Dow Dnda 8350 Nt 7 Linear Low Density Polyethylene Resin

Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin

    • Product Name: Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 883549
    Density 0.919 g/cm3
    Melt Index 190 C 2 16 Kg 0.75 g/10 min
    Melting Point 121 °C
    Vicat Softening Point 93 °C
    Tensile Strength At Yield 9.7 MPa
    Tensile Strength At Break 24.0 MPa
    Elongation At Break 800 %
    Flexural Modulus 172 MPa
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 400 g
    Haze 11 %
    Gloss 45 60 %

    As an accredited Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DNDA-8350 NT 7 LLDPE resin is supplied in 25 kg (55 lb) bags, palletized and stretch-wrapped for industrial shipping.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized bags of Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin, stretch-wrapped and securely braced.
    Shipping Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin is a non-hazardous solid, not regulated for transport. It is shipped in 25 kg bags, octabins, or bulk trucks/railcars. Keep containers sealed, dry, and away from direct sunlight, moisture, and ignition sources. Use standard industrial handling.
    Storage Store Dow DNDA-8350 NT 7 LLDPE resin in original, closed packaging in a cool, dry, well-ventilated area. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources and strong oxidizers. Avoid dust generation and static buildup. Use first-in, first-out rotation. Inspect containers regularly and follow local regulations.
    Shelf Life Shelf life is 24 months when stored in original, unopened packaging in a cool, dry, well-ventilated area, away from direct sunlight.
    Application of Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin

    Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin has a typical density of 0.918 g/cm³ under ISO 1183-1 and a melt index of 0.55 g/10 min under ASTM D1238 at 190 °C and 2.16 kg. On a three-layer blown-film line fitted with a 250 mm spiral mandrel die, a 2.4 mm die gap, and a dual-lip air ring, heavy-duty industrial liners are produced at a blow-up ratio of 2.2:1 and a melt temperature of 210 °C. A blend of 72 wt% Dow DNDA-8350 NT 7, 18 wt% reclaimed LLDPE, and 10 wt% carbon black masterbatch is extruded at a screw speed that maintains a specific output of 1.3 kg/(cm·h) across the die circumference. The extruder is a 65 mm grooved-feed machine with an L/D ratio of 30:1; barrel zones are set at 190 °C, 205 °C, 215 °C, and 220 °C from feed to metering. Melt pressure measured before the die entrance remains within 380 bar to 420 bar; excursions above 430 bar indicate accumulation of oxidized gel in the screen pack and require screen replacement after approximately 6 h of continuous operation. Frost-line height is held between 450 mm and 550 mm, because a frost line above 600 mm correlates with transverse gauge variation of ±8% and reduced bag drop resistance. The final web at 150 µm is tested for tensile strength under ISO 527-3, with a target machine-direction value not less than 35 MPa and a transverse-direction value not less than 30 MPa. Elmendorf tear resistance is assessed under ISO 6383-2; dart impact under ASTM D1709A is specified at 200 g minimum. Regulatory documentation for these liners includes REACH SVHC content below 0.1 wt% and packaging heavy-metal limits under 94/62/EC of combined lead, cadmium, mercury, and hexavalent chromium below 100 mg/kg. Terminal products include FIBC inner liners, chemical sack overwrap, and construction rubble bags, where antistatic decay time is controlled below 0.5 s according to IEC 61340-2-3 at 12% relative humidity.

    What Hot Tack Window Governs Vertical Form-Fill-Seal Line Speeds?

    Vertical form-fill-seal packaging of dry granular products deploys Dow DNDA-8350 NT 7 as a 20 µm sealant layer in a three-layer coextrusion with a total thickness of 55 µm. The sealant layer is blended with 20 wt% LDPE to depress seal initiation temperature. Differential scanning calorimetry shows a main melting endotherm peak at 122 °C; hot tack force at 0.4 s dwell is measured under ASTM F1921 and remains above 1.5 N/25 mm when the jaw temperature is maintained between 128 °C and 140 °C. Below 125 °C, hot tack declines to less than 0.8 N/25 mm, producing intermittent seal failure at line speeds exceeding 90 pouches/min. The fin seal bars are operated at 0.4 MPa cylinder pressure and 0.5 s dwell; the vertical sealing jaw temperature is set 10 °C higher than the cross-seal jaw to compensate for product contact cooling. Optical clarity of the sealant layer after blending and extrusion is measured by haze under ISO 14782, with a typical value below 12% for a 20 µm layer. Compliance for direct food contact relies on FDA 21 CFR 177.1520 for olefin polymers and EU 10/2011 overall migration limit of 10 mg/dm² under aqueous and fatty food simulants. Terminal products include dry soup pouches, rice packets, and sugar sachets.

    Representative sealant blend benchmarks for DNDA-8350 NT 7 / LDPE mixtures
    Blend ratio (DNDA-8350 NT 7 / LDPE, wt%)Seal initiation temperature (°C)Hot tack at 0.4 s (N/25 mm)Haze in 20 µm layer (%)Test standard
    100 / 01261.116ASTM F1921, ISO 14782
    80 / 201221.511ASTM F1921, ISO 14782
    60 / 401181.68ASTM F1921, ISO 14782

    For frozen vegetable and seafood packaging, monolayer blown film is produced with a die gap of 1.8 mm, a blow-up ratio of 2.6:1, and a melt temperature not exceeding 215 °C to limit oxidative gel formation. The formulation combines 80 wt% Dow DNDA-8350 NT 7, 15 wt% high-pressure LDPE, 3 wt% silica antiblock concentrate, and 2 wt% erucamide slip masterbatch. Screw cooling is increased in the feed section to prevent premature melting and bridge formation at the hopper; the rear barrel zone is held at 160 °C while downstream zones ramp to 210 °C. Low-temperature puncture resistance is screened by ASTM D5748 slow puncture at −18 °C; a target of 12 J/mm is applied for film intended to contain frozen peas and sharp seafood edges. Dart impact at −18 °C under ASTM D1709A is specified at 150 g minimum, and Elmendorf tear under ISO 6383-2 is maintained above 18 N in the machine direction and 22 N in the transverse direction to resist puncture propagation. Food-contact documentation includes FDA 21 CFR 177.1520 and EU 10/2011, with specific migration testing on the final structure under EN 1186 for total organic migration. Terminal products include pillow pouches for frozen beans, box liners for fish fillets, and quilted bags for ice cubes.

    If Oxygen Ingress Must Remain Below 1,500 cm³/(m²·day·atm)

    Agricultural silage bale wrap and greenhouse film built on Dow DNDA-8350 NT 7 are formulated with 70 wt% linear low-density polyethylene, 20 wt% metallocene LLDPE, 8 wt% ethylene-vinyl acetate with 18% vinyl acetate, 0.6 wt% hindered amine light stabilizer, and 0.4 wt% UV absorber. The blown-film tower uses a 400 mm die, a 2.0 mm die gap, and a blow-up ratio of 1.8:1; melt temperature is held at 205 °C to avoid deactivation of HALS. Oxygen transmission under ASTM D3985 at 23 °C and 0% RH is targeted below 1,500 cm³/(m²·day·atm) for a 120 µm film. At 150 µm, oxygen transmission drops below 1,100 cm³/(m²·day·atm), but the higher thickness reduces stretch retention on round bales. The finished wrap is tested under EN 13207 for silage film; film-to-film friction is controlled by adding 0.3 wt% of a migratory slip additive, but this addition must not exceed 0.5 wt% because higher loading lowers tack required for bale self-adhesion. Field storage inspections show that film tearing occurs where gauge variance exceeds ±12%, typically caused by uneven air-ring cooling during high ambient temperatures above 35 °C. Regulatory compliance includes REACH SVHC content below 0.1 wt% and packaging heavy-metal limits under 94/62/EC. Terminal products include round and square bale silage wrap, greenhouse side curtains, and temporary solarization films.

    Regulatory and test framework for DNDA-8350 NT 7 application areas
    Standard or regulationScopeLimit or methodRelevant application
    FDA 21 CFR 177.1520Olefin polymers in direct food contactEnd-test and specificationsForm-fill-seal, lamination, frozen food
    EU 10/2011Plastic food contact materialsOML 10 mg/dm²Food pouches, lidding
    REACH EC 1907/2006SVHC content0.1 wt%All EU industrial articles
    94/62/ECPackaging heavy metalsPb+Cd+Hg+Cr6+ 100 mg/kgTransport packaging, sack liners
    ASTM D1709ADart impact of filmVaries by targetHeavy-duty and frozen packaging

    Three-layer stretch-hood film for pallet stabilization is coextruded with a 15/70/15 layer ratio. The core contains 100 wt% Dow DNDA-8350 NT 7; each skin contains 90 wt% LLDPE and 10 wt% LDPE with 2 wt% polyisobutylene tackifier concentrate added only to the outer skin via a separate gravimetric feeder. The cast-film line operates with a chill-roll temperature of 22 °C, a line speed of 350 m/min, and a total film thickness of 60 µm. Transverse stretch retention is evaluated under ASTM D5459; the film is stretched to 100% elongation at 400 mm/min, and retained load after 60 s is specified above 55% of initial load. Blocking at warehouse temperatures above 35 °C is avoided by limiting PIB concentration in the skin to below 3 wt%; higher concentrations cause film-to-film adhesion that disrupts automatic pallet-wrapping heads. The process requires corona treatment to 48 mN/m for printed pallet labels; below 44 mN/m, ink adhesion fails after 24 h under 40 °C and 70% RH storage. Regulatory documentation references 94/62/EC and REACH SVHC content below 0.1 wt%. Terminal products include stretch-hood covers for construction blocks, bottled beverage pallets, and cold-chain distribution unit loads.

    Extrusion Lamination onto Aluminium Foil for Frozen Meat and Cheese Structures

    In tandem extrusion lamination of frozen meat and cheese webs, a 65 mm extruder with a 30:1 L/D feeds a slot die at 270 °C. Dow DNDA-8350 NT 7 is applied at 15 g/m² between biaxially oriented PET and aluminium foil; the melt curtain length is kept below 150 mm to prevent neck-in exceeding 10 mm. Adhesion is tested by T-peel under ASTM F904, with target values above 2.5 N/15 mm when corona post-treatment on the foil is maintained at 48 mN/m. If the melt curtain oscillates more than ±2 mm, the applied coat weight varies by ±15%, and peel strength falls below 1.2 N/15 mm along the oscillation bands. The laminate is immediately cooled on a 20 °C chill roll with nip pressure of 45 N/cm²; insufficient cooling leads to blocking in roll form after 8 h at 30 °C. Compliance for frozen meat and cheese peelable structures relies on FDA 21 CFR 177.1520 and EU 10/2011, with total migration below 10 mg/dm². Terminal products include vacuum-skin lidding for frozen beef, flow-pack film for shredded cheese, and membrane lidding for refrigerated ready meals.

    Free Quote

    Competitive Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin is a pelletized ethylene/alpha-olefin copolymer used primarily in air-cooled blown film and in selected lamination layers. The product carries a nominal density of 0.918 g/cm³ and a melt index of 0.55 g/10 min at 190 °C under a 2.16 kg load per ASTM D1238. The polymer backbone is predominantly linear with controlled short-chain branching, a structure that separates its tensile and puncture behavior from high-pressure branched low-density polyethylene. The NT 7 suffix identifies a manufacturer-specific additive and pelletization package rather than a public molecular specification; the exact slip and antiblock concentrations must be confirmed with the supplier certificate.

    Resin Architecture and Nominal Property Set

    The nominal property set from supplier-published data is presented in Table 1. Values for tensile strength at break are not consistently published for this grade in public literature and are therefore excluded.

    PropertyTest methodNominal value
    DensityASTM D7920.918 g/cm³
    Melt indexASTM D12380.55 g/10 min at 190 °C, 2.16 kg
    Melting peakASTM D3418122 °C
    Vicat softening pointASTM D1525104 °C

    The density places the resin at the low end of linear polyethylene density grades. The melting peak of 122 °C and Vicat softening point of 104 °C define short-duration thermal boundaries for hot filling and sealing. Continuous-use temperature limits depend on package geometry, internal stress, and contact time; published data for this specific configuration is limited.

    Primary applications are heavy-duty sacks, carrier bags, industrial liners, agricultural film, and laminated layer construction. The grade is specified where the converting operation uses air-cooled blown film equipment and where stiffness or puncture resistance must be maintained after gauge reduction. In coextruded film, DNDA-8350 NT 7 is used as the core toughness layer, often between LDPE skins. The selection of skin materials influences final film optics and seal initiation; therefore the product cannot be evaluated independently of the total structure.

    At the nominal melt index of 0.55 g/10 min, DNDA-8350 NT 7 exhibits moderate shear thinning. Because long-chain branching is absent, melt tension is lower than that of a high-pressure LDPE with the same melt index. The implication is reduced bubble stability, greater neck-in on flat-die extrusion, and a smaller die-gap window before melt fracture. Capillary rheometry per ASTM D3835 is recommended for screw design; publicly available viscosity curves specific to this grade are limited.

    For production-scale air-cooled blown film, the resin is processed on a single-screw extruder with a barrier or Maddock mixing section and an L/D ratio of 24:1 to 30:1. A die gap of 1.5–2.5 mm is applied. Narrow gaps below 1.0 mm produce high die-lip shear rates and surface irregularities. Melt temperature at the die is held between 190 °C and 210 °C. Below 190 °C, intermittent sharkskin may appear at line speeds above 50 m/min; above 220 °C, oxidative chain scission can deposit oxidized material at the die lip. Frost line height is typically 400–800 mm, depending on gauge and output. A dual-lip air ring with internal bubble cooling is preferred at blow-up ratios above 2.5:1; without internal cooling, bubble oscillation and gauge variation increase. On three-layer lines, interlayer waviness is a common failure mode when the DNDA-8350 NT 7 core is paired with high-viscosity HDPE skins. The corrective action is to match melt temperatures and select skin resins with similar flow activation energy, not to raise the core melt temperature above 220 °C solely to reduce viscosity.

    What Limits the Thickness Reduction Window in Heavy-Duty Sack Film?

    Heavy-duty sack film is downgauged only within the dart impact, tear, and puncture envelope. For a 100 µm monolayer film blown at a 2.5:1 blow-up ratio, solution-processed linear resins of this melt-index class typically show dart impact values in the 80–120 g range per ASTM D1709; supplier data specific to DNDA-8350 NT 7 should govern purchase specifications. Elmendorf tear strength measured per ISO 6383-2 is orientation-dependent. High machine-direction draw can reduce machine-direction tear relative to transverse-direction tear. A blow-up ratio of 2.0:1 to 2.5:1 and a frost line height near 600 mm reduce the imbalance. Below 80 µm, puncture resistance may decrease nonlinearly if cooling is non-uniform; therefore the limiting gauge is equipment-specific rather than a single resin property.

    Against a butene-based LLDPE of the same nominal density and melt index, the solution-processed material made with a higher alpha-olefin comonomer generally provides improved dart impact and puncture resistance at equal gauge. The trade-off is a narrower stable bubble window and higher melt viscosity at equivalent shear. On a 65 mm single-screw extruder, head pressure relative to LDPE at the same screw speed may rise; the exact percentage is line-specific. Published data for this specific configuration is limited.

    Specimen conditioning is carried out at 23 °C and 50% RH for 48 h per ASTM D618. Tensile properties are measured per ISO 527-3 or ASTM D882 at a crosshead speed of 500 mm/min. Tear resistance is tested per ISO 6383-2 or ASTM D1922. Thickness measurement should be controlled to ±1 µm because impact and tear values are normalized to gauge. Without that control, downgauging comparisons are not reliable.

    When Branched LDPE Is Replaced in Lamination and Carrier Bag Layers

    Extrusion lamination and carrier bag structures using DNDA-8350 NT 7 commonly incorporate high-pressure LDPE to recover melt strength. The linear resin alone has lower extensional viscosity and higher neck-in on cast-film and extrusion-lamination tooling. At a chill-roll air gap of 150–250 mm, the melt curtain may sag more than an equivalent-melt-index LDPE. The addition of 10–30 wt% high-pressure LDPE raises melt tension and stabilizes the curtain. Above 30 wt%, puncture resistance and tear propagation resistance begin to decline, reducing the gauge-reduction advantage. In heat-seal layers, the melting peak of 122 °C allows rapid seal initiation relative to higher-density polyethylene, but seal strength depends on jaw profile, dwell time, and cooling rate. On a 90 mm extruder with a 200 mm flat die, a melt temperature near 200 °C is a practical starting point. Published data for this specific configuration is limited; release should follow line trials.

    Compared with metallocene-catalyzed LLDPE, DNDA-8350 NT 7 generally favors broader processing latitude on older blown film equipment, while metallocene grades may provide higher dart impact and optical clarity at equivalent density. The selection should be made through a fixed-condition trial matrix rather than single-point data, because product-specific optical and impact values for DNDA-8350 NT 7 are not fully published.

    Food-Contact and Regulatory Documentation

    Raw resin compliance and finished-article compliance are distinct. The base olefin polymer is covered under FDA 21 CFR 177.1520(c) for olefin polymers in food-contact applications, provided the finished article meets the extraction and end-use limitations of the regulation. In the European Union, Regulation (EU) No 10/2011 applies to the finished package; overall migration testing is required because the 10 mg/dm² limit applies to the final article, not the raw resin. REACH registration applies to the resin; SVHC content should be confirmed with the supplier certificate. RoHS compliance is an article-level declaration, not a raw resin attribute.

    Instrument / regulationScopeApplication note
    FDA 21 CFR 177.1520(c)Olefin polymers in food contactBase polymer; final-article extraction limits apply
    Regulation (EU) No 10/2011Plastic food-contact materialsFinished-article migration testing required
    REACHRegistration and SVHCSupplier certificate required
    RoHS Directive 2011/65/EURestricted substances in articlesArticle-level declaration

    Ambient storage is adequate when pellet temperature remains above the dew point. Pellets moved from cold storage into a humid processing area should be allowed to reach room temperature before opening to avoid surface condensation; moisture can cause extruder surging and thin-film bubbles. When adding color or functional concentrates, a polyethylene-based masterbatch let-down of 2–4 wt% is typical. Loadings of 10 wt% or more may lower melt strength and require frost line height adjustment. Purging should be carried out with a polyolefin purge resin; ketone-based cleaners and PVC residues create gelled contamination in the linear polyethylene melt. Barrels and screws should be hardened for extended campaigns because the grade’s processing envelope is similar to other LLDPE grades.