Dow Dowlex 2032 Linear Low Density Polyethylene Blown Film Grade

Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade

    • Product Name: Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 545234
    Density 0.926 g/cm³
    Melt Index 190 C 2 16 Kg 2.0 g/10 min
    Melting Point 123 °C
    Vicat Softening Point 98 °C
    Tensile Strength At Break Md 36 MPa
    Tensile Strength At Break Td 30 MPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Dart Drop Impact 160 g
    Elmendorf Tear Strength Md 220 g
    Elmendorf Tear Strength Td 420 g
    Haze 11%
    Gloss 45 55
    Coefficient Of Friction 0.2
    Blocking 100 g
    Film Thickness Tested 1.0 mil

    As an accredited Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing DOWLEX™ 2032 is packaged in 25 kg polyethylene bags, palletized and stretch-wrapped, ensuring secure handling and transport.
    Container Loading (20′ FCL) 20′ FCL: Dow DOWLEX™ 2032 LLDPE Blown Film Grade, palletized 25 kg bags, shrink-wrapped, evenly distributed, secured in dry container.
    Shipping DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade, is typically shipped as non-hazardous pellets in 25 kg bags, palletized and stretch-wrapped, or in bulk bags/railcars. Keep dry, clean, and away from excessive heat or sunlight. No special hazardous-materials handling required; follow local transport and storage regulations.
    Storage Store DOWLEX™ 2032 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep bags or containers closed, clean, and palletized off the floor to prevent moisture pickup and contamination. Avoid prolonged UV exposure. Ensure labels remain legible and inspect containers regularly. Follow the manufacturer’s SDS and local regulations. Use first-in, first-out stock rotation.
    Shelf Life Stable under normal storage conditions; indefinite shelf life if kept dry, cool, and protected from direct sunlight, excessive heat, and contamination.
    Application of Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade

    Converters running three-layer coextrusion lines for heavy-duty industrial sacks specify a nominal melt index of 2.0 g/10 min per ASTM D1238 at 190 °C/2.16 kg and density of 0.926 g/cm³ per ASTM D792 because DOWLEX 2032 provides the combination of tear resistance and drawdown needed for liners that must survive filling speeds above 20 bags/min. A baseline structure places DOWLEX 2032 at 60–80 wt% in the core and inner layers, LDPE with melt index 0.25–0.5 g/10 min at 10–30 wt% for bubble stability, carbon black masterbatch at 2–4 wt% in the outer skin for UV resistance, and fluoroelastomer-based PPA masterbatch at 0.5–1.0 wt% to suppress melt fracture. Melt temperatures are maintained at 190–215 °C, die gap is set between 2.2 mm and 2.8 mm, blow-up ratio between 2.0:1 and 2.8:1, and frost line height adjusted to 8–12 die diameters to balance machine-direction and transverse-direction tear.

    LayerCompositionLoading range (wt%)FunctionTest method
    Outer skinDOWLEX 2032 / LDPE / carbon black MB / PPA MB63–75 / 15–25 / 2–4 / 0.5–1.0UV resistance, surface friction, melt fracture suppressionASTM D1003, ASTM D1894
    CoreDOWLEX 2032 / LDPE70–85 / 15–30Tear resistance, creep resistanceASTM D1922, ASTM D882
    Inner skinDOWLEX 2032 / LDPE / antiblock MB75–85 / 10–15 / 2–4Sealability, blocking resistanceASTM F88, ASTM D1894

    On 55 mm and 65 mm three-layer lines, die lip build-up becomes a recurrent failure mode when carbon black masterbatch exceeds 4 wt%, producing gauge bands at 40–50 mm intervals and elevated filter pressure. Screen packs at 40/60/100/200 mesh downstream of the breaker plate reduce degraded polymer particles. Bubble trembling is observed when core layer DOWLEX 2032 exceeds 85 wt% at blow-up ratios above 2.5:1, requiring either BUR reduction or addition of LDPE to the core. For dangerous goods sacking, the finished liner or sack is evaluated under ISO 21898:2004 and UN 13H4 certification protocols where applicable. Non-food industrial contact does not require EU 10/2011 compliance, but REACH Regulation (EC) No 1907/2006 Article 33 applies to SVHC communication. Terminal products include FIBC inner liners, valve sacks for polymer powders, heavy-duty shipping sacks for granulated fertilizers, and closure-sealed liners for mineral fillers.

    What Changes in Heat Seal Strength and Dart Impact Occur After Conditioning at −20 °C?

    The frozen food packaging sector uses blown film from DOWLEX 2032 in monolayer and three-layer structures where low-temperature puncture resistance and seal integrity through surface frost control package failure rates. A typical formulation combines 70–85 wt% DOWLEX 2032 with 10–20 wt% LDPE at melt index 0.25–0.5 g/10 min to improve hot tack and 2–5 wt% masterbatch delivering 1,000–3,000 ppm synthetic silica antiblock and 500–1,500 ppm erucamide slip. The processing window on a 60 mm, 24:1 L/D single-screw extruder with a barrier screw is 195–215 °C, die gap is set between 1.8 mm and 2.4 mm, and blow-up ratio is held at 2.0:1–2.6:1 with a lower frost line to promote transverse orientation and MD/TD tear balance. Heat seal initiation temperature is measured by generating heat seal curves per ASTM F2029, seal strength per ASTM F88, and hot tack per ASTM F1921. Cold-temperature dart impact testing follows ASTM D1709 Method A after conditioning at −20 °C for 24 h; published data for this specific film configuration is limited, so converter-side trials are required. Direct food contact compliance relies on FDA 21 CFR 177.1520(c) for olefin polymers and EU Regulation (EU) No 10/2011 with overall migration below 10 mg/dm² per EN 1186-1. Terminal products include IQF vegetable bags, frozen french fry pouches, ice cream pillow packs, frozen meat bags, and fish block film.

    When Greenhouse Film Exposure Exceeds 24 Months, HALS Loading Rather Than Base Resin Density Governs Residual Tensile Retention

    For greenhouse covers and silage films, DOWLEX 2032 is selected when 2.0 g/10 min melt flow permits lower extruder amperage in wide-web lines while retaining sufficient melt strength at high blow ratios. In a five-layer agricultural film structure, the resin is used at 80–95 wt% in core and skin layers; hindered amine light stabilizer masterbatch is added at 0.3–0.6 wt% active concentration, UV absorber at 0.1–0.3 wt%, and phenolic antioxidant at 0.05–0.15 wt%. For silage films requiring cling and puncture resistance, LDPE at 5–15 wt% and polyisobutylene at 0.5–1.5 wt% are added. The process uses die diameters from 800 mm to 1,800 mm, die gaps of 2.0–2.4 mm, blow-up ratios of 1.5:1–2.0:1, and internal bubble cooling to control frost line height and crystal morphology. The critical quality control parameter is accelerated weathering under ISO 4892-2 or EN 13206:2017 Annex A, with residual elongation at break measured per ISO 527-3 after 2,000–3,500 h exposure. Published data for this specific configuration is limited; however, agricultural film stabilization practice identifies HALS below 0.3 wt% active as a premature failure risk before 24 months in southern European solar exposure, while loadings above 0.6 wt% may produce surface bloom that reduces silage bag seal consistency. Greenhouse film compliance is assessed under EN 13206:2017; silage film under EN 13207:2018; silage film intended for fermented feed contact is assessed under EU Regulation (EU) No 10/2011; and REACH Article 33 SVHC communication applies. Terminal products include greenhouse side and roof covers, silage stretch film, silo bags, silage cover laminates, and mulch film.

    Lamination-grade sealant webs running at 250–350 m/min on solventless adhesive laminators demand a blown film layer with gel count controlled through 60/80/100/120 mesh screen packs, stable coefficient of friction, and stable wetting after corona treatment. DOWLEX 2032 is extruded in a two-layer or three-layer sealant configuration at 70–90 wt%, with 10–20 wt% LDPE and a combined masterbatch loading of 1–3 wt% delivering 2,000–6,000 ppm synthetic silica antiblock and 500–1,200 ppm erucamide slip. Film production uses a 90 mm, 30:1 L/D extruder with a double-flight barrier screw, die gap 1.5–2.0 mm, blow-up ratio 2.2:1–2.8:1, and corona treatment to 38–42 dyn/cm measured with contact angle test fluids before winding. Sealant webs are bonded to BOPP, PET, or metallized PET by two-component solventless polyurethane adhesive at 1.5–2.5 g/m² coat weight. Coefficient of friction is evaluated per ASTM D1894, and oxygen transmission contribution is measured per ASTM D3985 only as part of the completed laminate. Compliance is anchored to FDA 21 CFR 177.1520(c) for direct food contact and EU Regulation (EU) No 10/2011 with migration testing per EN 1186-1; lamination converters also apply EU Regulation (EC) No 2023/2006 GMP for printing inks and adhesives. Terminal products include snack pillow packs, condiment sachets, tea bag overwrap, and single-serve coffee stick packs.

    Coextruded Stretch Hood Film Demands High-Stalk Bubble Morphology and a Narrow Frost Line Window

    Stretch hood film production for pallet unitization uses blown film with high machine-direction tear and puncture resistance; DOWLEX 2032 is combined with LDPE and metallocene LLDPE to adjust cling, reverse creep, and holding force. A typical three-layer formulation uses 50–80 wt% DOWLEX 2032 in the core and inner layers, 20–30 wt% LDPE, and 5–15 wt% metallocene LLDPE with density 0.918–0.922 g/cm³; fluoroelastomer-based PPA masterbatch is added at 200–800 ppm active to suppress melt fracture on large dies.

    The process uses a high-stalk bubble with blow-up ratio 2.5:1–4.0:1, die gap 2.0–2.4 mm, melt temperature 200–220 °C, and frost line height set above 10 die diameters to maximize machine-direction orientation. Because high-stalk operation narrows the stability window, ambient air temperature fluctuations of ±2 °C around the bubble can produce gauge variation of ±5–7 %. Melt pressure deviations exceeding ±5 % at constant screw speed indicate die lip build-up and require purging. Testing follows ASTM D882 for tensile properties, ASTM D1709 for dart impact, ASTM D2732 for free shrink at 135 °C, and ASTM D5458 for cling force. Terminal products include stretch hood films for pallets of construction blocks, bagged cement, beverage trays, and white goods packaging.

    Produce Bag Seal Integrity and Optical Performance in Thin-Gauge Films

    If thin-gauge produce bags are run at 12–25 µm, DOWLEX 2032 is used as the base resin because its melt index and density combination permits stable bubble operation while retaining dart impact and seal initiation. A typical monolayer formulation includes 75–90 wt% DOWLEX 2032, 5–15 wt% LDPE, and 2–5 wt% masterbatch supplying 1,500–3,000 ppm antiblock and 800–1,500 ppm slip. The blown film line runs a 50–70 mm, 24:1 L/D extruder, die gap 1.2–1.6 mm, blow-up ratio 2.0:1–3.0:1, melt temperature 190–210 °C, with optional in-line perforation for breathable produce bags. Optical performance is measured per ASTM D1003 for haze and ASTM D2457 for gloss; dart impact per ASTM D1709 Method A; tensile per ASTM D882. Food-contact compliance is under FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011, with REACH Article 33 SVHC communication applicable. Terminal products include T-shirt grocery produce bags, roll bags for bakery and fruit, perforated leafy green bags, and overwrap for fresh produce trays.

    Free Quote

    Competitive Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade, is a solution-polymerized ethylene-octene copolymer supplied in pellet form for monolayer and coextruded blown film. Published base-resin data list a nominal density of 0.926 g/cm³ when tested according to ASTM D792 or ISO 1183-1:2019, and a melt index of 2.0 g/10 min at 190 °C under a 2.16 kg load according to ASTM D1238 or ISO 1133-1:2022. The octene comonomer creates short-chain branches that reduce lamellar thickness and increase tie-molecule probability relative to butene-based linear low-density polyethylene at equivalent melt index. The grade is specified for heavy-duty shipping sacks, industrial liners, high-toughness consumer films, and freezer packaging where gauge reduction, puncture resistance, and seal integrity are required. Because the resin is produced by a solution process, the comonomer distribution is more homogeneous than that of many gas-phase LLDPE materials; this narrows the melting range and influences heat-seal behavior. On standard blown film lines with die gaps between 1.0 mm and 2.0 mm, the resin is processed without routine pre-drying under dry conditions.

    Processing window and bubble geometry on conventional blown film lines

    On production-scale monolayer lines equipped with 63.5 mm or 75 mm grooved-feed extruders and 24:1 to 30:1 L/D barrier screws, the melt temperature is maintained between 190 °C and 220 °C. Higher temperatures decrease screw torque and improve dispersion of additives, but they lower bubble tension and can shift the frost line upward. The die gap is normally specified between 1.2 mm and 1.6 mm; a narrower gap can raise shear stress and induce melt fracture at high output, while a wider gap increases residence time and may promote oxidation. Blow-up ratio is set between 2.0:1 and 3.0:1 to balance machine-direction stiffness against transverse-direction tear. Frost-line height is adjusted in the range of 5 to 10 die diameters for many monolayer structures; lower frost-line heights increase transverse-direction orientation and reduce machine-direction elongation.

    Back pressure and adapter melt-temperature probes are specified because the solution LLDPE has moderate shear thinning and can develop heat more quickly than the barrel set points suggest at high screw speeds. Regrind additions up to 20 wt% are typically tolerated when the regrind is dried and free of fines; higher regrind levels may reduce bubble stability and increase gel counts. Internal bubble cooling is used on some heavy-duty film lines to raise output and lower melt temperature; however, cooling air flow must be balanced with exhaust volume to prevent frost-line instability. Output is limited by bubble cooling capacity rather than screw torque on many air-cooled systems.

    Mechanical film evaluation follows ASTM D882 for tensile properties, ASTM D1709 Method A for dart drop, ASTM D1922 for Elmendorf tear, ASTM D1003 for haze, and ASTM D2457 for gloss. Specimens are conditioned at 23 °C and 50 % relative humidity before testing. In DOWLEX™ 2032 films, machine-direction tensile yield typically occurs at a lower strain than in high-pressure LDPE, and elongation at break in both directions commonly exceeds 500 % at 25 µm gauge; published data for a specific gauge and line configuration remains limited. Dart drop and Elmendorf tear are highly dependent on blow-up ratio, frost-line height, and die gap. The grade is often selected when a converter must maintain a minimum dart drop after reducing film thickness by 15 % to 20 %; the octene comonomer preserves low-velocity impact resistance better than butene-based LLDPE of similar density. High-speed puncture testing according to ASTM D5748 shows a similar ranking, though end-use performance must be confirmed on the target line.

    Does octene comonomer architecture explain the property difference from butene LLDPE?

    The difference between DOWLEX™ 2032 and butene-based Ziegler-Natta LLDPE is primarily steric, not merely density-related. Butene comonomer introduces 2 carbon side chains; octene introduces 6 carbon side chains. The longer side chain is more effective at disrupting crystallinity and creating interlamellar tie molecules, so the octene grade exhibits higher dart impact and Elmendorf tear at equivalent density and melt index. In a blown film, the difference is amplified in the transverse direction because the tie-molecule network resists crack propagation across oriented lamellae. The effect is measurable in laboratory specimens but can be masked by excessive melt temperature or by poor bubble stability on a specific line. Published comparative data from resin suppliers generally place octene LLDPE above butene LLDPE in low-velocity puncture but below high-pressure LDPE in melt strength and foamability. The 0.926 g/cm³ density of DOWLEX™ 2032 gives higher stiffness than 0.920 g/cm³ film grades while retaining adequate sealability for many applications.

    The solution process also affects comonomer distribution. Compared with gas-phase butene LLDPE produced on heterogeneous catalysts, the solution-polymerized DOWLEX™ 2032 typically has a narrower molecular weight distribution and a more uniform short-chain branch distribution. This reduces low-molecular-weight fractions that can contribute to extractables and haze; however, it also reduces the shear thinning that high-pressure LDPE provides. On a high-speed line, the melt viscosity at typical shear rates of 200 s−1 to 500 s−1 is lower than that of a 0.926 g/cm³ high-pressure LDPE at the same melt index, because long-chain branching is absent or very low. This requires different bubble support settings and may require blending with LDPE to improve stability in very thin film or complex gusseted structures.

    High-pressure LDPE is frequently added at 10 wt% to 20 wt% to increase melt strength and broaden the processing window. The addition reduces dart drop in a nonlinear manner: the first 10 wt% may reduce dart drop by a measured amount that varies with gauge and orientation, while the loss of Elmendorf tear can exceed the proportional estimate. A blend with 20 wt% LDPE remains common for heavy-duty sacks where bubble stability and heat-seal characteristics justify the toughness reduction. Compared with a medium-density PE grade above 0.930 g/cm³, DOWLEX™ 2032 retains higher Elmendorf tear and dart impact at equal gauge; compared with a lower-density grade below 0.920 g/cm³, it provides higher modulus and better film-to-film slip. These trade-offs are assessed through thickness-normalized tear and impact values, not simple additive blending rules.

    When high-pressure LDPE is added as a processing aid, tear strength responds nonlinearly

    Processing lines that add high-pressure LDPE to DOWLEX™ 2032 observe improved bubble tension and greater tolerance to cooling-air fluctuations. The improvement is caused by the long-chain branching in LDPE, which increases elongational viscosity and stabilizes the freeze line. At 2 wt% LDPE, the effect on tear properties is often smaller than normal variation; at 15 wt% to 20 wt% LDPE, Elmendorf tear in the transverse direction can decline to levels approaching those of an LDPE-rich blend. The exact decrease is influenced by film gauge, blow-up ratio, and die land length, so laboratory blends should be prepared on the production line rather than on a small laboratory cast film line. The ideal addition level is also a function of extrusion head pressure; higher LDPE content lowers melt temperature and motor load, permitting faster screw rotation on torque-limited machines.

    When DOWLEX™ 2032 is blended with high-pressure LDPE, the seal initiation temperature remains strongly influenced by the LLDPE phase because heat-seal strength develops through melt fusion of the lamellar network. The LDPE phase contributes to hot tack and increases the maximum seal strength at short dwell times. For high-speed form-fill-seal operations, this combination is used to avoid seal weakening when the film contacts packaging product before cooling. In contrast, blending with metallocene LLDPE improves dart drop but may require higher melt temperature or a wider die gap because the metallocene resin has lower melt strength and higher shear viscosity at comparable melt index.

    Thermal and hydrolytic boundaries during conversion

    Thermal-oxidative degradation accelerates when melt temperature exceeds 240 °C. Prolonged residence time above 230 °C generates oxidation products that reduce film clarity, increase odor, and shorten the induction time of the stabilizer package. Therefore, the extruder profile is structured so that the final zones and die are below 220 °C unless a specific high-output configuration requires higher settings. The resin does not require routine pre-drying at relative humidity below 60 %. Surface condensation can occur when pellets are moved from cold silos into warm plant air at relative humidity above 80 %; this moisture appears as optical defects and bubbles in the film. A hopper dryer set at 60 °C to 80 °C for 2 h to 4 h is then specified.

    Care is required with additive masterbatches that are hygroscopic or contain amine-based slip agents. Free moisture and certain amine chemistries can react with polymer oxidation products and affect film clarity; no inherent incompatibility with common polyethylene processing-aid masterbatches is documented, but masterbatch carriers should be LLDPE-compatible. The use of fluoropolymer processing aids at 0.02 wt% to 0.05 wt% is used on some lines to delay melt fracture at high output. The exact addition level is calibrated by measuring die-pressure reduction and melt-fracture disappearance on the target line.

    In coextruded structures, DOWLEX™ 2032 is used as a core layer or skin layer with high-pressure LDPE seal layers. The octene LLDPE contributes toughness and downgauging potential; the LDPE seal layer lowers seal initiation temperature and improves hot tack on vertical form-fill-seal machines. Typical layer ratios for heavy-duty sacks range from 20 % to 30 % LDPE by weight, with the remaining layer DOWLEX™ 2032; when a three-layer structure is used, a metallocene LLDPE skin layer may be added to provide low-temperature seal strength. The resin has a density of 0.926 g/cm³, which gives a secant modulus higher than that of 0.918 g/cm³ grades but not as high as medium-density polyethylene. This is used to print webs with sufficient stiffness for register control without sacrificing puncture resistance.

    Regulatory and food-contact status is application-dependent. The resin is a polyolefin subject to FDA 21 CFR 177.1520 in the United States. For European food-contact applications, the final film must comply with Regulation (EU) No 10/2011; compliance requires migration testing of the finished article because the polymer’s overall migration and specific migration limits are influenced by gauge, layer structure, and additives. Directive 2011/65/EU restricts heavy metals and brominated flame retardants; DOWLEX™ 2032 is not formulated with these substances, but converter-specific verification is required if the film enters electrical/electronic equipment streams. REACH registration and SVHC status are addressed in the supplier’s safety data sheet; no intentional phthalates or bisphenol A are used in the base resin.

    Regulatory areaStandard or statuteVerification basis
    US food contactFDA 21 CFR 177.1520Olefin polymer compliance subject to conditions
    EU food contactRegulation (EU) No 10/2011Migration testing on final film
    RoHSDirective 2011/65/EUNo intentionally added restricted heavy metals
    REACHRegulation (EC) No 1907/2006Registration and SVHC confirmation via SDS

    The grade is not recommended for direct contact with strong oxidizing agents, aromatic hydrocarbons, or chlorinated solvents at elevated temperature because these media can swell or degrade polyethylene. In high-shear extrusion, static mixing elements and screens are recommended to avoid melt-temperature nonuniformity. Published data for film properties at extreme thicknesses below 10 µm or above 200 µm is limited; converters should qualify the grade on their own lines with the intended masterbatch and regrind ratio.

    Top