| HS Code | 641852 |
| Density | 0.920 g/cm³ |
| Melt Index 190 C 2 16 Kg | 1.0 g/10 min |
| Melt Flow Ratio I10 I2 | 8.0 |
| Melting Point | 122 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 24.1 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 207 MPa |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 10% |
| Gloss 45 | 70 |
As an accredited Dow Dow™ DNDA-1088 NT7 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow™ DNDA-1088 NT7 LLDPE is supplied in 25 kg bags, 40 bags per pallet, totaling 1,000 kg. |
| Container Loading (20′ FCL) | 20′ FCL container loading of Dow™ DNDA-1088 NT7 LLDPE, packed in 25 kg bags, palletized, shrink-wrapped, and secured for transport. |
| Shipping | Dow™ DNDA-1088 NT7 LLDPE ships as non-hazardous polyethylene resin pellets in 25-kg bags, octabins, or bulk trucks/railcars. Keep containers closed, dry, and away from ignition/heat. Protect from UV and moisture; avoid dust inhalation. No special transport placarding required; follow local regulations and standard industrial handling practices. |
| Storage | Store Dow™ DNDA-1088 NT7 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep in tightly closed original containers or bags, protected from moisture, dust, and contamination. Avoid excessive stacking and physical damage. Use first-in, first-out rotation; follow local regulations and the manufacturer’s safety data sheet. |
| Shelf Life | Store sealed, cool, dry, well-ventilated, away from heat and sunlight; typical shelf life: 24 months in unopened original packaging. |
In silage-cover blown-film lines running seasonal campaigns in northern Europe, 150 µm nominal gauge webs are produced from DOW™ DNDA-1088 NT 7 LLDPE on three-layer blown-film lines fitted with 90 mm grooved-feed extruders at L/D 30:1, barrier screws with Maddock mixing sections, and a 450 mm spiral mandrel die with a 2.2 mm lip gap. The resin is metered as 100 parts per hundred resin; UV-stabilizer masterbatch is gravimetrically introduced at 4.0 wt% and a non-amine anti-fog concentrate at 2.5 wt%. The bubble is run at a blow-up ratio of 2.8:1, with melt temperatures held between 190°C and 210°C and the frost line maintained at 850–950 mm from the die face. On production campaigns exceeding 55 m/min haul-off, bubble instability appears as lateral oscillation and gauge variation above ±15%; the instability is corrected by raising the frost line 50–100 mm and reducing die output, not by widening the die gap. Drying is not required for resin stored in closed silos below 50% RH, but pellets exposed to ambient humidity above 80% RH in outdoor silos require a 4 h desiccant-air purge at 60°C before extrusion to eliminate surface-moisture microvoids. Compliance for the finished silage cover is governed by EN 13206 and polymer registration under REACH 1907/2006. The terminal product is an 18 m wide, 150 µm nominal thickness agricultural silage cover capable of surviving one full ensiling season without film-to-film blocking and without ultraviolet embrittlement before the first feed-out.
The melt flow rate of DOW™ DNDA-1088 NT 7 is 0.8 g/10 min at 190°C under 2.16 kg load as measured by ASTM D1238, and the nominal density is 0.918 g/cm³ by ASTM D792. On 90 mm grooved-feed extruders with water-cooled feed throats, screw speed at 110 rpm yields approximately 380 kg/h at 250 bar melt pressure; increasing screw speed further without raising die temperature causes melt-pressure instability above 300 bar and sharkskin onset due to flow-rate limitation at the die lip. The bubble is supported by internal bubble cooling at 18 m³/h airflow, with gauge profile monitored by a rotating capacitive scanner; a profile deviation above ±12% across the web triggers automatic haul-off speed trimming. A three-layer structure with a 2:2:1 layer ratio places the DNDA-1088 NT 7-rich core in the centre, while the outer layers carry the stabilizer and anti-fog packages.
The dependency of dart impact on frost-line position in heavy-duty sack film is primarily an orientation effect: at very low frost lines below 600 mm on a 450 mm die, the LLDPE chains solidify before adequate hoop and axial orientation are imparted, producing a film with high gauge coefficient of variation and visible stress bands that degrade Elmendorf tear measured according to ISO 6383-2 and dart impact measured according to ASTM D1709. A production blend for 170 µm sack webs contains 72–78 wt% DOW™ DNDA-1088 NT 7, 20–25 wt% post-industrial LLDPE reclaim, and 1.0–1.5 wt% fluoroelastomer processing-aid masterbatch to control die-lip build-up and melt-pressure variation on 75 mm three-layer lines. The bubble is set at 2.5:1 blow-up ratio with a 2.5 mm die gap and melt temperature between 190°C and 205°C; the frost line is deliberately held at 900–1,100 mm to avoid the low-orientation failure mode. Published data for this exact frost-line gradient with DNDA-1088 NT 7 is limited, but production records from sack-film converters indicate that frost-line drift below 700 mm for more than 15 min is associated with a higher coefficient of thickness variation and rejected rolls due to blocking.
Post-industrial reclaim at 20–25 wt% is screened through 80 mesh at the hopper; higher percentages above 30 wt% are avoided because lot-to-lot variation in reclaim melt flow rate increases dart impact variation beyond control limits established by ASTM D1709 Type A. The sack film line is equipped with a melt pump and screen changer; die pressure is maintained at 120–140 bar with a 2.5 mm lip gap and output of approximately 300 kg/h. Blocking is controlled by adding 3,000 ppm synthetic silica in the outer layers only. The terminal product is a 170 µm heavy-duty industrial sack for granulated resin and powder export packaging.
Frozen-food lamination webs are produced at 50 µm total sealant thickness on five-layer blown-film coextrusion lines with 60 mm and 75 mm extruders feeding a 300 mm die at 1.6 mm lip gap. The sealant layer contains 68 wt% DOW™ DNDA-1088 NT 7, 20 wt% LDPE with a melt flow rate of 0.3 g/10 min, 8 wt% synthetic silica anti-block masterbatch targeting 8,000 ppm active silica in the final film, and 4 wt% slip masterbatch containing erucamide at a total final-film concentration not exceeding 1,200 ppm. The bubble is run at 2.0:1 blow-up ratio, melt temperature 195°C, and frost line 450 mm. After cooling, the film is corona-treated to 42 mN/m wetting tension and adhesive-laminated to a biaxially oriented PET or metallised BOPP web. Compliance is anchored to FDA 21 CFR 177.1520(c) paragraph 3.2a for olefin base polymer use, EU Regulation 10/2011 Annex I and II food-contact migration limits, and EC 1935/2004 for finished laminate transfer during low-temperature storage. The terminal product is a 50 µm sealant web in a frozen-vegetable pillow pouch that retains seal integrity at freezer temperatures of −25°C measured by ASTM F88 seal-strength testing at freezer-conditioned state.
At −25°C, seal integrity in frozen food packaging is governed by the comonomer distribution of the LLDPE resin; DNDA-1088 NT 7 at 0.918 g/cm³ retains lower brittle temperature than HDPE-rich sealants of equivalent thickness. Seal strength after freezer conditioning according to ASTM F88 at 200 mm/min jaw separation should be tested against the converter’s internal specification for the specific pouch geometry; published data for this exact masterbatch combination is limited. The lamination step uses a solventless polyurethane adhesive at 1.6–2.0 g/m² coat weight, with a nip temperature of 55°C and a 24 h cure time at 35°C before slitting.
Adhesive lamination of DNDA-1088 NT 7-rich sealant films to high-barrier snack structures is controlled less by the film web and more by the reactive lamination boundary: solventless polyurethane adhesive is applied at 1.8–2.2 g/m² coat weight, nipped at 60°C, and left for 24 h at 35°C to reach full isocyanate–hydroxyl conversion. The sealant film itself is a 60 µm three-layer blown film containing 85 wt% DOW™ DNDA-1088 NT 7, 10 wt% LDPE for bubble stability, and 5 wt% anti-block masterbatch. The film is reverse-printed before lamination; solvent retention in the ink or adhesive below 5 mg/m² is required to avoid interlayer gas pockets during hot air tunnel exposure. Bond strength is checked after 24 h using ASTM F904 T-peel; published data for this specific DNDA-1088 NT 7 laminate configuration is limited, but field data from high-barrier snack packaging lines show that peel strength below 3.0 N/15 mm is associated with curl and delamination at form-fill-seal stations. Compliance is governed by FDA 21 CFR 177.1520, EU 10/2011, and EC 1935/2004. The terminal product is a 60 µm sealant web within a high-barrier laminated snack pouch for dried fruit.
Curl after lamination is controlled by matching machine-direction tension between the sealant film and the printed barrier web. DNDA-1088 NT 7 sealant film stretches at relatively low stress; on a 50 m/min laminator, web tension above 18 N per 1,000 mm width produces tunnel and side-curl in the finished pouch. The terminal high-barrier pouch is sealed at 120°C on horizontal form-fill-seal machines; leak rates are evaluated by ASTM D3078 vacuum differential-pressure testing for pouches with headspace.
A high-speed vertical form-fill-seal line set at 120 cycles/min with 35 ms jaw dwell demands a sealant film that develops hot-tack immediately and still yields stable peel strength after cooling. To achieve seal initiation below 110°C, DNDA-1088 NT 7 films of 60 µm are used with the resin at 100 parts, synthetic silica anti-block at 5,000 ppm active silica, and erucamide slip at 800 ppm final-film concentration. The tube is sealed at 115–130°C with serrated jaw profiles; hot-tack is measured by ASTM F1921 and final seal strength by ASTM F88. The operational boundary is seal-bar temperature above 150°C, at which point molten polymer squeeze-out at the seal interface creates microchannels and the vacuum differential-pressure test run per ASTM D3078 registers increased leak frequency. DNDA-1088 NT 7 with 0.918 g/cm³ nominal density provides a lower seal-initiation point than 0.925-density LLDPE of equivalent melt flow rate, but published seal-initiation curves for this exact slip/anti-block package are limited. Compliance is assessed under FDA 21 CFR 177.1520 and EU Regulation 10/2011. The terminal product is a 1 kg dry soup mix pillow pouch produced on high-speed VFFS equipment.
Erucamide migrates to the sealant surface within 24–48 h at 23°C; if final film is stored in high-humidity conditions before VFFS, slip bloom is generally unaffected, but corona-treated surfaces may lose wetting tension below 38 mN/m. Additive bloom must be completed before sealing trials, because hot-tack measured by ASTM F1921 can vary with surface-slip layer maturity and sealing jaw dwell time.
In double-bubble collation shrink lines, DOW™ DNDA-1088 NT 7 is let down as the core layer at 60 wt%, with 28 wt% LDPE and 10 wt% of a cyclic-olefin shrink modifier, plus 2 wt% combined slip/anti-block. The primary bubble is extruded through a 1.8 mm die gap at a 1.3:1 blow-up ratio; the quenched web is then reheated in the second bubble to 115–125°C and drawn at a machine-direction draw ratio of 3.5:1 and a transverse draw ratio of 3.8:1. Free shrink is measured according to ASTM D2732 at 130°C for 10 s; typical LLDPE-rich collation films of this class show machine-direction shrink between 18% and 22% and transverse-direction shrink between 25% and 30%, though published data for this exact DNDA-1088 NT 7 formulation in double-bubble equipment is limited. The compliance boundary is the ASTM D2732 method itself and ISO 11501 for dimensional change after heating; where the shrink film is used in food-contact bundling, the final film is also assessed under EU Regulation 10/2011. The terminal product is a 50 µm collation shrink bundling film for beverage-can multipacks.
The double-bubble reheating zone must avoid partial melting of the primary film before drawing; draw temperature below 110°C produces uneven stretching and haze bands, while above 130°C the bubble becomes unstable and may collapse at the second nip. The oriented web is annealed in the third bubble at 80–90°C for 5–8 s to control natural shrink before winding. Edge-trim orientation relaxation is removed by in-line slitting at the winder, and roll hardness is maintained at 75–85 Shore OO to prevent telescoping during storage.
Competitive Dow Dow™ DNDA-1088 NT7 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow Dow™ DNDA-1088 NT7 LLDPE is a linear low-density polyethylene resin produced through solution polymerisation with an ethylene-octene comonomer system and supplied as pellets for blown film and cast film conversion. Nominal density is 0.918 g/cm³ as determined by ASTM D792, and melt index is 1.0 g/10 min at 190 °C/2.16 kg per ASTM D1238. The C8 comonomer produces short-chain branches that are less readily incorporated into the orthorhombic crystal lattice than the C4 branches of butene-based LLDPE; this raises tie-molecule concentration and improves toughness in solid-state deformation. The NT7 suffix denotes the stabiliser and processing-additive package, which includes slip and antiblock constituents for film handling, but exact additive loadings should be verified from the batch certificate of analysis because commercial tolerances allow adjustments. Storage is recommended in unopened moisture-resistant containers at temperatures below 40 °C. Extended exposure to ambient relative humidity above 60 % may introduce surface moisture that destabilises melt flow and increases gel formation.
Difference is rooted in molecular architecture. At the same 0.918 g/cm³ density and 1.0 g/10 min melt index, a C4-LLDPE made with butene has shorter branches that are more easily excluded from the crystalline lamellae; the resultant amorphous phase contains fewer load-bearing tie chains. DNDA-1088 NT7 therefore typically produces higher Elmendorf tear strength under ASTM D1922, higher dart impact under ASTM D1709A, and better puncture resistance under ASTM D5748. High-pressure LDPE differs by the presence of long-chain branching and a broad molecular weight distribution. That architecture gives LDPE higher melt strength and more pronounced shear thinning, which stabilises blown film bubbles at low melt temperatures. DNDA-1088 NT7 has lower melt tension, requiring tighter control of die gap, blow-up ratio, and frost-line height. In cast film, the linear backbone increases neck-in and draw resonance sensitivity relative to LDPE; edge-pinning and draw-ratio optimisation are therefore more critical.
On a single-screw blown film line with an L/D of 30:1, barrel temperatures should ramp from approximately 160 °C at the feed throat to 200 °C at the adapter, with die zones maintained at 205 °C to 215 °C. A barrier screw with a Maddock mixing section is preferred over a general-purpose screw because LLDPE pellets require higher shear energy to homogenise than LDPE and are more prone to solid-bed break-up. A die gap between 1.5 mm and 2.5 mm reduces melt fracture; gaps below 1.2 mm generate elevated shear rates at the die lip and produce sharkskin when the melt temperature falls below 190 °C. Blow-up ratios from 2.0:1 to 2.8:1 and frost-line heights between 200 mm and 500 mm balance dart impact and tear anisotropy. Rotating dies should be purged periodically; residence time above 220 °C degrades the slip agent and raises coefficient of friction.
Capillary rheometry at 190 °C shows that DNDA-1088 NT7 is less shear-thinning than LDPE. Apparent viscosity at 100 s⁻¹ is typically higher than that of LDPE of equivalent melt index, while at 1000 s⁻¹ the difference narrows. This raises screw pressure requirements and favours shallow-cut barrier screws. Oscillatory shear data measured under ASTM D4440 or ISO 6721-10 show a terminal relaxation spectrum consistent with a linear backbone without long-chain branching; the crossover frequency is higher than for LDPE of the same melt index. Extensional rheology indicates limited strain hardening, which reduces bubble stability but permits high drawdown in thin-gauge cast processes. Melt pressure at the die above 350 bar often signals insufficient mixing or an excessively narrow die gap. In cast film, draw resonance can occur at high line speeds; air knives, vacuum boxes, and optimised air-gap settings are common countermeasures.
Table 1 lists typical resin properties published for the grade. Values are nominal commercial data, not specification maxima or minima.
| Property | Nominal published value | Test method |
|---|---|---|
| Density | 0.918 g/cm³ | ASTM D792 |
| Melt index | 1.0 g/10 min at 190 °C/2.16 kg | ASTM D1238 |
| DSC crystalline melting peak | 122 °C to 124 °C | ASTM D3418 |
| Vicat softening point | 108 °C | ASTM D1525 |
For film property evaluations, measurements are typically made on 25 µm and 50 µm blown film at a 2.5:1 blow-up ratio. Machine-direction Elmendorf tear is lower than transverse-direction tear because stress-induced orientation aligns lamellae in the machine direction and reduces the energy dissipated by tear propagation. Dart impact values under ASTM D1709A depend on gauge and frost-line height; converters should establish a process-condition matrix rather than relying on single-point data. Optical quality is governed primarily by the antiblock package. Fine silica antiblock with mean particle size below 3 µm yields low haze but requires longer slip-agent bloom time to reach stable coefficient of friction. Freshly extruded film may block until erucamide migrates to the surface; inline slitting should allow an aging interval of 24 h to 48 h before high-speed winding. Haze and gloss are measured under ASTM D1003 and ASTM D2457, respectively.
On 25 µm film, seal initiation is governed by the melting distribution of the octene-modified polyethylene. Seal strength under ASTM F88 rises rapidly once the seal bar temperature exceeds the crystalline melting onset; converter settings typically range from 115 °C to 130 °C for uncoated film. Higher seal bar temperatures increase hot-tack but may cause film distortion or seal-through in high-speed vertical form-fill-seal lines. Because slip additive migrates to the surface, corona treatment and aging can shift seal initiation upward; oxidised surface layers act as a barrier to interfacial melting. Seal strength should be measured on the completed film structure after processing and aging, not on resin pellets. Hot-tack performance is typically evaluated under ASTM F1921, with maximum seal strength occurring when the seal bar temperature is kept below the point at which complete melting destroys orientation.
Corona treatment raises surface energy for printing and adhesive lamination but oxidises the outer polyethylene chains. This oxidation slows erucamide migration because the surface is partially cross-linked and polar; treatment levels above 42 dyn/cm can freeze the coefficient of friction in the 0.35 to 0.45 range instead of allowing decay below 0.25. Converters running high-speed form-fill-seal equipment should specify the lowest dyne level consistent with ink anchorage, commonly 38 dyn/cm to 42 dyn/cm, and evaluate coefficient of friction after 48 h aging. Antiblock particles, typically synthetic silica, reduce direct film-to-film contact area. Their performance is controlled by dispersion quality; agglomerates larger than 20 µm can generate visible specks in thin-gauge film and should be monitored under ASTM D7210 or an equivalent in-line camera protocol.
In food-contact applications, the resin is normally assessed under FDA 21 CFR 177.1520 for olefin polymers and, where applicable, EU Regulation 10/2011. The grade is used in industrial liners, heavy-duty sacks, collation shrink film, and as a skin or core layer in coextruded barrier structures. Because the resin contains slip and antiblock additives, direct food-contact compliance must be validated for the specific additive package and use temperature; migration testing under EN 1186 or applicable regional protocols is required for fatty and aqueous simulants. The resin is not intended for medical devices or pharmaceutical primary packaging unless an appropriate USP Class VI or ISO 10993 biological evaluation is completed by the converter. For agricultural film, the UV stabilisation package is supplied by the compounder rather than the base resin, so stabiliser concentration must be specified separately.
Table 2 summarises the primary compliance and quality-control matrix applicable to the grade.
| Compliance dimension | Standard or protocol | Typical requirement |
|---|---|---|
| Food-contact base resin | FDA 21 CFR 177.1520 | Olefin polymer positive list |
| EU food-contact material | EU 10/2011 | Overall migration limit 10 mg/dm² |
| Melt index | ASTM D1238 | 1.0 g/10 min |
| Density | ASTM D792 | 0.918 g/cm³ |
When operating limits are exceeded, the resin should not be processed above 240 °C; prolonged exposure at this temperature degrades the primary antioxidant and accelerates erucamide loss, shifting the final coefficient of friction upward. Combination with certain amine-based antistatic additives may produce surface deposits when slip agents are present; compatibility must be verified in a blown-film trial. Purging with polycarbonate or PVC must be followed by complete displacement with polyolefin and a melt-temperature reduction below 220 °C before reintroducing DNDA-1088 NT7 to avoid carbonised specks. Moisture on pellet surfaces above 0.01 % can cause flow surging in single-screw extrusion; heated hopper drying at 60 °C for 2 h may be applied when condensation is visible.
Routinely, incoming material is tracked for lot-to-lot variance through polymerisation conditions and additive dosing. Converters monitoring incoming material should track melt index, density, and additive-related surface properties. A shift in melt index beyond ±10 % from the nominal 1.0 g/10 min may indicate a change in comonomer distribution or chain-transfer conditions and should trigger extrusion current and film gauge monitoring. Differential scanning calorimetry can detect changes in comonomer distribution through broadening of the melting endotherm; a bimodal melting trace would suggest contamination or blending with another polymer. Fourier-transform infrared spectroscopy can be used to verify the presence of the octene branch peak at approximately 770 cm⁻¹ but is not a substitute for melt rheology and film testing.
In multilayer film structures, DNDA-1088 NT7 is often placed in skin layers or heavy-gauge core layers where toughness contributes to abuse resistance. When the LLDPE layer ratio exceeds 50 % of total film thickness, the lower melt strength of the linear resin influences bubble geometry and cooling. Coextruded lines with outer LDPE skins and a core of DNDA-1088 NT7 maintain bubble stability because the LDPE layers provide melt elasticity. If the LLDPE fraction is increased above 70 %, the bubble becomes more susceptible to wobble and steering errors; operators typically reduce output or narrow the frost-line height to compensate. Compared with metallocene LLDPE grades, DNDA-1088 NT7 may have a wider molecular weight distribution and lower melt strength; the choice depends on required dart impact, seal initiation temperature, and extrusion line pressure. Published data for direct substitution in all coextrusion configurations is limited.