| HS Code | 314920 |
| Density | 0.920 g/cm3 |
| Melt Index 190 C 2 16 Kg | 0.70 g/10 min |
| Melt Flow Ratio I21 I2 | 27 |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 27.6 MPa |
| Ultimate Elongation | 700% |
| Flexural Modulus | 240 MPa |
| Vicat Softening Point | 95 °C |
| Melting Point | 123 °C |
| Crystallization Temperature | 106 °C |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 10% |
| Gloss 45 | 65% |
| Coefficient Of Friction | 0.2 |
| Low Temperature Brittleness | < -70 °C |
As an accredited Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Typically supplied in 25 kg (55 lb) polyethylene bags, palletized, or 1,000 kg bulk bags for industrial transport. |
| Container Loading (20′ FCL) | 20′ FCL loaded with 25 kg bags of Dow DNDA-7144 NT 7 LLDPE resin, palletized, shrink-wrapped, secured for ocean freight. |
| Shipping | Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin is shipped as a non-hazardous solid resin. It is not DOT/IMDG/IATA regulated. Use 25-kg bags, bulk bags, or bulk hopper trucks/railcars. Keep clean, dry, and avoid ignition sources; no special placards or labels required. |
| Storage | Store Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep bags or containers tightly closed to prevent moisture, dust, and contamination. Avoid contact with strong oxidizers. Use first-in, first-out stock rotation, and protect pellets from prolonged high temperatures and UV exposure. |
| Shelf Life | Shelf life is typically 24 months from date of manufacture when stored unopened, cool, dry, and away from direct sunlight. |
Across high-output cast film assets with 90–120 mm single-screw extruders operating at 30:1 L/D, the resin is processed at 240–260 °C melt temperatures to keep shear viscosity low enough for 0.6–1.0 mm flat-die gaps. The nominal density of 0.918 g/cm³ per ASTM D792 and the melt flow index of 0.70 g/10 min per ASTM D1238 at 190 °C/2.16 kg place the material in the low-melt-index cast-film envelope, which favors high dart impact and high puncture resistance in 12–15 µm pallet-wrap structures. On a chill roll maintained at 18–28 °C, the web is stabilized by a vacuum box at 40–80 mbar and an air knife at 5–10 mbar; when the vacuum differential falls below 30 mbar, air entrainment produces repetitive transverse bands and thickness deviations of ±2–3 µm. Draw ratios of 200:1–300:1 are common, but premature draw resonance appears as line speed exceeds 700 m/min if the die-to-roll distance is not shortened or the melt temperature raised. Cling is not inherent to the resin; converters meter 0.5–1.5 wt% polyisobutylene or a proprietary cling agent into the outer layer while keeping the middle layer free of low-molecular-weight additives. Haze values below 2.5% per ASTM D1003 and dart impact above 100 g at 15 µm per ASTM D1709 are typical process-control targets, but published data for DNDA-7144 NT 7 at sub-10 µm gauges is limited; converter-specific trials are required because chill-roll surface finish and air-knife positioning shift both values.
Bubble instability becomes measurable on three-layer blown film dies with 1.2–1.8 mm die gaps and 200–250 mm die diameters when blow-up ratios exceed 2.8:1 unless the outer layers contain between 10 wt% and 20 wt% high-pressure LDPE. The absence of long-chain branching in the linear resin lowers extensional strain hardening relative to LDPE, which increases bubble sag and narrows the air-ring cooling window; frost line heights above 600 mm then produce high stalk motion and uneven film gauge. Incorporation of LDPE with a melt index of 0.2–0.5 g/10 min introduces strain hardening and lowers internal bubble pressure fluctuations to less than ±0.5 mbar on some lines, but the addition simultaneously reduces low-temperature dart impact. In 50 µm frozen-food structures, seal initiation is normally observed between 103 °C and 110 °C on hot-tack testers per ASTM F1921; the sealing window narrows in coextrusions with an EVOH or polyamide core because thermal transfer to the seal layer is slowed by the barrier polymer. Water vapor transmission rates of 1.5–2.5 g/m²/day at 38 °C/90% RH per ASTM F1249 are achievable at 50 µm in unfilled LLDPE, but frozen-food specifications requiring less than 1.0 g/m²/day need an additional barrier layer. Low-temperature dart impact failure at -20 °C is more often traceable to core-layer thickness than to variation in the skin resin; published data for this exact grade in frozen-food coextrusions is limited, and line-specific trials with ASTM D1709 and ASTM D1922 are necessary to set layer ratios.
The resin’s 0.70 g/10 min melt flow index becomes the controlling variable in form-fill-seal tubular film lines running at 80–120 m/min. Low seal initiation temperatures of 105 °C are regularly achieved with seal bar pressures of 0.4–0.6 N/mm² and dwell times of 0.4–0.8 s, but raising hot tack above 2.0 N/15 mm at 110 °C per ASTM F1921 requires either higher seal-bar temperature or longer dwell; both changes reduce the production window because the film stiffens at the web edge and triggers FFS jaw sticking. Heavy-duty sacks at 80–120 µm thickness are evaluated by dart impact per ASTM D1709 and Elmendorf tear per ASTM D1922; on high-stalk blown film lines, machine-direction tear can drop below 150 g when the stalk height exceeds 1.0 m, while transverse-direction tear values above 250 g are retained by maintaining blow-up ratios below 2.5:1. For contents above 25 kg, a film gauge below 80 µm risks burst failure because the density of 0.918 g/cm³ yields lower puncture resistance than medium-density polyethylene; converter specifications often require a minimum 120 µm gauge for palletized chemical bags. The resin is also used as a sealant web in FFS structures, where lubrication with 0.1–0.3 wt% erucamide reduces coefficient of friction to below 0.20 per ASTM D1894, but excess slip additive migrates to the seal interface and reduces seal strength below 2.5 kgf/15 mm within 48 h.
On tandem extrusion coating lines with 120 mm extruder diameters and 28:1 L/D, melt temperatures above 290 °C reduce neck-in but increase oxidation gel formation; coating weights of 12–25 g/m² are achievable only when the die gap is set to 0.5–0.7 mm and the air gap is kept below 200 mm. The resin as a pure extrusion-coating layer exhibits neck-in values in the range of 40–70 mm at 200 m/min; adding 10–15 wt% high-pressure LDPE with a 4–8 g/10 min melt index reduces neck-in by 15–25% and allows line speed to increase. Corona discharge to 38–42 dyn/cm at the laminating nip is required before the melt is bonded to aluminium foil or metallized polyester; peel adhesion below 2 N/15 mm per ASTM D1876 generally indicates insufficient surface oxidation or chill roll release agent transfer. In aseptic and liquid-packaging structures, the resin functions as the heat-seal layer, and the seal initiation window of 95–105 °C must remain stable after retort or hot-fill exposure at 75–90 °C. The resin has not been optimized for extrusion lamination onto paper without a tie layer because polar cellulosic surfaces require an EVA or ethylene-acrylic acid layer; published adhesion data for direct coating of DNDA-7144 NT 7 to paperboard is limited.
| Downstream segment | Line/equipment type | Melt temperature range | Process ratio or die gap | Line speed | Critical process limit |
|---|---|---|---|---|---|
| Cast stretch wrap | 90–120 mm single-screw cast film line, 30:1 L/D | 240–260 °C | 0.6–1.0 mm die gap; 200:1–300:1 draw ratio | 600–800 m/min | Draw resonance above 700 m/min without air-gap reduction |
| Blown film frozen-food coextrusion | Three-layer blown film die, 200–250 mm | 190–220 °C | 1.2–1.8 mm die gap; BUR 2.0:1–2.8:1 | 50–120 m/min | Bubble instability above 2.8:1 without LDPE |
| FFS heavy-duty sacks | Tubular blown film, high-stalk | 180–210 °C | 1.2–2.0 mm die gap; BUR below 2.5:1 | 80–120 m/min | Jaw sticking above 120 °C seal-bar temperature |
| Extrusion coating | Tandem extrusion coating line, 120 mm, 28:1 L/D | 290–320 °C | 0.5–0.7 mm die gap; air gap below 200 mm | 150–350 m/min | Neck-in above 70 mm without LDPE addition |
Agricultural film lines running 1.5–2.0 mm die gaps depend on outer-layer additive concentrates because the resin itself is not supplied with a UV stabilizer package. During three-layer agricultural film production, UV stabilizer masterbatches are added typically at 8–12 wt% into the outer layer only; the resin carries the additive package without requiring predrying at ambient relative humidity below 60%. Greenhouse and silage films of 150–250 µm thickness rely on high puncture resistance and long-term tensile retention rather than high transparency. Oxygen transmission rates of an unfilled LLDPE film at 150 µm are in the range of 1,000–2,000 cm³/(m²·day·atm) per ASTM D3985; anaerobic silage fermentation therefore depends on film thickness and surface puncture resistance rather than gas barrier, and structures requiring oxygen permeation below 500 cm³/(m²·day·atm) must include an EVOH or polyamide core. Anti-fogging performance is provided by migratory additives that reduce internal surface tension to below 35 mN/m; additive dose rates above 2 wt% often reduce interlayer adhesion and create haze bands. Weathering retention must be confirmed by ASTM D4329 or ISO 4892-2 using specified UV-A lamps and condensation cycles; published data for this specific resin in multi-year greenhouse exposure is limited.
| Regulation or standard | Designation | Application scope | Verification requirement |
|---|---|---|---|
| US FDA food contact | 21 CFR 177.1520(c) | Olefin polymer films and articles intended for food contact | End-use migration testing under the applicable FDA condition-of-use time/temperature class |
| European Union food contact | Regulation (EU) No 10/2011 | Plastic materials and articles in contact with food | Overall migration limit of 10 mg/dm²; specific migration limits for additives must be verified per food simulant |
| US film tensile properties | ASTM D882 | Thin film tensile strength and elongation | 1 in/min or 500 mm/min crosshead speed per specified method |
| US dart impact | ASTM D1709 | Free-falling dart impact resistance of plastic film | Phenolic dart geometry A or B; report failure weight |
| Heat seal and hot tack | ASTM F1921 / ASTM F88 | Seal strength and hot-tack of flexible packaging | Seal-bar pressure, dwell, and peel speed must be specified |
Post-consumer LLDPE recyclate with measured density drift to 0.850–0.950 g/cm³ and melt-flow indices between 0.3 g/10 min and 1.5 g/10 min is blended with the resin at 30–50 wt% on twin-screw extruders with 40:1 L/D to reduce melt-pressure fluctuation. Without the virgin linear component, extruder head pressure often oscillates above ±2.0 bar and film thickness variation exceeds ±5% at haul-off speeds above 100 m/min. The resin contributes a controlled 0.70 g/10 min melt flow index and narrows the molecular weight distribution sufficiently for blown film bubble stability at 2.0:1–2.5:1 blow-up ratios. In non-food heavy-duty liners, the recyclate blend is processed at 180–220 °C with screen packs of 80–120 mesh to remove metal and high-molecular-weight gel contaminants; gel counts above 5 per 10 cm² result in dart impact failure below 85 g at 100 µm per ASTM D1709. Because the resin does not contain a processing antioxidant package built for long-term recyclate thermal exposure, additional phosphite stabilizers are required when the blend is reprocessed more than two cycles; published data for DNDA-7144 NT 7 in multiple closed-loop recycling passes is limited.
Competitive Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin is a pelletised injection moulding grade of the LLDPE family. The nominal melt index is 20 g/10 min under ASTM D1238 conditions of 190 °C and 2.16 kg. The nominal density is 0.924 g/cm³ under ASTM D792. The resin is produced by Ziegler-Natta catalysis and is normally assigned to the butene comonomer class; the backbone is linear, with short-chain branching that differentiates it from high-pressure LDPE. The grade is supplied as natural-stabilised pellets and is used primarily for high-speed injection moulding of thin-wall articles such as caps, closures, overcaps, housewares, cosmetic packaging, and containers. The high melt index lowers injection pressure and shortens cycle time in multi-cavity tools, but it also reduces melt strength relative to extrusion-grade LLDPE; blown film, pipe, and extrusion blow moulding are not recommended processing routes.
Table 1 restates the nominal property profile published in supplier technical literature. The values are typical rather than specification limits and are affected by colour masterbatch, regrind, and moulding conditions.
| Property | Test method | Nominal value |
|---|---|---|
| Melt index | ASTM D1238 (190 °C/2.16 kg) | 20 g/10 min |
| Density | ASTM D792 | 0.924 g/cm³ |
| Tensile strength at yield | ASTM D638 | 9.3 MPa |
| Ultimate tensile elongation | ASTM D638 | 900% |
| Flexural modulus, 1% secant | ASTM D790 | 220 MPa |
| Notched Izod impact, 23 °C | ASTM D256 | No break |
| Vicat softening point | ASTM D1525 | 85 °C |
The shear viscosity at 190 °C and 1000 s⁻¹ is low enough to permit filling of 0.3 mm flow sections in short flow paths, but published data for this specific configuration is limited. Moulders should use cavity pressure transducers and verify short-shot progression through stage-wise filling studies rather than relying on melt-index alone.
Injection moulding trials on accumulator-assisted machines with general-purpose screws of 18:1 to 22:1 L/D ratio produce stable melt feed when the melt temperature is maintained between 180 °C and 220 °C. Barrel zones are commonly set flat or with a rear zone 10–15 °C lower than the front zone to avoid bridging in the feed throat. The low melt viscosity associated with 20 g/10 min melt index reduces hydraulic pressure demand, but the narrow molecular weight distribution of the resin also means that shear heating is less effective than with broad-MWD high-pressure LDPE. Back pressure is held at 0.5–1.5 MPa; higher back pressure at screw speeds above 150 min⁻¹ can raise melt temperature beyond 240 °C, causing oxidative degradation that appears as yellowing and acrid odour in the purged melt. The recommended mould temperature for dimensional consistency is 10–50 °C. At wall thicknesses below 0.5 mm, injection velocities above 100 mm/s are often required to prevent premature freeze-off; published data for this specific configuration is limited, but shear heating in hot and cold runner gates can generate local melt temperatures above 240 °C when runner diameters are below 2.5 mm. Residence time at full melt temperature should not exceed 6 min; during interruptions, the barrel is purged and the screw is pulled back.
On cold-runner multi-cavity cap tooling, the combination of 0.924 g/cm³ density and 20 g/10 min melt index produces low residual stress but also moderate mould shrinkage. Dimensional change measured after 48 h on unfilled plaques is governed by ASTM D955 shrinkage data; typical mould shrinkage is in the range 0.015–0.025 mm/mm, with the higher end observed in thick sections. Because the material is a butene-based LLDPE, it provides higher flexural modulus and tensile yield than a high-pressure LDPE at the same melt index, but lower rigidity than an injection-grade HDPE. For closures, the choice between DNDA-7144 NT 7 and an HDPE grade is usually determined by top-load force, hinge-strip stress cracking, and warp. The LLDPE grade often shows lower warpage in flat thin-wall lids because its density and crystallinity are below those of HDPE, but the top-load resistance is correspondingly lower. In living-hinge designs, the hinge is a controlled flow-front weld line; prototypes should be evaluated under ASTM D638 for tensile yield and under ASTM D256 for notched impact rather than assuming polypropylene-like hinge endurance.
Depending on tool design and wall thickness, replacement of a high-pressure LDPE resin with DNDA-7144 NT 7 shifts the solid-state stiffness upward while reducing long-chain branching and melt strength. A high-pressure LDPE injection grade at 0.920 g/cm³ density may have a flexural modulus around 180 MPa, whereas the LLDPE grade at 0.924 g/cm³ has a nominal flexural modulus of 220 MPa. This increase improves container wall rigidity and shortens cycle time through earlier ejection, but the linear architecture lowers melt strength. Blown film and extrusion blow moulding are not viable processing routes because bubble stability and parison sag under high melt index and low long-chain branching. Compared with an injection-grade HDPE of 0.952 g/cm³ density and similar melt index, DNDA-7144 NT 7 exhibits lower flexural modulus and lower Vicat softening point, but its environmental stress crack resistance under ASTM D1693 is typically higher at equivalent melt index. The environmental stress crack resistance comparison is sensitive to moulded-in stress and stress-cracking agent; published data for this specific configuration is limited. In cap applications, the LLDPE grade may be selected for improved stress cracking at the cost of top-load capacity.
Polymers in the DNDA series are supplied with a standard phenolic antioxidant package and acid scavenger. The resin should not be dry-blended with amine-based antistatic additives or certain amine-containing colour masterbatches, because amine interactions with the stabiliser package can produce plate-out and yellowing at processing temperatures above 220 °C. If a non-amine antistatic additive is required, the carrier resin should have a melt index within 5–20 g/10 min to limit viscosity mismatch and splay. Inventory is stored in a closed, dry location below 50 °C. Polyethylene does not hydrolytically degrade, but surface moisture from condensation at relative humidity above 60% causes splay and internal voids. Pre-drying at 60–80 °C for 1–2 h is recommended when pellet temperature is below dew point. Do not exceed 260 °C melt temperature even for colour changes, because oxidative degradation increases and produces gel particles in the melt stream. Purging with polypropylene or a commercial purging compound is performed at the lowest recommended melt temperature, with screw rotation at 30–60 min⁻¹.
The natural grade is often cited in supplier documentation as compliant with FDA 21 CFR 177.1520 for olefin polymers and with (EU) No 10/2011 when the material is used under conditions defined by the supplier. Compliance is limited to the unmodified, unpigmented base resin; colour concentrates, regrind, and processing aids must be independently assessed. For industrial packaging, regrind addition up to 30 wt% has been practised on returnable container lines, but melt index drift and colour shift must be monitored every 2 h when post-consumer content is introduced. The grade has no intentional slip or antiblock package; if closures require torque reduction or mould release modification, external additives must be evaluated for compliance with FDA 21 CFR 177.1520 and (EU) No 10/2011.
| Framework | Designation | Condition |
|---|---|---|
| US FDA food contact | 21 CFR 177.1520 | Unmodified natural resin, end-use conditions per supplier |
| EU food contact | (EU) No 10/2011 | Supplier declaration required for migration limits |
| REACH | 1907/2006 | SDS SVHC and registration status per supplier |
| RoHS | 2011/65/EU | Heavy metal restrictions for EEE applications |