| HS Code | 906990 |
| Density | 0.920 g/cm³ |
| Melt Index 190 C 2 16 Kg | 0.45 g/10 min |
| Melt Flow Ratio I10 I2 | 8.0 |
| Melting Point | 123 °C |
| Vicat Softening Point | 96 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 31.0 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 240 MPa |
| Hardness Shore D | 50 |
| Brittleness Temperature | -70 °C |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Strength Md | 300 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 10% |
| Gloss 45 | 70% |
| Coefficient Of Friction | 0.2 |
| Blocking | 50 g |
| Water Absorption | <0.01% |
| Thermal Conductivity | 0.33 W/m·K |
| Specific Heat | 2.3 J/g·°C |
| Coefficient Of Thermal Expansion | 2E-4 /°C |
| Volume Resistivity | >1E16 ohm·cm |
| Dielectric Strength | 18 kV/mm |
| Dielectric Constant | 2.3 |
| Dissipation Factor | 0.0002 |
As an accredited Dow DOWLEX™ 2025G Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow DOWLEX™ 2025G Linear Low Density Polyethylene is packaged in 25 kg polyethylene bags for safe handling and storage. |
| Container Loading (20′ FCL) | Dow DOWLEX™ 2025G LLDPE: 20′ FCL container loading, 25 kg bags, palletized, approximately 18–20 metric tons per container. |
| Shipping | DOWLEX™ 2025G LLDPE ships as non-hazardous, pelletized resin in 25 kg bags, 1000 kg bulk bags, octabins, or bulk trucks/railcars. Transport in clean, dry containers and keep packaging sealed to prevent contamination. Store cool and dry, away from direct sunlight and moisture. Standard industrial handling; no special hazard classification required. |
| Storage | Store DOWLEX™ 2025G in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original packaging closed to prevent moisture, dust, and contamination. Avoid prolonged outdoor exposure, UV light, and strong oxidizers. Maintain clean, segregated storage at ambient temperature with FIFO rotation. Handle pellets safely to prevent slipping. Follow local regulations and manufacturer’s SDS recommendations. |
| Shelf Life | Dow DOWLEX 2025G has indefinite shelf life when stored cool, dry, sealed, away from direct sunlight, moisture, and contaminants. |
On three-layer blown-film lines producing heavy-duty formwork liners and industrial sacks, DOWLEX 2025G, with nominal density 0.920 g/cm³ and melt flow rate below 1.0 g/10 min per ASTM D1238, is formulated with the polymer fraction consisting of 80–90 wt% DOWLEX 2025G and 10–20 wt% high-pressure LDPE; carbon black masterbatch is added at 2–4 phr only when the liner must block ultraviolet exposure during outdoor concrete curing or rubble storage. The LDPE fraction is not inert: its long-chain branching raises melt strength and stabilizes the bubble on high-stalk configurations, but exceeding 20 wt% depresses dart impact and Elmendorf tear below the neat LLDPE control. The finished film is typically manufactured on a single-screw extruder with 30:1 L/D barrier screw, internal bubble cooling, die gap 2.0–2.5 mm, blow-up ratio 2.5:1–3.0:1, and melt temperature 190–220 °C; thickness is held at 100–250 µm because film below 100 µm is inadequate for formwork puncture, while film above 250 µm can increase die-lip residence time and promote oxidation gels if melt temperature exceeds 230 °C. Tensile properties are controlled against ISO 527-3:2018, dart impact against ASTM D1709-16a method A, and tear propagation against ASTM D1922-09(2015). The resulting downstream product types are heavy-duty rubble sacks, formwork liners, construction debris bags, and furniture covers; for outdoor service, the carbon black grade must meet dispersion criteria under ISO 18553 when assessed on a 25 µm microtome section.
Three-layer silage covers and greenhouse tunnel films containing DOWLEX 2025G are usually run with a 20/60/20 layer ratio; the core layer polymer is 85–92 wt% DOWLEX 2025G with 8–15 wt% LDPE, while the outer weathering skin contains UV masterbatch at 6–12 phr of skin polymer, with active HALS at 0.2–0.6 wt% and a benzotriazole or triazine UV absorber at 0.1–0.3 wt% of total film mass. The skin also carries 1–3 phr silica antiblock to prevent film-to-film adhesion during storm-wind flapping. The extrusion line uses internal bubble cooling with a die gap of 1.8–2.4 mm, a blow-up ratio of 2.8:1–3.5:1, and a melt temperature of 200–230 °C; because silage film is typically 150 µm and greenhouse cover can reach 180 µm, the outer skin extruder must maintain a stable melt curtain at low die gap pressure to avoid draw resonance at the collapsing frame. Accelerated weathering is assessed by ISO 4892-2:2013 cycle 1; tensile retention after exposure is measured by ISO 527-3:2018, and tear retention by ASTM D1922-09(2015). Above 12 phr UV masterbatch, screw feeding becomes inconsistent and machine-direction tear increases sharply; below 6 phr, carbonyl index rises after 12 months of outdoor exposure in high-UV sites. Terminal products are silage bags, silage clamp covers, and greenhouse tunnel covers.
Stretch hood extrusion differs from cast pallet wrap because the bubble is collapsed into a gusseted hood that must retain load across top corners during transit. The polymer fraction is 70–85 wt% DOWLEX 2025G with 15–30 wt% metallocene VLDPE or plastomer; a low-migration tackifier is added at 0.5–2 phr. The VLDPE component is required for elastic recovery after 100% machine-direction elongation, while the tackifier reduces pallet slip without acting as a migratory adhesive at the levels used. The blown-film line is operated in high-stalk configuration with a die gap of 1.6–2.0 mm, a blow-up ratio of 3.5:1–4.5:1, a collapsing frame angle of 22–26°, and melt temperatures of 210–230 °C; film thickness is held between 60–120 µm because thinner hoods fail corner puncture tests and thicker hoods reduce the elastic recovery that the process relies upon at the frame. Compliance testing is conducted under ASTM D882-18 for tensile and elongation, ASTM D1922-09(2015) for tear, and ASTM D5459-95 for machine-direction elastic recovery and permanent deformation. Above 30 wt% plastomer, machine-direction tear and roll blocking increase; below 15 wt%, recovery after 100% elongation drops below the threshold required to maintain pallet load stability during transport vibration testing. The terminal product is a stretch hood for palletized building materials, white goods, and bagged chemicals.
DOWLEX 2025G is blended with the polymer fraction at 75–85 wt% and high-pressure LDPE at 15–25 wt%; anti-fog masterbatch is added at 2–4 phr, and slip/antiblock at 1–2 phr, for frozen vegetable pouches and ice bags. The LDPE co-component lowers seal initiation temperature on vertical form-fill-seal lines, while DOWLEX 2025G supplies the low-temperature impact strength required at freezer temperatures; too high an LDPE level reduces dart impact on 40 µm film at −25 °C. The three-layer coextrusion line is run with a frost line height of 300–500 mm, die gap 1.8–2.2 mm, blow-up ratio 2.0:1–2.5:1, and melt temperature 185–210 °C; lower melt temperature is preferred to limit anti-fog migration to the film surface before the roll is wound. Food-contact compliance is assessed under EU Regulation 10/2011 Annex I with an overall migration limit of 10 mg/dm² and under 21 CFR 177.1520(c) for olefin polymers; film properties are tested by ASTM D882-18 and ASTM D1709-16a. Anti-fog masterbatch above 4 phr raises seal initiation temperature and increases haze to unacceptable levels; if the frost line is below 300 mm, surface migration is too rapid and causes blocking on the finished roll. The downstream products are frozen vegetable pouches, ice bags, and frozen seafood overwrap.
LLDPE geomembrane panels based on DOWLEX 2025G use the resin at 100 phr base polymer, with carbon black masterbatch added at 2–3 phr and a hindered phenolic–phosphite antioxidant package at 0.1–0.5 phr; the carbon black must be dispersed sufficiently to meet the uniformity and content requirements of GRI-GM17 for LLDPE geomembranes. Flat-die sheet extrusion is the dominant downstream process for this configuration, with melt temperatures of 230–260 °C, die gap 2.0–3.0 mm, and polished roll stack temperatures of 70–90 °C; panel thickness is typically 0.75–2.00 mm, with thickness control verified according to ASTM D5199-12 at multiple points across the web. Puncture resistance is tested under ASTM D4833-07, tear resistance under ASTM D1004-13, and oxidative induction time under ASTM D3895-19. Carbon black masterbatch loadings above 3 phr may lower tensile yield and create surface pitting; loadings below 2 phr risk failing the carbon black content specification in GRI-GM17. Terminal products are smooth flexible geomembrane panels for pond liners, canal liners, landfill caps, and temporary containment cells.
Film recyclers running post-consumer LDPE/LLDPE blown-film reclaim can use DOWLEX 2025G at 20–35 wt% of total feed, with washed post-consumer LDPE/LLDPE flake at 65–80 wt%, to restore dart impact and tear strength in refuse sacks and recycled carrier bags. The virgin resin is gravimetrically dosed into washed flake before a single-screw extruder with a 80–100 mesh screen pack, die gap 2.0–2.5 mm, blow-up ratio 3.0:1, and melt temperature 190–220 °C. Below 20 wt% addition, post-consumer film at 100 µm fails the ASTM D1709-16a dart impact specification used for municipal refuse sacks; above 35 wt%, melt pressure on a 75 mm grooved-barrel extruder rises sufficiently to reduce screw speed and output by 10–15% when the screen pack is not changed more frequently. Recycled content is traceable under EN 15343:2007, and finished film is tested by ISO 527-3:2018 and ASTM D1922-09(2015). The primary finished products are post-consumer recycled refuse sacks, carrier bags, and light-duty industrial liners.
Competitive Dow DOWLEX™ 2025G Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DOWLEX™ 2025G Linear Low Density Polyethylene is supplied as a pelletised ethylene/1-octene copolymer produced by a solution polymerisation route. The resin is used in cast film, blown film, injection moulding, and compounding operations in which a nominal melt index of 2.5 g/10 min and a nominal density of 0.920 g/cm³ are appropriate. The 1-octene comonomer introduces short-chain branching that differs from the 1-butene branching found in many conventional LLDPE grades; the resulting molecular architecture changes melt relaxation, impact strength, and low-temperature toughness. DOWLEX 2025G occupies a medium-flow position within the DOWLEX family: its melt viscosity is lower than that of film extrusion grades with melt indices near 1.0 g/10 min, and higher than that of masterbatch-carrier or injection-moulding grades with melt indices above 10 g/10 min. For incoming resin evaluation, density and melt index are the primary control variables because they determine both processing pressure and final tensile performance.
Because sales specifications may change by region and production campaign, incoming resin evaluation should rely on the certificate of analysis supplied with each lot. Public datasheets list the following representative values. Melt index is determined at 190 °C under 2.16 kg load using ASTM D1238 or ISO 1133-1:2022. Density is measured on annealed compression-moulded plaques by ASTM D792 or ISO 1183. Melting peak temperature by differential scanning calorimetry is reported between 121 °C and 124 °C under ASTM D3418 or ISO 11357-3. Vicat softening temperature is reported between 107 °C and 110 °C under ASTM D1525 or ISO 306. Tensile yield strength is approximately 11 MPa at 50 mm/min crosshead speed under ASTM D638; elongation at break is typically greater than 800 %. Flexural modulus lies in the range 260–310 MPa under ASTM D790 or ISO 178.
| Property | Representative Value or Range | Test Method |
|---|---|---|
| Melt index | 2.5 g/10 min | ASTM D1238 / ISO 1133-1 |
| Density | 0.920 g/cm³ | ASTM D792 / ISO 1183 |
| Melting peak | 121–124 °C | ASTM D3418 / ISO 11357-3 |
| Vicat softening | 107–110 °C | ASTM D1525 / ISO 306 |
| Tensile yield strength | 11 MPa | ASTM D638 |
| Elongation at break | >800 % | ASTM D638 |
| Flexural modulus | 260–310 MPa | ASTM D790 / ISO 178 |
On production-scale blown-film towers fitted with 300 mm and 400 mm annular dies, field observations show that DOWLEX 2025G requires a larger die gap than high-pressure LDPE at the same melt temperature to avoid melt fracture. A starting die gap of 1.5–2.0 mm, barrel profile from 180 °C to 220 °C, and die temperature between 215 °C and 230 °C are common. Melt-temperature deviations greater than ±5 °C across the die circumference can produce gauge bands and reduce Elmendorf tear uniformity under ASTM D1922. When bubble flapping occurs at melt temperatures below 190 °C, reducing blow-up ratio from 3.0:1 to 2.5:1 or raising die temperature by 5 °C is used to restore bubble stiffness. Cast film lines operate with chill-roll temperatures between 15 °C and 30 °C; roll temperature is adjusted with line speed and film thickness to control blocking and haze. In injection moulding, the resin is processed at melt temperatures of 210–250 °C, mould temperatures of 20–40 °C, and injection pressures of 50–100 MPa depending on flow-length-to-wall-thickness ratio. Short-shot correction in thin-wall lids with flow-length ratios above 150:1 is more effectively achieved by increasing melt temperature to 230 °C and injection velocity than by raising hold pressure alone, because pressure drop in the cavity is shear-rate dependent.
Capillary rheometry at 190 °C yields shear-thinning behaviour that is typical of linear low-density polyethylene: apparent viscosity decreases from roughly 800 Pa·s to 150 Pa·s as shear rate increases from 100 s⁻¹ to 1,000 s⁻¹. These values are material-class reference points rather than grade-specific batch data. The resulting lower shear sensitivity compared with branched LDPE means that die-lip pressure does not fall as rapidly with increasing screw speed; screw-motor loads on 90 mm barrier screws are generally lower than those for a 1.0 g/10 min LLDPE at the same output. Published data for this specific configuration is limited.
After injection moulding, semi-crystalline solidification of DOWLEX 2025G produces anisotropic mould shrinkage. Under ASTM D955, unannealed linear low-density polyethylene of 0.920 g/cm³ density commonly exhibits flow-direction shrinkage of 1.5–2.0 % and transverse shrinkage of 1.0–1.5 % after 24 h at 23 °C and 50 % RH. These values are influenced by gate size, packing pressure, mould temperature, and part thickness; published data for this specific configuration is limited. Higher packing pressures in the range 60–80 MPa and longer hold times reduce voiding and dimensional scatter but can increase cycle time. For film gauges below 20 µm, slit-width variation and film blocking become more sensitive to ambient humidity and winding tension. Because film made from DOWLEX 2025G is semicrystalline, post-extrusion shrinkage measured after exposure to 80 °C for 30 min is usually below 2 % in the machine direction and below 1 % in the transverse direction; this value should be confirmed for slit rolls stored at elevated warehouse temperatures.
Cast film produced from DOWLEX 2025G at 50 µm gauge can show haze below 5 % under ASTM D1003 when the melt temperature is above 190 °C and the chill-roll surface is smooth. Blown film haze is higher because surface roughness and internal scattering increase with frost-line height. Heat-seal initiation under ASTM F2029 is typically in the range 95–105 °C for 0.920-density LLDPE, but the seal-initiation plateau shifts downward by 2–5 °C when the film is downgauged below 50 µm. Hot-tack strength under ASTM F1921 is lower than that of metallocene-catalysed LLDPE grades with a very narrow molecular-weight distribution, but the broader processing window of DOWLEX 2025G reduces the risk of melt fracture in cast film dies.
Compared with a butene-copolymer LLDPE of similar density and melt index, DOWLEX 2025G typically shows higher dart impact strength under ASTM D1709 and higher Elmendorf tear under ASTM D1922 at equal gauge. The improvement is attributed to the longer 1-octene short-chain branches, which increase the number of tie molecules connecting crystalline lamellae. The difference is most pronounced in film above 20 µm and becomes less reliable at severe downgauging or when pigment concentrates above 3 wt% are present because dispersion defects dominate failure. Compared with high-pressure LDPE, DOWLEX 2025G has higher tensile yield strength under ASTM D638, higher puncture resistance, and a more linear viscosity curve, but lower melt tension and less bubble stability in blown-film extrusion. Processors replacing LDPE with DOWLEX 2025G on an existing blown-film line may need to narrow the die gap to 1.5 mm, reduce melt temperature to 205 °C, or use a dual-lip air ring to maintain the frost line. In cast film, the lower melt strength is less restrictive because the web is mechanically supported by the chill roll.
Within the DOWLEX LLDPE range, the 2.5 g/10 min melt index of DOWLEX 2025G separates it from lower-melt-index blown-film grades and from higher-flow injection-moulding grades. A lower-melt-index DOWLEX film grade generates higher melt pressure and higher bubble stiffness but requires more screw torque and can limit output on extrusion lines with undersized motors. DOWLEX 2025G reduces pressure drop and improves injection-moulded surface replication in thin sections, but its lower melt strength makes it less forgiving in large-bubble blown-film production. The selection is therefore made by the dominant process constraint, not by a single property ranking.
Compared with metallocene-catalysed LLDPE grades of similar density, DOWLEX 2025G generally shows a wider blown-film processing window and lower hot-tack strength. The narrower molecular-weight distribution of metallocene grades raises melt tension and improves bubble stability in very thin film, but it also narrows the temperature range between melt fracture and bubble instability. DOWLEX 2025G is also not a direct substitute for polar copolymers such as ethylene-vinyl acetate where adhesion, surface tack, or high-melt-tension processing is required.
Food-contact suitability for polyethylene grades in this density range is generally assessed under FDA 21 CFR 177.1520(c) for olefin polymers, with the finished article required to meet extractables end-tests that depend on food type and use temperature. In the European Union, plastics intended for food contact are evaluated under EU Regulation No 10/2011, including the overall migration limit of 10 mg/dm² for migrants from the finished material or article. DOWLEX 2025G is a base polyolefin; the final regulatory status depends on the additive package, polymerisation residues, conversion conditions, and the geometry of the finished article. For pharmaceutical packaging, the resin may be evaluated against relevant European Pharmacopoeia polyethylene monographs, including tests for sulfated ash and extractable heavy metals. Under RoHS Directive 2011/65/EU, the base resin is not typically considered to contain cadmium, lead, mercury, or hexavalent chromium above the specified maximum concentration values, but the finished article must be assessed if conductive fillers or metal-based pigments are added. REACH obligations apply at the article level; manufacturers should confirm the current substance-of-very-high-concern status of any additives with the resin supplier.
Storage under dry ambient conditions is sufficient for pelletised DOWLEX 2025G; pre-drying is required only when bags are opened at high humidity or when condensation is visible. If surface moisture is present, drying for 2–4 h at 70–80 °C in a desiccant or hot-air drier returns the pellets to processable condition. The resin should not be exposed to strong oxidising agents, halogenated solvents, or open flame. Prolonged residence at melt temperatures above 250 °C in low-flow zones of the screw or die can cause thermo-oxidative degradation and gel formation; shutdown and start-up are best managed with a purge grade of low-melt-index polyethylene or a commercial polyolefin purge compound. Regrind incorporation up to 20 wt% is common in non-critical film and moulding, but repeated heat history reduces dart impact and increases odour potential. Addition of fluoropolymer processing aids at 200–500 ppm may be used when melt fracture appears in narrow-die-gap cast film lines. Long-term outdoor exposure of unpigmented DOWLEX 2025G is limited by oxidative degradation; carbon-black loading of 2–3 wt% is required for weatherable film applications, and ultraviolet stabiliser performance must be assessed under ISO 4892-2 or ASTM D4329 for the target service life.