| HS Code | 633107 |
| Density | 0.920 g/cm³ |
| Melt Index 190 C 2 16 Kg | 2.3 g/10 min |
| Melt Flow Ratio I21 I2 | 30 |
| Comonomer | Octene-1 |
| Peak Melting Temperature | 123 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 24.1 MPa |
| Ultimate Elongation | 800% |
| Flexural Modulus | 241 MPa |
| Dart Drop Impact F50 | 120 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 12% |
| Gloss 45 | 60 |
| Coefficient Of Friction | 0.6 |
| Slip Additive | No |
| Antiblock Additive | No |
As an accredited Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin supplied in 25 kg bags, 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Dow DNDA-7147 NT 7 LLDPE resin in 25 kg bags, palletized, shrink-wrapped, and secured for export shipment. |
| Shipping | Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin ships as non-hazardous general cargo, typically in 25 kg bags or bulk trucks/containers. Keep dry, cool, and out of direct sunlight. Avoid punctures, contamination, and prolonged heat exposure. No DOT, IMDG, or ADR hazardous shipping classification applies. |
| Storage | Store Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and open flames. Keep bags or containers tightly closed to prevent moisture and contamination. Avoid contact with strong oxidizers. Maintain clean, stable ambient conditions and follow first-in, first-out stock rotation. Protect from physical damage and prolonged UV exposure. |
| Shelf Life | Typically 24 months from date of manufacture when stored in original, unopened packaging in a cool, dry, well-ventilated area. |
In thin-wall injection moulding of food-contact containers, DNDA-7147 NT 7 is processed at melt temperatures from 190°C to 230°C, with mould temperatures held between 10°C and 40°C; the melt flow rate determined in accordance with ISO 1133-1:2022 at 190°C under 2.16 kg load is 50 g/10 min, and density measured by ASTM D792-20 Method B is 0.926 g/cm³. Compliance for food-contact use is assessed under FDA 21 CFR 177.1520 for olefin polymers and EU Regulation 10/2011 Annex I for plastic food-contact materials, with end-use migration testing governed by EN 1186-1:2002. Formulation addition follows a base-resin proportion of 100 wt% or a dry blend of 97–98 wt% DNDA-7147 NT 7 with 2–3 wt% of a polyolefin-based slip/antiblock concentrate; the concentrate itself contains 5–10 wt% erucamide or oleamide and 10–20 wt% synthetic silica in an LLDPE carrier. Downstream conversion uses high-speed injection moulding machines with clamp forces typically between 1,500 kN and 3,500 kN, accumulator-assisted injection speeds above 200 mm/s, and hot-runner valve-gated tools to fill wall stocks below 0.8 mm; cycle times on a 32-cavity rectangular container tool are shortened by the high melt flow, but gate freeze time must be controlled below 0.5 s to prevent short shots at the end of the flow path. Hot-runner thermal uniformity of ±5°C across all drops is required because viscosity variation in thin wall sections produces uneven filling and warpage after demoulding. Pre-drying is not normally required, but if surface condensation occurs at relative humidity above 80%, hopper drying at 60°C for 2 h is advised. Terminal finished products include thin-wall dairy cups, deli containers, portion cups, and flexible overcap lids intended for chilled and short-duration ambient food storage.
In colour and additive masterbatch production, DNDA-7147 NT 7 functions as the thermoplastic carrier. Regulatory compliance follows REACH (EC) 1907/2006, RoHS Directive 2011/65/EU, and ISO 11469:2016 for identification marking, while food-contact masterbatches are further evaluated under FDA 21 CFR 177.1520 when the final article requires olefin polymer clearance. Carrier addition ratio varies inversely with pigment oil absorption and bulk density: organic pigment concentrates are commonly formulated with 70–90 wt% carrier, carbon black masterbatches with 45–60 wt% carrier, and high-yield inorganic pigment or mineral filler concentrates with 30–55 wt% carrier; the residual mass consists of pigment/filler, dispersants, and low-melt waxes. Production equipment is typically a co-rotating twin-screw extruder with L/D ratio 44:1, modular screw elements, side stuffing at barrel 5–6, and vacuum devolatilisation at −0.08 MPa; melt temperature at the die should remain between 180°C and 220°C. The 50 g/10 min melt flow rate reduces apparent melt viscosity, allowing side-fed carbon black to wet out at loadings where a 2 g/10 min LLDPE would exceed extruder torque limits; when filler addition exceeds 60 wt%, melt pressure upstream of the die plate can rise above 8 MPa, requiring a gear pump and wider die holes. Screw speeds are typically maintained between 400 min⁻¹ and 800 min⁻¹ depending on filler type, but higher speeds above 800 min⁻¹ generate excessive shear heating and initiate gel formation in the carrier. Pelletising is typically underwater or water-ring strand, and terminal product types include single-pigment colour masterbatches, combined additive concentrates, UV stabiliser concentrates, and carbon black masterbatches for film, injection moulding, and sheet extrusion.
| Standard/Regulation | Designation/Clause | Relevant Evaluation |
|---|---|---|
| ISO 1133-1:2022 | Condition 190 °C/2.16 kg | Melt mass-flow rate |
| ASTM D792-20 | Method B | Density of resin |
| FDA 21 CFR 177.1520 | Olefin polymer clearance | Food-contact compliance for polyolefin articles |
| EU Regulation 10/2011 | Annex I | Food-contact plastic material documentation |
When snap-fit caps and overcaps are converted, DNDA-7147 NT 7 is used as the primary moulding resin or in a let-down with LDPE to control closure flexibility and stress-crack resistance. Compliance for single-use and repeated-use food closures is governed by FDA 21 CFR 177.1520 and EU Regulation 10/2011, with dimensional stability monitored by ISO 294-4:2018 for moulding shrinkage and ISO 291:2008 for conditioning. Formulation addition ratios include 100 wt% DNDA-7147 NT 7 for thin-wall overcaps, or 75–90 wt% DNDA-7147 NT 7 with 10–25 wt% LDPE homopolymer where improved hinge flex endurance is required; slip additives are incorporated at 0.5–1.0 wt% of a 5% erucamide concentrate. Production is carried out on multi-cavity injection moulding tools with 24–96 cavities, hot-runner valve gates, and cycle times of 8–15 s; mould temperature is held at 15–30°C, and injection pressure typically reaches 80–120 MPa in thin hinge sections to avoid short-fill. Gate diameter is reduced to 0.6–0.8 mm to generate capillary flow heating and to reduce gate vestige on the sealing surface. Terminal finished product types include flip-top caps for personal care bottles, snap-on overcaps for jars, and tamper-evident closure shells where LLDPE flexibility prevents stress whitening after demoulding.
Compounding of DNDA-7147 NT 7 into polypropylene impact copolymer targets low-temperature ductility without introducing high-viscosity domains that would compromise injection moulding fill. Material compliance for moulding compounds is assessed under ISO 19069-2:2016 and ASTM D4101-17e1 classification systems, with notched impact properties reported according to ISO 179-1:2023 and ASTM D256-23. The formulation addition ratio of DNDA-7147 NT 7 is restricted to 5–25 wt%; below 5 wt% the low-temperature impact improvement is statistically indistinguishable from the PP control under ASTM D256-23, and above 25 wt% the flexural modulus measured by ISO 178:2019 decreases sufficiently to exclude parts from rigid structural specifications. The downstream production process uses a co-rotating twin-screw extruder with melt temperature from 200°C to 230°C, screw speed 300–500 min⁻¹, and injection of DNDA-7147 NT 7 pellets via the main feed while talc or glass fibre is side-stuffed downstream; the screw configuration should contain two kneading blocks with 45° staggering to disperse the LLDPE phase without inducing excessive shear heating. Published data for exact LLDPE domain size distribution in this specific PP matrix is limited; however, the 5–25 wt% range is derived from industrial compounding practice, and domain sizes are controlled by maintaining screw residence time below 45 s. Terminal product types include automotive interior trim carriers, appliance housings, and industrial crates where impact loading occurs at temperatures below 0°C.
For non-food housewares moulded from post-consumer olefin recyclates, DNDA-7147 NT 7 is let down at 20–40 wt% into washed and regranulated HDPE or PP to counteract batch-to-batch melt flow variability. Compliance for recycled-content claims follows ISO 14021:2016, while material safety for articles placed on the European Union market is evaluated under REACH (EC) 1907/2006; food-contact status is not claimed for this stream because PCR traceability under EU Regulation 10/2011 cannot be maintained. Formulation addition ratio is selected by measuring the incoming regrind melt flow rate under ISO 1133-1:2022: when PCR lot MFI falls below 5 g/10 min, a 35–40 wt% addition of DNDA-7147 NT 7 is required to restore a target compounded MFI between 15 g/10 min and 25 g/10 min for thin-wall moulding; when PCR lot MFI is already 10–15 g/10 min, a 20–25 wt% addition is sufficient. Production comprises dry blending followed by twin-screw re-compounding at 190–210°C, filtration through a 120–150 mesh screen changer, and injection moulding with cold-runner tools; regrind moisture must be below 0.05 wt% before extrusion, requiring drying at 80°C for 3 h when lost-on-drying exceeds that threshold. Melt filtration pressure should not rise more than 3 MPa per hour, and a spike beyond 10 MPa signals fines or crosslinked contamination requiring a screen pack change. Terminal finished products include storage bins, waste containers, clothes hangers, and logistical crates for non-food distribution.
Competitive Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DNDA-7147 NT 7 is a solution-process linear low density polyethylene resin supplied in natural pellet form. The grade is produced with a Ziegler-Natta catalyst and uses 1-octene as the short-chain branching comonomer. Fundamental rheological characterisation lists a melt index of 4.0 g/10 min at 190°C/2.16 kg per ASTM D1238 and a density of 0.917 g/cm³ per ASTM D792. The NT 7 suffix identifies a natural-grade stabilised formulation containing a slip and antiblock additive package; the precise additive composition is proprietary. The material is intended for air-cooled cast film, thin-gauge stretch wrap, hygiene and medical packaging films, industrial liners, and coextruded webs. The product differs from butene-based linear low density polyethylene grades primarily through its longer short-chain branch length, which influences crystalline tie molecule behaviour, dart impact, and tear balance after conversion.
| Property | Test standard | Reported value |
|---|---|---|
| Melt index | ASTM D1238, ISO 1133-1:2022 | 4.0 g/10 min |
| Density | ASTM D792, ISO 1183-1:2019 | 0.917 g/cm³ |
| Vicat softening point | ASTM D1525 | 101°C |
| Melting peak temperature | ASTM D3418 | 124°C |
In Ziegler-Natta solution polymerisation, 1-octene incorporation produces hexyl branches on the polyethylene backbone, whereas 1-butene produces ethyl branches. At equivalent density and melt index, the hexyl branches in DNDA-7147 NT 7 increase the probability of tie molecule formation between adjacent lamellae. Tie molecules transmit stress across crystalline regions and are a primary structural variable governing slow and rapid fracture resistance. Dart impact measured by ASTM D1709/A on 25 µm cast film for this resin is reported above 80 g in representative converter datasets, although the exact value varies with air gap, draw ratio, and chill roll surface finish. Elmendorf tear measured by ASTM D1922 is more balanced between machine direction and cross direction than is typically observed for a butene-based linear low density polyethylene of equivalent density, where machine-direction tear may fall below cross-direction tear by a factor of 1.5–2.0. Tensile elongation at break under ASTM D882 should be generated on the converted film because film properties are not intrinsic. The density of 0.917 g/cm³ balances crystallinity and low-modulus recovery; lower density would improve toughness but reduce temperature resistance and film modulus, while higher density would reduce permeability but degrade dart impact.
On production-scale cast film lines equipped with single-screw extruders of 24:1 to 30:1 L/D and barrier screws, DNDA-7147 NT 7 feeds consistently at ambient temperature. Melt temperatures at the die lip are typically held at 240–260°C; higher temperatures accelerate oxidation of the polymer and migration of the slip additive, while lower temperatures increase melt fracture risk and reduce throughput. Die gaps between 0.5 mm and 0.8 mm are common for this melt index, and a vacuum box or air knife is used to pin the melt curtain to the chill roll. Chill roll surface temperatures between 15°C and 25°C provide sufficient quench to limit crystalline growth and preserve optical uniformity. Screen packs of 60/80/100 mesh and continuous screen changers reduce gel defects; lines processing post-industrial regrind may require finer filtration to 150 mesh. The resin does not require drying unless pellet surface moisture is present after storage in high-humidity environments. Surface moisture can produce bubble defects and reduce melt pressure stability; pellets stored at relative humidity above 60% should be conditioned or dried with low-temperature dehumidified air.
For screw design, the melt index of 4.0 g/10 min and density of 0.917 g/cm³ place DNDA-7147 NT 7 at the higher-flow end of cast film linear low density polyethylene grades. A 90 mm single-screw extruder with 24:1 L/D may generate die pressures between 150 bar and 250 bar at output rates of 200–300 kg/h, depending on die width and gap. This pressure range is not an intrinsic material property; it results from the combination of melt viscosity at die temperature, die lip opening, and throughput. Melt temperature at the die should be measured with an immersion probe rather than inferred from barrel set points. Melt temperature uniformity across the die width must be held within ±2°C to avoid gauge-band defects. If melt temperature variation exceeds ±5°C, gauge uniformity may fall outside ±3%, and the film may exhibit soft zones and stretch wrapper instability.
The NT 7 additive package is formulated to lower surface friction after the cast film has wound. Slip additives such as primary amides bloom to the film surface over time; this migration is influenced by film crystallinity, storage temperature, and pressure in the wound roll. Kinetic coefficient of friction is evaluated by ASTM D1894; a high-slip cast stretch film typically targets a value below 0.2 after 24 h of ageing at 23°C and 50% relative humidity. Blocking force is assessed by ASTM D3354 or ISO 11502; excessive winding tension before additive bloom can produce blocking force beyond the unwind capability of the stretch wrapper. On cast lines, the melt curtain is more stable with a slightly broader molecular weight distribution, but this resin is not as shear-thinning as long-chain-branched LDPE. Therefore draw resonance may appear when draw ratio exceeds 20:1 and air gap exceeds 150 mm, depending on die lip geometry and melt temperature. The use of an air knife or pinning jet is required to reduce melt curtain flutter. Converters should validate additive bloom kinetics at the actual roll diameter and winding hardness, because data collected on small laboratory samples may not predict telescoping or film blocking in large rolls.
The migration of primary amide slip agents follows time-temperature superposition. Cooling the film below the additive melting point initially slows migration, but later film storage at ambient temperature allows the additive to bloom. Optimum winding tension is therefore a compromise: high tension improves roll stability but reduces the free volume for additive migration. If the film is wrapped immediately after slitting, slip may not have fully developed; this can lead to film stretching on the wrapper instead of film sliding from the roll. ASTM D1894 kinetic coefficient of friction measurements should be made on both film surfaces after 24 h and 72 h ageing to capture the bloom curve. Antiblock particles, if present, reduce the contact area between film layers; their effectiveness is measured by blocking force rather than haze alone. Thus a converter evaluating DNDA-7147 NT 7 should not assume that low haze equates to low blocking, because the two properties are measured by different mechanisms.
Compared with a butene-based Ziegler-Natta linear low density polyethylene of the same nominal density and melt index, DNDA-7147 NT 7 generally provides higher dart impact at equivalent gauge and better machine-direction tear retention. The difference is not purely additive; the longer short-chain branches from octene create a more efficiently entangled amorphous phase. Compared with a metallocene-catalysed octene linear low density polyethylene, the molecular weight distribution of DNDA-7147 NT 7 is broader, which reduces melt pressure fluctuation and motor load variation on older extruders, but may produce slightly higher haze and lower gloss after conversion. Haze is measured by ASTM D1003 and gloss at 45° by ASTM D2457. Compared with high-pressure LDPE of melt index 4.0 g/10 min, this resin has lower melt strength, so the air gap should be shortened or the draw ratio adjusted to prevent draw resonance. In coextruded films, DNDA-7147 NT 7 is placed in the core or outer layers to improve toughness; blending with 10–30% LDPE improves melt curtain stability at the cost of some dart impact. Published data for a specific blend ratio on a given cast line is limited; acceptable LDPE addition is determined by the die gap, air gap, and quench rate.
The selection of DNDA-7147 NT 7 in coextruded structures is also governed by sealing behaviour. The resin has a seal initiation temperature that depends on film gauge and sealing pressure; laboratory heat-seal tests should be performed using ASTM F88 or ASTM F2029. Because the grade is an octene-containing linear low density polyethylene, its melting peak is lower than high-density polyethylene and slightly different from butene grades; this affects hot-tack strength and seal-through-contamination performance. Published data for specific heat-seal curves on this grade is limited; heat-seal performance must be validated on the target packaging line with the actual seal bar temperature, dwell time, and pressure. In multilayer cast films, DNDA-7147 NT 7 is frequently used as a toughness layer rather than as the seal layer when a metallocene plastomer is specified for low-temperature seal initiation.
At 12 µm gauge on a power pre-stretch casting unit, the octene-based architecture of DNDA-7147 NT 7 supports pre-stretch ratios of 250–300% with a lower pinhole frequency than a butene grade of equivalent melt index, provided the film is quenched rapidly and pinning is stable. Pinhole resistance is not a single-material property; it is a function of film thickness, gauge uniformity, and tensile stress under ASTM D882. The melt index of 4.0 g/10 min permits thin-gauge extrusion without excessive melt temperature, but does not provide the melt strength of a fractional-melt or long-chain-branched polyethylene. Therefore the cast line must operate with a reduced air gap, often below 120 mm, and a chill roll temperature near 20°C to freeze the film before the melt curtain necks in. The slip additive package must be allowed to bloom before finished rolls are palletised; stretch wrappers operating at high winding tension may otherwise experience film blocking or intermittent feed. Published data for specific pinhole counts at a given pre-stretch ratio on DNDA-7147 NT 7 is limited; converter trials should be conducted with the actual roll weight and wrapper force settings.
Two processing failure modes are commonly observed when DNDA-7147 NT 7 is run at the lower end of its melt temperature window. The first is sharkskin melt fracture, which appears as a rough surface pattern on the film edge and is a viscoelastic instability at the die lip. Raising die lip temperature by 5–10°C or reducing output often removes the defect. The second is draw resonance, a periodic thickness variation in the draw direction caused by a lack of melt strain hardening. It is controlled by shortening the air gap to below 120 mm, increasing melt temperature slightly, or adjusting quench roll speed until the draw ratio is outside the instability window. The addition of 5–15% high-pressure LDPE is a common remedy because long-chain branching increases extensional viscosity and stabilises the melt curtain.
Regulatory declarations for food-contact use must be obtained from the supplier for the specific end-use conditions. Polyethylene resins in pellet form may be evaluated under 21 CFR 177.1520(c) for food-contact articles, but the final fabricated film must meet the density, thickness, extractive, and use-condition limitations applicable to the food type and temperature. Under European Union Regulation (EU) No 10/2011, the finished article is subject to overall migration limits using the prescribed food simulants; resin certification alone does not establish compliance of the converted film. REACH and RoHS declarations should be requested from the supplier. The product should be stored in unopened packaging at temperatures below 50°C and away from direct sunlight. Prolonged storage at elevated temperature can cause additive bloom to the pellet surface and change the slip/antiblock balance before extrusion. Bags should be cleaned of external contamination before the pellets are transferred to hoppers, and conveyed air should be dried if ambient dew point exceeds 10°C.