| HS Code | 312228 |
| Density | 0.920 g/cm3 |
| Melt Index | 4.0 g/10 min |
| Melt Flow Ratio | 7.7 |
| Melting Point | 124 °C |
| Vicat Softening Point | 94 °C |
| Tensile Strength At Yield | 9.7 MPa |
| Tensile Strength At Break | 21.4 MPa |
| Ultimate Elongation | 800 % |
| Flexural Modulus | 240 MPa |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 220 g |
| Elmendorf Tear Strength Td | 480 g |
| Haze | 1.5 % |
| Gloss At 45 Degrees | 90 |
| Coefficient Of Friction | 0.2 |
As an accredited Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade is supplied in 25 kg polyethylene-lined bags, palletized for shipping. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Dow DOWLEX™ 2027A LLDPE cast film grade in 25 kg bags, palletized, stretch-wrapped, and secured for shipment. |
| Shipping | DOWLEX™ 2027A is shipped as non-hazardous polyethylene resin pellets in 25 kg bags, octabins, or bulk trucks/railcars. Transport in clean, dry equipment at ambient temperatures, avoiding moisture, contamination, and excessive heat. No special UN hazard classification required. Follow local regulations and keep packaging sealed. |
| Storage | Store Dow DOWLEX™ 2027A in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers or bags tightly closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Maintain clean, segregated storage, use first-in, first-out rotation, and follow the manufacturer’s SDS recommendations. |
| Shelf Life | Typically 24 months from date of manufacture when stored unopened in a cool, dry, well-ventilated area away from direct sunlight. |
On high-speed pallet-wrapping lines producing machine-grade stretch film, DOWLEX 2027A is processed as the core layer in ABA coextrusion because its nominal density of 0.917 g/cm³ per ISO 1183-1 and melt index of 2.3 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022 support draw ratios from 1:2 to 1:3 without significant melt resonance. The core layer is commonly maintained at 70–85 wt% of total throughput, with the cling layer formulated at 8–15 wt% low molecular weight polyisobutene and the release layer at 5–12 wt% LDPE or metallocene LLDPE. The core extruder is a 90 mm smooth-bore single screw with 25:1 to 30:1 L/D and a barrier mixing section; the skin extruders are 45–60 mm units. Melt temperature at the die lip is held between 240 °C and 265 °C; die gap is set to 0.8–1.5 mm, and air gap from die to chill roll is kept in the 10–80 mm range. Chill roll temperature of 18–30 °C reduces blocking while preserving film flatness. At 400–900 m/min line speed, neck-in and edge bead are controlled by adjusting edge-pinning devices and the draw ratio; the wound film gauge is typically 12–23 µm. Puncture resistance is evaluated per ASTM D5748, cling force decay per ASTM D5458, and elongation at break per ISO 527-3. In production audits, excessive draw resonance appears when the line speed exceeds the melt strength threshold and creates transverse gauge bands of ±5–8%; this is corrected by raising melt temperature no higher than 265 °C or by replacing 10–20 wt% of the core with LDPE. Winding tension is tapered from initial setpoint to 40–60% of initial value at full roll diameter to prevent blocking and core collapse. The terminal product is pallet unitization film with pre-stretch capability to 200–300% on powered rollers, used as 17 µm A-type machine wrap, 23 µm hand wrap, and 12 µm coreless high-performance wrap. Limitations include loss of cling at chill roll temperatures above 30 °C, and film with greater than 5 wt% edge trim regrind may exhibit gel points and localized puncture failure. Actual line values are extruder-specific and should be verified against the machinery manufacturer’s thermal homogeneity test.
| Parameter | Lower bound | Upper bound | Measurement basis |
|---|---|---|---|
| Die gap | 0.8 mm | 1.5 mm | Feeler gauge at die lip |
| Air gap | 10 mm | 80 mm | Laser displacement sensor |
| Chill roll temperature | 18 °C | 30 °C | Infrared pyrometer |
| Melt temperature at adapter | 240 °C | 265 °C | Submersion thermocouple |
| Line speed | 400 m/min | 900 m/min | Nip-driven tachometer |
| Winding tension taper | 40% | 60% | Load cell calibration |
Fresh-cut leafy-green packaging is typically produced as a coextruded cast lidding film with a sealant layer containing DOWLEX 2027A blended with 10–20 wt% LDPE to reduce seal initiation temperature. The targeted seal initiation is 85–105 °C at 0.5 N/25 mm sealing force on a heat-seal tester according to ASTM F88/F88M. Haze is measured at ≤8% on 38 µm film per ASTM D1003; gloss is measured at ≥70 on a 60° Gardner micro-gloss meter. Antifog performance is obtained by adding glycerol monostearate at 0.5–1.2 wt% to the sealant layer, but loadings above 1.2 wt% reduce coefficient of friction below 0.20 and cause film slip on vertical form-fill-seal transport belts. Chill roll temperature is set from 22 °C to 35 °C; higher temperatures increase haze due to surface replication defects, while lower temperatures can condense moisture and create optical defects in high-humidity plants. To maintain oxygen transmission through microperforated or lidding applications, the base film thickness is controlled between 25 µm and 50 µm; WVTR is then measured per ASTM F1249 at 23 °C and 90% RH. For compliance, the film is tested against EU Regulation 10/2011 with overall migration below 10 mg/dm² by EN 1186-1, and against US FDA 21 CFR 177.1520 for olefin polymers under conditions of use set out in 21 CFR 176.170(c) appropriate to the intended food-contact temperature. The terminal products include pillow packs for washed spinach, modified-atmosphere bags for shredded lettuce, and lidding film for fresh-cut fruit trays. Process limitation: migration of antifog additive to the film surface takes 24–72 h after extrusion, so films used immediately after slitting may exhibit fogging in cold-chain storage at 2–5 °C.
| Standard/Regulation | Relevant requirement | Test method | Acceptance criterion |
|---|---|---|---|
| EU Regulation 10/2011 | Overall migration | EN 1186-1 | 10 mg/dm² maximum |
| US FDA 21 CFR 177.1520 | Olefin polymer compliance | FDA extraction cell | Conditions of use per 21 CFR 176.170(c) |
| ASTM D1003 | Haze | Haze meter | ≤8% on 38 µm film |
| ASTM F88/F88M | Seal strength | Tensile tester with heated seal bar | ≥0.5 N/25 mm at 85–105 °C |
| ASTM F1249 | Water vapor transmission rate | Modulated infrared sensor | Application-specific barrier target |
For coextruded cast films used as automotive body-panel transit protection, the core layer of DOWLEX 2027A is combined with a pressure-sensitive adhesive tie layer and an outer slip layer; total film thickness is typically 50–80 µm. The film is processed on a 2.2 m die with 0.9–1.2 mm die gap and a chill roll polished to Ra 0.02–0.05 µm; surface corona treatment is set to 42–48 dyn/cm as measured by wetting fluids. Adhesive peel from painted steel substrate is measured per ASTM D3330 at 0.2–1.5 N/25 mm; higher values reduce residue but can deform on sharp fascia radii. For outdoor storage up to 6 months, the backing layer is compounded with a hindered amine light stabilizer at 0.15–0.40 wt% and a benzotriazole UV absorber at 0.10–0.30 wt%. Without this package, gloss retention on the core layer drops below 60% after 2,500 kJ/m² of artificial weathering per ISO 4892-2. Terminal products include bumper fascia transit film, rocker-panel film, and glass lamination interlayer protective film. The main operational boundary is contamination: rosin-based adhesive tie layers can cross-contaminate downstream food-grade film runs on the same line; complete purging with LDPE of 4–8 g/10 min melt index and dismantling of the feedblock is required when switching back to food-contact production.
When DOWLEX 2027A cast film is used as the adhesive web in thermal lamination of woven polypropylene sacks, the film is extruded at 220–250 °C and subsequently nipped to woven PP fabric before complete solidification. The bond strength of the laminate is evaluated by ISO 11339 T-peel; production values for 40 µm cast film bonded to 70 g/m² woven PP are typically in the range 4–9 N/15 mm, depending on nip pressure and fabric corona level. The woven fabric is pre-treated to 38–44 dyn/cm with a corona discharge unit immediately ahead of the laminator to improve mechanical interlocking. Failure mode in peel testing shifts from adhesive to cohesive within the film when the lamination speed exceeds 120 m/min and the melt curtain residence time falls below 180 ms; edge weave and curtain sag then create unbonded bands at the laminate edges. To suppress edge weave, the die exit temperature is maintained above 230 °C, and the die-to-nip distance is kept between 80 mm and 150 mm. For fertilizer and pet food sack applications, the laminate must pass a 6-m drop test per ISO 7965-2 in which the sack is filled with 25 kg and dropped from 1.2 m. The terminal products are woven PP valve sacks, FIBC liner laminations, and flexible intermediate bulk container patch films. Limitation: films containing excessive slip additives can reduce laminate bond below 4 N/15 mm; high-slip grades should not be reintroduced into the adhesive film stream at loadings above 5 wt% of edge trim regrind.
In high-speed VFFS lamination for dry beverage powders and seasoning mixes, DOWLEX 2027A is down-gauged to 25–40 µm and used as the sealant web against an oriented PET or biaxially oriented PP print web. It is laminated with a solventless adhesive at 1.5–2.5 g/m² coat weight and cured at 35–45 °C for 24–48 h. Seal initiation is targeted at 80–100 °C to match VFFS jaw speeds of 60–120 packs/min; hot tack measured per ASTM F1921 at 110 °C, 0.25 N/mm², 0.5 s must remain above 2.0 N/15 mm before the laminate is released. Edge trim and off-spec film are repelletized and metered back into the sealant layer at loadings below 8 wt%; above this threshold, gel counts above 25 gel/m² and seal strength decay of 15–20% at 100 °C have been recorded in line audits, although published data for this specific configuration is limited. The terminal products are stick packs, sachets, and pillow pouches for dried soups and instant coffee. Limitation: sealant layers containing regrind must not be used in contact with liquid or high-fat products unless migration testing under EU 10/2011 conditions D2 and D3 has been completed.
Frozen vegetable form-fill-seal operations require cast films based on DOWLEX 2027A only when the required service temperature is above −30 °C; below this temperature, the film’s tensile impact transitions from ductile to brittle unless compounded with 5–10 wt% metallocene LLDPE or plastomer. The film is typically extruded at 35–60 µm thickness with a chill roll temperature of 20–28 °C and treated to 36–40 dyn/cm for lamination or printing. Puncture resistance under ASTM D5748 is maintained above 30 N for 50 µm film to resist frozen peas and cut vegetable edges. Seal integrity is confirmed by vacuum leak testing per ASTM F2338 using dye penetration; seal parameters of 115–130 °C and 0.3–0.5 s dwell on a horizontal VFFS machine are used. The terminal products include bags for frozen green beans, broccoli florets, and ice cube overwrap. Limitation: the grade is not suitable for hot-fill or microwavable applications above 60 °C, and films stored at −20 °C for more than 12 months should be tested for cold-temperature seal fracture before shipment.
Competitive Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade is an ethylene-octene copolymer supplied in pellet form for monolayer and coextruded cast film structures. The resin is specified by a nominal density of 0.917 g/cm³ measured under ASTM D792 and a melt mass-flow rate of 2.3 g/10 min determined at 190 °C/2.16 kg using ASTM D1238. These values represent typical lot averages, not guaranteed upper or lower specification limits, and should be verified against the supplier certificate of analysis for the production lot. The grade is used in cast stretch wrap, industrial overwrap, form-fill-seal lidding, and liners where high elongation, puncture resistance, and film gauge reduction are specified. Relative to butene-based cast film LLDPE grades of similar density and melt index, DOWLEX 2027A typically provides higher dart drop impact and Elmendorf tear propagation resistance; relative to high-pressure LDPE, it has lower melt strength but higher toughness at equivalent thickness.
| Property | Test method or framework | Typical value |
|---|---|---|
| Density at 23 °C | ASTM D792 / ISO 1183-1 | 0.917 g/cm³ |
| Melt mass-flow rate | ASTM D1238 / ISO 1133-1, 190 °C/2.16 kg | 2.3 g/10 min |
| Comonomer type | Manufacturer declaration | Octene-1 |
| Food-contact framework | FDA 21 CFR 177.1520(c) | Subject to extraction and end-use limitations |
The cast film grade designation is significant because the molecular architecture is selected for melt curtain stability, chill roll contact, and post-quench toughness rather than for bubble stability in blown film. In cast processing, the resin is extruded through a flat die, drawn over a short air gap, and quenched on a polished chill roll. This permits the use of lower melt strength resins than would be acceptable in blown film, allowing DOWLEX 2027A to deliver toughness without requiring high-pressure LDPE blending in many structures.
The primary structural difference is the comonomer length. DOWLEX 2027A is an octene-1 copolymer; butene-based cast film grades use a shorter C4 α-olefin. During Ziegler-Natta polymerisation, octene introduces branches that are sufficiently long to participate in the crystal lattice only to a limited extent, while butene branches are more readily accommodated into the lamellar crystals. This affects the tie-chain population between crystalline lamellae and the way stress is transferred across the amorphous phase. Cast film made from octene LLDPE therefore tends to exhibit higher Elmendorf tear strength and dart drop impact strength at the same film gauge, as measured by ASTM D1922 and ASTM D1709. The difference is most pronounced in transverse direction tear and at thicknesses below 25 µm. Published data for direct gauge-for-gauge comparison against every commercial butene grade is limited; converter trials should be used to confirm specific downgauging margins.
The melt mass-flow rate of 2.3 g/10 min places the grade in the medium fluidity range for cast film. Compared with high-pressure LDPE, the absence of long-chain branching reduces elastic memory and die swell, but also reduces melt strength. In cast film, low melt strength is less limiting than in blown film because the melt curtain is supported by the chill roll at a defined air gap. Compared with metallocene-catalysed ethylene-octene grades, Ziegler-Natta DOWLEX 2027A generally exhibits broader molecular weight distribution, which can improve extruder throughput stability and reduce melt pressure at the same output but may sacrifice the low-haze optical values achieved with metallocene grades. In cast film, chill roll quench and gauge uniformity often dominate optical performance, making the broader distribution acceptable for many industrial packaging applications.
On cast film lines equipped with single-screw extruders having screw diameters from 75 mm to 120 mm and L/D ratios of 24:1 to 30:1, DOWLEX 2027A is typically processed with a barrier screw and a Maddock mixing section. Melt temperatures recorded at the die are commonly maintained between 240 °C and 270 °C. The lower bound is set by the need to minimise melt viscosity and eliminate unmelted resin pellets; the upper bound is set by oxidative degradation. At temperatures above 290 °C, die-lip oxidation can form gel specks that transfer to the film as visual defects and can destabilise the cast melt curtain along the die edge. Lines without nitrogen purge of the feed throat or die area typically require more frequent die-lip cleaning when run at the upper end of the temperature range.
Screen packs of 80/120/200 mesh are used on many cast lines to provide filtration and build backpressure; the exact configuration should be selected with the extruder manufacturer because excessive backpressure above the thrust bearing limit damages the gear reducer. Chill roll temperatures for DOWLEX 2027A are generally maintained between 18 °C and 30 °C. Chill water temperature control and roll surface polish affect film haze and blocking behaviour. If the roll temperature is set too low, moisture can condense from the surrounding air when relative humidity exceeds the dew point of the room, producing surface defects and roll wrap instability. If the roll temperature is set too high, the film may retain heat and block on the winder, especially in monolayer films at thicknesses below 15 µm.
Operation below 18 °C accelerates the quench rate of the cast melt, which can reduce haze and increase line-speed capability at the same roll wrap angle. However, the faster quench also reduces the time available for crystallisation and alters the distribution of crystal thickness. For LLDPE, rapid quenching can shift the film into a lower-density, lower-modulus state with a less stable crystal network. The film may exhibit lower blocking resistance because the outer surface remains sufficiently quenched, but the skin-core morphology can become anisotropic. In practice, cast film lines operating near 15 °C chill roll temperatures often require a decrease in melt temperature and an increase in air gap to maintain uniform melt curtain contact. Failure to adjust the air gap can produce transversal gauge bands because the melt curtain contacts the roll unevenly and the quench front moves across the web. Haze changes should be measured by ASTM D1003. Published data quantifying the exact haze change for DOWLEX 2027A at each chill roll temperature is limited, but production-scale observations indicate that chill roll temperature setpoints below 10 °C are usually unnecessary and may lead to condensation unless the line is enclosed with dehumidified air handling.
The dew point of the cast film line environment is the operational boundary. At a line-room temperature of 25 °C and relative humidity above 60%, a 15 °C chill roll will generate surface condensation. Therefore, chill roll setpoints below the ambient dew point require dry-air enclosures or an increase in room dew point control. Condensation on the chill roll before the melt contact point causes pitting and irregular quench marks; condensation on the inner side of the film after the wrap angle causes blocking on the winder. These are failure modes observed on production lines with open chill roll stands and no dehumidified air supply.
For food-contact applications in the United States, the finished polyethylene article may be evaluated for compliance with 21 CFR 177.1520(c), subject to density, maximum extractable fraction, and end-use temperature limitations. The resin itself is manufactured to support such compliance, but migration testing of the finished film or package is the responsibility of the converter or brand owner. In the European Union, plastic materials and articles intended for food contact are assessed under Regulation (EU) 10/2011, including the overall migration limit of 10 mg/dm²; compliance requires testing on the final article because additives, printing inks, and converting conditions influence migration. For industrial packaging, the EU Packaging and Packaging Waste Directive 94/62/EC sets heavy metal limits, generally 100 mg/kg total for lead, cadmium, mercury, and hexavalent chromium in the packaging material. DOWLEX 2027A is not recommended for prolonged immersion in strong oxidising agents, aromatic hydrocarbons, or chlorinated solvents at elevated temperature; such exposures can swell the polyethylene matrix and alter dimensions without necessarily reducing molecular weight.
In cast stretch film structures at thicknesses from 10 µm to 25 µm, DOWLEX 2027A is used as the core layer or as a full monolayer film when a balance of puncture resistance and clarity is required. Puncture resistance can be evaluated with ASTM D5748, tear propagation with ASTM D1922, and dart drop impact with ASTM D1709. A move from a butene-based LLDPE to DOWLEX 2027A may allow film gauge reduction only after wrapping trials have confirmed load retention and pallet stability on the target wrapper; published data for the specific gauge reduction is limited. Load retention testing is commonly carried out with a stretch wrapper fitted with a force transducer and a palletised test load, using a controlled pre-stretch ratio. The absence of long-chain branching in DOWLEX 2027A relative to LDPE means that the film’s machine-direction stretch behaviour is dominated by post-extrusion orientation and the pre-stretch setting rather than by melt-phase strain hardening.
For form-fill-seal lidding and industrial liners, the resin is selected when the finished article is exposed to aggressive loading or irregular product surfaces. The film is typically corona treated online to achieve a surface tension of 38–42 mN/m for ink adhesion; surface tension is checked according to ASTM D2578. Corona treatment should take place immediately before the winder to minimise surface tension decay. In coextruded cast films, DOWLEX 2027A is often combined with an outer layer of lower-melting or higher-gloss resin to optimise sealing and optics; however, the specific layer ratio depends on the coextruder feedblock and die design. In coextruded stretch wrap, the grade is typically placed in the core or bottom layer while an outer layer with lower melting point or higher surface tension controls cling and release balance. If the core layer is replaced with DOWLEX 2027A from a butene-based LLDPE, the converter may observe a change in neck-in and edge-trim behaviour at start-up; die width and air gap adjustments are required to maintain the same trimmed web width. Published data for the specific shrinkage forces and edge-bead profiles at all line speeds is limited, and line trials should govern final settings.