Dow Dnda 8320 Nt 7 Linear Low Density Polyethylene Resin

Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin

    • Product Name: Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 219630
    Density 0.920 g/cm³
    Melt Index 0.80 g/10 min (190°C/2.16 kg)
    Melting Point 124 °C
    Vicat Softening Point 104 °C
    Tensile Strength At Yield 9.7 MPa
    Tensile Strength At Break 26.2 MPa
    Elongation At Break 700%
    Flexural Modulus 241 MPa
    Dart Drop Impact 220 g
    Elmendorf Tear Strength Md 380 g
    Elmendorf Tear Strength Td 570 g
    Haze 12%
    Gloss 45 75
    Coefficient Of Friction 0.2

    As an accredited Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Typically packaged in 25 kg polyethylene bags, 55 bags per pallet, totaling 1,375 kg per pallet.
    Container Loading (20′ FCL) 20' FCL containing 25 kg bags of Dow DNDA-8320 NT 7 LLDPE resin, palletized, shrink-wrapped, and securely strapped for export.
    Shipping Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin is shipped as non-hazardous plastic pellets in sealed 25 kg bags, stacked on pallets and stretch-wrapped. Transport in clean, dry trucks or containers, avoiding moisture, contamination, and direct sunlight. Store in a cool, dry, well-ventilated area. Not classified as dangerous goods.
    Storage Store Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep bags or containers closed to prevent moisture, dust, and contamination. Protect from UV exposure and physical damage. Use appropriate handling to avoid static discharge. Maintain clean, stable conditions.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in original packaging at temperatures below 50°C.
    Application of Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin

    What Limits Bubble Stability in Heavy-Duty Sack Films at 2.5:1 Blow-Up Ratio?

    Resin with a published density of 0.924 g/cm³ (ASTM D792) and melt flow rate of 2.0 g/10 min (ASTM D1238, 190°C/2.16 kg) enters the hopper without predrying at ambient relative humidity below 70%. Condensation on pellet surfaces is removed with hopper air at 50°C and dew point below −20°C when storage conditions are humid. The extruder is a grooved-feed, single-screw unit with 30:1 L/D and barrel profile from 170°C at the feed throat to 205°C at the adapter. Melt temperature at the die is maintained between 190°C and 215°C. Die gap is set at 1.8 mm to 2.5 mm. At 2.5:1 blow-up ratio and frost line height of 600 mm to 900 mm, steady bubble geometry is obtained only when the air ring airflow remains below the point where the frost line oscillates more than ±50 mm. The conflict is structural. Higher blow-up ratio raises transverse direction tensile impact and puncture resistance. It also reduces machine direction stiffness and increases gauge non-uniformity. Lower blow-up ratio preserves tear strength but narrows the drop impact window. On a heavy-duty sack line converting 120 µm film into form-fill-seal constructions, continuous sealing requires seal-bar temperature between 150°C and 170°C and jaw pressure not exceeding 0.4 MPa. Seal strength is measured according to ASTM F88 after conditioning at 23°C and 50% relative humidity. Tensile elongation at break is measured by ASTM D882/ISO 527-3. Tear resistance is measured by ASTM D1922. Dart impact is measured by ASTM D1709 Method A. The converter may add 0.10 wt% to 0.30 wt% of a fluoroelastomer processing aid when total output exceeds 250 kg/h. The aid is not always required below that threshold. Gauge control is performed with a non-contacting capacitance sensor. Variation outside ±5% triggers automatic die lip adjustment. Heavy-duty shipping sacks manufactured under these conditions contain fertilizers, resins, and construction aggregates. The film must withstand drop loading at −20°C without splitting along the crease.

    Starting Process Window for Heavy-Duty Sack Film
    ParameterControl Range
    Melt temperature190°C–215°C
    Die gap1.8 mm–2.5 mm
    Blow-up ratio2.0:1–3.0:1
    Frost line height600 mm–900 mm

    Silage Cover Durability and UV Stabilizer Selection

    In silage clamp cover extrusion, the base resin is converted into monolayer film of 150–200 µm nominal thickness on a high-stalk bubble line. The melt temperature is held at 200–215°C. Die gap is widened to 2.5 mm to reduce frozen-in orientation in the thick gauge. The UV additive package is not supplied in the base resin. The converter compounds a hindered amine light stabilizer at 0.10–0.30 wt% and a benzophenone UV absorber at 0.05–0.15 wt% during dry blending or side feeding. Overdosing HALS beyond 0.30 wt% does not improve UV retention and may decrease print adhesion on corona-treated surfaces. Underdosing below 0.10 wt% shortens service life below one season in exposed clamps. Accelerated weathering is run under ASTM G154 Cycle 1 with UVA-340 lamps at 0.76 W/m² irradiance and 8 h UV at 60°C, followed by 4 h condensation at 50°C. Many agricultural film specifications require at least 50% retained elongation at break after 1000 h exposure. The measurement method is ASTM D882. The limiting failure mode is not tensile loss but crack formation at the clamp edges where the film is folded sharply. In practice, edge fold areas are protected by a thicker sacrificial strip of 250 µm. Carbon black masterbatch at 2.0–3.0 wt% is added when the cover must reduce light transmission to below 10% in the visible range. Light transmission is measured by ASTM D1003. Silage covers and greenhouse side curtains produced from this grade are post-consumer recyclable only if separated by polymer type. The film is not compostable under ASTM D6400. Its density remains below 1.0 g/cm³, so it floats in water used for density-based separation.

    Frozen food packaging laminates utilize the low-temperature toughness of the short-chain branching distribution. A converted blown film of 50 µm gauge is laminated as the inner sealant web to BOPP or BOPET print layers. The seal initiation temperature is established on a horizontal form-fill-seal line with jaw pressure of 0.35 MPa and dwell time of 0.5 s. Hot tack is measured according to ASTM F1921. At −25°C storage, seal strength is evaluated after conditioning by ASTM F88. Weak points occur when frozen condensate is entrapped in the seal track. The LLDPE sealant web requires a minimum seal plateau width from 110°C to 145°C to accommodate line-speed variation. Above 145°C, the sealant web begins to thin at the jaw edge. Below 105°C, incomplete wetting of the seal surfaces produces channel leaks. The formulation can be modified with a slip agent at 500–1000 ppm and an antiblock at 1000–2000 ppm to prevent blocking during reel storage. The additives are selected to comply with FDA 21 CFR 177.1520 and EU 10/2011. Frozen vegetable, seafood, and prepared meal packaging produced in this gauge range relies on the resin’s low-temperature dart impact. Dart impact is measured on the sealant web by ASTM D1709 Method A. The packaging is not designed for retort conditions above 100°C. Steam sterilization above that threshold collapses the orientation balance and delaminates the laminate.

    At web speed above 80 m/min, retail carrier bag conversion uses impulse sealers. The resin permits downgauging from 25 µm to 18 µm without seal burn-through at 130°C jaw temperature. No additional processing aid is required.

    When Recycled Content Dilutes the Short-Chain Branch Network in Industrial Liners

    When a three-layer coextrusion line incorporates post-consumer recycled LLDPE in the core layer, the melt viscosity and bubble stability shift. The line is configured with two 75 mm outer-layer extruders and one 105 mm core extruder, all with 30:1 L/D. The outer layers use 100% virgin DNDA-8320 NT 7. The core contains up to 40% washed PCR film. Screen packs are set at 80/120/80 mesh to remove unmelted gels larger than 100 µm. Increasing PCR to 40% reduces the stable bubble width by approximately 10–15% at the same air ring setting. The frost line must be lowered by 100–200 mm. Melt temperature is kept at 195–210°C. Published data for this specific configuration is limited, so each PCR lot is qualified by melt flow ratio and film tensile testing. The film grade is tested by ASTM D1238 at 190°C/2.16 kg and at 190°C/10.0 kg. The ratio between the two values must remain between 7.0 and 8.5 to approximate the shear-thinning behaviour of the virgin resin. Below 7.0, the core layer develops flow instabilities at the die exit. Above 8.5, the bubble is difficult to control above 2.0:1 BUR. Tensile strength is measured on 150 µm liner film by ASTM D882. Elongation at break is not allowed to fall below 400% in either direction. Industrial drum liners and FIBC liners produced under these conditions must survive a 4 m drop test with 50 kg load at −20°C. The test protocol follows ISO 2248 modified for liner bags and ISTA 2A. REACH and RoHS compliance is documented for heavy metals and short-chain chlorinated paraffins in the PCR stream under REACH Annex XVII and RoHS Directive 2011/65/EU. No chemical incompatibility between the butene LLDPE and typical drum contents is expected at ambient pressure. Contact with strong oxidizers above 50°C is excluded from the service envelope.

    High-speed bag-in-box converting runs the resin as the stiffening layer in a three-layer coextrusion with an EVA sealant layer. The LLDPE layer thickness is 25–40 µm. The film is surface treated to 38–42 mN/m for flexographic printing. Coefficient of friction is adjusted to 0.25–0.35 as measured by ASTM D1894 to prevent telescoping on rewind and to allow bag insertion into corrugated boxes. Slip and antiblock masterbatches are added at the hopper. The final structure is tested for water vapour transmission rate according to ASTM F1249 at 38°C and 90% relative humidity. The relevant food contact compliance is FDA 21 CFR 177.1520 and EU 10/2011. The converter must verify overall migration below 10 mg/dm² under EU 10/2011 test conditions for aqueous and fatty simulants. The resin itself is not a barrier to oxygen. Oxygen transmission through the LLDPE layer is governed by ASTM D3985 and is high relative to EVOH or metallized films. The package design therefore places the oxygen barrier in a separate laminate layer. Melt temperature at the die is held at 205–215°C to maintain adhesion to the EVA layer without degrading the vinyl acetate comonomer. Degradation of EVA releases acetic acid at temperatures above 220°C. The LLDPE layer functions within that limit.

    Food Contact Compliance Test Matrix for Bag-in-Box Structures
    Regulatory ReferenceScopeTest Method
    FDA 21 CFR 177.1520Olefin polymersEnd-use condition verification
    EU 10/2011Plastic food contact materialsOverall migration 10 mg/dm²
    ASTM F1249WVTR38°C, 90% RH
    Free Quote

    Competitive Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin is an injection molding grade supplied as natural-color pellets. The resin belongs to the linear low-density polyethylene class through ethylene/α-olefin copolymer architecture. Its published property envelope includes a density of 0.924 g/cm³ under ASTM D792 and a melt index of 20 g/10 min at 190°C/2.16 kg under ASTM D1238. These two values position the material as a high-flow, low-density injection grade rather than a film-extrusion or blow-molding resin. Manufacturer literature identifies thin-wall containers, lids, closures, and household articles as typical end uses. The designation NT 7 indicates natural pellet supply. Food-contact applications require article-specific evaluation under FDA 21 CFR 177.1520(c) or EU Regulation 10/2011; resin type alone does not constitute compliance.

    Table 1 summarizes typical physical properties. Specimens are conditioned at 23°C ± 2°C and 50% ± 5% relative humidity according to ASTM D618. Values are typical and are not guaranteed lot-release specifications.

    PropertyTest MethodTypical Value
    DensityASTM D7920.924 g/cm³
    Melt IndexASTM D123820 g/10 min
    Vicat Softening TemperatureASTM D152592 °C
    Tensile Yield StrengthASTM D63811.0 MPa
    Elongation at BreakASTM D638800 %
    Flexural Modulus, 1% SecantASTM D790290 MPa
    Hardness Shore DASTM D224052

    How Does a Melt Index of 20 g/10 min Constrain Injection Molding Conditions?

    The melt-temperature operating window is narrow relative to high-pressure LDPE because the resin’s low molecular weight and high melt flow reduce residence-time tolerance. Barrel settings from 190°C to 220°C are typical, with nozzle temperatures held at 200°C to 220°C. If melt temperature falls below 190°C, the plasticating unit may produce unmelted material and flow lines in sections below 1.0 mm. If melt temperature exceeds 250°C, thermal oxidative chain scission can accelerate stabilizer depletion and cause yellowing. The resulting melt flow shift may not be immediately visible but can reduce impact performance. Screw decompression of 1 mm to 3 mm after recovery is commonly used to control nozzle drool.

    On a hydraulic reciprocating screw with 20:1 to 25:1 L/D and compression ratio 2.5:1 to 3.5:1, back pressure in the range 0.5 MPa to 1.0 MPa and screw speed 50 rpm to 100 rpm are conservative starting points. Higher back pressure may elevate melt temperature beyond the set point through viscous dissipation. The high melt index permits filling of wall sections from 0.5 mm to 1.5 mm at high flow-to-wall-thickness ratios, but molded article validation requires pressure-drop measurements on the specific mold. Feed throat temperature should remain below 50°C to avoid premature pellet melting and screw slippage. Published data for specific configurations is limited.

    Mold temperatures between 10°C and 30°C are normally sufficient; higher mold temperatures can improve surface gloss but extend cycle time. Vent depth is a critical threshold. Low-viscosity high-flow LLDPE can flash through parting lines if vent depth exceeds 0.02 mm. Vents 0.01 mm to 0.02 mm deep are standard for polyethylene. Vacuum venting may be required for large projected areas or thin-wall packaging molds. If screw recovery time exceeds cooling time, a higher-capacity machine or a barrier-flight screw may be required.

    Pre-drying is not usually required because polyethylene does not undergo hydrolytic degradation. However, if storage humidity exceeds 60% RH, surface moisture can produce splay defects. A desiccant hopper dryer at 80°C for 2 h with a dew point of -30°C is adequate. Regrind usage of 20% to 40% by weight is common if the regrind is free of oil, paper, or silicone contamination; above this level, melt flow and color drift should be monitored. Additive bloom can occur at elevated regrind levels or excessive melt temperatures; white or waxy deposits on mold vents should prompt thermal history review.

    Slow-strain mechanical response under ASTM D638 includes a tensile yield strength near 11.0 MPa and elongation at break above 800%. The flexural modulus under ASTM D790 is approximately 290 MPa, placing the grade in the semi-flexible range. This combination is functional for snap-fit lids and living hinges if the hinge is designed with a thin cross-section and is flexed only after the part has cooled below 60°C. The Vicat softening temperature under ASTM D1525 is approximately 92°C, so continuous service above 70°C is not recommended without creep and heat-age testing. Low-temperature ductility is characteristic of LLDPE, but notched impact data on molded plaques should be generated according to ISO 179-1 or ASTM D256. Weld lines and sharp internal corners can reduce practical impact strength; gate locations should divert weld lines away from hinge and snap-fit features.

    Environmental stress-crack resistance is superior to HDPE injection grades of similar melt flow under many food-contact stress agents, but it is not unlimited. Aromatic hydrocarbons, chlorinated solvents, and high-temperature surfactant solutions can initiate cracking under strain. For packaging of essential oils, citrus oils, or alcohol-based sanitizers, stressed-cup testing under ASTM D1693 or notched constant-ligament stress testing should be performed on the finished article. Published data for DNDA-8320 NT 7 in aggressive food simulants is limited, and substitution without article-level testing is not recommended.

    Thermal Stability and Antioxidant Package Under Repeated Processing

    The resin contains a hindered phenolic/phosphite antioxidant system typical of linear low-density polyethylene. During repeated heat histories, the stabilizer package is consumed by radical scavenging. Melt flow can be used as an indirect indicator of chain scission; if melt index shifts by more than 20% relative to the virgin value at 40% regrind loading, processing temperatures or residence time should be reduced. Yellowness index according to ASTM E313 is a supplementary control for color-critical articles. Polymer characterization by differential scanning calorimetry under ISO 11357-3 typically places the peak melting endotherm of LLDPE in the range 120°C to 124°C; the exact value for this grade should be taken from the manufacturer’s certificate of analysis.

    For shutdown and purging, fractional MI LLDPE or LDPE at 190°C to 220°C is adequate. Avoid purging with polyoxymethylene or rigid PVC because their decomposition products can corrode screw and barrel surfaces. If production interruption exceeds 5 min, barrel temperatures should be reduced to 150°C to limit thermal degradation. Do not restart directly from high temperature with a full barrel of stagnant resin; discard the first several shots after restart.

    Differentiation from other polyethylene grades is controlled by melt flow and density. Film-grade LLDPE with melt index near 1.0 g/10 min has higher melt viscosity and melt strength, which support bubble stability in blown film; DNDA-8320 NT 7 is unsuitable for blown film because its 20 g/10 min melt index cannot maintain adequate bubble pressure. High-pressure LDPE of comparable density has long-chain branching and higher melt elasticity, making it preferable for shrink film and extrusion coating, but its tensile yield and environmental stress-crack resistance are generally lower than the linear structure of DNDA-8320 NT 7. High-density polyethylene injection grades with density between 0.945 g/cm³ and 0.965 g/cm³ provide higher flexural modulus and Vicat softening temperature, but lower ESCR and reduced low-temperature ductility. Metallocene LLDPE grades may offer different short-chain branch distribution and improved impact at equal density; direct substitution should be validated using instrumented puncture testing under ISO 6603-2 or equivalent.

    Rotomolding and profile extrusion are not appropriate for this grade. Rotational molding commonly requires melt index values between 3 g/10 min and 6 g/10 min; profile extrusion requires melt strength that high-flow LLDPE does not provide. The high shear rate viscosity can be approximated by a power-law model in the range 100 s⁻¹ to 5,000 s⁻¹: η = K γ̇ⁿ⁻¹. Published constants for this specific grade are limited, and mold-filling simulation requires measured capillary or slit rheometry data rather than single-point melt index.

    When Shrinkage and Warpage Are Evaluated Against Semi-Crystalline Solidification Rates

    Mold shrinkage for LLDPE injection grades is often reported in the range 1.5% to 2.0% under ASTM D955, but the specific value for DNDA-8320 NT 7 depends on wall thickness, packing pressure, gate size, and mold temperature. The density of 0.924 g/cm³ produces lower shrinkage than filled polypropylene but higher than amorphous polymers. Differential shrinkage between thick and thin sections is the primary driver of warpage. Part designs should limit wall-thickness transitions to 25% or less and use generous radii at intersections. Gate placement in the thickest section allows adequate packing before gate freeze.

    Packing pressure should be maintained until the gate seals; once the gate freezes, additional hold time does not reduce shrinkage. Gate land lengths of 0.5 mm to 1.5 mm provide a balance between shear heating and gate seal control. In thin-wall packaging, transfer from injection velocity to packing pressure at 95% to 98% of full part weight reduces flash and improves dimensional repeatability. Cavity pressure sensors may be placed at the last fill point to set transfer triggers. Post-molding crystallization continues for 24 h to 48 h; dimensional inspection should be delayed until this period has elapsed. If parts are stacked or restrained during cooling, molded-in stress may be fixed and later released as distortion. Published data for this specific resin in complex geometries is limited, so mold-filling simulation should use pressure-volume-temperature data from the material supplier.

    For regulatory compliance, lot-level certificates should be obtained from the supplier. The grade is typically manufactured to support food-contact use under FDA 21 CFR 177.1520(c) for olefin polymers, but colorants, processing aids, and regrind may alter the final article status. Under EU Regulation 10/2011, the final packaging article must meet overall migration limits and specific migration limits for additives in the intended food simulant. REACH registration applies to monomer and additive substances rather than the polymer as such. The resin is not intended for medical implant applications; biocompatibility testing under ISO 10993-1 would be required. High-temperature sterilization above 121°C is not recommended without creep, burst, and migration testing specific to the treated article.