Dow Dowlex 2027g Linear Low Density Polyethylene

Dow DOWLEX™ 2027G Linear Low Density Polyethylene

    • Product Name: Dow DOWLEX™ 2027G Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 204083
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.920 g/cm³
    Meltindex 1.0 g/10 min
    Meltindextestcondition 190 °C / 2.16 kg
    Meltingpoint 122 °C
    Vicatsofteningpoint 103 °C
    Tensilestrengthatyield 9 MPa
    Tensilestrengthatbreak 24 MPa
    Elongationatbreak 700%
    Flexuralmodulus 240 MPa
    Hardnessshored 50
    Dartimpact 120 g
    Elmendorftearmd 250 g
    Elmendorfteartd 400 g
    Haze 10%
    Gloss45degree 70

    As an accredited Dow DOWLEX™ 2027G Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DOWLEX™ 2027G Linear Low Density Polyethylene is supplied in 25 kg polyethylene bags, palletized for industrial transport and storage.
    Container Loading (20′ FCL) 20′ FCL container loading for Dow DOWLEX™ 2027G LLDPE: typically 25 kg bags, palletized, shrink-wrapped, and securely stowed for export.
    Shipping Dow DOWLEX™ 2027G LLDPE ships as non-hazardous resin pellets in 25-kg bags, 1,000-kg bulk bags, or bulk trucks/railcars. Keep containers closed; store dry and cool, away from ignition sources and direct sunlight. Protect from moisture and contamination. No special UN/DOT transport classification applies.
    Storage Store DOWLEX™ 2027G in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original containers closed to prevent moisture, dust, and contamination. Avoid contact with incompatible oxidizers. Stack securely to prevent package damage, and follow first-in, first-out inventory practices. Consult the SDS for complete handling and storage requirements.
    Shelf Life Dow DOWLEX™ 2027G LLDPE has a recommended shelf life of 24 months when stored in original packaging under cool, dry conditions.
    Application of Dow DOWLEX™ 2027G Linear Low Density Polyethylene

    In high-output cast stretch film lines running at 300–450 m/min, DOWLEX™ 2027G Linear Low Density Polyethylene is loaded as the primary polymer fraction at 94–96 wt%, with the balance comprising 2–3 wt% polyisobutylene cling masterbatch, 1–2 wt% slip/antiblock masterbatch, and processing aid to 100 wt%. The resin carries a nominal density of 0.917 g/cm³ and a melt index of 2.0 g/10 min as determined by ASTM D1238 at 190°C/2.16 kg. Compliance for logistics packaging films is anchored to EU Directive 94/62/EC Annex II Article 11, with combined lead, cadmium, mercury, and hexavalent chromium content held below 100 mg/kg; cling force and puncture propagation are specified under ASTM D5458 and ASTM D5748, respectively. Downstream conversion uses a cast film line with a 30:1 L/D barrier screw, die gap 0.5–0.8 mm, melt temperature 240–260°C, air knife–vacuum box pinning, chill roll temperature 18–30°C, and roll wrap angle 200–220°. Production-scale observations indicate that melt temperature excursions above 280°C initiate oxidation gel formation and reduce film clarity, while insufficient air-knife pressure increases edge neck-in and width variation beyond ±2 mm. Pre-stretch units operate in-line at 2.0–2.5:1 elongation before rewind. Terminal products are machine stretch wrap at 15–23 µm, hand stretch wrap, and pre-stretched rolls for pallet unitization.

    Blown Film Bubble Stability When Frost Line Height Drops Below 600 mm

    Frozen food packaging converters processing DOWLEX™ 2027G on mono-layer blown film lines use a polymer fraction of 85 wt% DOWLEX™ 2027G blended with 15 wt% high-pressure LDPE having a melt index of 0.25 g/10 min to increase bubble melt strength, with slip/antiblock masterbatch added at 1.0–2.0 wt% relative to the polymer blend. Direct food contact compliance is established under FDA 21 CFR 177.1520(c) 3.2a for olefin polymers and EU Regulation (EU) No 10/2011, with overall migration verified to EN 1186-1:2002 at limits below 10 mg/dm². Production parameters include die diameter 250–400 mm, die gap 1.8–2.4 mm, blow-up ratio 2.0–2.5:1, frost line height 600–900 mm, melt temperature 200–230°C, chill air temperature 8–12°C, and output 120–180 kg/h. If frost line height drops below 600 mm at maximum output, transverse-direction tear strength rises while machine-direction tear strength drops, requiring on-line monitoring of ASTM D1922 Elmendorf tear and ASTM D1709 dart drop. Terminal products include frozen vegetable bags, ice cream packaging, and processed fruit pouches at 40–80 µm.

    For three-layer PET/ink/adhesive/LLDPE dry food pouches, the sealant web is converted from DOWLEX™ 2027G at a layer ratio of 18–25% of total package thickness. The sealant film is either 100 wt% DOWLEX™ 2027G or a 70 wt% DOWLEX™ 2027G / 30 wt% LDPE blend when cast web flatness must be increased for wide-width lamination. Solvent-free laminating lines apply polyurethane adhesive at 1.6–2.0 g/m², with nip roller temperature 40–50°C, machine speed 250–350 m/min, and curing at 40°C for 24–48 h. The sealant web is extruded on a cast film line with die gap 0.5 mm, melt temperature 240–260°C, and corona treatment held at 42–46 dyn/cm before in-line lamination. Seal performance is verified to ASTM F88/F88M-21 for peel seal strength and ASTM F1921-20 for hot tack. Table 1 lists the compliance matrix for this direct food contact application. Terminal products are dry food pouches, powdered beverage sachets, and stand-up pouch inner sealant layers.

    Regulation / StandardClause / MethodTarget / Verification
    FDA 21 CFR 177.1520(c) 3.2aOlefin polymer food-contact status
    EU Regulation (EU) No 10/2011Annex IOverall migration limit 10 mg/dm²
    EN 1186-1:2002Total immersionMigration test method
    ASTM F88/F88M-21Peel seal strengthSeal strength in N/25 mm
    ASTM F1921-20Hot tack methodHot tack force in N/25 mm

    A Tear Propagation Threshold in Heavy-Duty Sack Film

    Heavy-duty sack film produced from DOWLEX™ 2027G is characterized by a balance of dart impact strength and machine-direction tear resistance, controlled by a polymer fraction of 90 wt% DOWLEX™ 2027G blended with 10 wt% high-pressure LDPE, with carbon black masterbatch added at 2–3 wt% relative to the polymer blend at 50% carbon black loading in an LLDPE carrier. Compliance is specified by ASTM D1922 for Elmendorf tear, ASTM D1709 for dart drop, ISO 527-3 for film tensile properties, and EU Directive 94/62/EC Article 11 for heavy metals below 100 mg/kg. Downstream conversion occurs on a blown film line with internal bubble cooling, die diameter 300–500 mm, die gap 2.0–2.5 mm, blow-up ratio 1.8–2.0:1, frost line height 800–1,200 mm, melt temperature 210–240°C, and output 150–220 kg/h. Operation above 250°C melt temperature reduces machine-direction tear strength despite higher throughput, so the equipment is maintained in the lower melt temperature range. Finished film is slit to 600–1,200 mm widths and formed into side-gusseted sacks on bottom-seal conversion machines. Terminal products include commercial ice bags, fertilizer sacks, and construction aggregate bags at 100–150 µm.

    On multi-layer nonwoven laminating lines, a cast embossed backsheet layer for hygiene articles is produced from DOWLEX™ 2027G at a film basis weight of 18–25 g/m². The polymer fraction is 95–97 wt% DOWLEX™ 2027G, with titanium dioxide white masterbatch added at 3–5 wt% containing 60% TiO₂, and polymer processing aid dosed at 0.5–1.0 wt% relative to the polymer fraction to suppress melt fracture at high cast line speeds. Compliance for hygiene articles is verified under REACH Regulation (EC) No 1907/2006 SVHC limits below 0.1% w/w per substance and under OEKO-TEX Standard 100 Class I for infant article components or Class II for adult articles, depending on the finished article. Slip/antiblock masterbatch is limited to ≤1.5 wt% because higher silica loadings degrade embossing pattern retention and adhesive peel strength. The cast film line uses a matte-finish embossed chill roll at 20–30°C, melt temperature 230–260°C, die gap 0.4–0.6 mm, line speed 200–300 m/min, corona treatment 38–44 dyn/cm, and in-line lamination to polypropylene nonwoven with peel strength 20–50 N/25 mm. Terminal products are diaper backsheet, adult incontinence backsheet, and feminine hygiene outer cover laminates.

    How Does Stretch Hood Film Maintain Load Integrity at -20°C?

    Stretch hood film extrusion systems operating at ambient temperatures down to −20°C use DOWLEX™ 2027G at 90–95 wt% blended with 5–10 wt% polyolefin plastomer or ultra-low-density polyethylene to increase low-temperature puncture resistance. Slip masterbatch is limited to 0.5–1.0 wt% relative to the polymer blend to maintain the coefficient of friction required by stretch hood application units. Tensile strength is specified under ASTM D882 and ISO 527-3, tear resistance under ASTM D1922, and packaging heavy metal compliance under EU Directive 94/62/EC Article 11. The blown film process operates at a high blow-up ratio of 3.5–4.0:1 to balance machine and transverse elongation, with die diameter 300–600 mm, die gap 2.0–2.5 mm, frost line height 1,200–1,800 mm, melt temperature 210–230°C, and film thickness 80–120 µm. Stretch hood machinery applies the finished covers at stretch ratios of 1.2–1.5:1 over palletized loads. Terminal products are stretch hood covers used for pallet loads of construction materials, beverage bottles, and bagged chemical products.

    Free Quote

    Competitive Dow DOWLEX™ 2027G Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2027G Linear Low Density Polyethylene is a pelletized, solution-process ethylene–octene copolymer supplied for blown-film, cast-film, sheet, and geomembrane applications in which stiffness, tensile yield strength, and slow crack growth resistance are required. The grade is specified at a nominal density of 0.941 g/cm³ by ASTM D792 or ISO 1183-1:2019 and a nominal melt index of 0.80 g/10 min by ASTM D1238 or ISO 1133-1:2022 at 190 °C under 2.16 kg. These values place the resin at the upper edge of the LLDPE density range and provide a crystalline fraction that is intermediate between general-purpose film LLDPE and typical MDPE/HDPE grades. The product is used in heavy-duty sacks, industrial liners, agricultural film, geomembranes, and coextruded structures that require a high-stiffness outer or core layer. Because it is a linear polyethylene rather than a high-pressure LDPE, the shear thinning is lower and the melt elasticity is lower; these differences require process settings that are not directly transferable from LDPE lines without adjustment.

    At the molecular level, the resin possesses a linear backbone with short-chain branches introduced by the octene comonomer. The density of 0.941 g/cm³ reflects a higher crystalline fraction than 0.918 g/cm³–0.920 g/cm³ butene-based film grades, but the branch distribution suppresses the large spherulitic morphology typical of HDPE. This structural feature helps retain puncture resistance and Elmendorf tear while increasing secant modulus under ASTM D882. Capillary rheometry according to ISO 11443 shows a less shear-thinning viscosity curve than high-pressure LDPE, which is one reason LDPE is added at 10%–30% by mass to modify bubble stability in some blown-film structures.

    What melt-processing envelope is reported for blown-film lines running DOWLEX 2027G?

    In single-screw blown-film lines with screw diameters of 45 mm to 90 mm and L/D ratios of 24:1 to 30:1, DOWLEX 2027G is processed at melt temperatures between 190 °C and 240 °C. Barrel profiles generally start at 160 °C–180 °C in the feed zone and rise to 200 °C–230 °C at the adapter and die. Die gaps are typically 1.2 mm to 2.0 mm; below 1.0 mm, high shear stress at the die lip can initiate sharkskin or melt fracture. Blow-up ratios between 2.0 and 3.0 are used to balance MD/TD orientation, and frost line height is adjusted to avoid excessive transverse shrinkage and roll blocking. The melt index of 0.80 g/10 min confers higher melt strength than many 1.0 g/10 min LLDPE film grades, but it also produces higher screw torque and head pressure. Mixed-shear or barrier screws with Maddock sections are preferred over low-shear metering screws; external bubble stabilization, internal bubble cooling, or oscillating haul-off improve gauge uniformity at commercial output rates.

    Because the resin has a narrow molecular weight distribution and linear backbone, shear thinning is lower than high-pressure LDPE. A higher melt temperature within the recommended range reduces viscosity and improves die flow but can increase oxidation risk if residence time exceeds 30 min at temperatures above 230 °C. Start-up practice typically begins with a lower melt temperature and low screw speed until the bubble is stable; the frost line is then raised to reduce orientation and limit dart impact losses. Downgauging trials should monitor backpressure, melt temperature variation, and bubble flutter because these are early indicators of extruder overload or inadequate temperature control.

    Resin parameters used in lot acceptance and process setup for DOWLEX 2027G
    ParameterStandard designationCondition
    DensityASTM D792 / ISO 1183-1:201923 °C immersion
    Melt indexASTM D1238 / ISO 1133-1:2022190 °C, 2.16 kg
    Melt peakASTM D341810 °C/min
    ESCRASTM D169350 °C, 10% Igepal CO-630

    When DOWLEX 2027G is run on flat-die sheet or geomembrane lines, melt temperatures of 200 °C to 230 °C are common. The die gap is generally set 0.5 mm to 1.0 mm above the finished sheet thickness, with draw ratios kept below 15:1 to limit neck-in and draw resonance. The resin can exhibit neck-in at high haul-off speeds because of the linear backbone; a short air gap, ozone treatment, or lower line speed can preserve width. Condensation on cold pellets transferred into a warm extrusion hall can introduce moisture-related surface defects even though polyethylene is not hydrolytically sensitive. When pellets are stored below 10 °C and then opened in air above 60 % relative humidity, drying at 70 °C for 2 h–4 h is recommended. The resin does not require pre-drying under normal ambient storage conditions.

    Tensile, tear, and slow crack growth benchmarks versus butene LLDPE and HDPE

    The 0.941 g/cm³ density places DOWLEX 2027G above conventional butene-based film LLDPE grades specified at 0.918 g/cm³–0.920 g/cm³. This density difference increases secant modulus and tensile yield strength under ASTM D882 because the crystalline fraction is higher. In mono- or multi-layer structures for heavy-duty sacks, the higher modulus permits thickness reduction while preserving load resistance, provided ASTM D1709 dart impact and ASTM D1922 Elmendorf tear remain above the end-use requirements. The octene comonomer in DOWLEX resins alters short-chain branching distribution relative to butene copolymers of the same density; this molecular difference usually produces a more favorable balance between stiffness and impact toughness, but film values are highly dependent on die gap, BUR, frost line height, and gauge.

    Environmental stress crack resistance is evaluated by ASTM D1693; in 10% Igepal CO-630 at 50 °C, higher-density octene LLDPE generally exhibits longer failure times than butene-based LLDPE of comparable melt index, although acceptance limits are end-user-specific. Compared with high-pressure LDPE, DOWLEX 2027G has higher tensile yield, tensile ultimate strength, and puncture resistance, but lower melt elasticity and lower shear thinning. This means LDPE is often blended at 10%–30% by mass to improve bubble stability and extrusion processing, at the expense of some stiffness and dart impact. Compared with a 0.949 g/cm³ HDPE film resin, DOWLEX 2027G is lower in modulus and upper service temperature but higher in dart impact and Elmendorf tear, making it suitable for large geomembrane and liner applications that require puncture resistance and field seaming.

    Heavy-duty industrial liner converters often trial DOWLEX 2027G at reduced gauges from 150 µm to 100 µm–120 µm against a reference film made from butene LLDPE at 0.920 g/cm³. A complete comparison requires conditioning films at 23 °C and 50 % relative humidity for at least 40 h before testing. Tensile properties are measured by ASTM D882; dart impact by ASTM D1709 Method A or B depending on gauge; tear propagation by ASTM D1922; and seal strength by ASTM F88 or ASTM F2029. Seal initiation temperature generally rises as density increases, so the seal jaws may require an additional 5 °C–10 °C compared with 0.918 g/cm³ LLDPE. Because the resin has a higher density, the film surface can block more readily on the winder; slip and antiblock additive levels are adjusted based on coefficient of friction measured by ASTM D1894. Published peer-reviewed data for this specific resin in all film structures is limited; converter trials remain the definitive basis for setting target specifications.

    Regulatory conformity is documented under food-contact and packaging migration clauses

    Food-contact declarations for DOWLEX 2027G must be verified against the current supplier certificate. Polyethylene resins of this type may be regulated under FDA 21 CFR 177.1520(c); final articles must comply with extractive limitations and the conditions of use for the relevant paragraph. In the European Union, plastic food-contact compliance is assessed under EU 10/2011, with an overall migration limit of 10 mg/dm² for surface-area-limited articles and 60 mg/kg for volume-limited articles. Specific migration limits for octene-1, catalyst residues, and additives are substance-specific and must be checked. Packaging and packaging waste obligations such as EU 94/62/EC set combined heavy metal limits of 100 mg/kg for lead, cadmium, mercury, and hexavalent chromium. REACH registration under EC 1907/2006 is separate from end-use food-contact status; SVHC content below 0.1 % w/w per article is a common documentation threshold. RoHS restrictions are generally not applicable to polyethylene packaging, but electrical and electronic equipment applications require a separate technical file.

    Compliance documentation matrix for DOWLEX 2027G
    Regulation / standardConditionTypical limit
    FDA 21 CFR 177.1520(c)Polyethylene food-contact articlesFinished article end-use restrictions
    EU 10/2011Overall migration10 mg/dm² or 60 mg/kg
    EU 94/62/ECHeavy metalsSum ≤ 100 mg/kg
    EC 1907/2006SVHC reporting0.1 % w/w per article

    Lot-specific certificates list the actual stabilizer and processing aid package. Because polymerization source and finishing additives can vary between production sites, no universal regulatory statement should be assumed for drinking-water, medical, or pharmaceutical applications. In such cases, the resin should be qualified under the appropriate standard, such as NSF/ANSI 61 for potable water contact or USP Class VI for medical device use, only after extraction testing on the finished article. Declaration of compliance under EU 10/2011 does not automatically cover all food simulants, high-temperature sterilization, or long-duration repeated-use conditions because migration depends on time, temperature, and food simulant type.

    Storage below 40 °C in dry, out-of-UV conditions preserves additive package stability. Prolonged exposure to ultraviolet light without a compounded light stabilizer can initiate photo-oxidation and reduce film elongation at break. The resin should not be stored in direct contact with aromatic hydrocarbons, chlorinated solvents, or strong oxidizing acids because solvent absorption can swell the polymer and degrade mechanical properties. In silos and hoppers, fine particle carryover from high-volume conveying can reduce flow if allowed to accumulate; rotary feeders and dust collection systems should be inspected at intervals consistent with total throughput. The resin is supplied in pellet form and does not require special ventilation. Good housekeeping prevents pellet contamination from other polymers, and purging with a lower-viscosity polyethylene or commercial purging compound is standard when changing from a dissimilar resin family.

    Top