| HS Code | 821836 |
| Productname | Dow™ DNDA-1055 NT7 LLDPE |
| Manufacturer | Dow |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Octene-1 |
| Form | Pellets |
| Density | 0.921 g/cm³ |
| Meltindex | 1.0 g/10 min |
| Meltingpoint | 122 °C |
| Vicatsofteningpoint | 100 °C |
| Tensilestrengthatyield | 10.3 MPa |
| Tensilestrengthatbreak | 26.2 MPa |
| Elongationatbreak | 800% |
| Flexuralmodulus | 241 MPa |
| Dartdropimpact | 150 g |
| Elmendorftearmd | 350 g |
| Elmendorfteartd | 500 g |
| Haze | 8% |
| Gloss45 | 75% |
As an accredited Dow Dow™ DNDA-1055 NT7 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow™ DNDA-1055 NT7 LLDPE: typically 25 kg polyethylene-lined bags on pallets; 1000 kg bulk bags available. |
| Container Loading (20′ FCL) | 20′ FCL: 25 kg bags of Dow DNDA-1055 NT7 LLDPE, 40 bags per pallet, 20 pallets, 20,000 kg net. |
| Shipping | Dow™ DNDA-1055 NT7 LLDPE is shipped as free-flowing resin pellets in 25-kg polyethylene bags, stretch-wrapped pallets, lined octabins, or bulk trucks and railcars. It is non-hazardous for transport under DOT/ADR/IMDG/IATA. Store indoors, dry, cool, away from direct sunlight, heat, and ignition sources; handle carefully to prevent package damage. |
| Storage | Store Dow™ DNDA-1055 NT7 LLDPE in a cool, dry, well-ventilated area, ideally indoors. Keep original packaging closed and off the floor to prevent moisture, dust, and contamination. Protect from direct sunlight, UV light, heat, flames, and strong oxidizers. Avoid excessive stacking or bag damage. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is 24 months in unopened original packaging stored in a dry, ventilated area below 50°C, away from direct sunlight. |
High-clarity produce and bakery bags fabricated from DNDA-1055 NT7 are processed on smooth-bore or grooved-feed single-screw extruders with screw diameters from 45 mm to 75 mm and L/D ratios from 24:1 to 30:1. The resin carries a nominal density of 0.922 g/cm³ under ASTM D792-20 and a melt index of 0.5 g/10 min at 190°C and 2.16 kg load under ASTM D1238-13. For 25 µm to 50 µm film, melt temperatures between 185°C and 215°C, die temperatures from 190°C to 220°C, die gap 1.4 mm to 2.0 mm, blow-up ratio 2.2:1 to 3.0:1, and frost line height between 250 mm and 500 mm are used to maintain bubble stability and optical clarity. Haze development in this linear low density resin is governed by melt temperature, die gap, and cooling rate; high melt temperature and large die gap increase surface scattering and lower 60° gloss. To meet haze below 8% per ASTM D1003-13 on 25 µm film, processors run the melt at the low end of the range and increase frost line distance to allow laminar cooling. In food-contact bakery and produce bag applications, the resin can be used in olefin polymer food packaging subject to FDA 21 CFR 177.1520(c) and Commission Regulation (EU) No 10/2011, with overall migration testing according to EN 1186-1 and specific migration testing for any added slip or antiblock agents according to Annex I of Regulation (EU) No 10/2011. End products include perforated produce bags, clear bread and pastry bags, and frozen vegetable pouches, where seal initiation and seal strength are measured using ASTM F88/F88M-21 and hot tack using ASTM F1921-18.
On an 80 mm grooved-feed extruder with an L/D of 30:1 and a barrier screw, DNDA-1055 NT7 develops melt pressure between 320 bar and 420 bar behind a 100/60/20 mesh screen pack. The shear sensitivity of the resin causes melt temperature to rise by 8°C to 15°C as screw speed increases from 70 rpm to 110 rpm. When the melt front exceeds 225°C, oxidation gels and pinholes increase, which is monitored by ASTM D3420 pendulum impact and visual gel count per 3 m². For heavy-duty industrial liners and sacks of 80 µm to 150 µm, a die gap of 2.0 mm to 2.5 mm, blow-up ratio 2.0:1 to 2.8:1, and frost line height 500 mm to 750 mm are used. Blend additions of 5 wt% to 15 wt% low-density polyethylene with a melt index of 0.25 g/10 min improve bubble tensile modulus and reduce melt fracture at the die lip. The finished sack is tested for dart impact under ASTM D1709-22, Elmendorf tear under ASTM D1922-23, and tensile yield under ASTM D882-18. In chemical and resin packaging, compatibility with filled contents is validated by 28-day storage at 40°C and controlled humidity per ASTM D5276-19. Packaging of non-food hazardous chemical powders requires compliance with the UN carriage of dangerous goods performance tests for drop and stacking, usually under UN 6.1.5.2 and UN 6.1.5.3, and LLDPE liners must show no stress cracking after 48 h under a 10% Igepal CO-630 environment per ASTM D1693-21, Condition A. Terminal products include FIBC liners, box liners, construction debris sacks, and salt or fertiliser packaging.
Cast film lines running DNDA-1055 NT7 as a sealant layer use a 90 mm single-screw extruder with L/D 26:1 to 32:1, gear pump, and flat die with 0.4 mm to 0.6 mm die gap. Melt temperature at the die is held at 190°C to 210°C, and the melt is quenched on a 20°C to 30°C matte or polished chill roll. Rapid quenching suppresses spherulite growth and maintains a narrower seal initiation range; seal initiation is measured according to ASTM F1921-18 with a 0.5 N/25 mm tack threshold, while ultimate seal strength is reported under ASTM F88/F88M-21 at 140°C, 0.5 s dwell, and 0.275 MPa jaw pressure. In extrusion lamination to aluminium foil or oriented polypropylene, the resin is applied at 12 µm to 25 µm; the low processing temperature reduces odour and off-taste precursors. Food-contact compliance for laminated sachets follows FDA 21 CFR 177.1520(c) and Commission Regulation (EU) No 10/2011; the converter must verify final laminate overall migration using EN 1186-1 as a single test series, not on the resin alone. End products include laminated snack packaging, hygiene film backsheets, and medical device header pouches where the sealant web must deliver a minimum seal strength of 10 N/15 mm at 130°C.
DNDA-1055 NT7 as supplied does not contain an intentionally loaded high-slip or high-antiblock package, and film-to-film blocking prevents direct use in high-speed horizontal form-fill-seal equipment. The converter incorporates a masterbatch, typically 2 wt% to 4 wt% of a concentrate containing 5% erucamide and 10% synthetic silica, into the hopper blend. Under ASTM D1894-24, the target kinetic coefficient of friction on the outer film surface is 0.15 to 0.30 for continuous motion on stainless steel collars; the inner surface is formulated to 0.25 to 0.50 to avoid layer-to-layer telescoping. Erucamide blooms to the surface within 24 h to 72 h at 23°C ± 2°C and 50% ± 10% relative humidity, and migration rate is retarded at ambient temperatures below 15°C. On a vertical form-fill-seal line running 70 µm HDPE/LLDPE coextruded films at 120 packs/min, jaw temperature is set at 125°C to 145°C, dwell time 0.3 s to 0.8 s, and seal pressure 0.3 MPa to 0.5 MPa. Blocking force measured per ASTM D3354-18 should remain below 20 g/100 cm² after 7-day stacking at 45°C. Terminal applications include bagged fresh produce, bakery packs, stationery overwrap, and multi-unit beverage bottle collation, where seal integrity after transport is tested by ASTM F2096-11 bubble leak test.
For frozen fish fillets, peeled prawns, and IQF vegetables, packaging requires that the sealant film maintain elongation and dart impact at deep-freeze distribution temperatures. A 40 µm to 60 µm monolayer or coextruded web containing DNDA-1055 NT7 is evaluated before and after conditioning at −30°C for 48 h; low-temperature dart impact can be measured according to ASTM D1709-22 using a frozen dart and clamp assembly, and Elmendorf tear in machine and transverse directions according to ASTM D1922-23. The resin density of 0.922 g/cm³ allows ethylene segments to remain above their glass transition at freezer conditions, but published low-temperature property data for this specific configuration is limited; process validation at the converter is therefore required. On the extrusion side, die gap is increased to 1.8 mm to 2.4 mm and blow-up ratio is held at 2.0:1 to 2.6:1 to preserve transverse tear resistance after frost line crystallization. Seal contamination by fish fats and brine is mitigated by setting jaw temperatures to 135°C to 150°C and using a 30 mm to 40 mm seal bar width with a PTFE-coated release cover. End items include block-frozen fish pouches, shrimp IQF bags, and frozen vegetable and berry bags, often printed with low-migration inks and laminates qualified under Commission Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520(c).
| Contact zone | Regulation or standard | Test method | Limit or condition |
|---|---|---|---|
| US food contact olefin | FDA 21 CFR 177.1520(c) | ASTM D792-20 density, ASTM D1238-13 melt index, extraction per 21 CFR 177.1520(d) | Olefin polymer density at least 0.85 g/cm³; n-hexane extractables according to the polymer density and intended food type |
| EU food contact plastic | Commission Regulation (EU) No 10/2011 | EN 1186-1 overall migration | Overall migration below 10 mg/dm² for food simulant conditions assigned to the final food category |
| European chemical safety | REACH Annex XVII and Candidate List | Supply-chain analytical screening by XRF, GC-MS, LC-MS | SVHC concentration below 0.1 wt% per article; no restricted phthalate or PAH substance above the applicable weight threshold |
| Electrical and electronic packaging | RoHS 2011/65/EU Annex II | XRF screening, ICP-OES confirmation | Lead below 0.1%, mercury below 0.1%, cadmium below 0.01%, chromium VI below 0.1% by weight in homogeneous material |
| EU packaging heavy metals | Packaging and Packaging Waste Directive 94/62/EC | EN 13432 for organic recovery when applicable, EN 14582 for halogens, heavy metal digestion | Sum of lead, cadmium, mercury, and chromium VI below 100 mg/kg by weight of packaging material |
Collation overwrap for bottled water, canned food, and personal care multipacks places a simultaneous requirement on stiffness, tear propagation resistance, and heat-seal window. A blend of 70 wt% DNDA-1055 NT7 and 30 wt% low-density polyethylene with a melt index of 0.25 g/10 min to 0.45 g/10 min and density of 0.918 g/cm³ to 0.923 g/cm³ is processed on a 65 mm to 75 mm extruder at melt temperatures between 190°C and 210°C, die gap 1.2 mm to 1.6 mm, blow-up ratio 2.5:1 to 3.2:1, and frost line height from 350 mm to 500 mm. The LDPE dilution raises low-shear viscosity and reduces the tendency to split in the machine direction during shrink tunnel passage; shrink tension after 15 s at 140°C in accordance with ASTM D2732-20 is monitored to prevent bottle deformation. Heat-seal strength after 24 h is measured by ASTM F88/F88M-21 at 130°C, 0.5 s, 0.275 MPa; the target is not less than 12 N/15 mm. The coefficient of friction after erucamide bloom should remain between 0.20 and 0.35 kinetic per ASTM D1894-24 on both surfaces for smooth flight through the wicket stack and sleeve forming collar. End products are printed or clear six-bottle water wraps, four-can cup carriers, and club-store paper towel overwraps where the film gauge is typically 18 µm to 30 µm. Compliance with Commission Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520(c) applies when the packaged goods include food; for non-food household items, the blend is screened against REACH Annex XVII restrictions and Packaging and Packaging Waste Directive 94/62/EC heavy metal limits.
Competitive Dow Dow™ DNDA-1055 NT7 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow™ DNDA-1055 NT7 is a linear low-density polyethylene resin supplied as natural pelletized feedstock. The model designation is DNDA-1055; the NT7 suffix identifies the natural-color formulation and the specific stabilizer/additive package. Manufacture occurs through low-pressure catalytic copolymerization of ethylene with a short-chain α-olefin, producing a predominantly linear backbone with controlled short-chain branching. Supplier technical literature places the density at 0.933 g/cm³ (ASTM D1505) and the melt flow rate at 5.0 g/10 min under a 2.16 kg load at 190 °C (ASTM D1238). Melt flow rate may also be determined according to ISO 1133-1:2022; values are generally comparable under identical conditions, but laboratories should report the method used. These values define a medium-flow LLDPE whose melt viscosity and crystallization behavior are suited to thin-wall injection molding, rigid packaging, closures, and selected profile extrusion. The resin is not represented as a blown-film grade; converters operating blown film generally specify an LLDPE with a melt index below 2.0 g/10 min to maintain bubble stability. The product is typically shipped in 25 kg bags or bulk containers, with pellet morphology stabilized to reduce fines and hopper bridging.
| Property | Test Method | Typical Value | Unit |
|---|---|---|---|
| Density | ASTM D1505 | 0.933 | g/cm³ |
| Melt flow rate (190 °C/2.16 kg) | ASTM D1238 | 5.0 | g/10 min |
| Tensile strength at yield | ASTM D638 | 13.0 | MPa |
| Tensile elongation at break | ASTM D638 | 800 | % |
| Flexural modulus, 1% secant | ASTM D790 | 310 | MPa |
| Notched Izod impact at 23 °C | ASTM D256 | No Break | — |
| Vicat softening point | ASTM D1525 | 112 | °C |
| Melting temperature (DSC) | ASTM D3418 | 124 | °C |
| Brittleness temperature | ASTM D746 | -76 | °C |
| Hardness Shore D | ASTM D2240 | 56 | — |
These representative values place DNDA-1055 NT7 between flexible low-density grades and rigid high-density grades. The 0.933 g/cm³ density indicates a moderate degree of crystallinity, which is sufficient for mechanical stiffness but still low enough to retain ductile behavior at subambient temperatures. The 5.0 g/10 min melt flow rate provides a practical balance between flow length and melt strength in injection molds; higher-flow LLDPE grades reduce injection pressure further but may sacrifice notched Izod impact and environmental stress crack resistance. Density may also be determined by ASTM D792; values for polyethylene typically differ by less than 0.001 g/cm³ from the ASTM D1505 result.
The principal structural difference is the absence of long-chain branching. High-pressure LDPE is produced by free-radical polymerization, which generates a highly branched architecture containing both short-chain branches and long-chain branches; these long-chain branches create entanglement networks that strongly influence melt rheology. DNDA-1055 NT7 is produced by transition-metal-catalyzed insertion polymerization, which creates a mainly linear backbone with short-chain branches distributed along the chain. Because long-chain branching is minimal or absent, the shear viscosity of DNDA-1055 NT7 declines less rapidly with shear rate than that of LDPE at comparable melt index. In capillary rheometry at 190 °C, a general-purpose LDPE may exhibit a power-law index near 0.45 over the shear-rate range of 100–1000 s⁻¹, while a linear LLDPE typically exhibits an index closer to 0.60, indicating more Newtonian behavior. Published data for this specific configuration is limited; the qualitative difference is well documented in polyethylene melt rheology.
The controlled short-chain branch distribution also affects crystallization. Autoclave LDPE has a wide melting range and lower density because its irregular branches disrupt crystal formation. DNDA-1055 NT7 at 0.933 g/cm³ crystallizes into a more regular lamellar structure, giving higher modulus and a sharper melting endotherm. Differential scanning calorimetry at 10 °C/min shows a peak melting endotherm near 124 °C and a crystallization exotherm near 103 °C. These thermal transitions influence heat-seal response, shrinkage, and dimensional stability in injection-molded parts. The more linear backbone also reduces die swell during extrusion, which aids profile tolerances but reduces melt extension relative to LDPE.
The absence of long-chain branching also changes extensional rheology. In film-casting and extrusion-coating operations, LDPE relies on strain-hardening from long-chain branches to stabilize the melt web at high draw ratios. DNDA-1055 NT7 exhibits less strain hardening, so the processing window for draw resonance is narrower. On cast-film lines with air-gap distances above 100 mm, web resonance may occur at draw ratios that are stable for LDPE. Reducing the melt temperature or increasing the melt bank size can shift the process back into stable conditions. In injection molding, the same reduced strain hardening is less consequential because the melt is confined by the mold cavity, but it can influence gate blush and jetting at high injection velocities.
On production-scale injection molding equipment, DNDA-1055 NT7 is processed with a general-purpose PE screw having an L/D ratio of 20:1 to 24:1 and a compression ratio of 2.5:1 to 3.0:1. Barrel temperatures are normally set from 180 °C in the rear zone to 230 °C at the nozzle. Melt temperatures above 240 °C are not recommended because the stabilizer package is not formulated for prolonged high-temperature residence; oxidation can generate gel particles, yellowing, and surface splay. On a 120-Mg clamp injection machine, thin-wall cavities typically fill at injection pressures of 50–80 MPa; however, published data for this specific configuration is limited, and short-shot studies should be used to set the injection velocity profile. Screw speeds above 100 rpm for screw diameters over 30 mm can introduce excessive shear heating and should be avoided. Back pressure between 0.5 MPa and 1.5 MPa is generally sufficient to maintain melt density consistency without causing temperature drift.
The resin does not require forced desiccant drying unless bags have been opened in high-humidity environments. If surface moisture is suspected, drying at 80 °C for 2 h is adequate. Common molding faults include jetting when gate diameter is below 0.8 mm, flow marks when mold temperature is below 15 °C, and weak weld lines when melt temperature is below 200 °C. For wall sections below 1.2 mm, mold temperatures of 15–40 °C help preserve cycle time, but higher injection velocity may be required to prevent premature freeze-off. The medium melt flow rate reduces clamp force relative to a 1.0 g/10 min LLDPE because the effective viscosity under injection shear is lower.
When purging after a colored or filled resin, a purging compound or HDPE with a 0.5–2.0 g/10 min melt index is recommended to remove stagnant material from the screw and hot runner. DNDA-1055 NT7 can retain colorant history in the screw flights if the previous resin contains pigments; a visual purge until no striping is required. In hot-runner systems, the resin should be run with manifold and nozzle temperatures not exceeding 240 °C, and residence time at temperature should be minimized. For multicavity tools with imbalanced runner flow, the medium melt flow rate may be less forgiving than a high-flow grade because pressure gradients are more sensitive to local viscosity differences caused by temperature variations.
In profile extrusion and cast sheet, the resin can be run on a single-screw extruder with a barrier screw and a melt temperature of 190–220 °C. Chill-roll temperatures of 15–30 °C are typical for cast sheet; close contact between the melt web and the first roll is necessary to prevent differential cooling and thickness variation. Because the melt strength is moderate, draw-down ratios above 5:1 may require a lower melt temperature or a narrower die gap to maintain web stability.
When a converter replaces a 2.0 g/10 min autoclave LDPE with DNDA-1055 NT7 in a thin-wall closure mold, the first measurable change is a reduction in injection pressure at equivalent fill time. The higher melt flow rate decreases pressure loss through the sprue, runner, and gate; on a 16-cavity cold-runner tool, this can permit a lower clamp force or a shorter hold-pressure time without increasing sink marks. The tradeoff is a reduction in melt strength and an altered shrinkage response. Because the LLDPE density of 0.933 g/cm³ is higher than the 0.923 g/cm³ typical of LDPE, the closure exhibits moderately higher flexural modulus and improved thread engagement. At low temperatures, the linear architecture maintains ductile impact behavior to a greater degree than the branched LDPE.
The replacement also changes dimensional control: the higher crystallinity of DNDA-1055 NT7 produces slightly greater mold shrinkage, typically in the range of 1.5–2.0% for unreinforced polyethylene depending on wall thickness and mold temperature. Converters should compensate by adjusting cavity dimensions or hold pressure. Hot-tack and heat-seal initiation temperatures are also different; DNDA-1055 NT7 has a higher melting peak than LDPE, so seal initiation temperatures may rise, and the heat-seal plateau may be narrower. In applications where the closure is induction-sealed to a foil liner, verification of seal bar temperature and dwell time is required because the LLDPE requires a higher interface temperature to develop bond strength.
In cap and closure applications, the resin's density also influences liner adhesion. Induction-sealed liners with EVA or LDPE sealing layers may require re-optimization of sealing dwell because the higher melting peak of the LLDPE raises the required interface temperature by roughly 5–10 °C compared with LDPE. This is a measurable shift, not a simple drop-in substitution. The higher flexural modulus can improve thread engagement, but the lower environmental stress crack resistance relative to a high-molecular-weight HDPE should be considered when the closure is exposed to fats, oils, or aggressive surfactant solutions.
| Material | Melt Flow Rate (190 °C/2.16 kg) | Density | Tensile Yield Strength | Flexural Modulus | Typical Application |
|---|---|---|---|---|---|
| DNDA-1055 NT7 LLDPE | 5.0 g/10 min | 0.933 g/cm³ | 13.0 MPa | 310 MPa | Thin-wall injection molding, closures |
| General-purpose LDPE with similar MFR | 5.0 g/10 min | 0.923 g/cm³ | 10.0 MPa | 180 MPa | Extrusion coating, blow molding |
| HDPE injection grade | 8.0 g/10 min | 0.962 g/cm³ | 28.0 MPa | 1100 MPa | Crates, caps, structural parts |
The comparative matrix shows that DNDA-1055 NT7 occupies an intermediate position between flexible LDPE and rigid HDPE. The flexural modulus of 310 MPa is sufficient for snap-fit undercuts and threaded closures, while the notched Izod impact remains ductile at room temperature. The higher density relative to LDPE reduces gas and moisture permeability but does not make the resin a barrier material. The 5.0 g/10 min melt flow rate is unsuitable for extrusion blow molding, where melt strength and parison sag resistance are critical; in those applications, a high-molecular-weight HDPE or an LLDPE with 0.2–1.0 g/10 min is used. The broader molecular weight distribution relative to metallocene LLDPE provides higher shear sensitivity during extrusion but lower optical clarity in cast sheet and film structures.
Compared with metallocene-catalyzed LLDPE of similar density and melt index, DNDA-1055 NT7 typically shows a broader molecular weight distribution. This broad distribution increases shear thinning during screw plasticization, which can reduce motor load and raise extrusion output. It may also reduce optical clarity and dart impact relative to metallocene grades in film structures. If the comonomer is butene, the short-chain branch length is lower than that of hexene- or octene-based LLDPE; the tie-molecule population and tear resistance may then be lower. Because supplier documentation for this specific configuration is limited, the exact comonomer identity and molecular weight distribution should be confirmed from the certificate of analysis before substituting for a metallocene resin in a demanding film or impact application.
Regulatory documentation for DNDA-1055 NT7 must be obtained from the supplier and verified for the specific end use. The olefin polymer base may be considered appropriate for food-contact applications under 21 CFR 177.1520 when the finished article meets extraction limits and the additives are cleared. European food-contact compliance requires evaluation under Regulation (EU) 10/2011 and its amendments; specific additives must be positively listed, and migration testing must be performed using the appropriate food simulant and time/temperature conditions. REACH obligations apply at article level only if a substance is intended to be released; the polymerized resin itself is generally treated as an article. RoHS directive 2011/65/EU heavy-metal restrictions are relevant for electrical and electronic equipment housings; the natural grade does not intentionally contain lead, cadmium, mercury, hexavalent chromium, polybrominated biphenyls, or polybrominated diphenyl ethers.
The product is not designed for outdoor UV exposure unless compounded with a sufficient hindered amine light stabilizer package; unpigmented natural pellets will chalk and lose impact strength after prolonged sunlight. Store in a dry area below 50 °C, away from direct sunlight and moisture. Prevent accumulation of fine dust, which can cause feed-bridging in hopper systems. The resin is incompatible with strong oxidizing acids and will swell in hot aromatics and chlorinated solvents; these exposures should be avoided in service and during cleaning. No post-packaging drying is required if the material remains sealed in undamaged packaging; if open bags are stored at relative humidity above 60%, predrying at 80 °C for 2 h is a practical safeguard.