| HS Code | 580823 |
| Polymertype | Linear Low Density Polyethylene |
| Comonomer | Octene-1 |
| Density | 0.918 g/cm³ |
| Meltindex | 0.8 g/10 min |
| Meltingpoint | 122 °C |
| Vicatsofteningpoint | 100 °C |
| Tensilestrengthatyield | 10.3 MPa |
| Tensilestrengthatbreak | 22.1 MPa |
| Elongationatbreak | 800% |
| Flexuralmodulus | 240 MPa |
| Dartdropimpact | 200 g |
| Elmendorftearstrengthmd | 350 g |
| Elmendorftearstrengthtd | 450 g |
| Haze | 10% |
| Gloss45 | 60 |
As an accredited Dow Dow™ DFDC-7047 NT7 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow™ DFDC-7047 NT7 LLDPE is supplied in 25 kg polyethylene bags, typically palletized for industrial bulk handling. |
| Container Loading (20′ FCL) | 20′ FCL Dow DFDC-7047 NT7 LLDPE: palletized 25 kg bags, shrink-wrapped, secured, loaded to container weight limit for ocean transport. |
| Shipping | Dow™ DFDC-7047 NT7 LLDPE is a non-hazardous linear low-density polyethylene resin. It ships as pellets in bags, supersacks, or bulk containers via dry van, railcar, or intermodal container. Not regulated for DOT/IMDG/IATA transport; no special labels required. Keep packaging closed and protect from moisture, heat, and contamination. |
| Storage | Store Dow™ DFDC-7047 NT7 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizing agents. Keep containers or bags closed, clean, and palletized to prevent moisture and contamination. Avoid prolonged UV exposure and extreme temperatures. Follow local regulations and the manufacturer’s safety data sheet for safe handling and storage. |
| Shelf Life | Shelf life is typically 24 months from manufacture when stored in original unopened packaging under cool, dry conditions, away from direct sunlight. |
On blown film lines running Dow DFDC-7047 NT7 for frozen food packaging, the melt temperature at the die is typically held between 200°C and 215°C, the blow-up ratio is maintained between 2.2 and 2.8, and the die gap is set at 1.6 mm to 2.0 mm on a 90 mm grooved-feed extruder with an L/D 30:1 barrier screw. The resin’s incoming melt index of 1.0 g/10 min under ASTM D1238 (190°C/2.16 kg) and nominal density of 0.918 g/cm³ under ASTM D792 function as lot-release gates; density drift outside ±0.003 g/cm³ or melt index drift outside ±0.2 g/10 min is treated as a batch-transfer prompt before dry blending. The film layer is typically a blend of 80 to 85 wt% DFDC-7047 NT7, 10 to 15 wt% LDPE, and 2 to 4 wt% of a slip/antiblock concentrate containing active erucamide at 500 to 1,000 ppm and synthetic silica at 2,000 to 5,000 ppm in the final web. Bubble cooling is provided through a dual-lip air ring with internal bubble cooling, and the frost line height is kept at 8 to 12 die diameters; deviations above this band produce gauge bands and reduce machine-direction tensile uniformity. At film thicknesses of 0.08 mm to 0.12 mm, heat-seal performance is tested with ASTM F88 after jaw dwell times of 0.5 to 1.0 s at 110°C to 130°C. Direct-contact compliance is governed by FDA 21 CFR 177.1520 for olefin polymer food-contact surfaces and by EU Regulation 10/2011, where overall migration must not exceed 10 mg/dm² under the assigned food simulant. Additive masterbatches are reviewed separately under national food-contact provisions; the base resin alone does not confer automatic approval of the finished structure. Terminal products include IQF vegetable pillow packs, frozen seafood bags, bakery wrap, and non-barrier sachets in which water-vapour transmission is managed by gauge rather than by barrier coating.
| Regulation or standard | Scope | Limit or method |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymer food-contact surfaces | Base resin clearance; additives reviewed under 21 CFR 176.170 where applicable |
| EU Regulation 10/2011 | Plastic materials and articles intended for food contact | Overall migration 10 mg/dm²; simulant assignment per Annex III |
| EU Directive 94/62/EC | Packaging and packaging waste | Sum of Pb, Cd, Hg, Cr(VI) 100 ppm |
| REACH 1907/2006 | SVHC screening and communication | Article 33 duty if SVHC > 0.1 wt% |
Heavy-duty sack formulations based on DFDC-7047 NT7 shift from the classic LDPE-rich composition to a ternary blend of 70 wt% DFDC-7047 NT7, 20 wt% HDPE, and 10 wt% clean post-industrial regrind. The HDPE fraction raises secant modulus and improves creep resistance, but at concentrations above 20 wt% the transverse-direction tear strength and low-temperature dart impact become line-specific and may no longer meet sack drop requirements under ISO 7965-2 or equivalent. Extrusion is carried out on a 120 mm grooved-feed extruder with an L/D 30:1 to 35:1 screw, a die gap of 2.0 mm to 2.5 mm, a blow-up ratio between 2.0 and 2.5, and a die temperature of 215°C to 235°C. Melt-pressure excursions above 350 bar at maximum screw speed are a practical ceiling; a filter-pack differential above 60 bar from carbon black or white pigment masterbatch carryover is a standard screen-change trigger. Dart impact is evaluated under ASTM D1709A and Elmendorf tear under ASTM D1922; the transition from LDPE to LLDPE/HDPE in 100 µm film frequently produces an MD-biased tear pattern that must be checked against sack closure mouth-tear requirements. Compliance for non-food industrial sacks is framed by EU Directive 94/62/EC, which caps the sum of lead, cadmium, mercury, and hexavalent chromium at 100 ppm by weight, and by REACH Regulation 1907/2006 SVHC communication duties at 0.1 wt% in the article. Terminal goods include free-standing fertilizer sacks, polymer resin bags, construction rubble sacks, and woven-sack inner liners. Published data for the exact 70/20/10 regrind blend at 100 µm thickness is limited; converters therefore maintain internal process capability studies using ASTM D1709A and ASTM D1922 before commercial lot acceptance.
In agricultural silage covers and greenhouse films, DFDC-7047 NT7 is dry-blended with 18 to 22 wt% EVA containing 14 to 18 wt% vinyl acetate, plus 0.3 to 0.6 wt% of a HALS/antioxidant combination and 0.2 to 0.4 wt% of an anti-drip concentrate. The EVA component lowers the processing melt temperature and improves flex-crack resistance, but it also narrows the thermal window: melt temperatures above 220°C risk vinyl-acetate decomposition and acetic acid release, which can corrode die lip surfaces and generate odour. Processing on a 140 mm extruder with an L/D 30:1 screw, a die gap of 2.0 mm, a blow-up ratio of 2.5 to 3.0, and an oscillating haul-off is standard; the melt temperature at the die is maintained between 190°C and 210°C. The final film gauge for silage covers is commonly 100 µm to 180 µm, while greenhouse films cluster between 150 µm and 250 µm. Weathering resistance is screened by accelerated aging under ISO 4892-2, but the correlation to outdoor life remains site-specific and must be validated against annual UV dose. Since the film is not designed for food contact, the relevant regulatory basis is REACH Regulation 1907/2006 and EU Directive 2008/98/EC; the material does not claim conformity with EN 13432 industrial composting and is allocated to mechanical recycling or energy recovery at disposal. Terminal products include greenhouse cladding, low tunnels, silage covers, and temporary fumigation panels.
When DFDC-7047 NT7 is redirected into a cast sealant web for lamination, the process differs from blown film in that bubble instability is absent but draw resonance and neck-in become the controlling defects. The resin is extruded through a 75 mm barrier screw with an L/D 30:1 and a flat die gap of 0.5 mm, with melt temperature at the die held between 240°C and 260°C. Line speeds of 80 to 120 m/min are common; once haul-off exceeds 120 m/min, the chill roll temperature between 18°C and 25°C becomes the primary variable for seal initiation and film flatness. Higher chill roll temperatures reduce crystallinity at the sealant surface and can improve hot tack, but they also increase blocking tendency when the wound roll is stored above 30°C. Erucamide migration from the bulk to the film surface proceeds over storage time and reduces coefficient of friction; excessive migration into a lamination interface can lower adhesive bond strength. The sealant web is validated by ASTM F88 seal strength and ASTM F1921 hot tack, with the adhesive layer reviewed separately under FDA 21 CFR 175.105 where applicable. Direct food-contact sealant layers are assessed against FDA 21 CFR 177.1520 and EU Regulation 10/2011, with overall migration limited to 10 mg/dm². Terminal products include printed lamination webs for liquid sachets, personal-care wipe packages, and pouch inner sealants where the primary barrier is supplied by a metallized or aluminium foil layer.
When a refuse sack converter downgauges from 50 µm to 35 µm using DFDC-7047 NT7, the formulation shifts to a five-component dry blend of 65 wt% DFDC-7047 NT7, 15 wt% LDPE, 15 wt% clean in-house regrind, and 5 wt% carbon black masterbatch. The regrind fraction reduces cost but increases gel-count variability; converters usually limit regrind inclusion to 15 wt% when the film must pass a visual defect threshold in star-seal operations. Extrusion is run on a 100 mm smooth-bore extruder with an L/D 30:1 screw, a die gap of 1.4 mm, a blow-up ratio between 3.0 and 3.5, and a melt temperature of 180°C to 200°C. High blow-up ratios improve tear resistance in the transverse direction, but above 3.5 the bubble can oscillate on lines without internal bubble cooling, producing gauge variation and folded-edge rupture. Tear is measured under ASTM D1922, dart impact under ASTM D1709A, and puncture under ISO 7765-1; downgauged sacks are also subjected to fill-drop tests according to line-specific specifications based on ISO 7965-2. Regulatory compliance is limited to packaging waste limits under EU Directive 94/62/EC, with the sum of lead, cadmium, mercury, and hexavalent chromium held below 100 ppm; food-contact testing is not required for the intended refuse and utility-sack service. Terminal goods include municipal refuse sacks, janitorial liners, and industrial utility bags.
Sealant layers for stand-up pouches are produced from a 70 wt% DFDC-7047 NT7 and 30 wt% LDPE blown film, typically at 40 µm to 60 µm thickness, to widen the heat-seal window and reduce seal initiation temperature relative to a 100% LLDPE sealant. The film is run at a melt temperature of 195°C to 210°C with a die gap of 1.6 mm, a blow-up ratio of 2.2 to 2.6, and a frost line height of 8 to 10 die diameters. Hot tack is measured under ASTM F1921 and seal strength under ASTM F88 across the packaging machine seal-bar temperature range of 110°C to 150°C; the target is a seal plateau that tolerates dwell-time variation from 0.3 to 0.8 s without thermal pinholing. The sealant web is laminated into a typical 12 µm PET / 7 µm aluminium / 60 µm PE structure, where the sealant side is compounded from the 70/30 blend and the foil layer provides oxygen and moisture barrier. Compliance is evaluated under FDA 21 CFR 177.1520 for the olefin sealant, EU Regulation 10/2011 for overall migration below 10 mg/dm², and CONEG heavy-metal screening for packaging components with a combined Pb/Cd/Hg/Cr(VI) limit of 100 ppm. Terminal products include dry-food side-gusset pouches, high-barrier liquid-packaging alternatives, and stand-up pouch structures where seal integrity and drop resistance are critical.
Competitive Dow Dow™ DFDC-7047 NT7 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow™ DFDC-7047 NT7 is a linear low-density polyethylene resin produced with a Ziegler-Natta catalyst and a butene comonomer. The product is supplied as natural pellets without slip or antiblock additives; film-to-film coefficient of friction must therefore be controlled through converter-added masterbatch and measured by ASTM D1894. The resin has a nominal melt index of 1.0 g/10 min determined at 190 °C under a 2.16 kg load in accordance with ASTM D1238 or ISO 1133-1:2022, and a nominal density of 0.918 g/cm³ determined in accordance with ASTM D1505 or ISO 1183-1:2019. The NT7 designation identifies the stabilization package; it does not denote a slip/antiblock surface chemistry. The grade is intended for monolayer and coextruded blown-film extrusion on single-screw lines with barrel L/D ratios from 24:1 to 30:1. Because the resin has less long-chain branching than a high-pressure LDPE, it exhibits lower extensional strain hardening, and bubble stability in high-stalk operation depends on air ring and internal bubble cooling hardware. The density and melt index place the product in the general-purpose film segment where converters evaluate toughness by ASTM D1709-16a, tear by ASTM D1922, and optics by ASTM D1003 on their own production film rather than on pellet data alone.
The principal differentiation is the combination of a butene copolymer, nominal 0.918 g/cm³ density, and 1.0 g/10 min melt index. Relative to a C8-copolymer LLDPE of equivalent density and melt index, the butene structure generally provides a lower tie-molecule concentration in rapidly quenched blown film. The practical consequence is that dart impact measured by ASTM D1709-16a and Elmendorf tear measured by ASTM D1922 can be lower at equivalent gauge, especially in the transverse direction. Converters that down-gauge film below 20 µm and require high puncture resistance often select a hexene or octene copolymer when the critical specification is dart impact. Relative to a fractional-melt LLDPE with 0.5 g/10 min melt index, DFDC-7047 NT7 reduces extruder energy demand but increases bubble sag; relative to a 2.0 g/10 min grade, it improves bubble stability on air-ring-only lines but may raise die pressure and melt temperature. Compared with a metallocene-catalyzed LLDPE of similar density, the Ziegler-Natta product usually shows broader molecular weight distribution, lower hot-tack performance by ASTM F1921, and higher haze by ASTM D1003 under identical film-fabrication conditions. Against high-pressure LDPE, the LLDPE has lower melt strength and may require a wider die gap to control sharkskin melt fracture. Selection among these products depends on whether the converting line uses internal bubble cooling, external bubble stabilization, or a pocket bubble configuration.
Because the grade specification is defined by melt index and density, a certificate of analysis reports those values rather than film optical or mechanical data. Converter film data must be generated under fixed fabrication conditions. A standardized laboratory comparison commonly uses a 40 mm single-screw blown-film extruder with a 2.3 mm die gap and 2.5:1 blow-up ratio to produce 25 µm film. Dart drop impact is measured under ASTM D1709-16a; Elmendorf tear is measured under ASTM D1922; tensile yield and ultimate values are measured under ASTM D882-18; haze is measured under ASTM D1003; and gloss is measured under ASTM D2457. For a 0.918 g/cm³ butene LLDPE with a 1.0 g/10 min melt index, film data commonly fall in the ranges of 80 g to 130 g for dart impact, 200 g to 350 g for MD tear, and 300 g to 450 g for TD tear. These ranges are not product specifications and are influenced by frost line height, melt temperature, die pressure, and winding condensation. The DSC peak melting temperature for this density class is typically 121 °C to 124 °C by ASTM D3418; the Vicat softening temperature is typically near 100 °C by ASTM D1525. Oxidative induction time measured at 210 °C by ASTM D3895 is stabilizer-dependent and should be checked after long storage.
Neat LLDPE pellets are not hygroscopic; moisture absorption is generally below 0.01% w/w at 23 °C and 50% RH. The dominant moisture source is surface condensation during transfer from outdoor silos to a warmer indoor hopper, especially at ambient relative humidity above 60%. If surface moisture remains on the pellets, processors may observe die-pressure variation, bubble instability, microvoids, and higher gel counts. A desiccant hopper dryer operating at 60 °C to 70 °C for 2 h to 4 h with a dew point below -20 °C is sufficient for surface drying. Pellets should not be held above 80 °C for more than 6 h, because antioxidant consumption and hopper-bridging can occur. Coextrusion with EVOH or polyamide requires a tie resin; direct melt contact without an adhesive layer does not provide adequate interfacial adhesion. Masterbatches containing high loadings of transition-metal salts or free-radical generators should be evaluated for oxidative degradation of the polyethylene matrix before production use. Clean edge trim can be reintroduced at levels up to 30% w/w without additional drying if the trim is free of print and moisture; higher recyclate fractions may reduce dart impact measured by ASTM D1709-16a and increase gel-related film defects.
On production-scale blown-film lines equipped with barrier screws of L/D 24:1 to 30:1 and grooved feed sections, the resin is processed with barrel set points from 180 °C to 220 °C and die-zone set points from 190 °C to 230 °C. Melt temperature at the die lip should be held below 240 °C to limit gel formation and additive loss. For a 250 mm die with a 2.3 mm die gap, die pressure commonly ranges from 250 bar to 400 bar depending on output and screen-pack condition. Because LLDPE is less shear-thinning than LDPE, motor load and die pressure at the same melt index are higher; this is a routine failure mode when an LDPE-purge screw is used without increasing torque capacity. Sharkskin melt fracture is corrected by increasing die gap from 1.0 mm to 1.8 mm or by raising die temperature. For 25 µm film, the bubble is typically run at a blow-up ratio of 2.0:1 to 3.0:1 with the frost line 300 mm to 700 mm above the die face. A low frost line reduces haze but increases blocking risk unless the air ring supplies sufficient cooling-air velocity. High-stalk operation can be used when internal bubble cooling and an external bubble stabilizer are present; without those devices, pocket operation near 2.0:1 BUR generally improves stability. Corona treatment for printing or lamination should be applied before the collapsing frame; surface tension levels of 38 mN/m to 42 mN/m are measured by ASTM D2578, and excessive treatment can reduce heat-seal strength.
In three-layer coextrusion, DFDC-7047 NT7 may be used as a skin or core layer. When it is placed between HDPE skins, the HDPE contributes stiffness while the LLDPE core improves tear propagation resistance. Direct LLDPE/EVOH contact without tie resin is not viable; the adhesive layer must have functionalized polyolefin chemistry. Post-industrial trim handling requires screening and melt filtration. A screen pack of 20/60/100 mesh is standard for removal of paper and gelled material. Fines from hopper loaders should be minimized because fines melt unevenly and can create gel-like optical defects. Long-term storage beyond 12 months may reduce antioxidant effectiveness; before use, oxidative induction time by ASTM D3895 and yellowness index by ASTM E313 should be checked. Blending with polypropylene or PET residues is not recommended because incompatible melt phases generate unmelted inclusions and can cause film splits at the winder.
Food-contact status cannot be established from the pellet alone; it depends on the finished film structure, layer distribution, food type, contact time, and temperature. The base olefin polymer may be covered by 21 CFR 177.1520(c)3.2a when the finished article satisfies the applicable extractive and end-use restrictions. For European Union applications, Regulation (EU) No 10/2011 requires final-article migration testing; the overall migration limit is 10 mg/dm² for food-contact plastics or 60 mg/kg for infant food under the prescribed test conditions. The following table lists relevant compliance frameworks that converters commonly evaluate.
| Framework | Designation or Clause | Condition | Limit or Requirement |
|---|---|---|---|
| United States FDA | 21 CFR 177.1520(c)3.2a | Polyolefin base resin; final article extraction | End-use conditions apply |
| European Union food contact | Regulation (EU) No 10/2011 | Overall migration and specific migration | OML 10 mg/dm²; infant food 60 mg/kg |
| REACH | Regulation (EC) No 1907/2006, Article 33 | Candidate-list SVHC notification | Threshold 0.1% w/w |
| RoHS | Directive 2011/65/EU | Homogeneous-material heavy-metal limits | Lead 0.1% w/w; cadmium 0.01% w/w |
Specific migration of antioxidants and neutralizers in the resin should be tested under the intended food simulant, such as 10% ethanol for aqueous foods, 3% acetic acid for acidic foods, 20% ethanol for low-alcohol products, or 95% ethanol and isooctane for fatty foods. These simulants are defined in Regulation (EU) No 10/2011; they are not interchangeable with simple water extraction. The base resin does not contain intentionally added heavy metals, but downstream masterbatch, printing ink, and coating components must be reviewed separately.
In 25 µm monolayer form, DFDC-7047 NT7 is used in general-purpose bags, liners, and over-wrap structures where moderate toughness and controlled haze are required. Puncture and slow-rate penetration should be evaluated by ASTM D5748 for packaged contents with sharp or abrasive geometry; heavy-duty sacks may require a C8-copolymer LLDPE layer or an HDPE stiffening layer. Seal initiation temperature and hot-tack should be measured on the final film using ASTM F88-21 and ASTM F1921; the butene comonomer may require seal bar temperatures approximately 10 °C to 15 °C higher than a metallocene LLDPE of equivalent density. Water-vapor transmission rate is measured by ASTM F1249-20 and oxygen transmission rate by ASTM D3985-17; these values depend on thickness, orientation, and layer structure. Coextruded structures with EVOH require tie layers; coextruded structures with HDPE skins can be used to increase stiffness while the LLDPE layer contributes tear resistance. For printed or laminated film, corona-treated surfaces should be processed within 24 h because surface tension decay occurs after oxidation. Published data for this exact grade in high-barrier coextruded structures is limited; performance validation should be generated on production equipment rather than inferred solely from density and melt index.