| HS Code | 196131 |
| Product Name | DOWLEX™ 2020G Linear Low Density Polyethylene |
| Manufacturer | Dow |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.920 g/cm³ |
| Melt Index 190 C 2 16 Kg | 2.0 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Point | 93 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 29.0 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 241 MPa |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 300 g |
| Haze | 6% |
| Gloss 45 | 80 |
| Comonomer | 1-Octene |
| Form | Pellets |
As an accredited Dow DOWLEX™ 2020G Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DOWLEX™ 2020G Linear Low Density Polyethylene pellets are supplied in 25 kg polyethylene bags or 1000 kg bulk sacks. |
| Container Loading (20′ FCL) | Dow DOWLEX™ 2020G Linear Low Density Polyethylene loaded in 20′ FCL: 25 kg bags, palletized, shrink-wrapped, and securely stowed for transport. |
| Shipping | DOWLEX™ 2020G Linear Low Density Polyethylene is a non-hazardous resin shipped as pellets. Standard packaging includes 25 kg polyethylene bags, stretch-wrapped pallets, bulk bags, or bulk trucks/railcars. No UN/DOT hazard classification applies. Store dry, away from heat and direct sunlight; avoid moisture and contamination. Handle per SDS. |
| Storage | Store DOWLEX™ 2020G indoors in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original containers closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive heat that may cause pellet blocking. Isolate from strong oxidizing agents. Practice first-in, first-out, and follow the safety data sheet and local regulations. |
| Shelf Life | Dow DOWLEX™ 2020G has a recommended shelf life of 24 months when stored in unopened original packaging under cool, dry conditions. |
Flat-die extrusion of DOWLEX™ 2020G for flexible geomembrane liners begins with gravimetric blending rather than tumble mixing. The pellet stream is combined with a carbon black masterbatch at a controlled ratio between 2.0 wt% and 3.0 wt%. Lower loadings do not provide adequate UV stabilization for exposed landfill cap service, while loadings above 3.5 wt% reduce elongation at break and can generate dispersion defects in a single-screw line. The natural resin is an ethylene-octene LLDPE with a nominal density of 0.920 g/cm³ (ASTM D1505) and a melt flow index of 2.0 g/10 min at 190°C/2.16 kg (ASTM D1238; ISO 1133-1:2022). These values permit an adapter melt temperature between 205°C and 230°C without excessive shear heating. Industrial flat-die lines use a single-screw extruder with an L/D ratio of 30:1 to 34:1 and a barrier mixing section. A screen pack of 40/60/80 mesh is common, and the die gap is set between 1.5 mm and 3.0 mm depending on target sheet thickness. Lot-to-lot melt flow index shift is typically held within ±0.2 g/10 min; if the shift exceeds this band, screw speed is adjusted before barrel temperature changes to avoid altering shear history.
The sheet is polished through a vertical or inclined roll stack maintained at 60°C to 85°C. Rapid quench below 40°C is avoided because differential cooling can generate internal stress that appears as curl or uneven shrinkage during field seaming. Gauge uniformity is not cosmetic; finished sheet is checked under ASTM D5199 with tolerance bands of ±10% for nominal thickness from 0.75 mm to 2.5 mm. Edge trim and start-up scrap are repelletized and reintroduced at up to 20 wt%. Above this level, gel content and melt pressure fluctuation become measurable, and puncture resistance under ASTM D4833 can drift downward. Tensile properties are monitored by ASTM D638 Type IV specimens, tear resistance by ASTM D1004, and stress crack resistance by ASTM D5397. Carbon black content is verified by ASTM D4218, and dispersion quality is rated on microtomed sections under ISO 18553; agglomerates above 25 μm act as stress concentrators during hot-wedge fusion seaming.
Field service limits are specific. Continuous exposure to a liner temperature above 60°C reduces modulus and accelerates consumption of the stabilizer package. Contact with strong oxidizing agents, aromatic solvents, or concentrated acids is outside the intended operating envelope. Seam integrity is validated by shear and peel tests under ASTM D6392. For exposed geomembranes, oxidative induction time testing under ASTM D3895 confirms residual stabilizer after sheet extrusion. Published data for DOWLEX™ 2020G-specific geomembrane aging beyond 30 years is limited; site-specific stress crack and OIT retention programs are required.
Thin-wall food-contact components are molded from DOWLEX™ 2020G with a barrel temperature profile that rises from 170°C in the feed zone to 210°C in the metering zone and 220°C at the nozzle. Melt temperature above 230°C increases oxidation and can produce yellowing in thin sections, while temperatures below 190°C produce short shots and visible flow lines. A general-purpose screw with an L/D ratio of 20:1 to 24:1 is adequate for the unfilled resin. Injection pressure is held between 70 MPa and 100 MPa, and hold pressure follows at 50% to 70% of the injection pressure. Mold temperature is controlled at 15°C to 35°C to balance cycle time against surface finish. Mold surface temperature above 35°C increases gloss but can cause sticking on untextured cores; below 10°C, condensation can generate surface splay when relative humidity exceeds 60% RH.
| Parameter | Typical range | Unit |
|---|---|---|
| Feed zone temperature | 170–190 | °C |
| Compression zone temperature | 190–210 | °C |
| Metering zone temperature | 210–225 | °C |
| Nozzle temperature | 205–220 | °C |
| Mold temperature | 15–35 | °C |
| Injection pressure | 70–100 | MPa |
| Hold pressure | 50–70 | % of injection pressure |
| Back pressure | 0.5–1.5 | MPa |
The target wall section for dry food storage containers and freezer drawers is 1.2 mm to 2.5 mm. Flow length-to-thickness ratios up to 150:1 are feasible in multi-cavity tools when the cold-runner system is balanced. Regrind content from edge trimming and rejected parts is maintained below 20 wt%; above this level, notched Izod impact under ASTM D256 and long-term stress crack resistance under ASTM D1693 decline. Food-contact compliance is evaluated under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011. Total migration into food simulants must not exceed 10 mg/dm², and the finished article must pass overall migration testing at 40°C for 10 days when fatty food contact is declared. Pre-drying is not required below 60% RH. If surface condensation is visible on cold-stored pellets, 2 h at 80°C in a desiccant dryer is sufficient. Lot-to-lot melt flow index variation above ±0.2 g/10 min is compensated by screw speed adjustment rather than barrel temperature changes; raising barrel temperature to lower viscosity risks thermal oxidation, while lowering it causes unmelts.
Terminal articles are stackable dry food storage boxes, freezer drawers, lids for dairy spread containers, and thin-wall overpacks. Hot-fill service above 70°C is outside the operating boundary because low crystallinity reduces upper service temperature. Microwave-only reheat of fatty foods is not recommended unless migration testing on the specific geometry demonstrates compliance. For high-temperature sterilization, HDPE or PP should be selected.
Injection-molded single-piece closures with tamper-evident bands are produced from DOWLEX™ 2020G when stress crack resistance at the knurl and hinge is the controlling requirement. The 0.920 g/cm³ density produces lower crystallinity than an HDPE closure resin, which reduces notch sensitivity but also lowers top-load resistance. Closure molding on multi-cavity cold-runner tools uses melt temperatures of 200°C to 220°C and mold temperatures of 10°C to 25°C. Cycle times for a 38 mm single-piece closure fall between 8 s and 14 s, depending on wall thickness and cooling channel efficiency.
Torque retention is affected more by liner compression set and bridge deformation than by resin hardness. Erucamide slip additive is dosed at 500 ppm to 1,000 ppm to control opening torque; overdose above 1,500 ppm can create surface bloom that interferes with liner adhesion. Color masterbatch loading is kept between 1 wt% and 2 wt% for non-food cosmetics and household closures. Food-contact grades use only pigments and additives listed under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011. Terminal articles include dry particulate food closures, personal care jar caps, cosmetic closures, and household chemical trigger spray overpacks.
The limiting condition is carbonated beverage service. The resin does not provide sufficient CO2 barrier or long-term top-load retention for soft drink closures. Hot-fill above 60°C and fatty food simulants require additional migration and seal force testing under ASTM D638 tensile and ASTM D1693 ESCR conditions.
On low-voltage cable jacketing lines, DOWLEX™ 2020G is metered into a single-screw extruder with a barrier screw and vacuum venting. A melt temperature at the crosshead of 200°C to 230°C is typical, and conductor preheat is set at 80°C to 120°C to promote adhesion during pressure extrusion. The base formulation includes a carbon black masterbatch at 2.5 wt% for UV resistance and a stabilizer concentrate at 0.1 wt% to 0.3 wt%. Line speed is set by insulation thickness and cooling trough length; single-core control wire jackets of 0.5 mm to 1.5 mm wall thickness run at 100 m/min to 300 m/min on modern lines. Post-extrusion shrinkback is controlled by staged water temperatures from 40°C to 20°C; a rapid cold-water quench alone can increase residual stress and reduce environmental stress crack resistance under ASTM D1693. Finished jackets are evaluated for tensile strength and elongation under ASTM D638, cold crack under IEC 60811-1, and carbon black content under ASTM D4218. Terminal uses include low-voltage control cable sheaths, fiber optic loose tube protective jackets, and non-flame-rated industrial cable jackets.
The resin is not suitable for riser or plenum cable without flame-retardant fillers such as ATH or magnesium hydroxide; addition of these fillers modifies rheology and requires a separate compounding pass. Published data for DOWLEX™ 2020G-specific flame-retardant cable formulations is limited. Medium-voltage insulation is outside the intended use envelope.
Unfilled DOWLEX™ 2020G enters large-format automotive interior panels when low gloss, low odor, and high notched impact resistance are specified. Sink mark control on thick ribs and bosses improves with a lower melt pressure profile than is typical for mineral-filled PP. Molding presses with clamp force between 10,000 kN and 25,000 kN are used for trunk side trim, door scuff plates, and seat back covers. Melt temperature is maintained at 200°C to 220°C, and mold temperature at 15°C to 40°C. Sequential valve gating prevents visible weld lines on long grained surfaces.
Flexural modulus is the main design constraint. Unfilled LLDPE has a much lower flexural modulus than a filled PP compound; therefore, components requiring static stiffness above approximately 500 MPa are modified by adding a talc masterbatch at 5 wt% to 15 wt% in a separate compounding pass. Emissions performance is checked according to VDA 278, VDA 270, and SAE J1756. Finished parts must also meet OEM-specific scratch and mar requirements after humidity exposure. DOWLEX™ 2020G is not specified for exposed Class A surfaces that require high gloss or resistance to aggressive sunscreens and DEET-based insect repellents.
Competitive Dow DOWLEX™ 2020G Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DOWLEX™ 2020G Linear Low Density Polyethylene is a pelletized ethylene/alpha-olefin resin with a nominal density of 0.920 g/cm³ and a nominal melt flow rate of 2.0 g/10 min under 190 °C/2.16 kg conditions in ISO 1133-1:2022. The product is positioned for general-purpose blown and cast film extrusion where toughness, elongation, and sealability are evaluated against high-pressure LDPE and butene-based C4-LLDPE alternatives. The DOWLEX solution polymerization platform produces a linear backbone without the long-chain branching characteristic of LDPE; comonomer selection in the DOWLEX family is typically octene, although the public datasheet for DOWLEX™ 2020G does not disclose the full short-chain branching distribution, molecular weight distribution, or additive package. The 2020G designation is generally read as a 0.920 g/cm³ density and 2.0 g/10 min melt flow rate, but certificate-of-analysis values should be used for lot release because normal variation in comonomer incorporation can shift the processing window.
At 0.920 g/cm³ the resin is at the lower end of conventional LLDPE density. This provides lower modulus and higher flexibility than fractional melt and medium-density grades in the 0.926–0.940 g/cm³ range, but also lowers heat resistance and tensile yield strength. The melt flow rate of 2.0 g/10 min is a compromise between drawdown in thin-gauge cast film and melt strength in blown film; lower MFR grades such as 1.0 g/10 min have higher bubble stability but require more extruder torque, while higher MFR grades such as 3.5–6.0 g/10 min process at lower pressure but may sacrifice dart impact and machine-direction tear. The resin is not positioned as a high-clarity grade; its haze and gloss depend strongly on die gap, frost line height, and chill roll temperature. The public datasheet does not explicitly declare an antiblock or slip package, so processors must add masterbatch to control blocking if the film is to be used as a monolayer skin.
Butene C4-LLDPE resins contain ethyl short-chain branches, whereas octene C8-LLDPE resins contain hexyl branches. At equivalent density, longer branches increase the probability of tie-molecule formation between lamellae; this shifts the dart impact and Elmendorf tear balance toward higher puncture resistance. The effect is measured under ASTM D1709-22 and ASTM D1922-15(2020), but public film data for this specific grade are limited. Processors commonly observe that an octene LLDPE at 0.920 g/cm³ and 2.0 g/10 min requires higher shear torque than a high-pressure LDPE of the same MFR because the linear structure creates a higher shear viscosity at typical extrusion rates. On a 75 mm 30:1 L/D grooved-feed single-screw extruder, die pressure may be in the range of 18–24 MPa at a melt temperature of 200 °C, but published data for DOWLEX 2020G in this configuration are limited. If branching distribution is critical, comparative gel-permeation chromatography with a refractive index detector and a light-scattering detector is used, because the datasheet does not report Mn, Mw, or polydispersity.
In blown film, the resin’s high melt viscosity relative to LDPE requires die gaps of 1.8–2.5 mm to avoid melt fracture at high output. A barrier screw with a Maddock mixing section is preferred; conventional metering screws may generate higher melt temperature and reduce output. Blow-up ratios of 2.0:1 to 3.0:1 are typical for balanced dart and tear; higher BUR increases transverse-direction tear but can reduce machine-direction tear. Because octene comonomer fractions alter the seal initiation temperature, the seal curve should be re-mapped for each blend ratio if DOWLEX 2020G is blended with LDPE or metallocene LLDPE. Blend rheology is not additive: a 20% LDPE addition can reduce melt pressure more than the weight fraction suggests because long-chain branching introduces shear thinning.
Processing on a 65 mm 24:1 L/D blown film line with a grooved-feed section is controlled by barrel setpoints from 190 °C at the feed throat to 215 °C at the die. Melt temperature should be kept between 190 °C and 230 °C; temperatures below 180 °C can increase melt fracture in LLDPE, while temperatures above 250 °C increase oxidation risk and gel formation. Because polyethylene is non-hygroscopic, pre-drying is not normally required, but pellet surface condensation can occur when cold pellets are exposed to air above 60% RH; in such cases a 80 °C hopper dryer for 2 h may be used. Frost line height is set at 2–4 die diameters to control bubble stability and film impact; an unstable bubble may cause gauge bands and reduce dart impact by more than 20% in affected regions. On cast film lines, chill roll temperatures of 15–25 °C and line speeds above 150 m/min are used, with edge trim systems to remove neck-in.
Blending with 10–20% high-pressure LDPE is used on blown film lines to improve bubble stability and clarity without eliminating the LLDPE toughness contribution. The blend ratio should be controlled gravimetrically because extrusion is not a precise distributive mixing operation. At LDPE additions above 30%, the dart impact and machine-direction tear move toward LDPE values. The optimum ratio depends on die diameter, BUR, and frost line height; published data for DOWLEX 2020G blends in these configurations are limited.
At 0.920 g/cm³ density and 2.0 g/10 min MFR, the resin is expected to exhibit lower tensile modulus and higher elongation at break than a 0.926 g/cm³ C4-LLDPE. Publicly available film property values for DOWLEX 2020G are not published in the current public datasheet; comparative testing on the intended line is required because blow-up ratio, frost line height, gauge variation, and cooling air temperature affect the measured values more than resin selection alone. Laboratories measuring film properties should use ASTM D882 for tensile stress and strain, ASTM D1922 for Elmendorf tear, and ASTM D1709 for dart drop impact. Haze is measured according to ASTM D1003, gloss at 60° according to ASTM D2457. The absence of published film data should not be interpreted as a performance limit; grade-specific validation is required.
| Parameter | Test method | Nominal value |
|---|---|---|
| Melt flow rate | ISO 1133-1:2022 | 2.0 g/10 min |
| Density | ISO 1183-1:2019 | 0.920 g/cm³ |
| Comonomer type | Internal DOWLEX platform | Octene (C8) typical; not disclosed in public datasheet |
| Additives | Internal | Stabilizer package only; slip/antiblock not specified in public datasheet |
Regulatory status for food-contact uses should be confirmed through the supplier’s regulatory statement. Polyolefin resins of this type are generally listed in FDA 21 CFR 177.1520(c), Table 1, for olefin polymers, provided the material meets extractables and end-use condition limitations. In the European Union, compliance is assessed under Regulation (EU) No 10/2011 with overall migration limits of 10 mg/dm² for plastic materials in contact with food. The resin is supplied with a safety data sheet; REACH registration under Regulation (EC) No 1907/2006 covers substance registration but does not guarantee end-article compliance. For medical or pharmaceutical packaging, additional ISO 10993 biocompatibility testing and specific extraction studies are required; published data for DOWLEX 2020G in these applications are limited.
| Framework | Reference | Condition |
|---|---|---|
| US FDA | 21 CFR 177.1520(c) | Olefin polymer for contact with aqueous and acidic foods up to heat treatment conditions; end-use verification required |
| EU plastics regulation | (EU) No 10/2011 | Overall migration <10 mg/dm² unless specific exemption applies; specific migration limits for monomers and impurities |
| REACH | Regulation (EC) No 1907/2006 | Substance registration; article compliance determined by downstream use |
Because DOWLEX 2020G is a 0.920 g/cm³ LLDPE, its seal initiation temperature is generally lower than that of a 0.926 g/cm³ LLDPE and higher than that of an EVA or ULDPE sealant. The exact seal initiation temperature for this grade is not published in the public datasheet; film processors routinely measure seal strength on a gradient sealer according to ASTM F2029 and hot tack according to ASTM F1921. In coextruded structures, the resin can serve as a sealant skin or as a core layer; when it is used as a skin, the absence of a slip/antiblock package may require masterbatch addition to control coefficient of friction. The supplier’s product datasheet does not specify coefficient of friction values: they are influenced by film gauge, corona treatment level, and storage time.
Compared with metallocene-catalyzed LLDPE grades of similar density, DOWLEX 2020G may provide a broader molecular weight distribution and different orientation behavior; metallocene grades often exhibit higher dart impact and lower extractables but may require higher extruder torque. The DOWLEX solution process allows comonomer uniformity not attainable in slurry C4 processes, reducing wax extraction and improving organoleptic performance in food packaging. However, the public documentation does not provide a quantitative comparison of extractables between DOWLEX 2020G and metallocene grades; such data must be generated under the intended processing conditions.
Operational boundaries include a melt temperature ceiling of approximately 250 °C to avoid oxidation and gel formation in polyethylene. The resin should not be processed above 280 °C for extended residence times, because degradation increases carbonyl index and reduces film toughness. Avoid combining with free radical initiators or peroxides unless the resulting crosslinking is intentional; residual unsaturation may accelerate gel formation. If the resin is stored outdoors, UV exposure over several months can shift the molecular weight distribution and increase gel particles. In-line screen packs of 80–120 mesh are used to remove char and crosslinked particles in film extrusion, but a rising screen pressure indicates degradation or contamination rather than a resin defect. The resin should not be dried with desiccant dryers at temperatures above 90 °C for prolonged periods, because pellet surface softening can occur.
End-use applications include heavy-duty sacks, carrier bags, liners, agricultural tunnels, frozen food packaging, and lamination films. These applications exploit the resin’s balance of puncture, tear, and sealability. For greenhouse film, UV stabilizer masterbatch addition is mandatory; DOWLEX 2020G does not contain an agricultural UV package as supplied. For frozen food packaging, the low-temperature toughness of LLDPE is maintained but the film must be gauged to compensate for stiffness loss at −20 °C. Published data for this specific grade in frozen food packaging is limited, and line-specific validation remains the governing requirement.