| HS Code | 287573 |
| Product Name | Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin |
| Chemical Family | Linear Low Density Polyethylene |
| Density | 0.920 g/cm³ |
| Melt Index 190 C 2 16 Kg | 0.8 g/10 min |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 27.6 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 207 MPa |
| Vicat Softening Point | 94 °C |
| Melting Point | 124 °C |
| Crystallization Point | 104 °C |
| Elmendorf Tear Strength Md | 300 g |
| Elmendorf Tear Strength Td | 400 g |
| Dart Drop Impact | 200 g |
| Haze | 10% |
| Gloss 45 | 60 |
| Coefficient Of Friction | 0.2 |
| Low Temperature Brittleness | -70 °C |
| Water Absorption | <0.01% |
As an accredited Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow DNDA-7340 NT 7 LLDPE resin is supplied in 25 kg bags, with 55 bags per pallet (1,375 kg net). |
| Container Loading (20′ FCL) | 20′ FCL: 18 pallets (24.75 MT) of Dow DNDA-7340 NT 7 LLDPE resin, 25 kg bags, palletized and stretch-wrapped. |
| Shipping | Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin ships as non-hazardous solid pellets, typically in 25 kg moisture-resistant bags, 500–1,000 kg bulk bags, or bulk trucks/railcars. Store dry, away from heat and UV. No DOT/IMDG/IATA special shipping labels required. |
| Storage | Store Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or containers closed, sealed, and off the floor on pallets. Protect from moisture, dust, and contamination. Avoid excessive stacking and prolonged UV exposure. Follow the manufacturer's SDS and local regulations. |
| Shelf Life | Shelf life is 24 months from manufacture when stored in original unopened packaging at temperatures below 50°C under dry conditions. |
Thin-wall injection moulding of dairy portion-control containers and snap-on lidding uses the 0.934 g/cm³ density of Dow DNDA-7340 NT 7, measured per ASTM D792-20, and the 7.0 g/10 min melt index, measured per ASTM D1238-20 at 190 °C/2.16 kg, as primary flow-selection criteria. In multi-cavity tools with 8–16 cavities, the resin is processed on a 120–180 t toggle-clamp injection machine with barrel zone temperatures from feed to nozzle of 180–220 °C and a mould coolant inlet temperature of 12–25 °C; lower mould temperatures reduce cycle time but raise frozen-in orientation and increase the probability of lid curvature after side-stacking. Thin-wall parts with nominal wall sections of 0.7–1.2 mm are filled through fan or edge gates having a land length below 0.8 mm and a gate depth of 0.6–0.8 times the nominal wall thickness, a geometry that suppresses stringing and limits gate blush on contact surfaces. The high melt index allows melt temperatures to remain in the lower portion of the processing window, but if the nozzle temperature falls below 190 °C, the cold slug can cause flow hesitation in ribs and hinge sections; if the nozzle temperature exceeds 240 °C, oxidative degradation reduces puncture impact under ASTM D3763 and may create off-taste in fatty dairy contents. Drying is generally unnecessary when the resin is stored at 20–30 °C and 50% RH or lower, but condensation on pellets introduced from outdoor silos in winter should be removed with a 60–70 °C dehumidified-air hopper dryer for 2 h before charging the machine. Food-contact compliance for dairy lidding rests on FDA 21 CFR 177.1520(c) for olefin polymers and on EU No 10/2011 for plastic food-contact materials, with migration testing performed under OM2 fatty-food simulant conditions and total migration limits as specified in the regulation. Converters should verify lot-specific certificates because additive packages and catalyst residues are controlled by the producer but may vary by production campaign.
Household bleach and liquid detergent closures are injection moulded from the resin when the cap must survive repeated opening under stress-crack-inducing surfactant exposure. Under ASTM D1693, condition A, at 50 °C in 100% Igepal CO-630, polyethylene closure grades are often specified with no failure before 1000 h; for DNDA-7340 NT 7 the datasheet ESCR value is relevant but prototype testing remains mandatory because gate vestiges and sharp thread roots create stresses absent from the notched plaque coupon. The cap design therefore uses a continuous thread profile with a root radius of at least 0.5 mm and a tamper-evident band connected by frangible bridges no thicker than 0.4 mm, because bridge thickness above this value reduces easy-opening performance and increases the probability of incidental tearing in transit. On the moulding line, the melt is held at 210–230 °C and the mould at 15–30 °C; hold pressure is limited to 45–60 MPa because overpacking raises residual stress and shortens crack-initiation time under capping torque. Torque retention is evaluated according to ASTM D2063 for continuous-thread closures, and if child-resistant features are present, the closure is classified using ASTM D3475. For hypochlorite bleach applications, ESCR after moulding should be verified with the actual filling solution because Igepal testing does not fully model oxidising stress cracking; published data for this specific configuration is limited. Addition of 2–4 wt% low-density polyethylene may improve ESCR but reduces top-load strength measured under ASTM D642, a trade-off that must be resolved before release of tooling. The resin should not be blended with amine-containing mould-release agents or certain phenolic antioxidants that promote discolouration in oxidising closures; a polyethylene-compatible lubricant at 0.05–0.15 wt% is used for demoulding only when ejection force is excessive.
| Application segment | Compliance standard | Test / condition |
|---|---|---|
| Dairy thin-wall lidding | FDA 21 CFR 177.1520(c) | Olefin polymer food-contact compliance |
| Dairy thin-wall lidding | EU No 10/2011 | Migration testing under OM2 fatty-food simulant |
| Household chemical closures | ASTM D1693 | ESCR, 50 °C, 100% Igepal CO-630 |
| Industrial crates and food totes | FDA 21 CFR 177.1520(c) | Direct food-contact suitability |
| Masterbatch carrier | REACH | SVHC and Annex XVII screening |
| Appliance drain pans | IEC 60335-1 | Material suitability, abnormal heat |
| Recreational / toy components | EN 71-3, ASTM F963 | Heavy metal migration, mechanical hazards |
Where collapse-resistance and cleaning tolerance are more important than optical clarity, moulders run the resin in solid-wall industrial totes and food-handling crates with wall thicknesses of 2.0–4.0 mm. On a 350–500 t hydraulic injection machine, a melt temperature of 215–240 °C and a mould temperature of 20–40 °C allow filling of reinforced corners without short shots, while the 0.934 g/cm³ density contributes to top-load capacity under ASTM D642. Vicat softening under ASTM D1525 is typically below 120 °C, so hot-water washing above 75 °C under constant load can reduce stack life. The resin’s ESCR under ASTM D1693 supports returnable crate service with hot-water washing and dilute alkaline detergents, but localised deformation occurs above the Vicat region and reduces stack life if wash water exceeds the indicated boundary. Jetting can occur if the sprue bushing is undersized; therefore, sprue diameter is held at 4.0–6.0 mm, and gate thickness is opened to at least 1.5 mm where flow orientation creates visible weld lines. Compliance for direct food contact uses FDA 21 CFR 177.1520(c), while industrial non-food crates are assessed under REACH and must not contain Annex XVII restricted substances above applicable thresholds. Pigment selection for grey and black crates should be limited to polyethylene-compatible masterbatches at 2–4 wt%, and additional ultraviolet stabilisers are required only for prolonged outdoor storage.
Because the melt index of 7.0 g/10 min is high enough to wet filler surfaces and lower compound viscosity, the resin is selected as a dilution vehicle in mineral-filled and carbon-black-loaded masterbatches destined for polyethylene film and injection moulding. In a co-rotating twin-screw extruder with 40:1 L/D and 60–75 mm screw diameter, the resin is fed upstream at a rate that maintains 70–80% torque at screw speeds of 300–500 min⁻¹; these figures are equipment-specific and should be re-established on the actual barrel configuration. Melt temperature at the die is held at 200–230 °C, and the pelletised compound is evaluated for melt flow under ASTM D1238-20 and tensile yield and elongation under ASTM D638-14. The terminal masterbatch, containing 40–50 wt% carbon black or 60–70 wt% calcium carbonate, is diluted to 2–5 wt% in natural resin; because the carrier and dilution resin share the same polyolefin backbone, delamination and surging at the injection machine are reduced. If calcium carbonate is used, stearic acid surface treatment at 0.5–1.0 wt% improves dispersion and prevents agglomerate formation, but excessive stearic acid can interfere with odour performance in food packaging. Published data for the specific throughput and specific energy input of this resin in a given compounding configuration is limited; pilot-scale runs should be used to define exact operating parameters.
Appliance drain pans moulded from the resin require balanced fill analysis because the combination of 0.934 g/cm³ density and 7.0 g/10 min melt index produces a crystallisation rate that creates differential shrinkage when cooling is non-uniform. The pan is typically moulded with a wall of 1.5–2.5 mm, using a 200–280 t injection machine and a mould coolant temperature of 15–30 °C; the coolant temperature differential across core and cavity is limited to 5 °C. If the core runs more than 10 °C hotter than the cavity, post-ejection warpage can exceed 2.0 mm over a 300 mm span after 48 h conditioning at 23 °C and 50% RH per ASTM D618; published data for this specific part geometry is limited, so tool trials are required to establish acceptable warpage. To compensate for differential shrinkage, toolmakers add negative draft of 0.5–1.0° on deep ribs and use post-mould cooling fixtures that hold the part against a temperature-controlled mandrel. Compliance for condensate contact in refrigeration appliances is assessed under IEC 60335-1 for material suitability and resistance to abnormal heat, while electrical and electronic articles must also satisfy RoHS Directive 2011/65/EU restricted-substance limits. Above 240 °C melt temperature, oxidative chain scission lowers elongation and can create odorous degradation products in trapped condensate. If flame-retardant requirements appear in appliance standards, a halogen-free polyethylene-compatible system must be selected because classical brominated systems are not normally used in this polyolefin.
For multi-component toy parts and recreational components that require cold impact resistance after abuse loads, the resin is injection moulded at a melt temperature of 200–220 °C and a mould temperature of 15–30 °C. The resulting parts, typically with wall thicknesses of 1.5–3.0 mm, are tested under ASTM F963 for sharp edges and small parts, and under EN 71-3 for migration of specific elements; compliance with the toy safety directive requires the absence of anti-blocking additives that can migrate during mouthing. The resin’s low-temperature impact resistance is influenced by moulded-in stress, so cold-runner gating with large radii and post-mould cooling fixtures is used to minimise notch sensitivity; if parts are snapped together in assembly, the snap-fit geometry should use a nominal strain below 5% and a root radius of at least 0.8 mm to prevent stress-whitening. Because the natural polyethylene grade does not normally contain a UV stabiliser package, outdoor recreational components exposed to sunlight require a UV masterbatch at 3–6 wt%, and the stabilised compound should be evaluated for tensile strength after 1000 h of accelerated weathering according to ASTM D4329 or ISO 4892-2. Colour concentrates for toys are selected from heavy-metal-free pigments only, and the moulding operation should avoid zinc stearate levels above 0.1 wt% where contact with food-simulating saliva is regulated under EN 71-3; published data for this specific weathering configuration is limited unless the masterbatch formulator provides a certificate of analysis.
Competitive Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin is a natural-pellet LLDPE supplied without slip or antiblock additives. The grade carries a density of 0.934 g/cm³ when determined under ASTM D792-20 and a melt flow rate of 0.75 g/10 min at 190 °C under a 2.16 kg load according to ASTM D1238-20 and ISO 1133-1:2022. The combination of higher density and lower melt flow rate distinguishes the resin from general-purpose film grades such as 0.920 g/cm³, 1.0 g/10 min LLDPE. The supplier designation DNDA-7340 NT 7 identifies the polymer family, density decade, and additive package; NT 7 denotes natural color and the absence of slip and antiblock. The resin is intended for heavy-duty blown film structures in which stiffness, tear resistance, and puncture resistance after downgauging are required. Because the base stabilization package is designed for processing and not for long-term ultraviolet exposure, outdoor service requires additional UV stabilizer masterbatch. The polymer is supplied as pellets and is hydrophobic, but feed-inlet moisture accumulation can still occur under high-humidity plant conditions.
The melt flow rate of 0.75 g/10 min is lower than the 1.0 g/10 min typical of many commodity LLDPE film grades, indicating a higher average molecular weight and a higher zero-shear viscosity. The viscosity at 190–230 °C remains sufficiently shear-thinning for spiral mandrel die distribution, but screw motor load and die pressure will be higher than those observed with a 1.0 g/10 min resin at identical screw speed and temperature profile. The crystalline melting point determined by ASTM D3418-21 is approximately 125 °C, and the Vicat softening point is approximately 118 °C under ASTM D1525-17. These values place the grade closer to medium-density polyethylene in thermal resistance than to low-density film LDPE.
| Property | Method | Typical Value |
|---|---|---|
| Density | ASTM D792-20 | 0.934 g/cm³ |
| Melt flow rate | ASTM D1238-20 / ISO 1133-1:2022 | 0.75 g/10 min |
| DSC melting peak | ASTM D3418-21 | 125 °C approximately |
| Vicat softening point | ASTM D1525-17 / ISO 306:2022 | 118 °C approximately |
| Additives | — | No slip; no antiblock |
| Form | — | Natural pellets |
Because the grade contains no slip or antiblock, freshly blown film exhibits elevated surface friction. Converters running high-speed form-fill-seal lines must add an erucamide or oleamide slip masterbatch at 1–3 wt% plus silica or synthetic antiblock at 0.2–0.5 wt% to reach coefficient-of-friction targets below 0.20–0.30. The letdown ratio depends on masterbatch carrier resin compatibility; LLDPE-compatible masterbatches with a melt index between 0.5 g/10 min and 2.0 g/10 min are preferred to minimize melt stratification.
Primary conversion is monolayer or coextruded blown film on single-screw extruders with 24:1 or 30:1 L/D barrier screws. A grooved feed section improves pellet conveying of the high-molecular-weight resin and reduces feed pressure fluctuation. Melt temperature measured at the adapter should be held between 195 °C and 230 °C; die zone set points of 190–210 °C are typically sufficient when the die gap is 1.5–2.5 mm. Starting blow-up ratios of 2.0:1–3.0:1 and a frost line height of 4–8 die diameters are recommended for bubble stability. At melt temperatures below 190 °C, unmelted crystallites and high melt elasticity can generate shark-skin melt fracture on the film surface. If shark-skin appears at line start-up, the correction is to raise the die zone set point by 5–10 °C while holding the frost line distance constant and increasing cooling air temperature by 5 °C at the air ring. Production-scale experience on 65 mm grooved-feed extruders with 250 mm spiral mandrel dies shows that die pressure can reach 20–28 MPa depending on output and melt temperature, which is a meaningful increase over 1.0 g/10 min LLDPE. The output loss relative to a 1.0 g/10 min LLDPE is commonly 5–15% at fixed screw speed. Pre-drying is not normally required, but pellets stored in open hoppers at relative humidity above 60% may require 2 hours at 80 °C if surface moisture leads to die-lip deposits or bubble breakage.
The following film data are manufacturer typical values for a 25 µm monolayer blown film produced at a 2.0:1 blow-up ratio and 2.0 mm die gap. The values are not specification limits and will shift with gauge variation, additive loading, frost line position, and coextrusion layer structure.
| Film Property | Method | Typical Value |
|---|---|---|
| Dart drop impact F50 | ASTM D1709-16a | 100 g |
| Elmendorf tear, machine direction | ASTM D1922-19 | 130 g |
| Elmendorf tear, transverse direction | ASTM D1922-19 | 310 g |
| Tensile strength at break, machine direction | ASTM D882-18 | 38 MPa |
| Tensile strength at break, transverse direction | ASTM D882-18 | 31 MPa |
| Elongation at break, machine direction | ASTM D882-18 | 650% |
| Elongation at break, transverse direction | ASTM D882-18 | 750% |
| 1% secant modulus, machine direction | ASTM D882-18 | 370 MPa |
| 1% secant modulus, transverse direction | ASTM D882-18 | 430 MPa |
The 0.934 g/cm³ density raises the 1% secant modulus above that of 0.920 g/cm³ LLDPE by approximately 20–30%, while the low melt index contributes to high dart impact and transverse-direction tear resistance. The mechanical data support downgauging in heavy-duty sack applications by approximately 10–20% relative to 100 µm LDPE film, provided that seal strength and creep resistance are validated for the specific filling line. The dart impact value of approximately 100 g at 25 µm is not a direct puncture-force measurement; for lower-speed puncture events, the transverse-direction Elmendorf tear and tensile elongation provide complementary toughness data.
Compared with DOWLEX 2045G LLDPE film resin, which has a density of 0.920 g/cm³ and a melt index of 1.0 g/10 min, DNDA-7340 NT 7 increases density by 0.014 g/cm³ and lowers melt flow rate by 0.25 g/10 min. The density increase elevates stiffness and reduces water vapor transmission; published data for this specific comparative configuration is limited, but the water-vapor-transmission-rate reduction for thicker crystalline layers is generally 10–15% at equal thickness. The lower melt index increases die pressure and reduces gross output under the same extruder conditions. Relative to high-pressure LDPE of similar melt index, the linear structure of DNDA-7340 NT 7 provides higher tensile strength at break and higher Elmendorf tear, but the absence of long-chain branching reduces melt strength and narrows the stable bubble window. Air rings with a dual-lip high-velocity design and internal bubble cooling are often required when running low melt index linear film at high output. Compared with metallocene-catalyzed LLDPE film grades, the conventional molecular architecture typically exhibits broader molecular weight distribution and different aesthetic properties; clarity is lower, but extrusion at low melt temperatures may be more forgiving in spiral mandrel dies. The resin does not contain the highly uniform comonomer distribution that gives metallocene grades their high dart impact at low thickness; converters should not assume equivalent dart impact at 20 µm without trial.
Food-contact status for the neat resin is represented under U.S. FDA 21 CFR 177.1520(c)3.1a for olefin polymers, subject to finished-article compliance with use conditions and any migration limits. For European food-contact use, the film is typically evaluated under Regulation (EU) No 10/2011 and its amendments, including the overall migration limit of 10 mg/dm² and the specific migration limits applicable to additives and monomers. The base pellet is not formulated with slip or antiblock; surface properties must be adjusted by the converter. Because the resin has higher density and crystallinity than 0.920 g/cm³ LLDPE, haze is higher and gloss is lower; the grade is not suitable for high-clarity display packaging. Continuous service above 60–70 °C or boiling-water immersion can reduce film integrity and should be validated before use. Autoclave sterilization is outside the normal recommendations for this grade. Outdoor use requires adequate UV stabilization; the base resin contains only processing stabilizer and will embrittle under extended ultraviolet exposure if unstabilized. The grade is not intended for medical implant or parenteral applications. Users must also assess articles for REACH SVHC notifications if masterbatch or ink components introduce substances of very high concern. The polymer in pellet form is generally considered exempt from REACH registration as a polymer, but downstream article obligations remain.
In heavy-duty sack production for 25 kg polymer granulate or fertilizer packaging, the resin is commonly extruded at 100–150 µm gauge with 2–4 wt% slip/antiblock masterbatch and, when needed, 3–5 wt% carbon black masterbatch. Sacks filled at high speed experience puncture, drop, and stacking creep. The 0.934 g/cm³ density provides creep resistance under stacked pallet loads, while the transverse-direction tear strength prevents tear propagation after puncture. Drop testing according to ISO 7965-2 is used to validate filled sack performance; manufacturers should specify drop height and fill mass because the resin alone does not determine sack failure. High-molecular-weight pellets can bridge in tall feed hoppers; hopper agitation or low-angle conical hoppers reduce feed interruptions. Nitrogen purging of the feed throat is used in humid plants to prevent moisture-induced feed blockage. Coextrusion with a 0.920 g/cm³ LLDPE skin layer or an LDPE skin layer can modify seal initiation and optics while retaining the stiffness of the core layer.