Dow Dow Dfda 7059 Nt7 Lldpe

Dow Dow™ DFDA-7059 NT7 LLDPE

    • Product Name: Dow Dow™ DFDA-7059 NT7 LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 571402
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene
    Density 0.918 g/cm3
    Melt Index 190 C 2 16 Kg 0.8 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 600%
    Dart Drop Impact 100 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 300 g
    Haze 12%
    Gloss 45 60
    Coefficient Of Friction 0.2

    As an accredited Dow Dow™ DFDA-7059 NT7 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow™ DFDA-7059 NT7 LLDPE resin is packaged in 25 kg (55 lb) polyethylene-lined bags, palletized and shrink-wrapped for shipment.
    Container Loading (20′ FCL) Container Loading (20′ FCL): approximately 18 MT net of Dow DFDA-7059 NT7 LLDPE in 25 kg bags, loose loaded, dry container.
    Shipping Dow™ DFDA-7059 NT7 LLDPE is non-hazardous and not regulated for transport. Ship as polyethylene resin pellets in dry, clean, closed trucks, railcars, or containers. Protect from moisture, contamination, direct sunlight, and excessive heat. Typical packaging: 25 kg bags, supersacks, or bulk. Follow the SDS and local rules.
    Storage Store Dow™ DFDA-7059 NT7 LLDPE in a cool, dry, well-ventilated warehouse. Keep original packaging sealed and palletized, away from direct sunlight, moisture, excessive heat, sparks, open flames, and incompatible materials. Avoid strong oxidizers, acids, and contaminants. Use first-in, first-out rotation, avoid excessive stacking, and follow the manufacturer’s SDS and local regulations. Ensure containers remain closed when not in use.
    Shelf Life Shelf life: 24 months when stored unopened in original packaging in a cool, dry, well-ventilated area away from direct sunlight.
    Application of Dow Dow™ DFDA-7059 NT7 LLDPE

    On blown film lines producing heavy-duty industrial sacks from Dow™ DFDA-7059 NT 7, bubble stability is derived from the grade’s nominal density of 0.918 g/cm³ when tested under ASTM D1505 and its nominal melt index of 2.0 g/10 min at 190 °C/2.16 kg under ASTM D1238 and ISO 1133-1:2022. The butene-copolymer structure reduces die swell relative to high-pressure LDPE, and converters compensate by adjusting die gap to 1.8–2.5 mm and blow-up ratio to 2.5:1–3.0:1. This configuration is used to replace 100% LDPE grades in export sack liners where reduced gauge is required without losing Elmendorf tear strength measured under ASTM D1922-15. Inclusion at 70–85 wt% with 15–30 wt% high-pressure LDPE of melt index 0.25–0.8 g/10 min is common, with an additional 2–4 wt% carbon black or UV/HALS masterbatch for outdoor storage. Extruder barrel lengths of 25:1–30:1 L/D with barrier screw geometry and dual-lip air rings are specified to maintain frost line height at 5–8 times the die diameter; melt temperatures are held between 205 °C and 230 °C, with barrel zone setpoints from feed to die typically 180 °C, 190 °C, 200 °C, 210 °C, and 215 °C. Screen packs of 60/80/100 mesh are installed to limit gel transfer to the final web.

    Regulatory documentation for industrial sack applications follows REACH Regulation (EC) No 1907/2006 Annex XVII heavy-metal limits and, where the liner contacts dry foodstuffs, compositional compliance is assessed under FDA 21 CFR 177.1520(c) item 2.2 and Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm². Tensile yield and elongation at break are reported per ASTM D882-18; dart impact resistance is measured under ASTM D1709-16a method A or B depending on gauge. Converters operating below 50 µm frequently raise the LDPE fraction to 20–30 wt% to maintain bubble tension, whereas converters above 100 µm can run neat resin provided backpressure and melt temperature are controlled. Final articles include FIBC inner liners, mineral and fertilizer sacks, resin packaging liners, and reusable bulk container liners for non-hazardous solids.

    What Changes When the Same Resin Transfers to a High-Speed Cast Stretch Film Line with Chill Roll Quench?

    In cast stretch film conversion, the resin’s melt index of 2.0 g/10 min supports draw rates sufficient for web speeds of 250–500 m/min through slot die widths of 1,800–2,200 mm. The absence of an air-guided bubble places stricter demands on melt homogeneity, so cast lines are equipped with 90 mm extruder screws at 30:1 L/D, gear pumps, and screen changers upstream of the die. Die gap is set to 0.5–0.8 mm; the air gap between die and chill roll is held at 15–30 mm; chill roll temperature is maintained at 15–25 °C. Film tensile behaviour is measured under ASTM D882-18, cling force under ASTM D5458-95, puncture resistance under ASTM D5748-19, and retained load under ASTM D4649 when the film is specified for rotary wrapping. Three-layer structures position Dow™ DFDA-7059 NT 7 in the core at 70–80 wt%. Metallocene LLDPE is included at 10–20 wt% for stretch force modification; polyisobutylene or sorbitan ester cling masterbatch is added in the outer layers at 2–4 wt% of the layer mass. Since the resin is not inherently cling-modified, neat monolayer cast film will exhibit release rather than cling; therefore the cling-agent masterbatch is mandatory for hand-wrap applications.

    Regulatory compliance for industrial stretch wrap falls under REACH Regulation (EC) No 1907/2006, and when the film is used in food contact, total migration must not exceed 10 mg/dm² under Regulation (EU) No 10/2011. Chill roll fouling and edge-neck-in are the principal production failure modes observed on-line; thermal imaging of the web at the die exit is used to adjust die bolt settings and reduce transverse thickness variation to less than ±3%. Finished articles include hand wrap, machine wrap, extended-core pallet wrap, and pre-stretched hand film with nominal stretch ratios up to 150–250% depending on gauge and film layer design.

    Where frozen food converters require puncture resistance at −25 °C, Dow™ DFDA-7059 NT 7 is incorporated into blown coextruded webs at 80–90 wt%, with 10–20 wt% metallocene or plastomer resin for low-temperature crack arrest. The film is produced on a coextrusion blown line with die gap 1.8–2.0 mm, blow-up ratio 2.0:1–2.5:1, and melt temperature 204–215 °C; internal bubble cooling is used to stabilize the high-stalk bubble and reduce blocking in the collapsed web. Dart impact is reported under ASTM D1709-16a, Elmendorf tear under ASTM D1922-15, and low-temperature puncture via ISO 7765-1:1988 using instrumented or falling-dart configurations. Because the resin is not formulated with a high-slip surface package in all lot distributions, 1–3 wt% slip/antiblock masterbatch is added for pouch converting; excessive slip dosage above 3 wt% is avoided because it can suppress hot-tack performance under ASTM F1921.

    For food contact, the web is evaluated under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011. A sealer layer of low-melting mLLDPE at 10–20 wt% of total structure lowers seal initiation to the range 95–110 °C, while the LLDPE layer contributes stiffness and bag drop strength. Converting operations require tight web tension and corona treatment to 40–44 dyn/cm before lamination or print. Finished products include frozen vegetable pouches, individually quick-frozen food bags, ice cream overwrap, and frozen seafood liners.

    When Greenhouse Film Converters Introduce a UV/HALS Masterbatch to General-Purpose LLDPE

    The greenhouse and silage film route for Dow™ DFDA-7059 NT 7 is based on the conversion of base resin with separate UV stabilization rather than a pre-stabilized agricultural grade. The addition ratio to this general-purpose LLDPE is 88–92 wt% resin with 8–12 wt% HALS/UV masterbatch; when higher infrared retention is specified, 2–5 wt% of an EVA containing 9–14% vinyl acetate or a metallocene-based clarity additive is included. Published product-specific data for DFDA-7059 in multi-season covers exceeding 12 months is limited; converters must qualify the finished structure under EN 13206:2017 for covering films and under EN 13207:2018 for silage films. Test requirements include tensile strength and elongation after accelerated weathering, impact resistance, and dimensional stability. Oxygen transmission rate is measured under ASTM D3985 when silage-barrier performance is specified.

    Production is generally performed on large-diameter blown film dies of 1,200–1,500 mm, die gap 1.6–2.0 mm, blow-up ratio 2.8:1–3.5:1, and melt temperature 210–220 °C. The high blow-up ratio increases transverse orientation, which is desired for greenhouse film layflat and for silage-wrap tear propagation resistance. External cooling cages and tower height are configured for layflat widths above 8 m when monolayer greenhouse covers are produced; multi-season structures are often coextruded with a UV-rich outer layer, a core, and an inner anti-fog layer. Terminal articles include single-season and multi-season greenhouse covers, silage stretch films, and mulch films for horticulture. In silage wrap formulations, the addition ratio shifts to 93–96 wt% resin with 4–7 wt% formulated cling/UV masterbatch, because the film must combine oxygen-barrier performance with cling.

    Downstream, high-speed vertical form-fill-seal lines selecting Dow™ DFDA-7059 NT 7 for dry food and powder packaging operate with heat-seal temperatures between 115 °C and 140 °C, dwell times of 0.3–0.8 s, and jaw pressures of 0.35–0.6 N/mm². The resin contributes stiffness and tear resistance to the package body, while seal properties are modified by blending 5–20 wt% low-melting LDPE or mLLDPE. On film production, the formulation is run on blown film lines with die gap 1.8–2.2 mm, blow-up ratio 2.0:1–2.8:1, and internal bubble cooling; the melt temperature is held at 200–220 °C. Seal strength is reported under ASTM F88/F88M-21, hot tack under ASTM F1921-20, and coefficient of friction under ASTM D1894-14.

    Food-contact compliance for the finished package is established under FDA 21 CFR 177.1520(c) for the olefin polymer composition and under Regulation (EU) No 10/2011 when the package is placed on the EU market. The converter must verify that any slip/antiblock masterbatch used at 1–2 wt% does not reduce hot tack below packaging line requirements; excessive antiblock can also increase coefficient of friction variability and interfere with printing ink adhesion. Pre-press treatment of the web to 40–44 dyn/cm is generally specified before flexographic or gravure printing. Finished products include dry food pouches, powder detergent bags, granular chemical packs, and retail packaging for coffee or confectionery.

    Carrier Selection Criteria in Gravimetric Feeding and Twin-Screw Compounding for PE-Based Colour Concentrates

    In masterbatch production, Dow™ DFDA-7059 NT 7 is used as a carrier resin for colour and additive concentrates because its melt index of 2.0 g/10 min under ASTM D1238 balances pigment wetting with pellet shape stability during strand cutting. The carrier content in a carbon black concentrate ranges from 50–70 wt%, with carbon black at 20–40 wt%, wax at 2–5 wt%, and processing aid at 1–3 wt%. The addition ratio is adjusted according to pigment oil absorption and filtration pressure rise; high-structure carbon black above 80 mL/100 g oil absorption reduces carrier loading to avoid over-torque. The formulation is compounded on a co-rotating twin-screw extruder with 44:1 L/D, screw speed 600–1,000 rpm, side feeding at barrel 6–8, and melt temperature 200–220 °C.

    Compliance for the masterbatch is evaluated under REACH Regulation (EC) No 1907/2006 and, when the final article contacts food, the colourant and carrier package must satisfy FDA 21 CFR 178.3297 and Regulation (EU) No 10/2011. Producers monitor filter pressure rise through a 5–10 µm melt filtration pack and control pellet size to 3.0–3.5 mm diameter by adjusting strand die temperature and pelletizer speed. Because the resin is a film-grade LLDPE, its use in masterbatch is restricted to polyolefin film and sheet applications where a 0.918 g/cm³ carrier density does not distort the base polymer density of the final let-down product. Terminal products include black masterbatch for agricultural film, white masterbatch for packaging, and multifunctional additive concentrates for blown film extrusion.

    Free Quote

    Competitive Dow Dow™ DFDA-7059 NT7 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow Dow™ DFDA-7059 NT7 LLDPE is a linear low-density polyethylene extrusion resin supplied as natural pellets. The material is categorized by a nominal density of 0.918 g/cm³ and a nominal melt index of 2.0 g/10 min as measured under ASTM D792 and ASTM D1238, respectively. The grade is intended for blown film applications in which thin-gauge drawdown, lower head pressure and balanced solid-state toughness are required. Typical application categories include general-purpose packaging film, consumer carrier bags, industrial liners and overwrap structures. The LLDPE designation indicates a substantially linear backbone with short-chain branches from alpha-olefin comonomer; the lack of long-chain branching differentiates the resin from tubular or autoclave LDPE and changes extensional flow behaviour in film melt.

    Lot acceptance for DFDA-7059 NT7 is controlled by the manufacturer’s certificate of analysis. Commercial lot-release windows for density and melt index are typically maintained at ±0.002 g/cm³ and ±0.3 g/10 min around nominal values, but the exact limits applicable to a specific production site and packaging batch should be read from the current technical datasheet. The resin is not hygroscopic; however, surface condensation after cold storage can introduce moisture-related bubble defects, so hopper storage should be below 40°C and protected from direct sunlight.

    When Thin-Gauge Blown Film Requires Balanced Bubble Stability and Drawdown

    Processors running monolayer and coextruded films on single-screw extruders with screw diameters from 40 mm to 90 mm and a length-to-diameter ratio of 30:1 select this resin for conversion to gauges below 25 µm. Barrel settings are typically set in a rising profile from 180°C in the feed zone to 230°C at the die head. Die temperatures below 190°C can improve stalk stability but raise melt viscosity and head pressure, increasing shear heating and reducing permissible output on torque-limited drives. Spiral mandrel dies with die diameters from 150 mm to 300 mm and die gaps between 1.5 mm and 2.5 mm are common. A blow-up ratio from 2.0:1 to 3.0:1 and a frost-line height from 200 mm to 600 mm above the die are used to balance machine-direction and transverse-direction tear properties.

    The 2.0 g/10 min melt index lowers melt viscosity relative to a 1.0 g/10 min LLDPE, which permits faster screw rotation or lower melt temperature during thin-gauge conversion. The trade-off is a reduction in bubble strength compared with lower-melt-index resins. Bubble instability on high-stalk configurations appears as gauge bands and is mitigated by raising die temperature to 220°C, lowering frost-line height, or blending 5–15% LDPE into the formulation. Internal bubble cooling is recommended above 250 kg/h output on larger production lines to remove process heat and control stalk diameter. Melt pressure at the breaker plate should remain below the extruder manufacturer’s limit; typical values depend on screw condition, die restriction and temperature profile. Gauge variation measured under ASTM D6988 increases when die lips are worn or when frost-line oscillation exceeds ±10 mm.

    Film property data are generated on a 30 µm monolayer blown film sample. Tensile strength at break and elongation at break are measured under ASTM D882; machine-direction values are typically higher than transverse-direction values because of orientation induced by the film stalk and blow-up ratio. Dart impact is evaluated under ASTM D1709 Method A, and Elmendorf tear is measured under ASTM D1922. Compared with LDPE at equal gauge, LLDPE films of this density class generally exhibit higher dart impact and puncture resistance but lower machine-direction tear and reduced clarity. Optical haze is measured under ASTM D1003, and gloss is measured under ASTM D2457. The presence of slip and antiblock additives can raise haze relative to non-additivated hexene LLDPE; therefore, optical applications should be validated on the target film line rather than from pellet data alone.

    Test methodParameterControl range
    ASTM D792Density at 23°C0.916–0.920 g/cm³
    ASTM D1238Melt index at 190°C/2.16 kg1.85–2.15 g/10 min
    ASTM D3418Melting point120–126°C
    ASTM D6988Film gauge consistency on target line±5% of target

    These ranges are based on commercial lot-to-lot variation for LLDPE film resins of this density and melt index class. Exact values for a specific lot are reported in the certificate of analysis. Because dart impact, tear strength and haze depend on film gauge, blow-up ratio, frost-line height and output rate, a single published film property value is unreliable without the corresponding fabrication conditions. Published data for this specific configured film structure may be limited; the manufacturer’s technical bulletin and line trials on the target equipment are the authoritative references.

    What Distinguishes the Seal and Blocking Response of DFDA-7059 NT7 from LDPE?

    The surface response of DFDA-7059 NT7 is governed by migrating slip additives and inorganic antiblock particles. Kinetic coefficient of friction is measured under ASTM D1894; slip migration is time-dependent, and films may require 24–48 h of ambient storage before stable readings are obtained. Blocking force is measured under ASTM D3354; antiblock particles create micro-roughness that reduces film-to-film adhesion. This behaviour differs from LDPE because the LLDPE backbone has a higher tendency to adhere to itself after film winding unless surface modification is present. Heat seal initiation temperature is determined under ASTM F88 with a seal pressure of 1.0 N/mm² and a dwell time of 0.5 s. LLDPE typically seals below equivalent-density LDPE because of shorter crystallite melting paths and a broader distribution of lamellar thickness. Hot tack strength is measured under ASTM F1921 and is critical for vertical form-fill-seal operations; insufficient hot tack causes seal creep and product leakage during jaw release. The lower melt strength of LLDPE relative to LDPE can appear as greater thinning at the seal perimeter when seal bar temperature exceeds 140°C.

    Compared with a non-additivated hexene LLDPE used for high-clarity films, DFDA-7059 NT7 may show reduced gloss and increased haze because of the antiblock package. Compared with a 1.0 g/10 min butene LLDPE, the higher melt index improves seal flow and wetting but reduces hot tack force at the same gauge. Processors should therefore validate seal strength and hot tack on the target packaging line. The exact additive formulation is not publicly disclosed in the general technical bulletin; lot-specific additive information and food-contact declarations should be obtained from the manufacturer’s product safety datasheet and certificate of analysis.

    For processors already running a 1.0 g/10 min butene LLDPE, DFDA-7059 NT7 offers a higher melt index for lower head pressure and improved drawdown, but may exhibit slightly lower dart impact and tear strength at equal gauge because shorter polymer chains reduce entanglement density. For processors running LDPE-only formulations, this LLDPE increases dart impact and puncture resistance but decreases melt strength and clarity; a blend of LLDPE and LDPE is often used to recover bubble stability while retaining toughness. When dry-blending, the carrier resin of color or processing-aid masterbatches should match the base resin density and melt index. Incompatible carrier resins can produce visible gels and dart-impact variation under ASTM D1709. Letdown ratios of 2–5% are typical for color and processing aids, but critical additive loadings should be confirmed by an extrusion trial.

    Compliance documentation for DFDA-7059 NT7 typically includes food-contact suitability under FDA 21 CFR 177.1520 for olefin polymers, provided the finished article meets extraction limitations for the intended food type and use condition. European Union compliance is evaluated under Regulation (EU) No 10/2011, with overall migration tested under EN 1186. REACH obligations are maintained under EC 1907/2006; SVHC content is not expected above 0.1 wt% but should be confirmed from the safety data sheet. RoHS compliance is not typically relevant for packaging, but the resin contains no intentionally added lead, cadmium, mercury, hexavalent chromium, PBB or PBDE.

    Regulatory scopeReferenceRequired verification
    US food contactFDA 21 CFR 177.1520Finished article extraction and end-use limitation
    EU food contactRegulation (EU) No 10/2011Overall migration and specific migration for additives
    REACH SVHCEC 1907/2006Safety data sheet confirmation of SVHC below 0.1 wt%
    RoHSDirective 2011/65/EUAbsence of restricted heavy metals

    Storage should be in a closed, dry area at ambient temperatures below 40°C. The resin is not hygroscopic, so drying is not required unless surface condensation is present after transfer from cold storage to warm humid air. If condensation occurs, a hot-air hopper dryer at 60°C for 2 h is sufficient. Prolonged storage beyond 12 months may require re-testing of melt index and density before use. The product should not be exposed to direct sunlight for extended periods because UV exposure can degrade the pellet surface and produce gels. Purging with a low-melt-index LDPE or a commercial LLDPE purge compound after shutdown is recommended to remove carbonized deposits from die lips. The resin should not be melt blended with PVC or acetal; acid by-products can corrode equipment and cause film defects. Coextrusion with EVOH or polyamide requires tie resin layers because adhesion to nonpolar polyethylene is insufficient for structural integrity at typical film peel levels.

    Top