Dow Dndb 7441 Nt 7 Linear Low Density Polyethylene Resin

Dow DNDB-7441 NT 7 Linear Low Density Polyethylene Resin

    • Product Name: Dow DNDB-7441 NT 7 Linear Low Density Polyethylene Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 466620
    Density 0.920 g/cm3
    Melt Index 0.75 g/10 min (190°C/2.16 kg)
    Melting Point 123 °C
    Vicat Softening Point 96 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 24.1 MPa
    Elongation At Break 800%
    Flexural Modulus 276 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 300 g
    Haze 12%
    Gloss 45 60

    As an accredited Dow DNDB-7441 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg (55 lb) moisture-resistant polyethylene bags, palletized at 1,000 kg per pallet for industrial storage and handling.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Dow DNDB-7441 NT 7 Linear Low Density Polyethylene Resin in 25 kg bags, palletized, shrink-wrapped, secured.
    Shipping Dow DNDB-7441 NT 7 is a non-hazardous LLDPE resin. Ship in dry, closed containers via truck, rail, or sea freight. Use 25-kg bags or bulk supersacks; protect from moisture, contamination, direct sunlight, and excessive heat. Follow SDS and local regulations. Handle as non-regulated, non-dangerous goods under normal freight conditions.
    Storage Store Dow DNDB-7441 NT 7 LLDPE resin indoors in original, closed packaging on pallets in a cool, dry, well-ventilated area. Keep away from heat, flames, sparks, direct sunlight, moisture, contamination, and strong oxidizers. Use first-in, first-out rotation. Avoid dust accumulation; ground handling equipment. Protect from physical damage, keep packages sealed when not in use, and follow manufacturer’s SDS/local regulations.
    Shelf Life Shelf life: Store in cool, dry, well-ventilated area away from sunlight and heat; typically 24 months in original packaging.
    Application of Dow DNDB-7441 NT 7 Linear Low Density Polyethylene Resin

    For heavy-duty shipping sacks converted from blown films in the 100–250 µm gauge range, DNDB-7441 NT 7 is introduced as the primary tough-layer resin because its density of 0.920 g/cm³ and melt flow rate of 0.75 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022 place it in the high-dart, high-tear segment of linear low-density polyethylene. In a typical sack formulation the resin is used at 85–100 wt%, with 0–15 wt% of a high-pressure LDPE such as a 0.30–0.50 g/10 min grade added to increase melt strength and reduce bubble chatter when the blow-up ratio exceeds 2.0; antiblock masterbatch is introduced at 1.5–3.0 wt% only when a coefficient of friction below 0.55 per ASTM D1894-14 is specified by the filling line. The production route is tubular blown film extrusion on a single-screw extruder with a barrier screw, a length/diameter ratio of 30:1, a die gap of 1.8–2.4 mm, and a melt temperature of 190–230 °C; the frost line height is maintained between 600 mm and 900 mm, and internal bubble cooling is used to sustain output rates of 300–450 kg/h without raising the melt above 240 °C, at which point low-molecular-weight fractions can deposit on the die lip. Mechanical verification follows ASTM D1709-16a for dart impact, ASTM D1922-15 for Elmendorf tear, and ISO 527-3:2018 for film tensile properties, while dry food-contact status is supported by FDA 21 CFR §177.1520(c) and EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm²; non-food finished goods additionally fall under REACH (EC) No 1907/2006 and RoHS Directive 2011/65/EU. Terminal products include 25 kg and 50 kg gusseted open-mouth sacks, valve sacks, mineral fertilizer sacks, and inner liners for FIBCs where the woven outer provides load-bearing strength and the LLDPE inner ply provides moisture-barrier continuity.

    How Much UV Stabiliser Can a Silage Film Carry Before Bubble Stability Suffers?

    Silage and greenhouse film made with DNDB-7441 NT 7 requires a UV-stabilised formulation capable of withstanding repeated outdoor exposure without losing tear propagation resistance during mechanical removal. The typical addition ratio is 90–95 wt% DNDB-7441 NT 7, 5–10 wt% UV/antioxidant masterbatch containing a HALS-UV absorber combination, and 0–5 wt% LDPE for extrusion stability when a three-layer line runs a 2.0–3.0 blow-up ratio. Higher masterbatch loadings, particularly above 10 wt%, can increase screen-pack differential pressure and produce cyclic bubble instability in thin-gauge silage covers below 80 µm; converters therefore split the stabiliser loading between outer layers while keeping the core layer at 100 wt% DNDB-7441 NT 7 in a 1:2:1 or 1:3:1 layer ratio. The downstream process is a three-layer coextrusion blown-film line with die gap 1.8–2.2 mm, melt temperature 190–220 °C, internal bubble cooling, and output 400–600 kg/h; the high output and high blow-up ratio require stable melt strength, which is why the LDPE fraction is kept at the lower end unless the line is equipped with automatic bubble diameter control. Outdoor durability testing is anchored to EN 13206:2017 for thermoplastic agricultural covering films and to artificial weathering per ISO 4892-2:2013, with film tensile retention measured by ISO 527-3:2018; the resulting films are finished as silage covers, bunker sheets, greenhouse cladding, low tunnel films, and silage bags.

    When frozen-food packaging is converted at line speeds above 120 m/min on high-stalk bubble geometries, the seal-through-contamination behaviour and low-temperature dart impact of DNDB-7441 NT 7 determine whether side-seal bags survive distribution at -25 °C. The formulation is run at 100 wt% DNDB-7441 NT 7 for maximum dart impact, or at 85–95 wt% with 5–15 wt% LDPE when film optics and bag-opening behaviour on automated packing lines take precedence; slip and antiblock masterbatch are added at 1.0–2.5 wt% to maintain a coefficient of friction of 0.30–0.50 per ASTM D1894-14. The conversion route is a high-stalk blown-film process with a die gap of 1.5–2.0 mm, a blow-up ratio of 2.0–2.5, a melt temperature of 185–210 °C, and output of 250–400 kg/h; the high-stalk configuration is selected because it reduces MD/TD orientation imbalance, which in frozen-food packs appears as split failure parallel to the machine direction when the frost line is too high. Compliance for food contact rests on FDA 21 CFR §177.1520(c) and EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm², while seal strength is measured by ASTM F88/F88M-21 and dart impact by ASTM D1709-16a. Terminal finished goods include side-seal frozen vegetable bags, wicketed bread bags, ice cube packaging, seafood films, and pillow pouches for frozen processed items.

    The 200 Litre Drum Liner Problem: Crease Resistance and Chemical Inertness

    Heavy-gauge drum liners for 200 L steel and plastic drums demand a film that retains pinhole resistance after the liner is folded and pleated into the drum mouth. DNDB-7441 NT 7 is used at 100 wt% when the packaged medium is chemically aggressive or when maximum pinhole resistance is required, because the comonomer distribution supports low-temperature toughness without the catalytic residues that can initiate oxidation in concentrated surfactants; if higher modulus is required for easier insertion, 10–20 wt% high-molecular-weight HDPE is blended at the expense of dart impact, which should be monitored by ASTM D1709-16a. The process is heavy-gauge monolayer blown-film extrusion at 200–300 µm, using a grooved-feed extruder with a barrier screw, a die gap of 2.0–2.5 mm, a blow-up ratio of 1.5–2.0, and a melt temperature of 200–230 °C; low frost line height below 500 mm and external air ring cooling are used to limit excessive machine-direction orientation that creates crease cracking along folds. Compliance includes FDA 21 CFR §177.1520(c) for liners used in food-ingredient drums, EU Regulation (EU) No 10/2011 for food-contact migration, and REACH (EC) No 1907/2006 for industrial chemicals; seal strength is tested to ASTM F88/F88M-21 at a 180 °C seal bar temperature, and tear resistance to ASTM D1922-15. Terminal products are 200 L drum liners, IBC inner liners, pail liners, bin liners for viscous resins, and pre-folded anti-static liners where a conductive additive masterbatch is introduced at 3–5 wt% in a separate outer layer.

    If Lamination Sealant Webs Are Corona-Treated Above 48 dyn/cm

    Lamination sealant webs produced from DNDB-7441 NT 7 operate as the inner heat-seal layer in multi-material flexible packaging, where surface oxidation before adhesive coating must be controlled because over-treatment above 48 dyn/cm can reduce seal strength and create retained solvent odour. The resin is used at 70–100 wt%, with 0–30 wt% of a lower-melting LDPE or metallocene LLDPE included to lower the seal initiation temperature from approximately 105 °C to 95 °C; slip and antiblock masterbatch are kept at 0.5–1.5 wt% to avoid interfering with adhesive wetting. The film is blown on a monolayer or coextrusion line with a die gap of 2.0 mm, a blow-up ratio of 2.0–2.5, and a melt temperature of 190–220 °C; inline corona treatment is set to 42–48 dyn/cm as measured by ASTM D2578-17, and adhesive lamination is performed after checking for uniform wetting. Compliance is based on FDA 21 CFR §177.1520(c) and EU Regulation (EU) No 10/2011 for food-contact laminate structures, with seal strength verified by ASTM F88/F88M-21; published data for the precise seal-initiation temperature of DNDB-7441 NT 7 in solventless lamination is limited, so converter trials should be run with differential scanning calorimetry and heat-seal profile tests before specifying laminate structures. Terminal products include two-ply and three-ply laminates, stand-up pouches, sachets, lidding sealant webs, and coffee packaging.

    Ordinarily, institutional refuse sacks and compactor bag films are converted at 250–400 kg/h on monolayer lines where gauge uniformity below 0.5% coefficient of variation per ISO 4593:2020 determines the minimum weight rating printed on the package. In this application DNDB-7441 NT 7 is dry-blended at 70–100 wt% with 0–30 wt% post-industrial recycled LLDPE/LDPE granulate that has been melt-filtered through 100–150 µm screens; the recycled fraction reduces resin cost but lowers dart impact, so ASTM D1709-16a values are tested at 25 ± 2 °C and compared with the customer threshold before the recycled content is increased. The production process is monolayer blown-film extrusion with a die gap of 1.5–2.0 mm, a blow-up ratio of 2.5–3.5, a melt temperature of 180–220 °C, and internal bubble cooling to maintain output on lines with 1600–2200 mm die diameters. Compliance for household and institutional waste sacks references EN 13592:2017 for plastic sacks for household waste, ASTM D1922-15 for tear, ISO 527-3:2018 for tensile, and REACH (EC) No 1907/2006 for chemical substances. Terminal finished goods are institutional can liners, janitorial sacks, compactor bags, heavy-gauge refuse sacks, and hospital-grade waste bags where a minimum thickness and leak resistance are specified by local regulations.

    Free Quote

    Competitive Dow DNDB-7441 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DNDB-7441 NT 7 is a linear low density polyethylene resin supplied by Dow as a pelletized ethylene-octene copolymer. The nominal melt index is 0.75 g/10 min when tested at 190 °C under a 2.16 kg load following ASTM D1238, and the nominal density is 0.918 g/cm³ following ASTM D792. These are typical values, not release limits. The resin is specified in blown film applications where low-temperature dart impact, tensile strength, and tear propagation resistance are required at gauges between 25 µm and 150 µm. Heavier end uses include industrial liners, heavy-duty shipping sacks, silage bags, and frozen food packaging. Compared with butene-based LLDPE, the octene comonomer produces a higher concentration of load-bearing tie molecules at the same density, which generally shifts dart impact and Elmendorf tear upward. The low melt index of 0.75 g/10 min also raises melt pressure relative to a 1.0 g/10 min resin, so extruder sizing and screen pack selection require attention.

    Melt Rheology and Single-Screw Extrusion Boundaries

    At 0.75 g/10 min, the resin operates in the low-melt-index film extrusion window. A 60 mm single-screw extruder with 24:1 L/D and a general-purpose barrier screw exhibits high melt pressure when the die gap is reduced below 1.2 mm; typical melt pressure values for such configurations fall between 20 MPa and 35 MPa depending on screen pack design and output. Melt temperatures should be maintained between 210 °C and 240 °C. Below 200 °C, screw torque increases and film optical quality may degrade because residual gel dispersion is less complete. Above 250 °C, the resin is susceptible to oxidative degradation and surface oxidation, which reduces dart impact and increases taste and odor migration. Pre-drying is not routinely required at ambient humidity below 60 % RH; when sacks are stored in unheated warehouses or exposed to condensation, hopper dryers at 60 °C for 2 h may be used.

    A 90 mm grooved-feed blown film line running DNDB-7441 NT 7 typically uses a blow-up ratio of 2.2:1 to 2.5:1 and a frost line height between 400 mm and 600 mm for film below 100 µm. The resulting bubble supports stable neck geometry, but draw resonance can appear when the film is drawn rapidly below 25 µm at high stalk heights. Use of an air ring with dual-lip geometry and internal bubble cooling stabilizes the frost line when output exceeds 150 kg/h. At these conditions, the lower melt index reduces melt fracture compared with a 1.0 g/10 min resin, but screen pack pressure can become the limiting factor rather than motor load. The product is often selected for heavy-duty sack lines that require a slow bubble and a collapsed frame width above 800 mm. Published data for this specific configuration is limited; the values stated represent operating ranges for similar 0.918 g/cm³ octene LLDPE resins observed on production-scale equipment.

    Coextruded structures place DNDB-7441 NT 7 in the inner sealing layer or as a core toughening layer. The seal initiation temperature is lower than that of a 0.926 g/cm³ LLDPE but higher than that of a metallocene grade with the same density, and is measured under ASTM F2029 or ASTM F88 on the final film. Contamination from HDPE regrind above 10 % can raise seal initiation temperature by 2 °C to 5 °C and should be excluded in low-seal-temperature applications. Tie-layer adhesion in coextruded sacks is typically governed by the melt temperature difference at the die rather than by the resin alone; a differential of less than 10 °C between layers is recommended when DNDB-7441 NT 7 is combined with high-density polyethylene outer layers.

    How Does Octene Branch Length Improve Dart Impact and Tear Balance?

    The octene comonomer in DNDB-7441 NT 7 introduces hexyl short-chain branches. These branches inhibit lamellar crystallization more effectively than butene branches, generate a broader interlamellar amorphous layer, and increase the number of tie chains that bridge adjacent crystalline lamellae. In a 25 µm film, this morphology increases dart impact resistance measured under ASTM D1709 and Elmendorf tear resistance measured under ASTM D1922 when compared with a conventional butene LLDPE of the same 0.918 g/cm³ density. The improvement is not uniform in both directions: machine-direction tear is typically the limiting value, and process conditions that increase orientation, such as high frost line height or high blow-up ratio, narrow the tear balance. Because the resin is not a metallocene-catalysed material, comonomer composition distribution remains broader than in a constrained-geometry catalyst resin, which limits ultimate dart impact but contributes to predictable screw pumping and fewer melt-pressure oscillations during extended runs.

    Blending with 10 % to 30 % low-density polyethylene in heavy-duty sack formulations is used to increase shear thinning and reduce melt pressure. The addition of LDPE lowers extensional viscosity at high extension rates, which improves bubble stability at low blow-up ratios but reduces dart impact and Elmendorf tear proportionally to the LDPE fraction. At 20 % LDPE, machine-direction tear strength may fall by approximately 15 % to 25 % relative to the neat resin; published data for this specific configuration is limited because tear reduction depends on LDPE molecular weight distribution and long-chain branching level. Slip and antiblock masterbatches are required only when film surface friction or blocking is observed; DNDB-7441 NT 7 does not contain talc or slip additives unless added downstream. Direct contact with copper or copper alloys in the melt path should be avoided at melt temperatures above 220 °C because copper ions catalyze thermo-oxidative degradation.

    When DNDB-7441 NT 7 Is Blended with LDPE for Heavy-Duty Sacks

    When the resin is blended with LDPE for heavy-duty sack production, the primary process conflict is between dart impact retention and die pressure reduction. A 80/20 DNDB-7441 NT 7/LDPE blend can be run through a 90 mm extruder at outputs near 180 kg/h without exceeding 35 MPa die pressure, but the dart impact measured under ASTM D1709 typically decreases relative to the neat resin. If the LDPE fraction exceeds 30 %, the film may lose the low-temperature toughness required for frozen or outdoor sack drop tests. The processing window for thicknesses below 38 µm is narrower: melt temperature must remain above 215 °C to prevent LDPE crystals from generating visible melt fracture, while remaining below 240 °C to avoid oxidation of the LDPE fraction. A grooved feed throat maintained at 40 °C to 50 °C prevents pellet bridging when regrind levels reach 20 %.

    Cast film and extrusion lamination are not primary application routes for this low-melt-index resin. The high molecular weight and low melt index produce a narrower draw-down window than a 2.0 g/10 min cast film LLDPE; neck-in on a 200 mm flat die at 100 m/min is wider, and edge bead control requires careful die lip adjustment. Published data for this specific configuration is limited, and blown film remains the more predictable processing route.

    DNDB-7441 NT 7 is supplied with a conventional antioxidant package for film extrusion. Extended exposure to ultraviolet light in silage bags or outdoor heavy-duty sacks requires the addition of hindered amine light stabilizers and UV absorbers at levels determined by the intended service life. In applications requiring more than 6 months of direct outdoor exposure, stabilizer addition should follow sequential accelerated weathering evaluation under ISO 4892-2 and not rely on the neat resin alone. Over-stabilization should be avoided because amine-based additives above their solubility limit can migrate to the film surface and affect seal and print adhesion.

    Interpreting Tensile and Tear Anisotropy in 25 µm Blown Film

    Tensile and tear values in Table 1 reflect the anisotropy introduced by bubble cooling. Machine-direction yield strength is higher than transverse-direction yield strength because the take-up direction preserves molecular orientation, while transverse-direction elongation is higher after bubble relaxation.

    PropertyTest methodRepresentative value
    Melt index (190 °C/2.16 kg)ASTM D12380.75 g/10 min
    DensityASTM D7920.918 g/cm³
    Tensile strength at yield, MD/TDASTM D88210.5/10.0 MPa
    Tensile strength at break, MD/TDASTM D88243/38 MPa
    Elongation at break, MD/TDASTM D882630/710 %
    Dart impact F50, 25 µm filmASTM D1709260 g
    Elmendorf tear, MD/TDASTM D192220/30 g/25 µm
    Haze, 25 µm filmASTM D100311 %
    Gloss 45°ASTM D245770

    Film values are generated on a 25 µm blown film sample at a blow-up ratio of 2.5:1, a frost line height of 500 mm, and a melt temperature of 220 °C. These are typical values and should not be used as purchase specifications. The data show that the resin retains high transverse-direction elongation and a dart impact value that supports heavy-duty sack drop performance, but machine-direction tear remains the orientation-limited property.

    What Regulatory Limits Apply to Food Contact Film Containing DNDB-7441 NT 7?

    Food contact status for polyethylene resins is established through olefin polymer provisions rather than substance-specific clearances. Relevant frameworks are listed in Table 2. Final article compliance requires evaluation of additives, colorants, and converted film under the intended use conditions.

    Regulation/StandardApplicable Clause or MethodRelevant requirement
    FDA 21 CFR177.1520(c)Olefin polymer clearance for food contact, subject to end-use extractive testing
    EC 10/2011Annex IOverall migration limit 10 mg/dm²
    REACHEC 1907/2006Registration and safety data sheet obligations for the neat resin
    RoHS2011/65/EUNeat polyethylene base resin is outside the electrical/electronic equipment scope unless compounded with restricted additives

    Warehouse storage at 25 °C and 50 % RH in sealed containers minimizes condensation. Bags should be purged with nitrogen if stored longer than 12 months under tropical conditions. During changeover from a lower-density LDPE, purge with DNDB-7441 NT 7 until melt pressure and motor load stabilize; contamination of as little as 2 % polypropylene can increase haze and reduce interlayer adhesion in coextruded structures.

    Top