| HS Code | 252744 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | 1-Octene |
| Density | 0.920 g/cm³ |
| Melt Index 190 C 2 16 Kg | 1.0 g/10 min |
| Melt Flow Ratio I21 I2 | 30 |
| Melting Point | 124 °C |
| Vicat Softening Point | 104 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 24 MPa |
| Ultimate Elongation | 800% |
| Flexural Modulus | 240 MPa |
| Dart Drop Impact F50 | 120 g |
| Elmendorf Tear Strength Md | 360 g |
| Elmendorf Tear Strength Td | 450 g |
| Haze | 10% |
| Gloss 45 | 55 |
As an accredited Dow DOWLEX™ 2021D Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow DOWLEX™ 2021D LLDPE is supplied as pellets in 25 kg polyethylene bags, with optional 1,000 kg bulk bags. |
| Container Loading (20′ FCL) | 20′ FCL container loading of Dow DOWLEX™ 2021D LLDPE: 25 kg bags, palletized, shrink-wrapped; approx. 24–25 MT net weight. |
| Shipping | Dow DOWLEX™ 2021D Linear Low Density Polyethylene is a non-hazardous LLDPE resin. Not regulated for DOT, IMDG, IATA, or ADR. Ship in sealed bags/octabins; protect from moisture, heat, UV, and contamination. Store cool, dry, ventilated. No special transport requirements apply. Use normal personal protective equipment. |
| Storage | Store Dow DOWLEX™ 2021D in a dry, clean, well-ventilated warehouse at ambient temperature. Keep bags or containers sealed, palletized, off the floor, and away from direct sunlight, heat, ignition sources, and oxidizing materials. Prevent moisture, dust, and contamination; avoid excessive stacking or UV exposure. Use first-in, first-out stock rotation and inspect containers regularly for damage. |
| Shelf Life | DOWLEX 2021D has a recommended shelf life of 24 months when stored in original packaging under cool, dry conditions, away from direct sunlight. |
In agricultural film production, DOWLEX 2021D with a nominal density of 0.920 g/cm³ and a melt index of 1.0 g/10 min at 190°C/2.16 kg per ASTM D1238-13 functions as the core or outer skin layer in three-layer coextruded blown film. The octene comonomer distribution reduces low-temperature brittle failure relative to butene-copolymer LLDPE after repeated folding, stone impact, and UV exposure. Addition ratios for silage cover and bale wrap structures typically allocate 60–80 wt% DOWLEX 2021D to the core layer, balance 20–40 wt% high-pressure LDPE for bubble stability, incorporate 1.0–2.5 wt% HALS-based UV stabilizer masterbatch, and add 0.5–1.0 wt% fluoroelastomer processing aid. The production process operates on a three-layer blown film line with a grooved-feed extruder diameter of 45–75 mm, L/D of 24:1–30:1, die gap of 1.8–2.2 mm, blow-up ratio of 2.2:1–3.0:1, melt temperature of 195–210°C, and frost line height held at 8–12 die diameters. If melt temperature exceeds 215°C, melt strength decreases and gauge variation can exceed ±8% across the layflat; below 185°C, melt pressure rises to 300–350 bar and homogenization deteriorates, producing visible gel-like specks from high-shear heating. Terminal finished product types include 25–50 µm silage pit covers, round bale stretch wrap, silo bags, and greenhouse side sheeting. Industry compliance for agricultural covering films is assessed under EN 13206:2017 for thermoplastic covering films used in agriculture and horticulture; where the film may contact feed, Article 17 of Regulation (EC) No 183/2005 requires that materials do not contaminate feed, and REACH registration obligations apply to the resin and compounded stabilizer packages.
| Application scenario | Standard or regulation | Test method or clause | Typical measured parameter |
|---|---|---|---|
| All food-contact packaging scenarios | FDA 21 CFR 177.1520(c) 3.2a | Extraction testing per food type | Olefin polymer compliance for food contact |
| All food-contact packaging scenarios | EU Regulation (EU) No 10/2011 | Overall migration test | Overall migration limit 10 mg/dm² |
| Resin quality and process reproducibility | ASTM D1238-13 / ISO 1133-1:2022 | Melt flow rate at 190°C/2.16 kg | 1.0 g/10 min nominal |
| Resin density | ASTM D1505-18 / ISO 1183-1:2019 | Density gradient column method | 0.920 g/cm³ nominal |
| Film tensile properties | ASTM D882-18 / ISO 527-3:2018 | Machine and transverse direction tensile | Application-specific strength and elongation |
| Low-temperature impact resistance | ASTM D1709-16A / ISO 7765-1:2004 | Dart impact, Method A or B | Gauge-dependent impact energy |
| Trouser tear resistance | ASTM D1922-17 / ISO 6383-2:1983 | Elmendorf tear propagation | Machine and transverse direction tear force |
| Hot-tack performance | ASTM F1921-12 | Hot-tack and seal strength after cooling | Seal window 120–140°C typical |
| Cling performance for cast stretch | ASTM D5458-12 | Peel cling test | Gauge-dependent cling force |
| Puncture propagation resistance | ASTM D5748-19 | Probe puncture energy | Gauge and formulation dependent |
Heavy-duty industrial liners and form-fill-seal sacks based on octene-copolymer LLDPE require a balance of puncture tolerance, low-temperature impact resistance, and seal reliability that cannot be met by conventional butene-copolymer LLDPE at equal gauge. DOWLEX 2021D is processed in monolayer extrusion at addition ratios of 85–100 wt%, with 0–15 wt% recycled plant scrap and 2–4 wt% carbon black masterbatch for outdoor storage. In coextruded A/B/A structures, the outer layers contain 60–80 wt% DOWLEX 2021D and 20–40 wt% high-pressure LDPE for bubble cooling, while the middle layer may be loaded with reprocessed edge trim. Production on a high-output blown film line uses a grooved-feed extruder of 90–120 mm diameter with L/D of 30:1, die diameter of 250–400 mm, die gap of 2.2–2.5 mm, blow-up ratio of 2.0:1–2.5:1, and output of 200–450 kg/h. Melt temperature is maintained at 200–220°C, melt pressure at 250–350 bar, and the air ring cooling capacity must be sufficient to avoid blocking at the collapsing frame when producing 100–150 µm film. At production scale, a batch-to-batch melt index variance of ±0.1 g/10 min can shift gauge profiles and sealing onset; the screw speed and nip take-up speed are trimmed accordingly. Terminal finished product types include 50–150 µm construction and demolition waste sacks, FIBC inner liners, chemical bag-in-box films, heavy-duty mailers, and industrial rollstock for automated sack lines. Industry compliance is anchored to ASTM D4976-12a for polyethylene extrusion materials, ASTM D1709-16A for dart impact, and ISO 7765-1:2004 for film impact. Where liners are installed inside UN-certified FIBC outer bags, the outer bag is certified under UN 13H4 or UN 13H3; the liner itself is not a stand-alone UN pack but must not reduce the completed packaging performance under top-lift and drop tests.
When frozen food packagers lower gauge from 50 µm to 35 µm, the limiting variable is not extruder capacity but the retention of low-temperature dart impact and hot-tack width on vertical form-fill-seal lines. DOWLEX 2021D is blended at 70–90 wt% with 10–30 wt% high-pressure LDPE to produce a three-layer coextruded film at 35–50 µm. The octene copolymer chain architecture provides retained impact after conditioning for 24 h at -18°C, measured per ASTM D1709-16A. The downstream blown film process uses a die gap of 1.6–2.0 mm, blow-up ratio of 2.2:1–2.8:1, melt temperature of 190–205°C, and bubble cage temperature of 10–18°C to stabilize the frost line. Seal initiation temperature is controlled below 110°C by the addition of 0.5–1.5 wt% slip/antiblock masterbatch; hot-tack strength is measured at 120–140°C sealing temperature on a laboratory heat-seal tester per ASTM F1921-12, and the package must survive product filling temperatures as low as -25°C without seal pop-off. Terminal finished product types include frozen vegetable pouches, ice cream packaging, frozen seafood films, and overwrap for frozen meat. Industry compliance is governed by FDA 21 CFR 177.1520(c) 3.2a for olefin polymers in food contact and EU Regulation (EU) No 10/2011, with an overall migration limit of 10 mg/dm². Operational boundaries include storage at 15–35°C and RH <60% to prevent surface condensation; no desiccant drying is required under normal conditions. Published data for this specific configuration on some proprietary VFFS machine geometries is limited, so start-up trials with a sealant temperature profile increment of 5°C are required to map the hot-tack window for each machine.
Cast film extrusion for machine pallet wrap based on an ethylene-octene resin with a melt index of 1.0 g/10 min introduces a viscosity-related processing boundary: the melt temperature must be raised to 240–270°C to obtain the required draw-down and die-exit stability, but temperatures above 285°C initiate gel formation and volatile odor bodies that can transfer to packaged goods. DOWLEX 2021D is used at addition ratios of 70–100 wt%, with 0–30 wt% metallocene plastomer for puncture enhancement and 1–3 wt% polyisobutylene cling masterbatch. The cast line configuration includes a 120–180 mm barrier screw with L/D of 30:1–36:1, die gap of 0.6–0.8 mm, die-to-chill roll air gap of 20–40 mm, chill roll temperature of 12–18°C, and line speed of 400–800 m/min. Neck-in below 8% of die width is maintained by adjusting air gap and melt temperature. At line speeds above 600 m/min, insufficient chill roll contact can create cling-layer delamination and telescoping rolls during winding; the variable of edge pinning and vacuum box pressure must be tuned to the resin melt strength. Terminal finished product types include 12–23 µm hand pallet wrap, 15–25 µm machine stretch film, and 20–30 µm silage bale wrap from cast lines. Compliance is anchored to ASTM D5458-12 for peel cling, ASTM D5748-19 for puncture propagation, and ISO 527-3:2018 for tensile properties. For food wrapping applications, the film must meet FDA 21 CFR 177.1520(c) 3.2a and EU Regulation (EU) No 10/2011; for non-food industrial pallet wrap, REACH Annex XVII restrictions apply to intentionally added substances.
As an extrusion lamination layer on woven polypropylene, paper, and aluminum foil, DOWLEX 2021D functions at coat weights of 10–25 g/m² and requires controlled oxidation at the melt curtain surface to build adhesion to polar substrates. The resin is processed at 100 wt% or blended with 10–20 wt% high-pressure LDPE to reduce neck-in and edge waste. The tandem extrusion lamination line operates with a 90–120 mm screw, melt temperature of 275–315°C, air gap of 125–250 mm, nip pressure of 30–60 N/mm, and line speed of 80–200 m/min. Substrates are corona treated to 38–42 mN/m immediately before lamination; woven polypropylene requires sufficient coat weight to cover surface fiber roughness, while paper requires moisture control below 6% to prevent steam blow-outs at the nip. Terminal finished product types include fertilizer sacks, cement bags, FIBC outer panel coating, thermal insulation facings, and flexible intermediate bulk container labels. Industry compliance for food-grade laminates is governed by FDA 21 CFR 177.1520(c) 3.2a and EU Regulation (EU) No 10/2011, with overall migration limited to 10 mg/dm²; REACH registration applies to the resin and its antioxidant package. Published data for specific adhesion values to epoxy-based woven PP inks is limited, so a production trial with a peel adhesion test per ASTM F88/F88M-15 is required to set air gap and melt temperature for each substrate lot.
When DOWLEX 2021D replaces a butene-copolymer LLDPE in high-speed vertical form-fill-seal sealant layers, the difference in seal initiation and hot tack must be addressed through formulation and machine settings. Addition ratios in the sealant layer typically use 80–100 wt% DOWLEX 2021D combined with 0–20 wt% LDPE, 2–3 wt% synthetic silica antiblock, and 0.05–0.15 wt% erucamide slip by total layer weight. The downstream process is three-layer coextruded blown film with a die gap of 1.8–2.2 mm, blow-up ratio of 2.4:1–3.0:1, melt temperature of 190–220°C, and a calibrated bubble cage that keeps the frost line at 8–10 die diameters. Sealant films of 25–40 µm are then used on vertical form-fill-seal lines running 60–120 bags/min. If line speed exceeds 30 m/min and sealing temperature rises above 140°C, surface stickiness may cause product buildup on sealing jaws; the slip package is then reduced or the sealing jaw release coating is changed to a higher-release fluoropolymer. Terminal finished product types include dry food pouches, frozen snack films, pet food bags, and hygiene packaging laminates. Industry compliance is anchored to FDA 21 CFR 177.1520(c) 3.2a and EU Regulation (EU) No 10/2011; seal strength after cooling is measured per ASTM F88/F88M-15, and hot-tack strength is measured per ASTM F1921-12. For low-temperature packaging of frozen snacks, the sealant layer must not show cohesive failure when the package is dropped from 1.0 m at -20°C; this is verified by a production-line drop test rather than by a standardized ISO method alone.
Competitive Dow DOWLEX™ 2021D Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DOWLEX™ 2021D Linear Low Density Polyethylene is an ethylene–1-octene copolymer produced by solution polymerization. The grade is used in cast film, coextruded sealant webs, surface-protection film, and lamination structures where low-temperature sealing force and puncture resistance are specified. Two resin control values are commonly quoted: melt mass-flow rate of 1.0 g/10 min measured under ISO 1133-1:2022 at 190 °C with 2.16 kg load, and density of 0.917 g/cm³ measured under ISO 1183-1:2019. The comonomer is 1-octene; this yields hexyl short-chain branches rather than the ethyl branches produced by 1-butene in a C4-LLDPE. At equal density and melt flow rate, the octene branch is more effective at reducing crystallinity, which changes seal initiation, dart impact, and tear behavior.
Solution-phase synthesis produces a narrower short-chain branching distribution than many gas-phase Ziegler-Natta C4-LLDPE grades and does not create the long-chain branching associated with autoclave LDPE. The absence of long-chain branching reduces extensional viscosity and melt strength compared with LDPE at equivalent melt index. On blown film lines this is a processing boundary; on cast film lines it reduces melt drawing instabilities. Catalytic residue is lower than in some gas-phase Ziegler-Natta systems, which lowers the probability of gel formation during extended residence time. The resin remains a hydrocarbon and oxidatively degrades if held at melt temperature above 260 °C for prolonged periods.
Incoming resin may be tested under the following analytical matrix. Values are typical published figures for quality control, not batch-product specifications.
| Parameter | Method | Typical value or condition |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | 1.0 g/10 min, 190 °C / 2.16 kg |
| Density | ISO 1183-1:2019 | 0.917 g/cm³ |
| DSC melting peak | ISO 11357-3:2018 | 121 °C, onset range 118–124 °C |
| Vicat softening point | ASTM D1525 A50 | 100 °C, range 98–102 °C |
| Food-contact base resin | FDA 21 CFR 177.1520; EU Regulation 10/2011 | Olefin polymer |
Thermal analysis by differential scanning calorimetry under ISO 11357-3:2018 displays a broad melting endotherm rather than a single sharp peak. The low-temperature tail of the endotherm is functionally important because sealant layers begin to flow when low-melting crystallites melt; seal initiation is therefore not governed solely by the peak melting point. The crystallization temperature during cooling from the melt is observed between 102 °C and 106 °C, which is lower than butene LLDPE at equal density.
Material stored at ambient conditions typically contains less than 300 ppm moisture. Pre-drying at 80 °C for 2 hours is usually unnecessary below 60% RH; above that threshold surface moisture can generate splay and microvoids in cast film. Resin exposed to high humidity should be bag-closed immediately after use because condensation on cold pellets is the primary source of moisture-related defects.
A cast film configuration using a single-screw extruder with 24:1 to 30:1 L/D, a barrier screw, a spiral Maddock mixing tip, and screen pack of 80/120/80 mesh is typical. Melt temperature should be maintained from 220 °C to 250 °C; die-zone temperature above 260 °C increases carbonyl index and gel formation in the melt film. Die gap of 1.5 mm to 2.5 mm is adequate for 20 µm to 80 µm film. Air gap between die exit and chill roll is generally set from 4 cm to 12 cm; longer air gaps can accelerate neck-in and reduce edge stability. The chill roll is operated at 15 °C to 30 °C. Lower temperatures may increase haze by promoting condensation, while higher temperatures reduce quench rate and raise crystallinity.
Reducing melt temperature from 250 °C to 220 °C typically raises melt pressure by 12% to 18% on a 90 mm extruder at constant screw speed. The pressure increase should be monitored through the screen pack. A screen change is indicated when pressure differential across the pack exceeds 80 bar to 120 bar, depending on extruder rating. Residence time should be kept below 8 min at set temperature; longer times at 250 °C may generate oxidized gel specks.
On a coextrusion cast line with a 65 mm extruder running the skin layer at 30% thickness, the resin typically runs at 220 °C to 240 °C without screw cooling. If screw cooling is required to prevent pellet bridging in the feed throat, the feed-throat temperature is above the pellet softening point and should be reduced to 40 °C to 50 °C.
Film haze and gloss are measured on 50 µm monolayer cast film under ASTM D1003 and ASTM D2457. Haze values below 3% and gloss values above 80 at 45° are representative for clean, high-polish chill rolls; however, published data for this specific grade at every cooling roll configuration is limited.
The property balance of DOWLEX 2021D is usually evaluated by three film tests. Dart impact is measured under ASTM D1709 Method B on 50 µm film; typical values for octene LLDPE of this density and melt-flow-rate fall in the 180 g to 260 g range, with higher values at lower frost-line height or faster chill-roll quench. Elmendorf tear is measured under ASTM D1922; machine-direction tear is typically lower than transverse-direction tear because orientation in cast film is greater in the machine direction. For DOWLEX 2021D, published data for this exact film thickness is limited, but octene LLDPE grades generally show a narrower MD/TD elongation ratio than butene LLDPE.
Machine-direction secant modulus measured under ASTM D882 on 50 µm film is generally 130 MPa to 170 MPa; transverse-direction values are 110 MPa to 150 MPa. The MD/TD modulus ratio reflects machine-direction orientation and increases with line speed. For this grade, a cast line speed above 150 m/min can raise the MD/TD tensile modulus ratio to 1.5–2.0.
Seal initiation is measured under ASTM F88/F88M using a 15 mm wide specimen and seal dwell of 0.5 s at 2.8 bar. The onset of a seal strength of 2 N per 15 mm typically occurs between 95 °C and 105 °C. This is 5 °C to 8 °C lower than a comparable butene LLDPE at the same density and melt flow rate. Hot-tack strength under ASTM F1921 follows a similar depression of the seal window; the maximum hot-tack force occurs at 100 °C to 115 °C on a 30 µm coextruded sealant layer.
In blown film, the lower melt strength of solution LLDPE manifests as reduced bubble stability compared with LDPE. A conventional blown film line with a 75 mm grooved-feed extruder, 30:1 L/D, and dual-lip air ring may require blow-up ratio from 2.0:1 to 2.5:1 and frost-line height 800 mm to 1,200 mm. Blending with LDPE at 20 wt% to 30 wt% increases melt strength and is common for lamination film. Blending above 70 wt% DOWLEX 2021D can reduce bubble stability unless internal bubble cooling is active.
In cast film, replacement of butene LLDPE with DOWLEX 2021D usually permits downgauging because the octene architecture increases dart impact retention at lower film thickness. If a converter reduces film thickness from 30 µm to 25 µm, dart impact drops, but the octene grade retains a higher fraction of the 30 µm value than butene LLDPE under ASTM D1709. This is due to greater tie-chain concentration in the amorphous phase. The edge trim from this resin can be recycled into the same cast film feed at up to 20 wt% without observable gel formation if the trim is not thermally degraded; higher recycle ratios may require melt filtration at 80 mesh.
Within the DOWLEX film portfolio, the 2021D grade is differentiated from higher-density grades such as DOWLEX 2045G, which is typically reported at 0.920 g/cm³ and 1.0 g/10 min. The 0.003 g/cm³ density difference changes secant modulus and seal initiation by a measurable amount; however, published cross-grade data for this specific pair is limited.
Regulatory conformance is normally documented by a certificate of compliance. The base resin is classified as an olefin polymer under U.S. FDA 21 CFR 177.1520 and is formulated to meet the framework of EU Regulation 10/2011 for plastic food-contact materials. REACH Regulation 1907/2006 requires that substances of very high concern are not intentionally added. The resin does not contain intentionally added per- or polyfluoroalkyl substances. These statements are for the neat resin; converter-added masterbatch, printing ink, and adhesive layers require separate compliance assessments.
The operational boundaries are clear. The grade is not intended for continuous exposure above 80 °C without oxidative stabilizer evaluation, is not supplied with UV-stabilizer packages for long-term outdoor exposure, and is not recommended for contact with strong oxidizing acids at elevated temperature. Film intended for medical device packaging must be validated under ISO 11607-1:2019 and cannot rely solely on the base-resin food-contact status.