Dow Dow Dfdc 7087 Nt7 Lldpe

Dow Dow™ DFDC-7087 NT7 LLDPE

    • Product Name: Dow Dow™ DFDC-7087 NT7 LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 537885
    Productname Dow DFDC-7087 NT7 LLDPE
    Polymertype Linear Low Density Polyethylene
    Comonomer Octene
    Density 0.918 g/cm³
    Meltindex 0.80 g/10 min
    Meltflowratio 28
    Meltingpoint 123 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatyield 10.3 MPa
    Tensilestrengthatbreak 24.1 MPa
    Elongationatbreak 700%
    Flexuralmodulus 207 MPa
    Dartdropimpact 120 g
    Elmendorftearmd 250 g
    Elmendorfteartd 400 g
    Haze 12%
    Gloss45degree 65

    As an accredited Dow Dow™ DFDC-7087 NT7 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow™ DFDC-7087 NT7 LLDPE is supplied in 25 kg moisture-resistant polyethylene bags, stacked on 1,000 kg pallets for shipment.
    Container Loading (20′ FCL) 20′ FCL container loaded with Dow DFDC-7087 NT7 LLDPE in 25 kg bags, securely stacked and strapped for ocean transport.
    Shipping Dow™ DFDC-7087 NT7 LLDPE is typically shipped in 25-kg polyethylene bags, palletized and stretch-wrapped, or in bulk trucks/railcars. Keep dry, away from heat and UV. It is non-hazardous under normal conditions; handle according to SDS and local regulations. Ensure bags remain intact and protected from moisture during transport.
    Storage Store Dow™ DFDC-7087 NT7 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and ignition sources. Keep containers or bags closed, clean, and palletized to prevent moisture, dust, and contamination. Avoid excessive stacking and prolonged outdoor exposure. Maintain moderate ambient temperatures, use first-in, first-out stock rotation, and follow local regulations and supplier recommendations.
    Shelf Life Shelf life is 24 months from manufacture when stored in unopened original packaging under cool, dry conditions, away from sunlight.
    Application of Dow Dow™ DFDC-7087 NT7 LLDPE

    In blown-film conversion of Dow™ DFDC-7087 NT7 LLDPE into heavy-gauge industrial liner stock, the process conflict is concentrated in the temperature window between 195 °C and 230 °C at the adaptor, where the resin exhibits sufficient melt strength for a 2.0:1 to 3.0:1 blow-up ratio but becomes sensitive to frost-line fluctuations above 8 die diameters. The equipment specification is a monolayer or coextrusion blown-film line with a barrier screw, L/D ratio 25:1–30:1, screen-pack sequence 20/40/80 mesh, and die gap 2.0–2.8 mm; die land temperature is held within ±3 °C of set point to avoid bubble wander and gauge variation. Film gauge for construction sheeting is typically 80–150 μm; at 80 μm, the transverse-direction tear resistance measured by ASTM D1922 decreases when the frost-line is lowered below 5 die diameters because the quenched film retains anisotropic orientation. Terminal products include rubble sacks, pit liners, temporary containment enclosures, dust covers, one-trip bulk container liners, and demolition debris bags.

    Formulation addition ratios for this sector are dominated by carbon black masterbatch at 1.5–3.0 wt%, ultraviolet stabilizer masterbatch at 0.2–0.5 wt%, and polymer processing aid at 0.02–0.08 wt%. Post-industrial trim is reintroduced at 0–20 wt% after size reduction and screening through 80 mesh; above 30 wt% rework fraction, bubble stability narrows and surface melt fracture appears on wide die lips. A carbon black loading above 6 wt% is not recommended without pilot-scale evaluation because particle agglomerates above 20 μm increase melt filtration pressure and create pinholes in the liner. Compliance is anchored to REACH Regulation (EC) 1907/2006 Annex XVII for restricted heavy metals and polycyclic aromatic hydrocarbon contamination from black masterbatch; temporary site films referenced in EU tenders are additionally assessed under EN 13501-1 reaction-to-fire classification when specified. No pre-drying is required unless the resin is transferred from cold storage to a humid production hall with visible surface condensation; in that case, a hopper dryer at 65 °C for 2 h is applied.

    What die-lip deposits appear when PIB tackifier masterbatch exceeds 2.0 wt% in cast pallet-stretch film?

    Cast pallet-stretch film converting with DFDC-7087 NT7 as a core-layer dilution resin limits polyisobutylene tackifier masterbatch to 1.0–1.5 wt% in the cling layer. Beyond 2.0 wt%, low-molecular-weight PIB migrates to the die lip and chill roll, forming a tacky film that creates coating streaks, roll-wrap events, and inconsistent unwind force. The cast line is specified with a slot die gap of 0.5–0.8 mm, chill roll temperature 18–25 °C, air-knife pressure 0.2–0.4 MPa, and line speed 350–600 m/min. The core layer formulation adds DFDC-7087 NT7 at 20–35 wt% to a cast-grade octene LLDPE or metallocene LLDPE at 60–75 wt%; the skin layer uses the same DFDC-7087 NT7 blend with PIB masterbatch at 1.0–1.5 wt% and slip/antiblock masterbatch at 0.2–0.5 wt%. Cling force is measured under ASTM D5458 with a target of 0.6–1.5 N per 25 mm; puncture resistance is tested under ASTM D5748, and tensile properties under ASTM D882. For food-contact pallet wrap used with packaged goods, compliance follows FDA 21 CFR 177.1520 and EU Regulation 10/2011 Annex I. Terminal products include machine stretch wrap, manual hand wrap, bundling film, and surface-protection film. The main operational boundary is that PIB concentrations above 2.0 wt% require frequent die-lip cleaning and may be incompatible with in-line slitting at speeds above 500 m/min due to roll blocking.

    Converting routeAdditive systemTypical addition ratioControl standard
    Heavy-duty industrial linerCarbon black masterbatch / UV stabiliser / polymer processing aid1.5–3.0 wt% / 0.2–0.5 wt% / 0.02–0.08 wt%ASTM D1922
    Cast pallet stretchPIB tackifier masterbatch1.0–1.5 wt%ASTM D5458
    Agricultural cover filmHALS / UVA / slip-antiblock0.25–0.60 wt% / 0.15–0.40 wt% / 0.3–0.8 wt%ISO 4892-2
    Frozen food form-fill-sealSlip / antiblock0.5–1.5 wt% / 0.2–0.8 wt%ASTM F2029
    Stretch hoodLDPE blend modifier10–20 wt%ISO 527-3
    Extrusion lamination sealantLDPE / adhesion promoter10–30 wt% / 0–10 wt%ASTM D903

    Agricultural Silage Cover Film and HALS Stabilizer Loading Profiles

    Long-life agricultural film based on DFDC-7087 NT7 is processed on blown-film lines with a die gap of 2.0–2.8 mm, blow-up ratio 2.0:1–2.8:1, melt temperature 200–230 °C, and gauge 50–150 μm. The weathering package is added as a hindered amine light stabilizer masterbatch at 0.25–0.60 wt% and a UV absorber masterbatch at 0.15–0.40 wt%; the slip/antiblock masterbatch is dosed at 0.3–0.8 wt% to maintain winding without excessive surface bloom. Below 0.10 wt% UV absorber, silage cover films exposed to direct sunlight for more than 12 months exhibit premature edge cracking; above 0.8 wt% HALS, the surface oxidation level after corona treatment may be insufficient for water-based ink adhesion. The bubble is collapsed below 45 °C to avoid blocking on idler rolls. Compliance for agricultural use is verified under REACH Regulation (EC) 1907/2006 for stabiliser substances, and where the film is used as a silage cover under EN 13206 covering films for ensiled crops; tensile properties are measured under ISO 527-3, and weathering retention under ISO 4892-2 accelerated ageing. Terminal products include silage cover sheets, greenhouse side curtains, tunnel film, horticultural ground covers, and protective over-wintering film.

    Sub-zero form-fill-seal packaging lines running DFDC-7087 NT7 into frozen poultry and seafood pouches impose a narrow seal plateau because the resin, when combined with high slip loadings, shifts hot-tack strength after surface frost temperatures drop below −25 °C. The film is produced at 25–60 μm on blown-film equipment with a die gap 1.8–2.5 mm, blow-up ratio 2.0:1–2.5:1, and melt temperature 190–220 °C. Slip masterbatch is added at 0.5–1.5 wt%, antiblock masterbatch at 0.2–0.8 wt%, and polymer processing aid at 0.03–0.06 wt%; excess slip above 2.0 wt% reduces seal initiation temperature and increases solvent extractables, which conflicts with EU Regulation 10/2011 overall migration limits below 10 mg/dm². On vertical form-fill-seal jaws, sealing temperature is set to 115–145 °C, dwell 0.3–0.8 s, and pressure 0.4–0.8 MPa; below 110 °C, hot-tack failure occurs on high-speed machines, while above 150 °C, seal shrinkage and stringing produce leaker spoilage. Compliance follows FDA 21 CFR 177.1520 for olefin polymers and EU Regulation 10/2011 Annex I with migration testing under EN 1186-1. Terminal products include frozen fish portions, poultry bags, ice cube pouches, and frozen vegetable packs.

    When stretch-hood film runs below 0.920 g/cm³ density, elastic recovery and dart impact move in opposite directions

    Stretch-hood converting of DFDC-7087 NT7 below 0.920 g/cm³ density exposes a trade-off between elastic recovery and dart impact strength. On a high-stalk blown-film line with die gap 1.8–2.5 mm, blow-up ratio 2.5:1–3.5:1, and melt temperature 200–225 °C, the resin is blended with LDPE at 10–20 wt% to improve bubble stability and reduce cross-direction shrinkage; LDPE fractions above 25 wt% reduce puncture resistance and lower the elastic recovery ratio measured by ISO 527-3. For hooding film of 60–100 μm, the web is surface-treated to 38–42 mN/m and slit to lay-flat widths from 600 mm to 2,000 mm. The formulation includes slip/antiblock masterbatch at 0.3–0.9 wt% and process aid at 0.02–0.05 wt%; no tackifier is added because containment relies on film retraction rather than cling. The absence of PIB eliminates die-lip plate-out but limits reuse of post-consumer hood film contaminated with high-cling stretch wrap. Compliance for logistics packaging is verified under REACH Regulation (EC) 1907/2006 and EU Packaging Directive 94/62/EC heavy metal concentration limits. Terminal products include appliance pallet hoods, building material wraps, and automated pallet containment for glass and ceramic loads. Published data specific to DFDC-7087 NT7 in stretch-hood configurations is limited; the processing limits are derived from general linear low-density polyethylene behaviour and should be confirmed on the target high-stalk line.

    Sealant Web Extrusion Lamination Requires Pre-Extrusion Drying of Coextruded Surfaces

    Extrusion lamination with DFDC-7087 NT7 as a sealant web on BOPP, PET or metallized substrates uses a tandem lamination line with a 90–120 mm slot-die extruder, L/D 28:1–30:1, melt temperature 280–320 °C, and an air gap 100–180 mm to promote oxidative adhesion before the cooling nip. The resin is blended with LDPE at 10–30 wt% to reduce neck-in and with polyolefin adhesion promoter at 0–10 wt% when sealing to aluminium foil or metallized PET; the coating thickness is controlled at 15–30 μm. Pre-extrusion drying is required only when stored reels or resin pellets show visible surface condensation after cold warehouse transfer; a hopper dryer at 65–70 °C for 2 h is used before processing when the production hall relative humidity exceeds 60%. The main incompatibility is excessive corona treatment of the substrate above 50 mN/m, which can create pin-hole defects when the hot melt contacts the oxidised surface. Food-contact compliance is verified under FDA 21 CFR 177.1520 and EU Regulation 10/2011 Annex I; total migration testing follows EN 1186-1. Terminal products include flexible food pouches, sachet stock, lidding components, and tube laminate sealant webs.

    Free Quote

    Competitive Dow Dow™ DFDC-7087 NT7 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow Dow™ DFDC-7087 NT7 LLDPE is a linear low density polyethylene resin produced by a solution polymerization route, yielding a narrow molecular weight distribution and controlled incorporation of a higher alpha-olefin comonomer. The grade is supplied as natural pellets for cast film, extrusion coating, and lamination webs. Manufacturer-published typical values include a polymer density of 0.918 g/cm³ determined under ASTM D792 and a melt mass-flow rate of 1.0 g/10 min at 190°C/2.16 kg using ISO 1133-1:2022. These values place DFDC-7087 NT7 in the conventional LLDPE cast-film segment rather than in the plastomer or ultra-low-density class. Compared with a butene-based LLDPE of equivalent density and melt flow rate, the higher alpha-olefin comonomer is associated with improved tear propagation resistance and elevated dart impact in thin films. The resin is not a direct substitute for high-clarity metallocene grades when haze below 5% on a 25 µm film is required; its optical package is competitive for general packaging but is not a low-haze optical grade.

    Extrusion feed systems for DFDC-7087 NT7 tolerate hopper throat temperatures of 30–50°C. Pre-drying is not mandatory when sealed containers are stored in ambient relative humidity below 60%. At higher humidity, surface-adsorbed moisture can produce pinholes and melt-pressure fluctuation; a desiccant-bed or dehumidified-air hopper dryer set to 60–70°C for 2–4 h is used before processing. Extended melt residence time above 280°C promotes oxidized gel formation, die-lip buildup, and loss of optical quality. Strong oxidizing additives, high-acid-number concentrates, and transition-metal salt masterbatches require validation because they may catalyze chain scission under cast-film conditions. Batch-to-batch pellet surface lubricant variation is a known source of feed-throat bridging on single-screw extruders; hopper vibrators or feed augers with controlled torque reduce irregular feed.

    Why Is Chill-Roll Temperature Tighter for DFDC-7087 NT7 Than for Butene-Based Cast Film Grades?

    On production cast film lines equipped with 30:1–35:1 L/D single-screw extruders and slot dies of 250–350 mm, the adapter and die melt temperature for DFDC-7087 NT7 typically falls between 230°C and 260°C. Die gap is maintained at 0.5–0.8 mm. The quench drum surface temperature is held in the 15–30°C range because cooling rate influences the growth of crystalline domains and the resulting haze, scratch resistance, and curl. A lower quench temperature increases film orientation and can improve puncture energy absorption, but it may also produce higher curl in asymmetric extrusion-lamination structures. Shoulder-length neck-in and edge-bead formation are controlled by air-knife positioning and vacuum box pressure; edge trim is commonly set at 8–12% of web width. In comparative production observations, butene-based grades of similar melt index often show lower melt strength and may allow lower chill-roll temperature without curl, while DFDC-7087 NT7 requires tighter air-knife positioning to prevent pinholes at high line speed. Melt-pressure fluctuation of ±3–5% can be observed when pellet lot changes alter external lubricant; this is a processing boundary, not a film-property failure, and is addressed by lip cleaning at intervals determined by die deposit severity.

    Tensile property evaluation of cast film at 25 µm thickness follows ISO 527-3 or ASTM D882. Machine-direction elongation at break is generally greater than 400% for films free of melt defects, while transverse-direction tensile strength depends on quench orientation and edge-bead distance. Elmendorf tear values obtained under ASTM D1922 are directionally anisotropic: transverse-direction tear resistance is typically higher than machine-direction tear resistance because of preferential molecular orientation along the machine direction. Dart impact values determined under ASTM D1709 are dependent on film thickness, method A or B, and quench rate. In comparative tests with butene LLDPE of density 0.918 g/cm³, the higher alpha-olefin comonomer of DFDC-7087 NT7 generally shifts the tear–dart balance toward improved puncture and tear without changing density. Puncture resistance measured by a slow-puncture fixture or ASTM D5748 is enhanced by rapid quench and by increased tie-chain probability associated with higher alpha-olefin incorporation. Published data for this specific configuration at high line speeds above 300 m/min is limited; interlaboratory repeatability for tear values should be considered when setting specifications.

    Tear Propagation, Dart Impact, and Puncture Resistance in Higher Alpha-Olefin Cast Film Structures

    In cast stretch film, hygiene backsheet, and extrusion lamination structures, the selection of DFDC-7087 NT7 rests on its combination of melt index and comonomer type. The solution-process molecular architecture reduces low-molecular-weight extractables that can initiate tear propagation under stretch. In contrast with butene-based LLDPE of the same density and melt flow rate, the resin generally exhibits higher machine-direction tear resistance, deeper puncture resistance, and improved dart impact. However, optical haze may be slightly higher than in a metallocene LLDPE or plastomer with a density below 0.905 g/cm³. For turret stretch wrappers operating at prestretch ratios above 250%, downstream converters may blend DFDC-7087 NT7 with an EVA or metallocene grade to reduce film blocking and improve load retention. In extrusion lamination, adhesion to substrates such as biaxially oriented polypropylene and polyethylene terephthalate depends on the oxidized melt curtain temperature and on the presence of a tie layer; this grade provides a processable low-density sealant layer but is not an adhesive resin. No organoleptic or odor-controlling additive package is assumed unless specified on the certificate of analysis.

    The resin is positioned for use in food-contact layers only when the finished film, lamination, or coating complies with the applicable food-contact legislation. Under U.S. federal regulations, polyethylene may be eligible as an olefin polymer subject to FDA 21 CFR 177.1520(c); end-use extraction tests and condition-of-use limitations are the converter’s responsibility. In the European Union, plastic food-contact materials are evaluated under EU 10/2011, with verification of overall migration by EN 1186-1 using food simulants selected according to the intended use. For industrial packaging, electrical and electronic equipment packaging is assessed under RoHS Directive 2011/65/EU; concentrations of restricted substances are controlled by the raw-material supplier. REACH compliance requires confirmation that substances of very high concern do not exceed 0.1% w/w per Article 33 of EC 1907/2006. Each regulatory claim must be confirmed against the current certificate of analysis and supplier regulatory letter; no blanket compliance conclusion is made.

    Regulatory RequirementApplicable Standard or RegulationKey Numeric Limit or TestVerification Boundary
    U.S. food-contact polyolefinFDA 21 CFR 177.1520(c)End-use extraction per conditions of useConverter responsibility with supplier letter
    EU plastic food-contactEU 10/2011; EN 1186-1Overall migration 10 mg/dm² for general conditionsFood simulant selection required
    RoHS packaging2011/65/EUPb 0.1% w/w; Cd 0.01% w/w; Hg 0.1% w/w; Cr(VI) 0.1% w/w; PBB/PBDE 0.1% w/wSupplier confirmation for scope
    REACH SVHC communicationEC 1907/2006 Article 33SVHC above 0.1% w/w triggers communicationSupplier confirmation required

    This grade is not recommended for injection molding, blow molding, or rotational molding; its melt index and molecular architecture are intended for film and coating processes. It is not a sealant for high-retort structures; autoclave conditions above 121°C can reduce seal strength and alter additive migration. Incompatible processing combinations include extended contact with amine-based slip concentrates that may generate color bodies under acid catalyst residues, and excessive levels of recycled materials with high ink or adhesive carryover that can raise gel counts. Published data for this specific resin in high-retort or high-pressure applications is limited. The technical assessment ends at the process boundary described.