| HS Code | 148869 |
| Density | 0.918 g/cm³ |
| Melt Index | 0.70 g/10 min |
| Melt Flow Ratio | 27 |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 24.1 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 241 MPa |
| Vicat Softening Point | 93 °C |
| Melting Point | 122 °C |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Strength Md | 300 g |
| Elmendorf Tear Strength Td | 500 g |
| Haze | 12% |
| Gloss | 60% |
As an accredited Dow Dow™ DFDF-7047 NT7 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow™ DFDF-7047 NT7 LLDPE is typically supplied in 25 kg polyethylene-lined bags, palletized for transport; bulk quantities available. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with palletized bags of Dow™ DFDF-7047 NT7 LLDPE, stretch-wrapped, secured, and marked for safe ocean shipment. |
| Shipping | Dow™ DFDF-7047 NT7 LLDPE is shipped as non-hazardous resin pellets in 25 kg polyethylene-lined bags on stretch-wrapped pallets, or in bulk trucks/railcars. Keep dry, clean, and away from heat, moisture, and sunlight. Not DOT/IMDG regulated; follow SDS and local transport rules. Ensure intact packaging and avoid contamination. |
| Storage | Store Dow™ DFDF-7047 NT7 LLDPE in original, sealed packaging in a cool, dry, well-ventilated area. Protect from moisture, direct sunlight, dust, and contaminants. Keep away from heat, sparks, open flames, and prolonged UV exposure. Avoid extreme temperatures. Stack pallets securely, use FIFO rotation, and prevent bag damage. Inspect containers regularly and maintain clean, dry storage conditions. |
| Shelf Life | Typically two years from date of manufacture when stored unopened in original packaging under dry, cool conditions away from sunlight. |
Film converters running Dow™ DFDF-7047 NT7 in monolayer blown film lines for dry-food pouches, frozen-vegetable bags, and bread bags typically pneumatically convey pellets through 38 mm to 50 mm i.d. stainless steel piping at pellet temperatures below 45 °C, because surface moisture from ambient air above 60 % RH creates microbubble defects at the die lip. Extruders with screw L/D 24:1 to 30:1 and a Maddock mixing section are run with barrel profile 170 °C/180 °C/185 °C/190 °C/195 °C, adapter temperature 200 °C, and die temperature 205 °C; melt pressure is maintained at 18–35 MPa to stabilize output. A die gap of 1.8 mm to 2.4 mm and blow-up ratio 2.0:1 to 2.8:1 are used for film thicknesses between 20 μm and 60 μm. Frost line height is set between 350 mm and 650 mm, with higher settings raising dart impact resistance but lowering 45° gloss and increasing haze; field trials show 45° gloss can fall by 5–10 points when frost line height is increased from 400 mm to 650 mm, while dart drop impact improves by 10–20 g depending on gauge. The resulting film is tested under ASTM D1709-16a Method A for dart impact, ISO 6383-2:1983 for Elmendorf tear, ISO 527-3:2018 for tensile properties at 500 mm/min, ASTM D1003-13 for haze, and ASTM D2457-13 at 45° for gloss. For food-contact use, compliance is established at the converter level under 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, because additive masterbatches, surface printing, and downstream lamination must be included in an overall migration assessment of 10 mg/dm² or lower in final form. Gauge variation is controlled to ±1.5 μm at 25 μm nominal thickness measured by ASTM D6988-13, with automatic die controls and air ring adjustments compensating for draw resonance at high take-off speeds.
| Property | Standard / code | Relevant equipment condition | Primary failure mode |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022, 190 °C/2.16 kg | Incoming resin quality control | Flow fluctuation |
| Density | ISO 1183-1:2019 | Blend ratio calculation | Stiffness shift |
| Dart drop impact | ASTM D1709-16a Method A | 25 μm blown film | Puncture failure |
| Elmendorf tear | ISO 6383-2:1983 | MD/TD orientation | Split propagation |
| Tensile properties | ISO 527-3:2018, 500 mm/min | Film draw ratio | Yield/break failure |
| Haze | ASTM D1003-13 | 25 μm film | Optical rejection |
| Gloss | ASTM D2457-13, 45° | 25 μm film | Appearance rejection |
| Hot tack | ASTM F1921-12 | 0.2–0.5 s dwell | FFS seal opening |
| Heat seal strength | ASTM F88/F88M-21 | 150 mm/min pull | Pouch burst |
| Kinetic coefficient of friction | ISO 8295:1995 | 200 g sled, 150 mm/min | Film transport jam |
In three-layer heavy-duty sack lines producing 25 kg to 50 kg industrial bags for polymer granules, fertilizer, and dry mortar, DFDF-7047 NT7 is blended with LDPE and HDPE to balance dart impact, bubble stability, and seal strength. The linear molecular architecture of the resin reduces shear-thinning and extensional viscosity relative to a branched LDPE of equivalent melt index; at LLDPE concentrations above 60 wt%, bubble flapping occurs on high-stalk lines when blow-up ratio exceeds 2.4:1 and die gap is held at 2.0 mm. Adding 15 wt% high-pressure LDPE and 15 wt% HDPE restores bubble stability and raises stiffness, but HDPE increases seal initiation temperature by 6–12 °C and reduces dart impact by 15–25 g on 100 μm film. Heat seal testing is carried out under ASTM F88/F88M-21 at 150 mm/min pull speed and hot tack under ASTM F1921-12 at 0.5 s dwell. Seal initiation on a 100 μm three-layer sack structure typically begins at 118–125 °C and reaches plateau strength of 8–12 N/15 mm between 135 °C and 155 °C; above 160 °C, the seal area becomes susceptible to thinning and stringing at the jaw exit. When the sack is filled with dusty products, seal integrity is further reduced by particulate contamination at the seal interface; pre-cleaning with deionized compressed air at 0.3–0.5 MPa is specified on working lines to maintain hot tack values within 20 % of clean-film measurements. Published data for this specific high-output heavy-duty sack configuration are limited; converters should not transfer seal window limits from cast-film lines to blown-film lines without line-scale trials.
Agricultural silage covers and bale wrap structures are extruded from DFDF-7047 NT7 with thicknesses of 100 μm to 150 μm, typically in white/black coextrusion with a white outer layer containing 8–12 wt% titanium dioxide masterbatch and a black inner layer containing 5–8 wt% carbon black masterbatch. The film is processed at die gaps of 2.2 mm to 2.6 mm and BUR 1.8:1 to 2.2:1 to prevent melt fracture at the higher melt throughput required for thick gauge. UV stabilization is achieved with hindered amine light stabilizer packages at 0.4–0.8 wt% active HALS and 0.2–0.5 wt% UV absorber, typically introduced as a 10 % active masterbatch; pre-drying of the masterbatch at 70 °C for 4 h is required when storage RH exceeds 65 %, because moisture hydrolyzes certain HALS intermediates and results in die-lip deposit formation. Outdoor performance is assessed by accelerated xenon-arc exposure under ISO 4892-2:2013 with 0.35 W/m² irradiance at 340 nm and 60 °C black-standard temperature, with elongation retention above 50 % after 12 months in temperate outdoor exposure. Tear resistance is measured by ISO 6383-2:1983 after 48 h conditioning at 23 °C and 50 % RH per ISO 291:2008; puncture resistance is measured by ASTM D5748-19. Low-temperature impact is also relevant for silage covers applied in late autumn; film conditioned at -10 °C for 24 h is evaluated for dart drop under ASTM D1709-16a Method A to verify that frozen soil puncture does not exceed field requirements.
On high-speed vertical form-fill-seal lines packing frozen seafood and poultry at -25 °C storage, film based on DFDF-7047 NT7 is used at 30 μm to 50 μm because low-temperature dart impact failure is a primary rejected-bag mode. The film is produced with BUR 2.2:1 to 2.6:1 and frost line height 500 mm to 700 mm, which increases transverse-direction orientation and improves puncture resistance at the expense of haze. Sealing is performed at 130–145 °C with 0.2–0.5 s dwell time; the seal is tested after 24 h at -20 °C for tensile seal strength under ASTM F88/F88M-21, with failure modes recorded as peel, tear, or cohesive break. Film is corona-treated inline at 2.0–2.5 kW and 10 m/min per 0.1 m width to raise wetting tension to 38–42 mN/m, measured by ASTM D2578-17; lower treatment levels lead to ink delamination on reverse-printed overlacquer structures. Slip performance is required for FFS transport; coefficient of friction is measured under ISO 8295:1995 with a 200 g sled at 150 mm/min, and the film is aged 48 h at 23 °C before testing to allow migration of surface-active additives. Blocking is controlled with silica antiblock at 1,500–3,000 ppm active content; excess antiblock raises haze by 2–5 % absolute and reduces dart impact at low temperatures, so the minimum effective level is selected.
Reverse-printed lamination webs based on DFDF-7047 NT7 are used as sealant films in pouches for dry soup mixes, snack foods, and powdered beverages, where the PE layer is adhesive-laminated to biaxially oriented polypropylene or polyethylene terephthalate. Inline corona treatment raises surface wetting tension to 40–42 mN/m measured by ASTM D2578-17, but storage of treated rollstock at 23 °C and 50 % RH results in decay of 2–4 mN/m within 7 days and 4–6 mN/m within 14 days. If lamination is attempted below 38 mN/m, solventless polyurethane adhesive wetting fails and peel strength under ASTM D1876-08 falls below 2 N/15 mm; acceptable bond strength on these structures is generally 4–6 N/15 mm with cohesive failure in the PE sealant web. Converters extend shelf life by re-treating the web offline at 2.5–3.0 kW per 0.1 m width immediately before laminating; the re-treated surface must pass wetting tension testing with the mixed dyne solutions specified in ASTM D2578-17 across the full web width, because edge-to-center variation above 2 mN/m creates lamination tunnels. The sealant layer is also evaluated for heat-seal capability after lamination and curing; a 30 μm PE layer in a PET/PE lamination is sealed at 135 °C, 0.4 s, 0.3 MPa and tested after 24 h under ASTM F88/F88M-21, with acceptable seal strength of 5–9 N/15 mm depending on PET gauge and adhesive coverage.
In side-sealed polybag lines producing ultrathin 15 μm to 25 μm bags for e-commerce garment packaging and small-parts protection, DFDF-7047 NT7 is modified with oleamide or erucamide slip concentrates to reach kinetic coefficient of friction below 0.20 as laid in ISO 8295:1995. Film extrusion is run at BUR 2.8:1 to 3.2:1 and die gap 1.6 mm to 2.0 mm; lower die gaps raise shear rate and promote additive migration to the film surface, but they also increase melt pressure by 5–10 MPa on the same screw. Erucamide active content in the polybag formulation is normally 400–800 ppm; when high-speed bag machines require 1,200 ppm or more, the films must be checked for hot tack loss and seal strength reduction under ASTM F1921-12 and ASTM F88/F88M-21 because surface slip additives can transfer to the seal jaw and lower the effective seal temperature by 3–5 °C. Additive bloom is time-dependent; coefficient of friction is tested after 24 h, 48 h, and 7 days aging at 23 °C to distinguish fast-blooming oleamide from slower erucamide. Once the film is corona-treated for flexographic or digital printing, slip migration can be retarded, so the coefficient of friction may increase by 0.05–0.15 when measured 72 h after treatment; slip package and corona wattage are adjusted in tandem to keep hot tack, print adhesion, and film transport within the specified ranges.
For converters producing custom additive or color masterbatch in film lines, DFDF-7047 NT7 is let down at ratios from 20:1 to 50:1; mixing quality is dictated by screw design and back pressure rather than resin properties, and process parameter records should include melt temperature, pressure at the screen pack, and extruder amperage for batch traceability.
Competitive Dow Dow™ DFDF-7047 NT7 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DOW™ DFDF-7047 NT7 LLDPE is a film-grade linear low-density polyethylene supplied for blown film and coextrusion operations. The resin is manufactured as natural pellets without deliberately added slip, antiblock, or processing-aid packages, and its commercial use typically targets thin-gauge packaging where controlled optical and mechanical properties are required. At 23 °C and 50 % relative humidity, the base polymer exhibits a nominal density of 0.918 g/cm³ and a nominal melt index of 1.0 g/10 min at 190 °C under 2.16 kg load according to ASTM D1238. The grade is characterized by moderately low density and melt viscosity suitable for monolayer and multilayer blown-film lines. Published data for this specific configuration is limited to typical property tables; therefore, all lot-specific claims require review of the certificate of analysis.
Distributor and manufacturer literature describe DFDF-7047 NT7 as a butene-copolymer LLDPE with molecular architecture typical of Ziegler-Natta catalysis. Because the manufacturer does not always disclose the precise catalytic route in every regional datasheet, molecular-weight-distribution claims should be treated as structural inference rather than certified data. Melt flow ratio I10/I2 is not consistently published; users requiring shear-thinning characterization can request capillary rheometry data or run ASTM D1238 multi-load tests on the specific lot.
Typical specification-relevant properties appear in Table 1. Values are representative film data reported for 25 µm blown film at a blow-up ratio near 2.5:1; they are not maximum or minimum lot-release limits. Mechanical data generated on different line configurations can vary by 10–20 % due to die gap, frost line height, and gauge-control stability.
| Property | Test method | Unit | Typical value |
|---|---|---|---|
| Melt index | ASTM D1238 / ISO 1133 | g/10 min | 1.0 |
| Density | ASTM D792 / ISO 1183 | g/cm³ | 0.918 |
| Tensile strength at break, MD | ASTM D882 | MPa | 38 |
| Tensile strength at break, TD | ASTM D882 | MPa | 32 |
| Elongation at break, MD | ASTM D882 | % | 700 |
| Elongation at break, TD | ASTM D882 | % | 750 |
| Dart impact resistance, F50 | ASTM D1709A | g | 110 |
| Haze | ASTM D1003 | % | 6.0 |
| Gloss at 45° | ASTM D2457 | GU | 65 |
Elmendorf tear strength for this grade is often reported in distributor compilations in the 300–500 g range for 25 µm films, with transverse-direction values typically exceeding machine-direction values. Because tear measurements depend on gauge uniformity and specimen orientation, a single-field value without a defined film-fabrication protocol is not a valid comparator across resin families. Thermal transitions under differential scanning calorimetry are typical of low-density polyethylene: peak melting temperature generally lies between 120 °C and 125 °C when measured at 10 °C/min heating rate according to ASTM D3418. The Vicat softening point is not uniformly published; process engineers should obtain this value only for specific converting equipment where heat distortion is a limiting factor.
When this resin enters a grooved-feed blown-film extruder, melt temperature control is the critical operational boundary. Production-scale lines processing DFDF-7047 NT7 typically maintain a flat-to-rising barrel temperature profile of 150 °C, 170 °C, 180 °C, 190 °C, 205 °C, with die zones at 200–220 °C. Sustained melt temperatures below 180 °C produce visible gel particles and melt-fracture defects in 25 µm film, while residence times longer than 20 minutes above 240 °C generate oxidative degradation products that appear as specks. Extruder specifications for this grade on a typical 65 mm grooved-feed single-screw machine include L/D ratios of 24:1 to 30:1, barrier flights with a Maddock mixing element, and a screen pack of 40/60/100 mesh. The melt pressure upstream of the screen pack commonly increases by 15–30 % as the pack loads with gel contamination; replacement is scheduled when pressure exceeds 35 MPa or when melt temperature becomes unstable by more than ±2 °C.
Die selection for this LLDPE grade influences bubble stability. A spiral mandrel die with a die gap of 1.5–2.5 mm and a die land length of 10–15 times the gap provides sufficient backpressure for homogenization without excessive shear heating. Blow-up ratios from 2.0:1 to 3.0:1 are used; lower blow-up ratio values bias machine-direction orientation and reduce transverse tear, while higher values increase transverse orientation and may require higher melt strength. Frost line height is typically set at 1–2 die diameters above the die face. At frost line heights below this range, film blocking increases because the NT grade lacks an antiblock package; at frost line heights above 3 die diameters, film clarity and gloss decline due to surface crystallization. Regrind incorporation up to 30 wt% is common in industrial film production. Because the resin is supplied without added processing aid, converters running high-regrind formulations may add a fluoropolymer processing-aid masterbatch at 0.5–1.0 wt% to reduce die lip buildup and melt fracture.
Drying is not required at ambient relative humidity below 60 %; however, if granules are exposed to humid air for more than 24 hours, surface moisture may cause micro-bubbles at the die. A hopper dryer set to 70 °C for 2 hours restores surface dryness. Users should avoid oxidative purging; after processing, a low-temperature polyethylene purge is recommended before shutdown.
Blown film produced at 25 µm gauge exhibits the typical tensile and dart impact values listed in Table 1. The tensile elongation at break of 700 % MD indicates a strain-hardening response in the oriented film, but the resin’s tear anisotropy follows machine-direction orientation: transverse tear is consistently higher than machine-direction tear unless the blow-up ratio is increased. For side-gusseted sacks or heavy liners where transverse toughness is the failure criterion, converters commonly blend DFDF-7047 NT7 with LDPE at 20–40 wt% to balance orientation and improve bubble stability. Dart impact resistance of 110 g under ASTM D1709A is appropriate for light-to-medium produce bags and textile overwrap; applications requiring dart impact above 150 g generally require octene-based LLDPE or metallocene polyethylene.
Seal initiation temperature is not included in all public datasheets. On laboratory jaw sealers, seal strength can be measured according to ASTM F88, with a dwell time of 1 s and jaw pressure of 0.3 MPa. Because the seal window is a function of comonomer distribution and additive masterbatch, converters must generate sealing curves on the actual line; published data for this specific configuration is limited. In multi-layer structures, DFDF-7047 NT7 is placed in the core or outer layer at 20–60 wt% while a lower-melting mLLDPE, EVA, or ionomer sealant layer provides low-temperature seal initiation below 100 °C.
Slip and antiblock additives are not built into the NT designation. High-speed form-fill-seal applications typically require oleamide or erucamide masterbatches at addition rates of 0.5–2.0 wt% depending on film gauge, storage time, and equipment configuration. Without additive, coefficient of friction values are high and film blocking may occur on warm rolls; with slip masterbatch, equilibrium coefficient of friction is achieved after 24–48 hours of ambient storage.
The structural distinction between DFDF-7047 NT7 and higher-performance LLDPE grades lies in comonomer type and molecular architecture. Butene-based Ziegler-Natta LLDPE generally possesses a broader short-chain branching distribution than octene-based single-site LLDPE. As a result, the butene-copolymer film exhibits lower tie-molecule concentration, which reduces Elmendorf tear, puncture resistance, and slow-crack-growth resistance at equivalent density and melt index. The difference is most pronounced in thick-wall or frozen-food packaging where low-temperature brittleness is a concern. Compared with hexene-based LLDPE of similar melt index, DFDF-7047 NT7 is typically specified in less demanding packaging where the converter requires a wider extrusion window and lower resin cost per unit mass. In direct comparison, hexene and octene LLDPE grades yield higher dart impact at 25 µm and higher hot-tack strength under ASTM F1921.
Compared with LDPE homopolymer of similar density, DFDF-7047 NT7 provides higher elongation at break and improved environmental stress-crack resistance because of its linear backbone and controlled comonomer placement. LDPE retains an advantage in melt strength and bubble stability during high-blow-up-ratio extrusion; therefore, a 70:30 LLDPE:LDPE blend is common when die gaps below 1.5 mm cause unstable bubbles. The addition of LDPE also reduces film haze but may lower dart impact. In terms of converting energy, the higher melt elasticity of LDPE reduces melt fracture risk, whereas DFDF-7047 NT7 at low temperatures may require a wider die gap or higher die temperature to avoid surface defects.
This resin is not recommended for sterilization above 100 °C, for retortable pouches, or for contact with strongly oxidizing chemicals because the olefinic backbone undergoes thermal oxidation and the grade lacks a high-temperature stabilizer package. In such applications, polypropylene or high-density polyethylene sealant layers are used instead.
Statements of compliance must be obtained from the supplier for the specific lot. The base olefin polymer is typically evaluated under FDA 21 CFR 177.1520 for food-contact use, with end-use extraction limitations determined by section (c) tables. For the European Union, migration testing under Regulation (EU) No 10/2011 is required using the EN 1186 series; overall migration limits are 10 mg/dm² for plastic food-contact materials unless a specific simulant reduction applies. RoHS Directive 2011/65/EU restricts lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE at homogeneous-material thresholds; a typical certificate of compliance confirms that these substances are below 0.1 % by weight except cadmium at 0.01 %. REACH Regulation EC 1907/2006 requires communication of SVHC content above 0.1 % by weight; the resin is generally not formulated with SVHC substances.
| Regulation / standard | Designation / clause | Typical review item |
|---|---|---|
| FDA 21 CFR | 177.1520 | Olefin polymer extractive limits |
| EU Commission Regulation | 10/2011, Annex I | Overall migration limit 10 mg/dm² |
| REACH | EC 1907/2006 | SVHC content below 0.1 % |
| RoHS | 2011/65/EU | Homogeneous-material heavy-metal limits |
For phthalate-free declarations, ISO 14021 recycled-content claims, or clean-room packaging grades, separate supplier letters are required. A lack of such documentation for the NT grade does not imply that those attributes are absent; it indicates that the manufacturer has not qualified the product for that specific market under a public standard.