Dow Dow Grsn 9802 Nt7 Lldpe

Dow Dow™ GRSN-9802 NT7 LLDPE

    • Product Name: Dow Dow™ GRSN-9802 NT7 LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 422475
    Density 0.920 g/cm³
    Melt Index 190 C 2 16 Kg 0.85 g/10 min
    Melting Point 124 °C
    Vicat Softening Point 103 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 25.5 MPa
    Elongation At Break 800%
    Flexural Modulus 241 MPa
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 350 g
    Haze 12%
    Gloss 45 50

    As an accredited Dow Dow™ GRSN-9802 NT7 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow™ GRSN-9802 NT7 LLDPE is typically supplied in 25 kg moisture-resistant bags, 40 bags per pallet, totaling 1,000 kg.
    Container Loading (20′ FCL) Dow™ GRSN-9802 NT7 LLDPE: 20′ FCL holds 10 pallets, 25 kg bags, 1.375 MT/pallet, total 13.75 MT net.
    Shipping Dow™ GRSN-9802 NT7 LLDPE is typically shipped as non-hazardous, solid resin pellets in 25 kg bags, octabins, or bulk hopper trucks/railcars. Store in cool, dry conditions, away from direct sunlight, heat, and ignition sources. Keep containers sealed; handle with standard industrial hygiene. No special UN classification required.
    Storage Store Dow™ GRSN-9802 NT7 LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and moisture. Keep original bags or containers tightly closed, palletized off the floor. Avoid contamination, excessive stacking, and prolonged UV exposure. Store only in labeled packaging and follow the manufacturer’s SDS and local regulations. Do not expose to temperatures above recommended limits.
    Shelf Life Typically 24 months when stored sealed in original packaging, dry, cool, and away from direct sunlight; consult Dow technical data for exact conditions.
    Application of Dow Dow™ GRSN-9802 NT7 LLDPE

    When gauge reduction on a five-layer cast stretch line drops below 12 µm, the limiting variable for GRSN-9802 NT7 is not tensile yield but edge pinning turbulence and die-lip gauge band retention. The resin is fed through 30:1 L/D barrier screws into a 2,500 mm slot die maintained at 240 °C to 260 °C, while automatic die bolts hold transverse thickness variation below ±3% at a line speed of 450–550 m/min. A vacuum box and air knife press the melt curtain onto a 600 mm diameter chill roll at 18 °C to 24 °C, with an air gap of 80–120 mm to prevent draw resonance. The formulation for pallet wrap in this segment is typically 75–85 wt% GRSN-9802 NT7, 10–20 wt% metallocene ultra-low-density polyethylene or plastomer, 2–4 wt% polyisobutylene tackifier masterbatch, and 0.4–0.8 wt% synthetic amorphous silica antiblock. Melt flow rate is checked according to ASTM D1238 at 190 °C/2.16 kg and density according to ISO 1183-1. Cling force is measured by ASTM D5748 at 23 °C/50% RH; values below 60 g per 25 mm width create pallet instability, while values above 180 g per 25 mm width generate unwind noise and web blocking on rotary arm winders. Elastic recovery and stretch retention are evaluated under ASTM D5459, and haze is measured by ASTM D1003. The terminal product is pre-stretched machine pallet wrap in 500 mm width at 15–20 µm nominal gauge, used on automatic wrapping stations set to 150–250% prestretch. REACH compliance requires SVHC concentration below 0.1 wt% in the finished article under EC 1907/2006 Article 33. No food-contact declaration is required for this application.

    Standard or regulationMeasured or controlled parameterApplication boundary
    ASTM D1238Melt flow rate at 190 °C/2.16 kgExtruder head pressure stability and draw resonance control
    ISO 1183-1DensityFilm stiffness and seal initiation trend
    ASTM D882Tensile strength at breakStretch film and sack film load-holding capability
    ASTM D1709Dart impact, method AHeavy-duty sack puncture tolerance
    ASTM D5748Cling forcePallet wrap unwind and load stability
    ASTM F88Heat seal strengthSeal integrity on form-fill-seal lines
    FDA 21 CFR 177.1520Olefin polymer extractablesFood-contact lidding compliance

    When slip migration is deliberately suppressed in food-contact lid films

    Food-contact lidding for dairy cups and fresh-cut produce requires a different additive package from pallet stretch because the film must pass organoleptic tests while developing a stable coefficient of friction after 24 h of aging. On a three-layer blown film line with a 1.8 mm die gap and internal bubble cooling, the sealant layer is formulated from 80–90 wt% GRSN-9802 NT7, 10–20 wt% LDPE for lower seal initiation, 500–1000 ppm erucamide slip, and 2500–4000 ppm synthetic amorphous silica antiblock. The outer layers are compounded with a similar slip-antiblock balance but contain no tackifier. Melt temperature is held at 190–210 °C, blow-up ratio at 2.2–2.5, and frost line height at 6–8 die diameters to limit haze caused by excessive surface crystallization. Seal initiation is verified under ASTM F2029 with a 0.5 s dwell and 3.0 N/mm² seal pressure; hot tack strength should remain above 2 N/15 mm at 105 °C for dairy filling lines running above 120 cups/min. Seal strength is tested at 180 °C and 1.0 s dwell according to ASTM F88. Haze is measured by ASTM D1003 and gloss by ASTM D2457 at 60°. For the finished lidding structure, compliance with FDA 21 CFR 177.1520 is required for olefin polymers in food contact, with extractable limitations evaluated under the conditions stated in 21 CFR 177.1520(c). For the European market, the finished article must meet the overall migration limit of 10 mg/dm² under EU 10/2011 Annex V using simulants specified for the food type. Slip migration is deliberately slowed by using a high-molecular-weight erucamide grade and by storing rolls at 20–25 °C for 24–72 h before slitting, which reduces blocking without pushing coefficient of friction below 0.20.

    Agricultural silage wrap made from GRSN-9802 NT7 on a three-layer blown line with internal bubble cooling and surface winding requires a stabilization strategy that maintains puncture resistance after 12 months of UV exposure and mechanical abrasion against baler grips. The core layer is usually 92–98 wt% GRSN-9802 NT7 with 1–3 wt% carbon black or white HALS masterbatch; the skin layers contain 0.5–1.5 wt% UV stabilizer masterbatch based on hindered amine light stabilizers and 1–2 wt% processing aid concentrate to reduce melt pressure in the die. Blow-up ratio is set at 2.5–3.0, die gap at 2.0–2.4 mm, and melt temperature at 190–220 °C to limit oxidative gel formation in the stabilizer masterbatch. The film is wound in 750 mm width at 25 µm nominal gauge, and edge folding is applied before surface winding. Puncture resistance is tested according to ASTM D3420, tensile elongation at break according to ASTM D882, and tear resistance by ASTM D1922. Accelerated weathering is carried out under ISO 4892-2 cycle 1 with xenon-arc exposure; retention of at least 50% of initial elongation after 1500 h is a common control point, but published lot-specific data for this exact resin and masterbatch combination is limited. The terminal product is round-bale silage wrap for forage conservation, where the film must resist puncture from stalk ends and maintain anaerobic conditions during ensiling.

    Heavy-duty sack film seal initiation and impact retention in recycled-content blends

    Heavy-duty sacks for fertilizer and polymer pellet transport are produced from GRSN-9802 NT7 in a three-layer blown film structure that carries post-industrial reclaim in the core layer to reduce cost without sacrificing dart impact. The core layer is typically 40–60 wt% GRSN-9802 NT7, 30–50 wt% sorted LLDPE/LDPE film reclaim, and 5–10 wt% HDPE for bending stiffness; the skin layers are 90–98 wt% virgin GRSN-9802 NT7 to protect sealing and gloss. Extrusion is performed on a grooved-feed extruder with a 2.2 mm die gap, internal bubble cooling, and a blow-up ratio of 2.0–2.4. Melt temperature is held at 200–230 °C, while screen pack filtration below 200 µm is used to remove gelatinous particles from the recycled fraction. Dart impact is measured by ASTM D1709 method A; a 100 µm three-layer sack film should retain a dart drop value above 350 g for palletized fertilizer filling lines, but actual values decline when reclaim content approaches 50 wt%. Seal strength is tested by ASTM F88 at 180 °C and 1.0 s dwell; the seal initiation temperature must remain below 115 °C to match vertical form-fill-seal dwell times. Tensile modulus and elongation are measured by ISO 527-3 at 500 mm/min, and tear strength by ASTM D1922. REACH SVHC content must remain below 0.1 wt% per finished article. The terminal product is an 80–120 µm printed sack with back-seam or bottom-gusset geometry.

    How does oscillating haul-off alter gauge distribution in 15 µm stretch hood film?

    Stretch hood film for pallet load containment is run at 15–30 µm on three-layer blown lines with oscillating haul-off and rotary die technology to prevent hard gauge bands that weaken the folded edges. The base formulation is 80–90 wt% GRSN-9802 NT7 and 10–20 wt% ultra-low-density polyethylene or plastomer; EVA is used only when low-temperature stretch below 5 °C is required, but it increases die lip deposition and should be limited to 10 wt% in this resin system. Blow-up ratio is set at 2.8–3.2, frost line height at 8–10 die diameters, and die gap at 2.0 mm to preserve transverse direction tear resistance. The oscillating haul-off amplitude is set between 100 mm and 300 mm depending on roll face width; higher amplitude reduces edge bead formation but increases web wander on the winder. Tensile elongation at break is measured by ASTM D882, with machine direction elongation above 500% and transverse direction elongation above 600% used as internal control points for stretch hood performance. Tear resistance is measured by ASTM D1922, and puncture resistance by ASTM D3420. The finished hood is welded on an automatic pallet hooder that stretches the film by 40–70% before pulling it over the load. No food-contact declaration is required under normal use.

    Process variableCast stretch filmFood lid blown filmHeavy-duty sack film
    Melt temperature240–260 °C190–210 °C200–230 °C
    Die gap0.5–0.8 mm1.8 mm2.2 mm
    Blow-up ratioNot applicable2.2–2.52.0–2.4
    Chill roll or frost line setting18–24 °C chill roll6–8 die diameters frost lineInternal bubble cooling with 2.0–2.4 BUR
    Primary additive loading2–4 wt% tackifier concentrate500–1000 ppm erucamide30–50 wt% reclaim in core

    Woven sack lamination using GRSN-9802 NT7 as the coating layer requires only 0.2–0.5 wt% synthetic amorphous silica antiblock and a die temperature in the 300–320 °C range to achieve acceptable adhesion to polypropylene cloth; all other process parameters follow standard LLDPE extrusion coating practice.

    Free Quote

    Competitive Dow Dow™ GRSN-9802 NT7 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow™ GRSN-9802 NT7 Linear Low Density Polyethylene is an ethylene–α-olefin copolymer commonly specified for thin-gauge cast film and high-clarity packaging structures. Supplier literature typically positions the product with a nominal density of 0.918 g/cm³ and a nominal melt flow rate of 2.0 g/10 min when measured under ISO 1183-1:2019 Method A and ISO 1133-1:2022 at 190°C/2.16 kg. These values are not independent release criteria; comonomer content, molecular-weight distribution, and additive package can vary within the sales specification. The “NT7” suffix is a supplier designation rather than a guaranteed slip or antiblock package. The material is therefore released to a high-speed form-fill-seal line only after incoming melt-flow, density, and film-optics verification against the supplier’s current technical data sheet.

    Why Hexyl Branches Raise Puncture and Tear Without Raising Density

    LLDPE grades cannot be compared by melt index and density alone because the α-olefin comonomer determines short-chain branch length. Incorporation of 1-octene introduces a hexyl side group; incorporation of 1-butene introduces an ethyl side group. The longer hexyl branch is more effective at disturbing polyethylene lamellae and at generating tie molecules that link adjacent crystalline regions. At a given density, an octene-based LLDPE therefore tends to exhibit higher dart impact by ASTM D1709 Method A, higher Elmendorf tear by ASTM D1922 or ISO 6383-2, and greater puncture resistance by ASTM D5748 than a butene-based LLDPE at similar melt flow rate. The trade-off appears in non-isothermal crystallization: differential scanning calorimetry under ISO 11357-3 at a cooling rate of 10°C/min typically shows a lower peak crystallization temperature for the octene grade. The film line must therefore maintain sufficiently aggressive chill-roll quenching to prevent haze and blocking in wound rolls. The relationship between comonomer distribution and seal initiation is not captured by density alone; a heat-seal curve per ASTM F1921 over a jaw temperature range of 95–125°C should be generated for the actual film.

    What Extrusion Conditions Are Observed on High-Draw Cast Film Lines?

    High-draw cast film operations for this grade are typically run on single-screw extruders with 30:1 to 34:1 L/D and a barrier screw with a Maddock mixer. A temperature profile from 185°C in the feed throat to 230°C at the adapter is used, with melt temperature controlled between 220°C and 250°C at the die. Die gaps of 0.45–0.90 mm are common for 20–30 µm films; narrower gaps raise shear rate and may induce sharkskin, while wider gaps reduce draw-down orientation and may increase transverse-direction thickness variation. Screen packs of 100/80/60 mesh are typical for cast film to balance gel removal against pressure drop. Melt pressure upstream of the screen pack is monitored continuously; a rising pressure trend at constant screw speed indicates filter blockage, not necessarily resin degradation. The melt web is quenched on a chrome-plated chill roll maintained at 15–30°C with an air knife and vacuum box to stabilize neck-in and edge beads. Published data for this specific resin on a single production line is limited; starting parameters should be generated from capillary rheometry and cast-film pilot trials rather than transferred from another polyethylene grade.

    Pilot-line data on a 45 mm cast film unit with a 300 mm die do not transfer directly to a 75 mm, 2,000 mm die production line because residence-time distribution, shear heating, and die chill-roll geometry differ. When the grade is scaled up, melt pump suction pressure and die pressure should be recorded at the same specific output. A change in barrel temperature profile of only 5°C can shift the melt temperature above 240°C on a high-output line and change gel counts. Published data for this specific resin under those conditions is limited, so converters should build an internal operating window using capillary rheometry data instead of assuming pilot-line parameters will hold.

    Drying is not normally required for this LLDPE when storage remains dry and indoor. If the resin is exposed to relative humidity above 60% or moved from cold storage into a warm converting hall, condensation on pellets can be removed in a desiccant dryer at 60–70°C for 2–4 h. A dew-point of -20°C or lower at the dryer inlet is required for effective surface moisture removal. Startup after a resin change from a higher-viscosity polyethylene should be preceded by a purge with a lower-viscosity grade; the purge volume should equal at least 3–5 barrel capacities. Residence time above 20 min at melt temperature above 240°C can increase gel formation and consume processing stabilizer, so shutdown sequences should include reducing barrel temperatures, purging the die, and stopping screw rotation before heat is removed from the adapter. Film property drift during a batch is often associated with additive concentration gradients in the feed hopper; converter trials should monitor coefficient of friction on material from the beginning, middle, and end of the resin lot.

    Optical Haze, Machine-Direction Orientation, and Surface Additive Migration

    Cast film haze is controlled by surface roughness, bulk crystallite scattering, and additive bloom. Haze is measured under ASTM D1003 Procedure A; clarity under ASTM D1746. Films made from this octene LLDPE class generally show lower haze than equivalent butene-copolymer film because the longer comonomer reduces large spherulitic superstructures. However, optical quality is not determined solely by resin architecture: an unbalanced draw ratio or a chill roll with excessive roughness will dominate haze before crystallite scattering becomes measurable. Chill roll surface topography measured by profilometry should be maintained between 0.2 µm and 0.5 µm Ra; smoother rolls may create blocking, while rougher rolls increase surface haze. Machine-direction orientation induced by the draw gap creates anisotropic tensile response. Tensile strength and elongation are measured per ISO 527-3 on 25 mm wide strips cut in machine and transverse directions. Slip and antiblock additives, if present, migrate to the film surface by diffusion through the amorphous phase. This migration is temperature-dependent; film stored above 35°C may show a lower coefficient of friction on the outer lap than a freshly wound roll. For critical packaging lines, a 48-hour room-temperature aging period is commonly used before evaluating ASTM D1894 coefficient of friction.

    If the natural grade is supplied without slip and antiblock, masterbatch addition is required for high-speed packaging lines. Typical cast film loadings are 0.5–2.0% for antiblock and 0.5–1.5% for slip, but the optimum depends on film gauge and unwind speed. Addition above 3.0% total masterbatch can raise haze and reduce heat-seal strength by creating a low-molecular-weight surface layer. For unsupported film below 25 µm, excessive slip can increase roll telescoping on high-speed unwind, so converter trials should include a wound-roll stability test after 24 h at 38°C.

    When Replacing LDPE in a Coextruded Sealant Web

    GRSN-9802 NT7 is not a direct drop-in for high-pressure LDPE in every coextrusion. In a coextruded film used as a sealant web, the LLDPE layer usually provides higher dart impact, higher tear resistance, and improved puncture resistance relative to an LDPE layer of the same thickness, while LDPE contributes better melt strength, lower neck-in, and easier bubble stability in blown-film processes. The substitution therefore changes the balance of the line. For cast-film lines, the resin can be used as a skin or sealant layer; the die gap should be kept at the upper end of the LLDPE range until melt-pressure data confirm that the narrower gap is acceptable. Table 1 summarizes relative property relationships based on standard test methods, not absolute values for a specific converter.

    Relative property balance across polyethylene film resins
    Property / test methodOctene LLDPE (GRSN-9802 NT7 class)Butene LLDPEHigh-pressure LDPEMetallocene octene LLDPE
    Dart impact, ASTM D1709HighMediumMedium–highVery high
    Tear resistance, ISO 6383-2HighMediumMediumHigh
    Haze, ASTM D1003LowMediumMedium–lowVery low
    Melt strengthModerateModerateHighLower
    Neck-in on cast film lineModerateModerateLowModerate–high

    The comparison is not symmetrical under all gauges. At film thickness below 15 µm, the puncture advantage of an octene LLDPE can be reduced if the cast line runs excessive melt temperature and the resin degrades. Conversely, at thickness above 50 µm, the lower melt strength of the LLDPE may require a wider die gap to prevent edge surging. The appropriate selection should therefore be made from a designed experiment on the actual coextrusion line, with tensile, tear, and haze samples collected from at least three positions across the web.

    Compliance Is Governed by Regional Migration Limits and Lot-Specific Declarations

    For food-contact structures, GRSN-9802 NT7 must be evaluated in the finished article under the relevant jurisdiction. Polyolefin food-contact clearances commonly rest on FDA 21 CFR 177.1520(c) in the United States and Commission Regulation (EU) No 10/2011 in the European Union. Substances used in the resin must comply with REACH (EC) No 1907/2006. For electrical and electronic packaging applications, RoHS Directive 2011/65/EU Annex II thresholds apply to cadmium, lead, mercury, hexavalent chromium, PBB, and PBDE. Table 2 lists verification points, with the caveat that the resin supplier’s regulatory data sheet and the converter’s migration testing on the final laminate control compliance.

    Regulatory verification matrix for polyolefin packaging structures
    RequirementScopeVerification method
    FDA 21 CFR 177.1520(c)Olefin polymers for food contactSupplier declaration; extraction tests per 21 CFR 176.170(c)
    EU Regulation 10/2011Plastic materials and articles intended for food contactOverall migration 10 mg/dm² per EN 1186-1; specific migration per EN 13130-1
    REACH (EC) No 1907/2006SVHC communicationSupplier safety data sheet, Article 33 disclosure
    RoHS Directive 2011/65/EU, Annex IIRestricted substances in electrical equipmentHomogeneous material thresholds: 0.1 wt% lead, mercury, hexavalent chromium, PBB, PBDE; 0.01 wt% cadmium
    ASTM D4976-21Polyethylene classification for molding and extrusionCertificate of analysis; density, melt flow rate, and lot traceability

    Compliance statements are specific to the supplied formulation and do not automatically cover the multilayered film after printing, lamination, or surface treatment. A change in sealant layer concentration, corona treatment intensity, or lamination adhesive can alter overall migration and organoleptic performance; the finished structure must be tested under the intended food simulant and time–temperature exposure before commercial release.