On production lines, the most frequent failure is not film break but unwind telescoping caused by insufficient edge trim removal before the winder. Edge beads exceeding 3 µm over nominal thickness lead to roll deformation within 4 h to 6 h of winding at 600 m/min line speed.

    For stretch hood applications, the same cast film construction is converted into heavier gauge sheet from 60 µm to 100 µm, where the limiting parameter shifts from cling force to tear initiation resistance. Elmendorf tear is measured per ASTM D1922, and industrial stretch hood film requires machine-direction tear values above 12 g/µm in the orientation direction. DOWLEX™ 2035 retains sufficient melt strength for the lower draw ratios used in thick gauge cast film, but die lip deposit from reused edge trim is a recurring bottleneck. Trim containing cling masterbatch and oxidized polymer is reintroduced at 10% to 20% reclaim content. At reclaim levels above 25%, film clarity declines and the number of gel particles larger than 200 µm increases, causing machine-direction streaks. A continuous melt filter with 100 µm to 150 µm screen pack is required. The upper reclaim limit for stretch hood is constrained not by gel count but by the reduction in cling force after repeated heat history. Each pass through the extruder degrades the tackifier domain, and at more than 20% reclaim the tackifier must be refreshed by an additional 1.0 wt% to 1.5 wt% cling masterbatch. Without this refresh, the film fails to hold a palletized load during transport on a truck trailer because the cling force drops below 0.5 N/50 mm after repeated vibration. Reverse-roll gravure application of cling agent to the outer surface is an alternative used to decouple the cling property from the bulk film formulation, but it requires an additional drying section and is not common on high-speed cast film lines producing thin pallet wrap.

    Why Does Chill-Roll Temperature Govern Haze Below 4% in Produce Overwrap?

    In direct food-contact produce overwrap, the cast film is converted at 18 µm to 23 µm, and the primary visual requirement is a haze value below 4% measured per ASTM D1003. Haze development in cast LLDPE is controlled less by the polymer itself and more by the quench rate and the surface replication of the chill roll. The DOWLEX™ 2035 resin has a broad short-chain branching distribution typical of the DOWLEX™ product family, which suppresses spherulite growth compared with a homopolymer. On a fast quench line, the polymer is extruded at 250°C and brought into contact with a polished chill roll at 20°C to 30°C within an air gap of 25 mm to 40 mm. The air gap itself must be minimized, because long air-gap residence gives the melt surface time to oxidize and develop a rough skin layer. The critical threshold is a quench temperature differential of approximately 220°C between melt and roll surface. If the chill roll surface temperature drifts above 32°C, the cooling rate is insufficient to pin the amorphous fraction before large crystallites form, and haze increases by 2% to 3% in the final film. Below 12°C, moisture condensation on the roll surface creates pits and optical defects that cannot be removed by downstream orientation. The process window of 12°C to 32°C is therefore narrow, and closed-loop chiller control with ±1°C stability is mandatory on high-clarity grades.

    The film formulation for produce overwrap includes a slip agent such as erucamide at 800 ppm to 1,500 ppm and an antiblock such as synthetic silica at 2,000 ppm to 4,000 ppm. These loadings are lower than those used in blown film because the cast process orients the film primarily in the machine direction and produces a smoother surface for a given slip package. Coefficient of friction after 72 h of migration is measured at 0.10 to 0.20 kinetic, per ASTM D1894. The migration time is critical: films packed immediately after slitting often exhibit blocking because the slip agent has not yet migrated to the surface. A 24 h to 72 h curing period at 23°C to 30°C is required before the film can be wound into converter rolls. This curing requirement is a production scheduling bottleneck, not a polymer limitation. For food contact status, the finished film must comply with FDA 21 CFR 177.1520 for olefin polymers and, in the European Union, with Commission Regulation EU 10/2011. Overall migration limits are specified as 10 mg/dm² of food contact surface area. The antioxidants and slip additives used in DOWLEX™ 2035 formulations must be selected from positive lists with specific migration limits, and converter declarations must state the additive package. Without this documentation, the film is not accepted for direct produce contact in retail wet markets, where fatty or acidic food surfaces can extract low molecular weight species from the polymer matrix.

    Standard or RegulationMethod or ClauseMeasured Parameter
    FDA 21 CFR 177.1520Olefin polymers, end-test complianceFood contact status for LLDPE cast film
    EU 10/2011Overall migration testing per food simulant10 mg/dm² maximum
    ASTM D1003-21Haze measurement, illuminant C<4% for produce overwrap
    ASTM D1894-14Kinetic coefficient of friction0.10 to 0.20
    ASTM D2578-23Wetting tension of polyethylene film≥38 mN/m after corona treatment

    Corona treatment for produce overwrap is applied at 1.5 kW to 2.5 kW discharge power on a single-side treater, producing a wetting tension of 38 mN/m to 42 mN/m measured at 23°C. The treated surface decays over time due to migration of slip additives, so treatment must be performed in-line immediately before winding. A treated film stored for more than 30 days at ambient temperature can fall below 36 mN/m, which is insufficient for reliable print adhesion in converter operations. The film is printed using flexographic or rotogravure presses with solvent-based inks, and the cast surface provides a consistent roughness for ink transfer. However, the presence of erucamide reduces ink adhesion on the treated surface, and converters often specify a slip-free outer skin or a coextruded layer with a different additive package. In monolayer produce overwrap, the trade-off between slip migration and print adhesion is unresolved: reducing slip to improve printability raises reel breakage during high-speed form-fill-seal conversion. The typical compromise is a two-stage slitting process that applies corona treatment after the film has already been slit and aged for 48 h, but this adds a second unwind-wind cycle and increases film handling defects.

    Lamination Sealant Webs Cannot Tolerate Gel Counts Above 10 Particles per 100 cm²

    As a sealant web in multi-layer flexible packaging, cast film produced from DOWLEX™ 2035 is down-gauged to 25 µm to 50 µm and laminated to biaxially oriented polyester or biaxially oriented polypropylene. The sealant function requires a low seal initiation temperature, high hot-tack strength, and a gel-free surface that does not disrupt the adhesive bond. Seal initiation temperature for this density class is measured per ASTM F1921, and the target is usually below 115°C. The broad molecular weight distribution of DOWLEX™ 2035 contributes to a lower seal initiation temperature than a mLLDPE of similar density, but the difference is small. The more important variable in cast lamination grade film is the absence of oxidized gel particles, because gel particles above 200 µm create adhesive voids and channels through which the packaged product can penetrate the laminate structure. The specification for high-barrier laminated pouches is often fewer than 10 gel particles larger than 200 µm per 100 cm². This is not a food-contact migration limit but a converter defect criterion based on leak-test failure.

    The cast film line for lamination sealant is run with a deeper melt filtration setup than standard film operations. A primary screen pack of 60/80/100 mesh is followed by a second-stage continuous melt filter with 80 µm candle elements. The additional back pressure raises melt temperature by 3°C to 5°C, which must be compensated by lowering barrel zone set temperatures. If barrel temperatures are not reduced, the polymer undergoes oxidative crosslinking and generates new gel particles in the filtration system, defeating the purpose of the filter. The die gap is set at 0.7 mm for a 40 µm final film and the draw ratio is kept below 20:1 to minimize machine-direction orientation. Excessive orientation in the cast film creates a seal-strength anisotropy: the seal fails in the cross direction at 80% of the machine-direction seal strength because the molecular chains are aligned in the machine direction. Seal strength is measured per ASTM F88/F88M-21 after sealing at 130°C, 0.28 MPa jaw pressure, and 0.5 s dwell time. The minimum acceptable seal strength for a 40 µm sealant web is 2.5 N/15 mm, and the mode of failure must be interfacial peel rather than film tear. A film tear mode indicates that the sealant layer is too strongly bonded or that the film itself is too thin, while an interfacial peel mode confirms that the seal can open at the intended interface without fracturing the film.

    The lamination adhesive is applied to the cast film surface after corona treatment at 38 mN/m to 40 mN/m. Solventless polyurethane adhesives require a wetting tension above 36 mN/m at the point of application, but the treated surface decays quickly due to internal slip additive migration. For lamination applications, the slip additive level is therefore kept below 600 ppm to preserve dyne level during the lamination step. In the absence of slip, the cast film surface has a high coefficient of friction, and the film cannot be easily unwound from the laminator. The converter must use a back-side matte chill roll to impart a rough surface on the non-sealant side, which reduces blocking without the need for high slip additive content. The surface roughness is measured as Ra 0.4 µm to 0.8 µm by contact profilometry. Too rough a surface on the sealant side reduces the visual clarity of the final laminate, while too smooth a surface creates blocking and web tracking failure. The chill roll is therefore specified with a mirror finish on the sealant side and a matte finish on the adhesive side in a single-pass cast film process.

    Laminate structures for liquid packaging containing DOWLEX™ 2035 as a sealant web are typically of the construction PET 12 µm / adhesive / LLDPE 40 µm or OPP 20 µm / adhesive / LLDPE 30 µm. The LLDPE layer contributes puncture resistance and flex-crack resistance in the filled pouch. Flex-crack resistance is measured according to ASTM F392 using a Gelbo flex tester, and a 40 µm cast LLDPE sealant web typically withstands more than 1,000 flex cycles before pinhole formation. This value is highly dependent on the film density: a lower density LLDPE of 0.915 g/cm³ would resist flex cracking better but would have lower stiffness and poorer hot-tack. DOWLEX™ 2035 at a nominal density of 0.919 g/cm³ represents a compromise between flex-crack resistance and machineability. The hot-tack strength measured at a seal temperature of 125°C with 0.5 s dwell is sufficient to hold liquid product on vertical form-fill-seal machines without seal creep. Critical process limits are the die lip deposit accumulation and the draw resonance onset at line speeds above 400 m/min for a 25 µm film. Draw resonance appears as a periodic thickness variation in the machine direction, visible as alternating transverse bands. It is suppressed by increasing air gap to 50 mm and reducing draw ratio. However, increased air gap reduces film clarity because the melt cools partially before quenching, producing a hazy edge band. The stable operating point is therefore established at 350 m/min to 380 m/min for thin lamination webs.

    For pressure-sensitive adhesive coating lines, the cast film substrate is unwound, corona-treated to a wetting tension of 40 mN/m to 44 mN/m, and coated with a solvent-based or hot-melt adhesive. The final application determines the required film thickness and surface geometry. A 30 µm to 40 µm cast film from DOWLEX™ 2035 is used for carpet protection film, appliance masking film, and printed circuit board temporary surface protection. In these applications, the film must combine a sufficiently high modulus to lie flat without curling and a low elastic recovery in the machine direction to maintain the adhesive bond without lifting after unwinding. The 1% secant modulus in the machine direction for 30 µm cast film is measured per ASTM D882, and the value is typically in the range of 120 MPa to 150 MPa for LLDPE cast film of this density. A lower modulus results in film stretching during coating and lamination, which causes misregistration of the adhesive pattern. A higher modulus creates excessive curl when the adhesive is applied, because the adhesive layer shrinks during drying and bends the film substrate. Anticurl treatment is performed on the opposite surface by applying a water-based acrylic curl-control coating or by embossing a reverse curl with a heated nip. Without this treatment, the film rolls into a tube on the coating line, making die-cutting and linerless conversion impractical.

    The cast film surface for pressure-sensitive adhesive coating is produced with a chill roll that has a controlled matte finish to permit adhesive anchoring. The surface roughness must be sufficient for mechanical interlocking but not so high that adhesive coverage becomes discontinuous. A roughness of Ra 0.3 µm to 0.6 µm is specified for general-purpose masking films. After corona treatment, the surface energy is measured per ASTM D2578, and the minimum acceptable dyne level is 38 mN/m. The film is then coated within 24 h of corona treatment, because the dyne level decays below 36 mN/m after extended storage. On the coating line, the unwinding tension is maintained at 50 N/m to 80 N/m of web width to prevent stretch marks. The film is pulled through a floating roll dancer system, and the web tension must be constant within ±5 N/m to avoid coating thickness variation. When the tension oscillates, the adhesive coat weight varies in the machine direction, producing visible banding in the protective film. The most common production defect is telescoping of the coated roll during slitting, caused by web camber introduced by uneven edge trim on the cast film line. To prevent camber, edge beads are controlled to less than 2 µm over nominal thickness across the entire web width. Edge bead measurement is performed with a capacitance gauge array scanning at 1 mm intervals across the web. Correction is made by adjusting die bolt heaters in the edge zones until the bead is reduced below the threshold. Published data for the specific adhesive anchoring values on DOWLEX™ 2035 surfaces are limited, but converter practice indicates that the polyolefin surface provides adequate peel strength for temporary protection only, not for permanent structural adhesion, because the film is semicrystalline and nonpolar. For permanent adhesive systems, the polyolefin surface requires an additional primer or the film is coextruded with an ethylene-vinyl acetate outer layer.

    When Cast Film Crosses Into Freezer-Grade Form-Fill-Seal Rollstock

    Frozen food packaging converted on vertical form-fill-seal equipment uses cast film from DOWLEX™ 2035 in thicknesses from 50 µm to 100 µm. The primary mechanical requirement is low-temperature puncture toughness, because frozen meat pieces, vegetable stems, and sharp frozen edges penetrate the film during filling and transport. Low-temperature impact resistance is assessed by the dart drop method per ASTM D1709, but the more informative test for frozen applications is the slow puncture test at -20°C using a 19 mm hemispherical probe. The film must withstand a displacement of 20 mm without puncturing at -20°C. The broad molecular weight distribution of DOWLEX™ 2035 improves low-temperature toughness compared with narrower-distribution mLLDPE grades of similar density, but it also raises sealing temperature. The seal initiation temperature is measured per ASTM F1921, and the freezer-grade film must seal below 130°C to avoid burning through the film on short dwell machines. The heat-seal jaw temperature is set at 135°C to 145°C, with dwell time of 0.5 s to 1.0 s and jaw pressure of 0.28 MPa. At this condition, the seal strength per ASTM F88 must be at least 3.0 N/15 mm at -20°C after sealing. Seal strength is not the same as hot-tack strength, and on vertical form-fill-seal machines hot-tack measured at 0.3 s after seal opening is the controlling quantity. The film must maintain a hot-tack strength above 1.5 N/15 mm at 120°C to withstand the weight of frozen product dropping into the pack immediately after sealing. If hot-tack is insufficient, the bottom seal opens and product falls through before the seal cools.

    Freezer-grade cast film is usually formulated without a cling agent because the film is not stretch-wrapped. Slip and antiblock levels are moderate: erucamide at 500 ppm to 1,000 ppm and silica antiblock at 1,500 ppm to 3,000 ppm. The coefficient of friction is measured at 23°C and at -20°C per ASTM D1894. The room-temperature kinetic coefficient is maintained below 0.20, but at -20°C the value can increase to 0.35 because the slip agent migration is suppressed. On vertical form-fill-seal machines, the film is pulled through the forming collar with a surface temperature below 10°C, and the friction between the film and the metal collar is critical. The form-fill-seal machine is equipped with a stainless steel collar with a mirror polish, and the film is treated on both sides to a wetting tension of 38 mN/m to 40 mN/m for sealing and printing. One-sided treatment is insufficient for freezer rollstock because the treated surface on the sealing side enables a lower seal initiation temperature. The corona treater is positioned immediately before the winder, and the line speed is set at 250 m/min to 350 m/min for 70 µm to 90 µm film. A thinner freezer film of 50 µm is produced at higher speeds but suffers from blocking on the winder because the heavier roll weight creates higher interlayer pressure. The cast film is wound under taper tension control from 100 N/m to 50 N/m from core to outer layers. Without taper tension, the inner wraps near the core are compressed and blocking defects appear as crescent-shaped surface bands after unrolling.

    The frozen food film requires a thermal history that avoids post-crystallization during storage. The film is cast and quenched rapidly, then stored at -18°C to -25°C after conversion. Some LLDPE formulations can develop increased haze and decreased impact at freezer temperatures if the original quench rate was too slow or if the film was annealed unintentionally on a hot slitter. The DOWLEX™ 2035 resin has a density of 0.919 g/cm³, which limits crystallinity and minimizes low-temperature embrittlement compared with a higher-density LLDPE. The flexural modulus at 23°C is moderate, and the film retains sufficient stiffness on the packaging line without becoming brittle. Pinhole resistance after flex testing at -20°C is evaluated per ASTM F392 with modifications to the specimen conditioning temperature. A 70 µm cast film passes 500 Gelbo flex cycles at -20°C without visible pinholes. This performance is dependent on film thickness uniformity; gauge bands thinner than 65 µm at the seal area become pinhole initiation points. The cast film line uses a gauge control system with a beta scanning head that measures thickness across the web. The die bolt heaters respond to the measured profile, but the control loop must be tuned to avoid oscillation of the web profile at the edge zones. The typical process stability target is a ±3% thickness variation across the web for 80 µm film. If the variation exceeds ±5%, the film is downgraded for freezer rollstock because the seal area may fall below the minimum thickness required for mechanical integrity.

    Hygiene Backsheet Breathability Gradients in Filled Cast Film Mono- and Co-Extrusion

    Cast film backsheet layers for baby diapers and adult incontinence products are produced from DOWLEX™ 2035 blended with ground calcium carbonate at loadings from 40 wt% to 55 wt%. The calcium carbonate is a fine particle filler with a median particle size of 2 µm to 3 µm, surface-coated with stearic acid to aid dispersion and to create microvoids during machine-direction orientation. The breathing mechanism in filled cast film is microvoid formation at the polymer-particle interface: as the film is drawn in the machine direction, the polymer matrix pulls away from the inflexible calcium carbonate particles, forming elongated voids that permit moisture vapor transmission while blocking liquid water. The breathability is measured as moisture vapor transmission rate per ASTM E96 at 38°C and 90% relative humidity. A filled cast film at 25 µm thickness with 50 wt% calcium carbonate typically achieves a MVTR of 1,500 g/m²·24 h to 3,000 g/m²·24 h after orientation, depending on the draw ratio and filler dispersion. This value is highly sensitive to the particle coating quality and the dispersive mixing history. On a 75 mm twin-screw compounding line used to make the filler masterbatch, the specific energy input is controlled between 0.12 kWh/kg and 0.18 kWh/kg. Insufficient specific energy results in large agglomerates that act as stress concentrators and cause film breaks during stretching. Excessive specific energy strips the stearate coating from the calcium carbonate, exposing the hydrophilic core and destroying the interfacial void structure.

    The filled cast film line is configured differently from a standard cast film line because the web must be stretched in the machine direction after quenching. The quenched film is passed over a set of heated rolls at 60°C to 80°C and then drawn between two roll groups with a speed ratio of 2:1 to 4:1. This machine-direction orientation step is where the microvoids develop. The draw ratio is constrained by the melt strength of the LLDPE matrix and by the filler loading. At 55 wt% filler, a draw ratio above 3.5:1 causes frequent web breaks because the matrix cannot bridge the particle interfaces without tearing. At 40 wt% filler, a draw ratio of 4:1 is possible with acceptable film integrity but the breathability is lower. The DOWLEX™ 2035 resin provides a balance of melt strength and low gel content for this process. The melt flow rate of 2.5 g/10 min at 190°C under 2.16 kg is low enough to resist draw resonance during orientation but high enough for the die flow to remain stable at widths above 2 m. The die gap is set narrower than in standard cast film, typically 0.6 mm to 0.8 mm, because the film is oriented after casting. The initial cast film before orientation is thicker than the final breathable film; a final thickness of 20 µm is produced from a 60 µm cast precursor. The draw ratio is therefore not the only process variable; the precursor thickness and the roll temperature profile together determine the void morphology.

    The primary process failure in breathable filled cast film is die lip buildup. Calcium carbonate masterbatch and LLDPE have different thermal expansion coefficients, and the filler particles migrate to the die lip and accumulate as a hard, white residue within 2 h to 4 h of continuous operation. The residue disrupts the melt flow at the lip edge and creates machine-direction streaks in the film. To reduce this effect, the die exit temperature is kept below 245°C. A higher temperature accelerates the formation of the deposit. The use of a fluoropolymer processing aid in the DOWLEX™ 2035 masterbatch at 200 ppm to 400 ppm reduces die lip buildup and improves lubrication at the melt-metal interface. The processing aid also reduces melt pressure fluctuations in the die, which translates into more uniform precursor thickness. After machine-direction orientation, the film is annealed on a set of cooling rolls at 30°C to 40°C to set the void structure and prevent post-stretching shrinkage. The film is then slit and wound under low tension, because a filled breathable film has higher surface roughness and lower tear resistance than a neat LLDPE cast film. The tear strength in the machine direction is reduced by the orientation step, and the film must be handled at lower winding tension to prevent core crush and internal splits. Winding tension for a 20 µm breathable film is typically below 60 N/m, compared with 100 N/m for a neat 20 µm cast film. The film is supplied to hygiene converters as either monolayer or coextruded breathable film, with a coextruded skin layer of neat DOWLEX™ 2035 or an ethylene-vinyl acetate copolymer for thermal bondability. In a three-layer cast film, the core layer contains the filler, while the outer layers are unfilled to provide seal strength and low surface friction. The core-to-skin thickness ratio is typically 80:10:10, and the skin layers protect the filled core from moisture pickup during storage. Published industrial data for the specific air permeability of DOWLEX™ 2035 in this configuration is limited, but the filler masterbatch process parameter range is considered the main determinant of MVTR uniformity.

    In a coextruded breathable backsheet, the extruder configuration uses two or three extruders feeding a feedblock and a coat-hanger die. The core extruder is a 105 mm twin-screw machine or a 120 mm single-screw machine with high-dispersion mixing sections, while the skin extruders are smaller, at 45 mm to 60 mm, running neat LLDPE. The melt streams are combined in a feedblock, and the skin layers protect the filled core from exposure to the die lip. This reduces the die lip buildup compared with monolayer filled film, but the core melt still contacts the die lips at the edges if the skin encapsulation fails at the web sides. Edge encapsulation is monitored by cross-sectional microscopy of the cast film edge bead. If the core breaks through the skin at the edge, the exposed filler creates a rough edge that fractures during machine-direction orientation. The edge trim from the oriented film is collected and recycled back into the core layer at up to 20% reclaim. However, the filler particles have already undergone microvoid formation, so the reclaim material contains voids and fractured particle-polymer interfaces. At reclaim levels above 20%, the core layer loses continuity and the breathable film develops elongated pinholes that fail diaper leak tests. The reclaim ratio is therefore controlled gravimetrically and limited to 15% in most production lines.

    Free Quote

    Competitive Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade, is an ethylene-octene copolymer produced by solution polymerization and supplied in pellet form for cast film extrusion. The grade is identified by a melt mass-flow rate of 6.0 g/10 min at 190 °C/2.16 kg per ASTM D1238 and a nominal density of 0.935 g/cm³ per ASTM D792. These are typical lot-average values and are not specification limits. The 1-octene comonomer contributes hexyl short-chain branches that reduce crystallinity relative to high-density polyethylene and alter solid-state deformation behavior. Because the backbone remains predominantly linear, the resin exhibits lower strain hardening than high-pressure low-density polyethylene; this limits its use in conventional blown film but is acceptable in cast film where the melt curtain is supported over a short draw distance.

    On cast film lines equipped with single-screw extruders of 75 mm to 120 mm diameter and 30:1 to 33:1 L/D, DOWLEX 2035 is typically processed with barrel setpoints from 190 °C to 260 °C and die temperatures from 240 °C to 280 °C. These ranges are drawn from general LLDPE cast film practice; published data for this specific grade at all die configurations is limited. Barrier screws with Maddock mixing sections are preferred because conventional three-zone screws may deliver inhomogeneous melt at high throughput, producing visible gels and gauge bands. The resin does not require pre-drying at ambient storage relative humidity below 60 % because polyolefin moisture absorption is negligible. Condensation on cold pellet surfaces introduced directly into a hot feed throat can create surface streaks and should be prevented by equilibrating resin to ambient temperature before opening the package.

    A Cast Film Grade Positioned for High-Draw Stretch Operations

    The cast film designation reflects chill roll quenching behavior rather than a separate chemical backbone. In pallet stretch film coextrusions, DOWLEX 2035 is commonly placed in the core layer to provide tensile strength and puncture resistance, while outer layers containing ethylene-vinyl acetate or metallocene plastomers control cling and unwinding force. The following nominal identification values are derived from manufacturer documentation and are typical, not guaranteed:

    PropertyTest methodTypical lot-average value
    Melt mass-flow rate, 190 °C/2.16 kgASTM D1238, ISO 1133-1:20226.0 g/10 min
    DensityASTM D792, ISO 1183-1:20190.935 g/cm³
    Vicat softening pointASTM D1525, ISO 306124 °C

    The density of 0.935 g/cm³ is higher than that of typical cling-layer LLDPE grades, which often fall between 0.918 g/cm³ and 0.925 g/cm³. The higher density reduces tack and blocking in the core but also lowers ultimate elongation relative to lower density copolymers. This crystallinity-driven trade-off influences elastic recovery under load: a higher density core may retain holding force after wrapping, but low-temperature impact resistance must be confirmed for end-use temperatures below -20 °C. Tensile properties of cast film are measured by ASTM D882 or ISO 527-3; reported values for octene-based LLDPE cast film at 25 µm thickness often fall between 30 MPa and 50 MPa machine-direction tensile strength at break, but published data for this exact grade is limited and final properties depend on draw ratio, chill roll temperature, and gauge.

    What Distinguishes DOWLEX 2035 from Butene-Based LLDPE in Cast Film?

    The principal structural distinction is comonomer chain length. Butene-based LLDPE carries ethyl branches of two carbons from the alpha-olefin insertion, whereas DOWLEX 2035 carries hexyl branches from 1-octene. During crystallization, the longer hexyl branch is less easily incorporated into the orthorhombic polyethylene lattice, so it remains concentrated in the interlamellar amorphous phase and increases the probability of stress-transmitting tie molecules. For films of equal density and melt index, octene-based LLDPE typically shows higher machine-direction Elmendorf tear strength measured according to ASTM D1922 and higher dart impact resistance measured according to ASTM D1709. Dart impact per ASTM D1709, Method A, uses a 38.1 mm diameter dart and reports the weight at 50% failure; Elmendorf tear per ASTM D1922 reports force in grams per 25.4 µm. Microstructural differences also affect orientation: after high-draw stretching in cast film, tie molecules are oriented in the machine direction, and transverse tear resistance may be better retained in octene-based LLDPE than in butene-based LLDPE of equivalent crystallinity. Compared with high-pressure LDPE, DOWLEX 2035 lacks long-chain branching; the resulting lower melt tension is accommodated by the short draw distance of cast film but would create bubble instability in blown film without blending.

    Because cast film quenching suppresses spherulitic crystallization, chill roll temperature and air knife velocity control the optical and surface properties of DOWLEX 2035. A polished chrome roll maintained at 20 °C to 35 °C freezes the web rapidly and reduces haze by limiting crystal growth. Without slip and antiblock additives, the cast surface can develop blocking forces that interfere with unwinding on powered stretch wrappers. Converter trials commonly target a coefficient of friction below 0.35 by addition of erucamide or oleamide slip masterbatch. Corona treatment to a wetting tension of 38 dyn/cm to 42 dyn/cm per ASTM D2578 is used before printing, coating, or lamination. Published data for surface energy decay of this exact grade after corona treatment is limited; durability of treatment should be confirmed on the finished roll before laminating because post-treatment decay varies with storage temperature and humidity.

    Rheological and Thermal Boundaries During Cast Film Extrusion

    Like other linear polyolefins, DOWLEX 2035 exhibits pseudoplastic shear thinning; apparent viscosity decreases as screw speed and die throughput increase. The relationship is measurable by capillary rheometry according to ISO 11443, but published viscosity curves for this specific grade are limited. Production-scale experience with analogous octene-based LLDPE indicates that melt pressure before the die can rise to 20 MPa to 30 MPa on narrow-gap dies when screen pack contamination accumulates, making continuous screen changers and pressure alarms necessary to prevent die lip damage. Draw resonance in the melt curtain becomes more probable when the draw ratio exceeds approximately 15:1; above this threshold, reducing the die-to-roll distance or blending with a high-melt-strength component may be required. Sustained melt temperatures above 300 °C accelerate chain scission and gel formation, while temperatures below 180 °C increase melt pressure and can produce visible melt fracture.

    Thermal and additive boundaries define safe operating limits for this resin. Oxidative degradation in solution-process octene LLDPE is limited below 250 °C for short residence times, but exposure to oxidizing acids or prolonged ultraviolet radiation without a stabilizing package reduces molecular weight and film tear resistance. When fluoropolymer polymer processing additives are used to reduce die lip build-up, capillary studies on linear polyethylene have documented apparent shear stress reductions of 20 % to 40 % at shear rates above 500 s⁻¹. The product should not be stored in direct sunlight for extended periods unless the supplier has incorporated a UV stabilizer; otherwise, surface oxidation can reduce corona retention and heat-seal performance. Coextrusion with tackifier-rich cling layers requires the melt curtain to remain below the decomposition temperature of the specific tackifier; many polyterpene-based tackifiers degrade near 180 °C to 200 °C, so barrel settings must be selected accordingly.

    When Line Speeds Exceed 450 m/min on Single-Stage Cooling Rolls

    At operating speeds above 450 m/min, edge pinning and air knife geometry control yield and web flatness. The melt curtain must be attached to the chill roll before measurable neck-in occurs; compressed-air edge pinning or electrostatic edge pinning is required for stable operation. Industrial observations on cast film lines indicate that LLDPE neck-in can consume 25 mm to 50 mm per edge depending on die-to-roll distance and melt temperature. Thin film below 20 µm is feasible with the 6.0 g/10 min melt mass-flow rate, but the extruder drive must supply sufficient torque at low melt temperatures; older single-screw extruders with fixed-speed drives may become torque-limited before reaching maximum throughput. Retrofitting with a barrier screw and Maddock mixing section improves thermal homogeneity and reduces gauge variation at these speeds. Published data for DOWLEX 2035 at line speeds above 600 m/min is limited; qualification on the target line is required before commercial commitments.

    Compared with metallocene-catalyzed LLDPE, DOWLEX 2035 is produced with a conventional coordination catalyst and generally exhibits a broader molecular weight distribution. This broadening improves processability on cast lines not equipped for the high extrusion pressure and shear heating associated with narrow-distribution metallocene grades, but it may reduce ultimate clarity and dart impact at equivalent density. The trade-off is structural rather than formulation-dependent. In coextruded stretch film, a common construction places DOWLEX 2035 in the core and a metallocene plastomer or ethylene-vinyl acetate copolymer in the cling layers, assigning the higher-density core to the load-bearing function while the outer layers manage cling and puncture compliance. No tie resin is required because adjacent polyolefin layers fuse in the die and in the melt curtain.

    Food contact compliance for olefin polymers is referenced to FDA 21 CFR 177.1520 and EU Regulation 10/2011 for specific polymers and additives; converters must verify that the finished film, including masterbatch or printing ink, meets the intended food contact conditions. The product as supplied does not normally require desiccant drying or special ventilation, but warehouse storage above 40 °C can soften pellets and cause agglomeration in silos. REACH and RoHS obligations for the resin are generally limited, but heavy-metal pigments or processing aids introduced by converters may impose article-level restrictions.