Dow Dow Dfda 7074 Nt7 Lldpe

Dow Dow™ DFDA-7074 NT7 LLDPE

    • Product Name: Dow Dow™ DFDA-7074 NT7 LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 110724
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 0.80 g/10 min
    Melt Flow Ratio I21 I2 27
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 20.7 MPa
    Elongation At Break 700%
    Flexural Modulus 241 MPa
    Vicat Softening Point 93°C
    Melting Point 122°C
    Dart Drop Impact 120 g
    Elmendorf Tear Strength 88.3 kN/m
    Haze 10%
    Gloss 60%

    As an accredited Dow Dow™ DFDA-7074 NT7 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow™ DFDA-7074 NT7 LLDPE is packaged in 25 kg polyethylene-lined paper bags, supplied on pallets, or 1,000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL container loading: Dow™ DFDA-7074 NT7 LLDPE, 25 kg bags, 55 bags/pallet, 18 pallets, total 24.75 MT.
    Shipping Dow™ DFDA-7074 NT7 LLDPE is typically shipped as non-hazardous resin pellets in 25 kg polyethylene bags, 500–1000 kg bulk bags, or bulk trucks/railcars. Pallets are stretch-wrapped and labeled. Keep dry, avoid excessive heat, and follow the SDS and local transport regulations.
    Storage Store Dow™ DFDA-7074 NT7 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep in original sealed packaging or suitable containers to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and temperatures above recommended limits. Maintain clean floors to prevent slipping from spilled pellets. Follow local regulations and SDS guidance.
    Shelf Life Typical shelf life: 24 months if stored unopened in original packaging, cool, dry, away from direct sunlight and moisture.
    Application of Dow Dow™ DFDA-7074 NT7 LLDPE

    Film Toughness Retention Across Frozen Storage Conditions

    Across spiral mandrel blown film lines processing DFDA-7074 NT7 at die diameters from 150 mm to 350 mm, the resin enters the screw as a pellet with density 0.919 g/cm³ determined under ASTM D1505 and melt flow rate 1.0 g/10 min under ASTM D1238 at 190 °C/2.16 kg. Melt temperature is held between 195 °C and 215 °C, die gap is set at 1.8–2.5 mm, blow-up ratio is maintained at 2.2:1–2.8:1, and frost line height is positioned at 5–8 die diameters. In this frozen food packaging segment, the formulation employs 100 wt% DFDA-7074 NT7 or a blend containing up to 20 wt% high-pressure LDPE with melt index 0.3–0.7 g/10 min for improved bubble stability; slip masterbatch is dosed at 1.0–2.0 wt% and antiblock masterbatch at 2.0–5.0 wt%. Compliance is verified against FDA 21 CFR 177.1520(c) 3.2a for food-contact polyolefins and EU Regulation (EU) No 10/2011 Annex I, with overall migration not exceeding 10 mg/dm². Downstream conversion runs on three-layer coextrusion lines with 30:1 L/D barrier screws and internal bubble cooling; when DFDA-7074 NT7 exceeds 80 wt% in the skin layer on lines without internal bubble cooling, bubble flutter may appear at blow-up ratios above 2.6:1. The grade does not require predrying at ambient relative humidity below 60%, but cold-to-warm transfer surface condensation should be removed with 60 °C dry-air hopper circulation for 2 h. Terminal finished product types span frozen vegetable pouches, fish block bags, and pre-formed freezer bags at 40–70 µm gauge, with acceptance criteria based on ASTM D1709-16a Method A for dart impact, ASTM D1922-15a for Elmendorf tear, and ASTM D882-18 for tensile properties.

    When sack film output targets exceed 350 kg/h on a three-layer blown line with 30:1 L/D screw geometry and an 800 mm die, DFDA-7074 NT7 is run as the load-bearing core layer at 60–70 wt% while the outer layers are formulated with high-pressure LDPE or clean post-industrial recycled PE. Die gap is set at 2.0–2.4 mm, blow-up ratio at 2.0:1–2.5:1, and melt temperature at 200–220 °C. The formulation for 80–120 µm heavy-duty transit sacks includes 1.0–2.0 wt% slip masterbatch and 2.0–5.0 wt% antiblock masterbatch, with antioxidant levels retained from the resin supply specification. Industry compliance for this segment derives from UN Model Regulations Chapter 6.1 where the sack enters dangerous goods outer packaging service, and from ASTM D1709-16a and ASTM D1922-15a as mechanical acceptance standards. The downstream production process uses high-speed bottom-gusset sealing and hot-knife conversion; coefficient of friction on the film surface is typically managed to 0.20–0.40 to prevent slippage on inclined transit conveyors. Terminal finished product types include resin pellet sacks, cement and dry bulk powder sacks, insulation packaging sacks, and export-grade woven bag liners where the PE film functions as the moisture barrier membrane.

    What Controls Dart Impact in Thin-Gauge Ice Bag Conversion?

    The limiting factor in 25–35 µm ice bag conversion is not melt strength alone but the interaction between bubble cooling rate, frost line height, and transverse direction orientation. In high-stalk bubble operation, blow-up ratio is set at 2.8:1–3.2:1 and die gap at 1.8–2.0 mm to reduce melt orientation and preserve impact strength. The formulation is 100 wt% DFDA-7074 NT7 with 1.0–2.0 wt% slip masterbatch and 2.0–4.0 wt% antiblock masterbatch; some converters add 5–10 wt% metallocene LLDPE to increase hot tack at seal temperatures from 110 °C to 130 °C. Compliance follows FDA 21 CFR 177.1520(c) 3.2a and EU Regulation (EU) No 10/2011, with overall migration below 10 mg/dm² for frozen water contact. The production process uses single-groove feed extruders with 25:1–30:1 L/D and an annular die gap of 1.8 mm; frost line height is kept at 7–9 die diameters, and output is limited by bubble instability rather than extruder capacity. Terminal product types are ice cube bags, produce bags, and small-bag applications. Published exact dart impact values for this specific configuration are limited; converters therefore establish production screens using ASTM D1709-16a Method A and ASTM D1922-15a rather than relying on nominal resin datasheet values alone.

    Regulation / standardApplication contextCompliance threshold / clause
    FDA 21 CFR 177.1520(c) 3.2aFood contact blown film and sealant websPolyolefin food-contact article; extraction testing according to food type and use condition
    EU Regulation (EU) No 10/2011Food contact plastic materialsOverall migration limit 10 mg/dm² per Annex I
    REACH Regulation (EC) No 1907/2006 Article 33Industrial, agricultural, and food packaging filmSVHC communication threshold 0.1 wt% in article
    EN 13206:2017Agricultural cover filmsMechanical and weathering requirements per product class
    UN Model Regulations Chapter 6.1Dangerous goods outer packaging and inner linersPackaging compatibility, drop, and stack testing

    Because silage cover and clamp film are exposed to ultraviolet radiation, surface condensation, and abrasive soiled substrates, DFDA-7074 NT7 is processed as a 150–200 µm monolayer or as the outer layer of a three-layer agricultural film structure. UV stabilizer masterbatch is added at 1.5–3.0 wt% and carbon black masterbatch at 2.0–3.0 wt%; the base resin remains at 95–100 wt%. The process uses die gap 2.4–3.0 mm, blow-up ratio 2.0:1–2.5:1, and melt temperature 190–210 °C; lower blow-up ratio reduces transverse shrink and improves lay-flat conformity during clamp sealing. Compliance is anchored to EN 13206:2017 for thermoplastic agricultural covers and REACH Regulation (EC) No 1907/2006 Annex XVII for restricted additive substances. Terminal finished product types include silage clamp cover film, temporary storage cover, and agricultural lay-flat sheeting. Outdoor service beyond one season requires the stabilizer package to be verified by accelerated weathering under EN ISO 4892-2:2021, and film intended for direct silage contact must be checked for fermentation acid resistance on the actual production line because published data for this specific configuration are limited.

    When DFDA-7074 NT7 Is Coextruded as a Sealant Layer in Stand-Up Pouches

    A three-layer coextrusion line placing DFDA-7074 NT7 in the sealant skin typically runs the sealant layer at 20–50 µm with die gap 1.5–2.0 mm, blow-up ratio 2.0:1–2.5:1, and melt temperature 190–210 °C. The sealant formulation contains 80–90 wt% DFDA-7074 NT7 with 10–20 wt% metallocene LLDPE to broaden hot tack window, plus 0.5–1.5 wt% slip masterbatch and 1.0–3.0 wt% antiblock masterbatch. Compliance is required under FDA 21 CFR 177.1520(c) 3.2a and EU Regulation (EU) No 10/2011; the overall migration limit is 10 mg/dm². Downstream production includes adhesive lamination to PET or metallized barrier substrates, followed by pouch making on form-fill-seal lines with heat-seal jaw temperatures between 110 °C and 135 °C. Seal initiation must be confirmed on the actual line because quench rate and film aging shift surface crystallinity and can raise seal initiation by several degrees. Terminal finished product types include dry food stand-up pouches, frozen food pouches, and non-food detergent refill pouches where the sealant web remains the primary failure boundary in drop testing.

    Industrial Liner Film for Liquid Bulk Packaging and Bag-in-Box Applications

    Mechanically, puncture resistance in 80–120 µm industrial liner film is governed by gauge distribution, die-gap orientation, and the concentration of recycled diluent. DFDA-7074 NT7 is processed as 100 wt% virgin resin or as a 90/10 blend with high-pressure LDPE on monolayer or two-layer blown lines with die gap 2.2–2.6 mm, blow-up ratio 2.0:1–2.4:1, and melt temperature 195–215 °C. Processing aid masterbatch may be introduced at 1.0–2.0 wt% only when surface melt fracture is observed on grooved-feed extruders; the grade does not require predrying below 60% relative humidity. Compliance follows REACH Regulation (EC) No 1907/2006, UN Model Regulations Chapter 6.1 or Chapter 6.5 where the liner enters dangerous goods IBC or drum service, and FDA 21 CFR 177.1520(c) for food-grade liquid bag-in-box applications. The downstream manufacturing process uses high-frequency or hot-bar sealing of folded tubular film into pre-cut liners, with seal strength verified by ASTM F88/F88M-21 on production samples. Terminal product types include 200–1000 L bag-in-box liners, drum liners, and IBC inner liners for food syrups, dairy liquids, or non-food industrial fluids; field trials are required for aggressive chemical concentrates because oxidative degradation accelerates above 230 °C melt temperature and under prolonged contact with high-peroxide liquids.

    Free Quote

    Competitive Dow Dow™ DFDA-7074 NT7 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow Dow™ DFDA-7074 NT7 LLDPE is a linear low-density polyethylene resin supplied in pellet form for cast film, extrusion coating, and lamination layers. The nominal melt index is 7.0 g/10 min at 190 °C under 2.16 kg load when tested in accordance with ASTM D1238 or ISO 1133-1:2022. The nominal density is 0.925 g/cm³ when measured by ASTM D792 or ISO 1183-1:2019. The NT7 suffix identifies the pellet additive formulation; published datasheets do not always state whether slip or antiblock agents are present, and lot-specific additive statements should be requested before food-contact conversion. The resin is an ethylene/α-olefin copolymer with a linear molecular backbone; its density places it in the low-density band, but its comonomer distribution and melt-index position give a different processing profile from high-pressure low-density polyethylene and metallocene-catalysed grades. The base polyolefin falls under FDA 21 CFR 177.1520(c)3.2a for olefin polymers with density above 0.885 g/cm³. In European food-contact films, the final structure must comply with Regulation (EU) No 10/2011 overall migration limits of 10 mg/dm² or 60 mg/kg; the resin alone cannot carry compliance for a multilayer lamination. Heavy-metal and SVHC status under RoHS 2011/65/EU and REACH 1907/2006 should be confirmed by certificate of compliance for the specific lot.

    Which Published Physical and Mechanical Values Characterise This Grade?

    Typical values below are based on supplier literature and are not specification limits. Lot-to-lot variation, specimen preparation, and conditioning under ASTM D638-14 and ISO 527-1 should be controlled for comparability.

    PropertyTypical valueTest method
    Melt index7.0 g/10 minASTM D1238, ISO 1133-1:2022
    Density0.925 g/cm³ASTM D792, ISO 1183-1:2019
    Vicat softening point96 °CASTM D1525, ISO 306
    Peak melting temperature by DSC121 °CASTM D3418, ISO 11357-3
    Tensile yield strength11 MPaASTM D638-14
    Elongation at break>300 %ASTM D638-14
    Tensile secant modulus at 1 % strain240 MPaASTM D882

    On cast film lines, the resin is typically processed with a barrier-fed single-screw extruder of 24:1 to 30:1 L/D. A screen pack of 60/100 mesh is used to remove gels, and the die adapter melt temperature is held between 220 °C and 250 °C. The die lip gap is generally set between 0.4 mm and 0.8 mm; the air gap is maintained at 50 mm to 150 mm, and the chill roll temperature is controlled between 15 °C and 30 °C. Higher chill roll temperatures up to 40 °C may improve film flatness and clarity but can increase roll-blocking tendency; release behaviour should be monitored against ASTM D1003 haze data and coefficient-of-friction measurements under ISO 8295. At high line speeds, sharkskin melt fracture appears when wall shear stress at the die lip exceeds approximately 0.2–0.3 MPa. The 7.0 g/10 min melt index reduces die pressure at a given throughput relative to lower-flow grades, but if melt fracture is observed, 200–500 ppm of a fluoroelastomer polymer processing aid is a common extrusion aid.

    Production-scale failure modes observed on cast film lines include motor overload when the chill roll temperature is below 10 °C because the film becomes stiff and increases tension; edge tear from air gaps above 150 mm; and die-lip build-up from prolonged melt temperatures above 250 °C. Batch-to-batch variation in melt index should be monitored by ASTM D1238 every lot. A variation of ±0.5 g/10 min shifts viscosity and may require an adjustment of barrel temperature by 5–10 °C. Published data for this specific resin-lot sensitivity is limited, and processors should establish internal SPC ranges for their line geometry.

    When Lower Melt Index LLDPE Grades Are Replaced in Thin-Gauge Cast Film

    Replacement of a 1.0 g/10 min butene LLDPE such as DFDA-7047 NT7 with DFDA-7074 NT7 changes the processing envelope. The higher melt index corresponds to lower melt viscosity under ASTM D1238; on a 90 mm, 30:1 L/D single-screw cast line, extruder motor amperage and head pressure typically decrease. This allows thinner-gauge cast film and lower melt temperature, but the lower molecular weight of the resin reduces tensile strength and dart impact. Under ASTM D1709/A, the F50 dart impact of the 7.0 g/10 min grade is typically lower than that of a 1.0 g/10 min grade at equivalent gauge; the actual reduction is lot-dependent. In blown film and high-stalk processes, the lower melt strength of the 7.0 g/10 min resin produces greater bubble instability than DFDA-7047 NT7. Therefore the high-flow grade is not a direct substitute where bubble cooling and frost-line geometry control film gauge uniformity.

    Because the melt index of 7.0 g/10 min is higher than typical blown film LLDPE, the shear viscosity at the die is reduced. Capillary rheometry under ISO 11443 shows that melt viscosity of a 7.0 g/10 min linear polyethylene is lower than that of a 1.0 g/10 min grade at 210 °C and 100 s⁻¹; exact numerical values should be measured because molecular weight distribution and comonomer type influence viscosity. This lower viscosity allows lower melt temperatures but also reduces the maximum draw ratio before tension-thinning instability.

    Extrusion coating lines with a 65 mm screw and 28:1 L/D can process the grade, but neck-in is higher than high-pressure LDPE. A blend with 10–30 wt% high-pressure LDPE is used to maintain drawdown and adhesion to substrates. The chill roll temperature for coating paper or board is typically 15–25 °C, and the melt temperature is held at 240–250 °C to achieve oxidation-mediated adhesion; however, prolonged exposure above 250 °C increases gel formation. Adhesion to aluminium foil and oriented polyester may require a tie resin or primer because LLDPE alone does not provide polar bonding. In multilayer food packaging, the DFDA-7074 NT7 layer may be used as a sealant or bulk layer, but direct contact with high-fat foods above 60 °C may require migration testing under ASTM F1308 or EN 1186 in addition to compositional compliance.

    Mechanical and Optical Property Trade-Offs Against High-Pressure LDPE and Metallocene LLDPE

    Compared with high-pressure LDPE of similar melt index and density, the linear structure of DFDA-7074 NT7 provides higher tensile yield strength and elongation when tested under ASTM D638-14. The absence of long-chain branching in LLDPE, however, reduces melt strength and neck-in control in extrusion coating; blending 10–30 wt% high-pressure LDPE is a standard industrial control for high-melt-index LLDPE. Against metallocene octene LLDPE of similar density, the non-metallocene DFDA-7074 NT7 is expected to have a broader molecular weight distribution, though published data for this specific configuration is limited. This generally reduces die pressure at equivalent throughput and may improve cast film processability. Metallocene grades may provide higher dart impact under ASTM D1709/A, lower seal initiation temperature under ASTM F2622, and higher hot-tack strength under ASTM F1921. Optical properties are thickness-dependent; a cast film gauge of 25 µm may show haze below 5 % under ASTM D1003 only when chill roll temperature and air gap are optimised, and published data for this specific configuration is limited.

    Regulatory documentation should be obtained for the exact lot because the NT7 additive package can change. The base polyolefin typically falls under FDA 21 CFR 177.1520(c)3.2a for food-contact olefin polymers. For EU food-contact use, the final film must meet Regulation (EU) No 10/2011 overall migration limits of 10 mg/dm² or 60 mg/kg under the intended food simulants; the compliance of DFDA-7074 NT7 in a specific food-contact application depends on the total film structure, not just the resin. RoHS 2011/65/EU and REACH 1907/2006 confirmations of heavy-metal and SVHC status are issued as supplier certificates.

    Compliance areaStandard or regulationApplicability
    US food contactFDA 21 CFR 177.1520(c)3.2aOlefin polymer class; final article conditions apply
    EU food contactRegulation (EU) No 10/2011Overall migration limit 10 mg/dm² or 60 mg/kg
    Packaging heavy metalsDirective 94/62/ECSum of lead, cadmium, mercury, hexavalent chromium ≤ 100 ppm
    REACH1907/2006SVHC confirmation for each lot
    RoHS2011/65/EURestricted substances in electrical and electronic equipment

    Storage, Reprocessing, and Quality Control Boundaries

    Pellets should be stored below 40 °C in ultraviolet-shielded packaging. The resin is non-hygroscopic; pre-drying is typically unnecessary unless surface condensation occurs when cold pellets are moved into a warmer processing hall. If surface moisture is present, a hot-air dryer at 60 °C for 2 h is adequate. Oxidation induction time under ASTM D3895 should be monitored for material stored longer than 12 months. Clean edge trim can be re-introduced at up to 20 wt%, but recycle addition changes melt index, gel count, and film impact; converters should verify ASTM D1238, ASTM D3351 gel count, and ASTM D1709/A after recycle addition. Avoid processing at a melt temperature above 260 °C for more than 15 min residence time, because oxidative degradation can create gel defects and die-lip deposits.

    Top