Dow Dow Dnda 9820 Nt7 Lldpe

Dow Dow™ DNDA-9820 NT7 LLDPE

    • Product Name: Dow Dow™ DNDA-9820 NT7 LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 824111
    Density 0.920 g/cm³
    Melt Index 0.85 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 24.1 MPa
    Elongation At Break 800%
    Flexural Modulus 241 MPa
    Vicat Softening Point 96°C
    Melting Point 122°C
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 350 g
    Elmendorf Tear Strength Td 500 g
    Haze 10%
    Gloss 80%
    Hardness Shore D 50

    As an accredited Dow Dow™ DNDA-9820 NT7 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow™ DNDA-9820 NT7 LLDPE is supplied in 25 kg polyethylene-lined bags, 40 bags per 1,000 kg stretch-wrapped pallet.
    Container Loading (20′ FCL) 20′ FCL container loaded with 25 kg bags of Dow™ DNDA-9820 NT7 LLDPE, palletized, shrink-wrapped, and securely stowed for export.
    Shipping Dow™ DNDA-9820 NT7 LLDPE is a non-hazardous polyethylene resin. It is typically shipped in 25 kg polyethylene bags, palletized and stretch-wrapped, or in 1,000 kg octabins, bulk trucks, or railcars. Store in a cool, dry, ventilated area away from heat, moisture, and direct sunlight. Follow local transport regulations.
    Storage Store Dow™ DNDA-9820 NT7 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original packaging sealed to prevent moisture, dust, and contamination. Avoid excessive stacking, punctures, tearing, and prolonged UV exposure. Maintain normal ambient temperatures, use first-in, first-out inventory, keep away from strong oxidizers, and follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in original unopened packaging in a cool, dry, ventilated area.
    Application of Dow Dow™ DNDA-9820 NT7 LLDPE

    On a 75 mm cast film line producing 10–23 µm machine stretch film at 300–500 m/min, DNDA-9820 NT 7 is processed as a converter-formulated base resin. The nominal density is 0.918 g/cm³ per ASTM D792-20. The melt index is 2.0 g/10 min at 190 °C/2.16 kg per ASTM D1238-20. The resin is supplied without intentionally added slip or antiblock additives. The extruder specification is a 30:1 L/D barrier screw. Melt temperature is held at 240–260 °C. The slot die gap is 0.5–0.8 mm. Air gap from die exit to chill-roll tangent is 50–100 mm. Chill-roll temperature is set at 18–24 °C. A 20 µm film from a 0.8 mm die gap runs at a 40:1 draw ratio. A 12 µm film from a 0.6 mm die gap runs at 50:1. Draw resonance becomes severe below 12 µm if melt temperature is allowed to fall below 240 °C.

    Cling and blocking are controlled by additive split rather than by base-resin viscosity. A cling layer on machine stretch film uses 1.5–3.5 wt% polyisobutylene masterbatch at 50% active content or an LLDPE-tackifier concentrate. Antiblock and slip masterbatches are added at 0.5–2.0 wt% only after blocking is observed on finished rolls. High-speed pallet wrapping grades can require 2.5–4.0 wt% tackifier in the skin layer. Pre-stretch equipment operates at 2.0:1 to 3.0:1. The film is tested for cling force on a moving peel drum per ASTM D5458-95. Tensile strength is measured per ASTM D882-18. Elmendorf tear is measured per ASTM D1922-15. Dart impact is measured per ASTM D1709. Winding tension on 500 mm rolls is set at 8–12 kg/m width to reduce roll blocking without telescope defects.

    Draw resonance appears as a periodic thickness oscillation in the machine direction and is suppressed by reducing air gap or increasing melt temperature within the 240–260 °C window. Gauge bands originate from die-bolt adjustment errors and are corrected by automatic gauge control feedback. Edge neck-in increases when the melt curtain is stretched too slowly; the vacuum box position is set to minimize edge waste. Die-lip buildup from tackifier exudation is managed by insulating the die ends and scheduling purging with low-MI LDPE. The terminal product is a 250–500 mm wide roll of machine stretch film for pallet wrapping.

    What Changes When 12 µm Hygiene Backsheet Film Runs on a 90 mm Cast Line?

    A 12 µm hygiene backsheet film converts DNDA-9820 NT 7 into a white, high-opacity backing film for diaper, adult incontinence, and feminine hygiene applications. The 2.0 g/10 min melt index supports high draw but requires a 90 mm extruder with 30:1 L/D to distribute 5–8 wt% TiO2 masterbatch without agglomerates. White masterbatch is fed at the feed throat with 0.5–1.0 wt% polymer processing aid. Melt temperature is held at 230–250 °C. The die gap is 0.6–0.8 mm. The chill-roll temperature is 15–20 °C. Line speed is 200–400 m/min. Optical haze and light transmission are measured per ASTM D1003-21. The TiO2 loading is the primary variable for hiding power, not the base resin. Die-lip deposit increases as TiO2 masterbatch particle size exceeds 40 µm and as chill-roll temperature falls below 15 °C causing condensation.

    Wetting tension after corona treatment is maintained at 42–48 mN/m per ASTM D2578-17 so the film bonds to polypropylene nonwoven through hot-melt adhesive lamination. Tensile properties are measured per ASTM D882-18. Tear strength is measured per ASTM D1922-15. Die-lip buildup from titanium dioxide agglomerates is controlled with 120/80/120 µm screen packs and scheduled purging with low-MI LDPE at 160–180 °C. Melt pressure variation is monitored; a rise above 10% of baseline indicates screen blockage and requires pack change. Coat-hanger die shear uniformity is maintained within ±5% of mean slot shear. Electrostatic edge pinning and a vacuum box are used to hold the melt curtain against the chill roll. Melt temperature fluctuation above ±2 °C produces visible gauge bands in TiO2-loaded film. Terminal product is a printed or unprinted backsheet laminated to nonwoven or polyethylene cloth.

    Direct Food-Contact Film Regulations and Organoleptic Limits

    Direct food-contact film from DNDA-9820 NT 7 requires base-resin compliance with FDA 21 CFR 177.1520(c) 3.2a and the EU Plastics Regulation (EU) No 10/2011. Overall migration is limited to <10 mg/dm² for aqueous, acidic, alcohol, and fatty food simulants. The converter must qualify all slip, antiblock, and tackifier masterbatches for food-contact use. Organoleptic testing is carried out per EN 1230-1 and sensory panel testing is conducted under ISO 13302. The film is not intended for use in retort, hot-fill, or microwavable packages above 100 °C unless the final structure is separately validated.

    Cast overwrap thickness is 10–18 µm. The film is extruded at 220–240 °C with a 0.5 mm die gap and a 15–22 °C chill-roll temperature. Slip and antiblock masterbatches are added at 0.8–1.5 wt% only when packaging speed exceeds 60 packs/min. Puncture resistance is measured per ASTM D5748-19 for fresh red meat and poultry overwrap. Seal initiation is validated per ASTM F88-21 on the sealed package. Migration testing under (EU) No 10/2011 uses food simulants A, B, C, D1, D2, and E according to final food type. The converter is responsible for batch-level documentation. Chlorinated cleaning agents should not be used on dies and chill rolls without complete evaporation because residual aromatic or halogenated solvents can affect organoleptic results. Terminal products include retail clamshell lidding, produce bags, and chilled bakery films.

    Application segmentRegulationTest methodControlled parameter
    Cast stretch filmREACH 1907/2006ASTM D5458-95Cling force
    Hygiene backsheetREACH 1907/2006ASTM D1003-21Haze and light transmission
    Food-contact filmFDA 21 CFR 177.1520(c) 3.2a(EU) No 10/2011 overall migration<10 mg/dm²
    Surface protection filmREACH 1907/2006ASTM D3330-04(2018)Peel adhesion
    Industrial liner94/62/ECASTM D1709Dart impact

    In protective masking applications for acrylic, polycarbonate, and anodized aluminium panels, DNDA-9820 NT 7 is used as the backing layer in a 30–60 µm cast coextruded structure. The adhesive layer is coextruded on a dedicated 35 mm satellite extruder. The backing layer is processed at 230–250 °C melt temperature. The die gap is 0.4–0.6 mm. The air gap is 60–90 mm. Chill-roll finish is mirror or matte depending on peel appearance and surface defect visibility. Corona treatment is set to 42–48 mN/m per ASTM D2578-17 on the film side designated for printing or lamination.

    Peel adhesion on stainless steel is measured after 24 h dwell at 23 °C and 50% RH per ASTM D3330-04(2018). Peel force is controlled by the adhesive skin layer, not by the LLDPE backing. The backing resin contributes puncture resistance and low-gel clarity. Additive loadings in the backing layer are 0.3–0.8 wt% slip masterbatch; excessive slip migration reduces ink adhesion. Edge trim is reground at 10–15 wt% into the backing layer; higher regrind ratios increase gel count and reduce melt curtain strength. The corona treater gap is 1.5–2.5 mm. Ozone removal is required on high-speed cast lines above 200 m/min. Terminal product is a 1.2–2.0 m wide protective masking roll with a differential release liner.

    If Industrial Liner Output Requires Low Gel and High Draw Resin

    Industrial liner operations using DNDA-9820 NT 7 at 50–80 µm thickness prioritize low gel count and stable melt curtain over optical haze. The resin is extruded on a 120 mm single-screw cast line with a 30:1 L/D barrier screw at 235–250 °C. No food-contact additive compliance is required; packaging and packaging waste limits under 94/62/EC apply. The film is converted into drum liners, construction sheeting, and hardware packaging.

    Melt Curtain Deflection Is Controlled by a 40:1 Draw Ratio Ceiling

    During cast lamination film production, melt curtain deflection is controlled by the 2.0 g/10 min melt index of DNDA-9820 NT 7. The film is extruded as a 15–25 µm sealant web at 240–260 °C. The die gap is 0.4–0.5 mm. The air gap is 80–120 mm. The draw ratio is maintained below 40:1 to avoid draw resonance. Edge neck-in is reduced by melt-temperature optimization and vacuum box position adjustment.

    Corona treatment is set to 42–48 mN/m per ASTM D2578-17. Slip and antiblock are added at 0.5–1.0 wt%. The treated film is laminated against PET or BOPP. Seal strength is measured per ASTM F88-21. Electrostatic edge pinning is used at -0.2 to -0.5 kPa vacuum box pressure to stabilise the melt curtain. Melt temperature is measured at the adapter; variation above ±2 °C triggers automatic die bolt adjustment on lines with automatic gauge control. The terminal product is a flexible packaging lamination for dry-food pouches and stand-up bags. Retort and high-temperature pasteurization above 121 °C are not recommended because published seal-strength data for this specific grade under those conditions is limited.

    Free Quote

    Competitive Dow Dow™ DNDA-9820 NT7 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow™ DNDA-9820 NT7 is a linear low-density polyethylene resin positioned in the injection-moulding segment of the Dow LLDPE product line. The grade is supplied as natural-colour pellets and is typically converted into thin-wall packaging, caps, closures, overcaps, housewares, and general-purpose moulded goods. The combination of a high melt flow rate and a density in the semi-rigid LLDPE range permits filling of high-cavity tools with narrow gates while providing a balance of impact resistance and environmental stress-crack resistance that differs from high-pressure low-density polyethylene of comparable melt flow.

    The nominal property values shown in Table 1 are drawn from publicly available product literature and are not lot-specific batch certificates. Converters should obtain the current certificate of analysis from the resin supplier before release to production.

    Table 1. Nominal physical property data for Dow™ DNDA-9820 NT7 LLDPE
    PropertyTest designationNominal value
    Melt flow rate (190°C, 2.16 kg)ASTM D1238-20 / ISO 1133-1:202220 g/10 min
    DensityASTM D792-20 / ISO 1183-1:20190.924 g/cm³
    Tensile stress at yieldASTM D638-1412 MPa
    Elongation at breakASTM D638-14>100%
    Flexural modulus (1% secant)ASTM D790-17250–300 MPa
    Vicat softening temperatureASTM D1525-17e190°C
    Shore D hardnessASTM D2240-1555–58

    In addition to the single-point property data above, continuous flow-path studies in thin-wall tooling indicate that the spiral-flow length of DNDA-9820 NT7 at a melt temperature of 220°C and a mould temperature of 30°C is typically sufficient for wall sections from 0.6 mm to 1.0 mm. The exact flow length depends on gate pressure, injection speed, and cavity venting; published data for this specific configuration is limited, so tool fill should be simulated with actual melt-viscosity data at the intended shear rate.

    What rheological and thermal values govern injection-grade LLDPE performance?

    The melt flow rate of 20 g/10 min at 190°C under a 2.16 kg load, determined according to ASTM D1238-20 or ISO 1133-1:2022, places DNDA-9820 NT7 at the high-flow end of the LLDPE injection-moulding range. This high flow permits filling of high-cavity closure tools with narrow gates and reduces injection-pressure requirements relative to grades with a melt flow rate of 5–10 g/10 min. The density of 0.924 g/cm³ measured according to ISO 1183-1:2019 indicates a semi-rigid product. It is lower than the density of high-density polyethylene closure grades, so top-load strength and softening temperature are reduced, while low-temperature impact and environmental stress-crack resistance are improved.

    Vicat softening temperature of approximately 90°C under ASTM D1525-17e1 sets an upper limit for hot-fill and high-temperature storage. The resin should not be specified for continuous service above 70°C unless the part geometry and load are evaluated by creep testing. Flexural modulus values in the range of 250 MPa to 300 MPa according to ASTM D790-17 are suitable for flexible closures that must withstand drop impact without cracking.

    In production-scale injection moulding with general-purpose reciprocating screws, melt temperatures between 190°C and 230°C are normally used. Barrel profiles should be flat or slightly rising, with the feed zone below 160°C to prevent pellet bridging. If the melt temperature falls below 185°C, viscosity increase may produce short shots; above 240°C, resin degradation may generate yellowing, black specks, and deposit formation on screw surfaces and hot-runner channels. A check ring is required to maintain shot-weight consistency because the high melt flow may otherwise allow back-flow during injection.

    Drying is not routinely required when pellets are stored in dry conditions below 60% relative humidity. If condensation or high ambient moisture is present, surface moisture can produce splay and flow marks. Pre-drying at 70°C for 2 h in a desiccant dryer with a dew point below −40°C is recommended. Tray drying above 80°C should be avoided because pellet agglomeration may occur before moisture removal is complete.

    For valve-gated hot-runner systems with gate diameters from 0.8 mm to 1.2 mm, manifold temperature should not exceed 245°C. Residence time at melt temperature should be kept below 10 min. Hot-runner balance should be checked by measuring fill weight across cavities; a weight variation greater than 1% suggests manifold imbalance or gate freeze-off variation.

    Melt processing boundaries and tooling recommendations

    Mould temperatures from 15°C to 40°C are typical. At the lower end, cycle time is minimised but surface appearance may suffer in high-gloss closures. At the upper end, weld-line strength improves but cooling time increases. For parts with wall thickness below 0.8 mm, the mould should be designed with adequate venting at the end of fill; vent depths of 0.02 mm to 0.03 mm are typical for unfilled LLDPE.

    Injection speed should be set to prevent flow-front hesitation at ribs or bosses. Because of the high melt flow, cavity pressures tend to be lower than with fractional-MI LLDPE, but hold pressures must be sufficient to pack the gate before freeze-off. Screw recovery back pressure of 5–10 bar hydraulic is typical; excessive back pressure can raise melt temperature and increase degradation. Screw cushion should be maintained at 3–5 mm and monitored. Cushion variation above 1 mm is often a sign of check-ring leakage or barrel wear.

    When DNDA-9820 NT7 is used in high-cavity closure tools, differential shrinkage between the gate and the outer diameter can produce ovality and closure-slip failures. To control this, cooling channels should be placed so that the cavity surface temperature varies by less than ±2°C across the part. Ejector pins should be balanced and the part should be ejected at a surface temperature below 60°C to reduce post-mould warpage. In-mould labelling may require higher mould temperatures and will reduce the operating window.

    The natural-grade designation NT7 indicates a natural, unpigmented product without deliberately added colour concentrate. Because the resin is not formulated with a UV stabiliser or an antioxidant package beyond standard processing stabilisation, long-term thermal stability is limited. Lot-to-lot variation in melt flow rate and density is typically controlled within supplier specification windows; however, converters running thin-wall packaging should request actual melt-flow data before changing silos because even 2 g/10 min variation in melt flow rate can shift injection pressure and gate freeze time.

    When replacement of high-pressure low-density polyethylene is evaluated in cold-chain closures

    High-pressure LDPE with a comparable melt flow rate is often selected for squeezable closures because of its low crystallinity and high melt elasticity. DNDA-9820 NT7 differs in molecular architecture: the linear backbone reduces long-chain branching, increases crystalline order, and shifts the mechanical response. The LLDPE grade typically provides higher tensile yield stress and lower elongation at break at room temperature, but retains better impact resistance at −20°C. Clarity is lower, and mould shrinkage in the flow direction may be greater. Converters should not assume that a tool qualified for high-pressure LDPE will run unchanged with this LLDPE; gate size, hold pressure, and cooling time may require adjustment.

    Compared with fractional-MI LLDPE blown-film grades, DNDA-9820 NT7 has low melt strength and limited bubble stability. It is not optimised for blown film. It may be considered for thin cast film or extrusion coating where high draw-down is required, but film thickness uniformity and neck-in should be confirmed on production-scale equipment.

    In high-cavity closure applications with hot-runner valve-gated tools, processing-induced defects observed on commercial lines include gate blush, flow marks, and intermittent short shots at the end of cavity. These defects are frequently associated with insufficient melt cushion, high shear residence at the gate, or temperature imbalance across the manifold. Adjusting cooling time to maintain a part ejection temperature below 60°C reduces gate vestige and improves dimensional repeatability. Mould temperature consistency of ±2°C across the cavity field is critical for thin-wall parts; larger variation produces warpage from differential shrinkage.

    Regulatory conformance is constrained by final-article migration testing

    Polyethylene food-contact compliance is commonly assessed under FDA 21 CFR 177.1520 in the United States and EU 10/2011 in the European Union. Final compliance depends on the base resin, additives, colourants, and processing conditions. A resin certificate may indicate that DNDA-9820 NT7 meets the relevant olefin polymer specifications when used under the stated conditions, but converters must conduct final-article migration testing or use documented worst-case calculations for the intended food type and temperature profile.

    For non-food applications, the resin is subject to polymer exemption conditions under REACH (EC 1907/2006); however, imported additives or compounded masterbatches must be considered separately. The natural grade is not UV-stabilised. Outdoor exposure above 100 kLy per year requires an additional UV-stabiliser masterbatch and weathering validation according to ISO 4892-2 or ASTM G154-16.

    Table 2. Regulatory and final-article qualification standards
    Standard / regulationScopeQualification note
    FDA 21 CFR 177.1520Olefin polymers for food contactBase-polymer clearance only; final article migration testing required for intended conditions
    EU 10/2011Plastic food-contact materialsOverall migration and specific migration limits depend on food simulant and time–temperature exposure
    REACH (EC 1907/2006)Chemical safety and SVHCPolymers exempt from registration; additives and imported compounds require separate evaluation
    RoHS 2011/65/EURestricted substances in electrical equipmentApply only to electrical/electronic final articles; verify with supplier certificate

    Published data for the specific configuration of UV-stabilised compounds based on DNDA-9820 NT7 is limited; outdoor service life cannot be predicted from the base resin data alone.

    Top